JPS5390138A - Soldering alloy for al and al alloy - Google Patents
Soldering alloy for al and al alloyInfo
- Publication number
- JPS5390138A JPS5390138A JP444077A JP444077A JPS5390138A JP S5390138 A JPS5390138 A JP S5390138A JP 444077 A JP444077 A JP 444077A JP 444077 A JP444077 A JP 444077A JP S5390138 A JPS5390138 A JP S5390138A
- Authority
- JP
- Japan
- Prior art keywords
- alloy
- soldering
- soldering alloy
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP444077A JPS5390138A (en) | 1977-01-20 | 1977-01-20 | Soldering alloy for al and al alloy |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP444077A JPS5390138A (en) | 1977-01-20 | 1977-01-20 | Soldering alloy for al and al alloy |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS5390138A true JPS5390138A (en) | 1978-08-08 |
Family
ID=11584268
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP444077A Pending JPS5390138A (en) | 1977-01-20 | 1977-01-20 | Soldering alloy for al and al alloy |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5390138A (en) |
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6182994A (en) * | 1984-09-28 | 1986-04-26 | Nippon Handa Kogyo Kk | Solder alloy with excellent fatigue resistance |
CN103273218A (en) * | 2013-06-17 | 2013-09-04 | 东莞市宝拓来金属有限公司 | Solder materials used in automotive glass heating coating tape and its application |
-
1977
- 1977-01-20 JP JP444077A patent/JPS5390138A/en active Pending
Cited By (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6182994A (en) * | 1984-09-28 | 1986-04-26 | Nippon Handa Kogyo Kk | Solder alloy with excellent fatigue resistance |
CN103273218A (en) * | 2013-06-17 | 2013-09-04 | 东莞市宝拓来金属有限公司 | Solder materials used in automotive glass heating coating tape and its application |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB2004489B (en) | Brazing alloy | |
JPS5429816A (en) | Zirconiummtitanium alloy containing transition metal elements | |
JPS5641344A (en) | Titaniummaluminum alloy | |
JPS5620138A (en) | Titaniummaluminium alloy | |
JPS5481146A (en) | Solder flux | |
JPS5693845A (en) | Three component alloy | |
JPS52126659A (en) | Brazing alloy | |
GB1556626A (en) | Alloy steel | |
JPS53117627A (en) | Dental alloy | |
JPS5496422A (en) | Copper based alloy | |
JPS5499731A (en) | Casting alloy | |
JPS5447817A (en) | High permeability alloy | |
JPS5439052A (en) | Bissphosphine metal complex | |
JPS53119721A (en) | Abrassionnresistant high permeability alloy | |
JPS53137817A (en) | Heattresistant cast alloy | |
JPS55134157A (en) | Ironnnickel alloy | |
AU512691B2 (en) | Ag-sno alloy | |
JPS5399031A (en) | Dental alloy | |
JPS5390138A (en) | Soldering alloy for al and al alloy | |
JPS5461050A (en) | Metal brazing alloy | |
JPS5434057A (en) | Silverrbase metal based alloy contact | |
JPS53117658A (en) | Welding alloy | |
JPS5669343A (en) | Cobalttchromium alloy | |
JPS5490013A (en) | Ironnnickel alloy | |
GB2003178B (en) | Cupro-nickel alloys |