JPS48101331A - - Google Patents
Info
- Publication number
- JPS48101331A JPS48101331A JP3366772A JP3366772A JPS48101331A JP S48101331 A JPS48101331 A JP S48101331A JP 3366772 A JP3366772 A JP 3366772A JP 3366772 A JP3366772 A JP 3366772A JP S48101331 A JPS48101331 A JP S48101331A
- Authority
- JP
- Japan
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electrochemical Coating By Surface Reaction (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3366772A JPS5245650B2 (xx) | 1972-04-03 | 1972-04-03 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3366772A JPS5245650B2 (xx) | 1972-04-03 | 1972-04-03 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS48101331A true JPS48101331A (xx) | 1973-12-20 |
JPS5245650B2 JPS5245650B2 (xx) | 1977-11-17 |
Family
ID=12392795
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3366772A Expired JPS5245650B2 (xx) | 1972-04-03 | 1972-04-03 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5245650B2 (xx) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50131825A (xx) * | 1974-03-20 | 1975-10-18 | ||
JPS54110946A (en) * | 1978-02-20 | 1979-08-30 | Osaka Denki Co Ltd | Welding line contouring device |
US5064512A (en) * | 1988-07-19 | 1991-11-12 | Henkel Kommanditgesellschaft Auf Aktien | Process for dyeing anodized aluminum |
US5409592A (en) * | 1990-10-29 | 1995-04-25 | Henkel Kommanditgesellschaft Auf Aktien | Electrolyte additive for a colorant bath for coloring aluminum and process for coloring aluminum |
-
1972
- 1972-04-03 JP JP3366772A patent/JPS5245650B2/ja not_active Expired
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS50131825A (xx) * | 1974-03-20 | 1975-10-18 | ||
JPS54110946A (en) * | 1978-02-20 | 1979-08-30 | Osaka Denki Co Ltd | Welding line contouring device |
JPS5639985B2 (xx) * | 1978-02-20 | 1981-09-17 | ||
US5064512A (en) * | 1988-07-19 | 1991-11-12 | Henkel Kommanditgesellschaft Auf Aktien | Process for dyeing anodized aluminum |
US5409592A (en) * | 1990-10-29 | 1995-04-25 | Henkel Kommanditgesellschaft Auf Aktien | Electrolyte additive for a colorant bath for coloring aluminum and process for coloring aluminum |
Also Published As
Publication number | Publication date |
---|---|
JPS5245650B2 (xx) | 1977-11-17 |