[go: up one dir, main page]

JPH11224049A - Label forming base material - Google Patents

Label forming base material

Info

Publication number
JPH11224049A
JPH11224049A JP3809198A JP3809198A JPH11224049A JP H11224049 A JPH11224049 A JP H11224049A JP 3809198 A JP3809198 A JP 3809198A JP 3809198 A JP3809198 A JP 3809198A JP H11224049 A JPH11224049 A JP H11224049A
Authority
JP
Japan
Prior art keywords
label
tack
labels
base material
shrink
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP3809198A
Other languages
Japanese (ja)
Other versions
JP3992350B2 (en
Inventor
Yoshihiro Shiomi
祐宏 塩見
Takuji Kashiwa
拓二 栢
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fuji Seal Inc
Original Assignee
Fuji Seal Inc
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fuji Seal Inc filed Critical Fuji Seal Inc
Priority to JP03809198A priority Critical patent/JP3992350B2/en
Publication of JPH11224049A publication Critical patent/JPH11224049A/en
Application granted granted Critical
Publication of JP3992350B2 publication Critical patent/JP3992350B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PROBLEM TO BE SOLVED: To provide the label forming base material which forms no partially strained selling while rolled even if a tack label is stuck in advance. SOLUTION: As for the long belt-like label forming base material 1 formed by successively connecting cylindrical shrink labels 10 to be mounted on the bodies of PET bottles in such a state that they are folded in sheets, tack labels 20 as application seals for a gift campaign are stuck on shrink labels 10. The tack labels 20 are so stuck on blank spaces as to avoid the display parts of the design, characters, bar code, etc., given on the shrink labels 10 and the sticking positions of the labels 20 are alternately shifted so that the tack labels 20 stuck on the adjacent shrink labels 10 are dispersed in the width direction of the label forming base material 1.

Description

【発明の詳細な説明】DETAILED DESCRIPTION OF THE INVENTION

【0001】[0001]

【発明の属する技術分野】この発明は、PETボトル等
の容器に装着される筒状のシュリンクラベル等がシート
状に折り畳まれた状態で連続的に繋がった長尺帯状のラ
ベル形成基材に関する。
BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a long strip-shaped label-forming base material in which a cylindrical shrink label or the like mounted on a container such as a PET bottle is continuously connected in a state of being folded into a sheet.

【0002】[0002]

【従来の技術】近年、缶コーヒー等の缶飲料には、タッ
クラベルによって形成される応募シールが貼着されてお
り、缶飲料の購入者が缶から剥がした応募シールを葉書
に貼って応募することで、種々の景品が当たるといった
キャンペーンが頻繁に行われるようになっている。
2. Description of the Related Art In recent years, canned beverages such as canned coffee have been provided with an application sticker formed by a tack label, and a purchaser of a canned beverage applies an application sticker peeled off from a can on a postcard. As a result, campaigns in which various prizes are won are frequently performed.

【0003】ところで、こういった缶飲料の景品キャン
ペーンを、飲料がポリエチレンテレフタレート製ボトル
(PETボトル)等のボトル容器に充填されたボトル飲
料に適用する場合、ボトル自体に直接応募シール等のタ
ックラベルを貼着すると、使用済みのボトルをリサイク
ルする際に、応募されずにそのボトルに残ったタックラ
ベルを1枚ずつ剥がすといった非常に手間のかかる作業
を行わなければならず、効率的にリサイクルを行うこと
ができないという問題がある。
By the way, when such a canned beverage premium campaign is applied to a bottled beverage in which the beverage is filled in a bottle container such as a polyethylene terephthalate bottle (PET bottle), a tack label such as an application seal is directly applied to the bottle itself. When you recycle used bottles, you have to perform very laborious work, such as peeling off the tack labels left on the bottle without being applied, one by one. There is a problem that can not be done.

【0004】このため、応募シール等のタックラベル
は、ボトル自体に直接貼着するのではなく、ボトルに装
着されていても切断することにより簡単に外せるシュリ
ンクラベルに貼着しておくことが望まれており、従来は
シュリンクラベルをボトルに装着した後、そのシュリン
クラベルに応募シールであるタックラベルを貼着してい
た。
[0004] For this reason, it is desirable that a tack label such as an application sticker is not stuck directly to the bottle itself, but is stuck to a shrink label that can be easily removed by cutting even if it is attached to the bottle. Conventionally, after attaching a shrink label to a bottle, a tack label, which is an application seal, is attached to the shrink label.

【0005】[0005]

【発明が解決しようとする課題】しかし、ボトル飲料の
製造ライン上では、ボトルの位置決めが行われておら
ず、各ボトルの向きが統一されていないのが一般的であ
るため、上述したように、シュリンクラベルがボトルに
装着された状態でタックラベルを貼着しようとすると、
シュリンクラベルの決められた位置にタックラベルを確
実に貼着することが難しく、貼着されたタックラベルに
よって、シュリンクラベルに施されたデザイン、文字、
バーコード等の表示が隠蔽されてしまうおそれがあっ
た。
However, bottles are generally not positioned on a bottled beverage production line, and the orientation of each bottle is not unified. If you try to attach a tack label while the shrink label is attached to the bottle,
It is difficult to securely attach the tack label to the determined position of the shrink label, and the attached tack label allows the design, characters,
There is a possibility that a display such as a barcode may be hidden.

【0006】こういった問題を解決するために、シュリ
ンクラベルをボトルに装着する前に、シュリンクラベル
に施された表示に影響を与えない所定位置に予め応募シ
ール等のタックラベルを貼着しておくことが考えられ
る。
In order to solve such a problem, before attaching the shrink label to the bottle, a tack label such as an application sticker is attached to a predetermined position which does not affect the display on the shrink label. It is possible to put.

【0007】ところで、この種のシュリンクラベルは、
多数のシュリンクラベルがシート状に折り畳まれた状態
で連続的に繋がった長尺帯状のラベル形成基材を順次切
断することで、シュリンクラベルを形成しながらこれを
ボトルに装着するのが一般的であり、上述した長尺帯状
のラベル形成基材は、通常ロール状に巻回した状態で保
管され、搬送され、使用される。
By the way, this kind of shrink label is
It is common to cut a long strip-shaped label forming base material that is continuously connected in a state where many shrink labels are folded in a sheet shape, and then attach this to a bottle while forming a shrink label. In addition, the above-described long band-shaped label-forming base material is usually stored, transported, and used in a state wound in a roll shape.

【0008】従って、タックラベルが各シュリンクラベ
ルの決められた所定位置に予め貼着されたラベル形成基
材をロール状に巻回すると、タックラベルが貼着された
部分だけが歪に盛り上がった状態となり、シュリンクラ
ベルにしわが寄ったり、巻回したロールが崩れたりする
等、保管、搬送、使用のそれぞれにおける取り扱いに支
障が生じるといった問題がある。
Accordingly, when the label forming base material in which the tack label is preliminarily adhered to the predetermined position of each shrink label is wound in a roll, only the portion where the tack label is adhered is distorted. Therefore, there is a problem that handling in storage, transportation, and use is hindered, such as wrinkling of the shrink label and collapse of the wound roll.

【0009】そこで、この発明の課題は、予めタックラ
ベルを貼着しておいても、ロール状に巻回した状態にお
いて部分的に歪な盛り上がりが生じないラベル形成基材
を提供することにある。
SUMMARY OF THE INVENTION It is an object of the present invention to provide a label-forming base material in which even when a tack label is attached in advance, a partially distorted swelling does not occur in a state wound in a roll. .

【0010】[0010]

【課題を解決するための手段】上記の課題を解決するた
め、この発明は、容器に装着される筒状のシュリンクラ
ベルまたはストレッチラベルがシート状に折り畳まれた
状態で連続的に繋がった長尺帯状のラベル形成基材にお
いて、その全長にわたって、その幅方向に分散されるよ
うに位置をずらしながら、前記シュリンクラベルまたは
ストレッチラベル毎にタックラベルを貼着したものであ
る。
SUMMARY OF THE INVENTION In order to solve the above-mentioned problems, the present invention relates to a long continuous sheet in which a cylindrical shrink label or stretch label attached to a container is folded in a sheet shape and is continuously connected. In a strip-shaped label-forming base material, a tack label is attached to each of the shrink labels or the stretch labels while shifting the position so as to be dispersed in the width direction over the entire length.

【0011】以上のように構成されたラベル形成基材
は、その幅方向の一部分にだけタックラベルが貼着され
ているのではなく、その幅方向に分散してタックラベル
が貼着されているので、このラベル形成基材をロール状
に巻回した状態では、幅方向の一部分にだけ盛り上がり
が生じることがなく、幅方向の全域にわたってほぼ均一
に盛り上がる。
In the label-forming base material configured as described above, the tack label is not adhered to only a part of the width direction, but the tack label is attached in a dispersed manner in the width direction. Therefore, in a state where the label-forming base material is wound in a roll shape, swelling does not occur only in a part of the width direction, and swells almost uniformly over the entire area in the width direction.

【0012】[0012]

【発明の実施の形態】以下、実施の形態について図面を
参照して説明する。図1に示すように、このラベル形成
基材1は、ペットボトルの胴部に装着される筒状のシュ
リンクラベル10がシート状に折り畳まれた状態で連続
的に繋がった長尺帯状のものであり、同図に二点鎖線で
示す位置で順次切断することで個別のシュリンクラベル
10が形成されるようになっている。
Embodiments will be described below with reference to the drawings. As shown in FIG. 1, the label-forming base material 1 is a long strip-shaped one in which a cylindrical shrink label 10 attached to the body of a PET bottle is continuously connected in a state of being folded into a sheet. In addition, individual shrink labels 10 are formed by sequentially cutting at the positions indicated by the two-dot chain lines in FIG.

【0013】前記ラベル形成基材1は、ポリエステル、
スチレン・ブタジエン共重合体、ポリ塩化ビニル等の厚
さ20〜80μmの熱収縮性フィルムによって形成され
ており、繋がった各シュリンクラベル10毎に、景品キ
ャンペーン用の応募シールとなるタックラベル20がそ
れぞれ貼着されている。
The label-forming substrate 1 is made of polyester,
It is formed of a heat-shrinkable film having a thickness of 20 to 80 μm, such as a styrene-butadiene copolymer or polyvinyl chloride, and a tack label 20 serving as an application seal for a prize campaign is provided for each connected shrink label 10. It is stuck.

【0014】前記タックラベル20は、紙、合成紙、合
成樹脂製フィルム等よりなる基材の裏面に、剥離後葉書
等に再接着可能な粘着剤が塗布されたものであり、シュ
リンクラベル10に施されたデザイン、文字及びバーコ
ード等の表示部分を避けるように空きスペースに貼着さ
れていると共に、同図に示すように、隣接するシュリン
クラベル10に貼着されたタックラベル20が、ラベル
形成基材1の幅方向に分散されるように、その貼着位置
を交互にずらしてある。
The tack label 20 is formed by applying an adhesive which can be re-adhered to a postcard or the like after peeling, on the back surface of a substrate made of paper, synthetic paper, synthetic resin film or the like. As shown in the figure, the tack label 20 attached to the adjacent shrink label 10 is attached to the empty space so as to avoid the displayed portion of the design, the character, the bar code, and the like. The sticking positions are alternately shifted so as to be dispersed in the width direction of the forming base material 1.

【0015】従って、図1に示すように、このラベル形
成基材1をロール状に巻回しても、その外周面の幅方向
の一部分だけが歪に盛り上がることがなく、概ねフラッ
トな外周面を有する巻回体となるので、巻回することに
よってラベル形成基材1にしわが寄ったり、巻回したロ
ールが崩れたりすることがなく、保管、搬送、使用のそ
れぞれにおいて、良好な取扱性が確保される。
Therefore, as shown in FIG. 1, even when this label-forming substrate 1 is wound into a roll, only a part of the outer peripheral surface in the width direction does not rise due to distortion, and a substantially flat outer peripheral surface is formed. Since it becomes a wound body having no wrinkles, the label forming base material 1 is not wrinkled by the winding, and the wound roll does not collapse, and good handling properties are secured in each of storage, transport, and use. Is done.

【0016】なお、タックラベル20の貼着位置は、上
述したように、交互にずらさなければならないというこ
とはなく、図2に示すように、隣接する2枚のシュリン
クラベル10毎に、または3枚以上のシュリンクラベル
10毎にその貼着位置をずらすようにしてもよい。
The sticking positions of the tack labels 20 do not have to be alternately shifted as described above, and as shown in FIG. 2, every two adjacent shrink labels 10 or 3 The sticking position may be shifted for every shrink label 10 or more.

【0017】また、タックラベル20の貼着位置は、上
述したように、折り畳まれたシュリンクラベル10の片
面側だけでずらしてもよいが、図3に示すように、シュ
リンクラベル10の両面側にわたってずらすことも可能
であり、タックラベル20の貼着箇所も上述した2ヶ所
に限定されるものではなく、例えば、ラベル形成基材1
の幅方向の両端部及び中央部の3ヶ所、あるいは4ヶ所
以上に設定することも可能である。但し、シュリンクラ
ベルは、容器に嵌挿するときにその幅方向の中央部を吸
着して筒状に開口されることが多いため、タックラベル
20の貼着位置を、中央部を除く幅方向の2ヶ所に設定
しておくことが望ましい。
The sticking position of the tack label 20 may be shifted only on one side of the folded shrink label 10 as described above. However, as shown in FIG. It is also possible to shift, and the sticking position of the tack label 20 is not limited to the two places described above.
It is also possible to set three or four or more at both ends and the center in the width direction. However, when the shrink label is inserted into the container, the central portion in the width direction is often sucked and opened in a cylindrical shape. Therefore, the sticking position of the tack label 20 is changed in the width direction excluding the central portion. It is desirable to set two places.

【0018】また、このラベル形成基材1は、上述した
ように、筒状のシュリンクラベル10がシート状に折り
畳まれた状態で連続的に繋がったものであるため、折り
目部分となる幅方向の両端部は中央部分より若干厚くな
るため、幅方向の両端部から少なくとも5〜10mm程
度の間隔をあけてタックラベル20を貼着することが望
ましい。
Further, as described above, the label-forming base material 1 is formed by continuously connecting the tubular shrink labels 10 in a state of being folded into a sheet shape. Since both end portions are slightly thicker than the central portion, it is desirable to attach the tack label 20 with an interval of at least about 5 to 10 mm from both end portions in the width direction.

【0019】また、タックラベル20が非収縮性である
場合は、ボトルに装着したシュリンクラベル10の2次
曲面となる部分に貼着することが望ましく、どうしても
シュリンクラベル10の3次曲面となる部分に貼着しな
ければならない場合は、貼着するタックラベル20にも
熱収縮性能を付与しておくことが望ましい。
In the case where the tack label 20 is non-shrinkable, it is desirable that the tack label 20 be adhered to a portion of the shrink label 10 attached to the bottle, which is a secondary curved surface. When it is necessary to adhere to the tack label, it is desirable that the tack label 20 to be adhered also be given heat shrinkability.

【0020】また、上述した実施形態では、タックラベ
ル20をシュリンクラベル10の外表面に貼着している
が、これに限定されるものではなく、例えば、筒状のシ
ュリンクラベル10の内面にタックラベル20を貼着し
ておいてもよい。このように、タックラベル20をシュ
リンクラベル10の内面に貼着することにより、ボトル
飲料を購入せずに応募シールだけを剥がすといった不正
行為を未然に防止することができる。但し、シュリンク
ラベル10の内面にタックラベル20を貼着する場合
は、シュリンクラベル10を筒状に形成する前に予めタ
ックラベル20を貼着しておく必要があると共に、ボト
ル飲料を購入した人がタックラベル20を簡単に剥がす
ことができるように、シュリンクラベル10にミシン目
等の破断手段を形成しておく必要がある。
In the above-described embodiment, the tack label 20 is attached to the outer surface of the shrink label 10, but the present invention is not limited to this. For example, the tack label may be attached to the inner surface of the cylindrical shrink label 10. The label 20 may be pasted. In this way, by attaching the tack label 20 to the inner surface of the shrink label 10, it is possible to prevent improper acts such as peeling off only the application seal without purchasing a bottled beverage. However, when sticking the tack label 20 on the inner surface of the shrink label 10, it is necessary to stick the tack label 20 in advance before forming the shrink label 10 into a tubular shape, and to purchase the bottled beverage. However, it is necessary to form breakage means such as perforations on the shrink label 10 so that the tack label 20 can be easily peeled off.

【0021】なお、上述した実施形態では、熱収縮によ
って容器に装着する筒状のシュリンクラベルの場合につ
いて説明したが、本発明は、弾性伸縮によって容器に装
着する筒状のストレッチラベルについても適用すること
ができる。
In the above-described embodiment, the case of a cylindrical shrink label attached to a container by heat shrinkage has been described. However, the present invention is also applied to a cylindrical stretch label attached to a container by elastic expansion and contraction. be able to.

【0022】[0022]

【発明の効果】以上のように、この発明のラベル形成基
材は、予め貼着しておくタックラベルを、幅方向に分散
させながらシュリンクラベルまたはストレッチラベル毎
に配置するようにしたため、ロール状に巻回した状態で
も、その幅方向の一部分だけが歪に盛り上がることがな
く、保管、搬送、使用のいずれにおいても良好な取扱性
が確保される。
As described above, the label-forming base material of the present invention is arranged such that the tack labels to be adhered in advance are arranged for each shrink label or stretch label while being dispersed in the width direction. Even in a wound state, only a part in the width direction does not rise due to distortion, and good handling properties are secured in any of storage, transport, and use.

【図面の簡単な説明】[Brief description of the drawings]

【図1】この発明にかかるラベル形成基材の一実施形態
を示す斜視図である。
FIG. 1 is a perspective view showing one embodiment of a label-forming base material according to the present invention.

【図2】タックラベルの貼着位置のずらし方の別の態様
を示す平面図である。
FIG. 2 is a plan view showing another mode of shifting a tack label attaching position.

【図3】タックラベルの貼着位置のずらし方の別の態様
を示す平面図である。
FIG. 3 is a plan view showing another mode of shifting a tack label attaching position.

【符号の説明】[Explanation of symbols]

1 ラベル形成基材 10 シュリンクラベル 20 タックラベル DESCRIPTION OF SYMBOLS 1 Label forming base material 10 Shrink label 20 Tack label

Claims (1)

【特許請求の範囲】[Claims] 【請求項1】 容器に装着される筒状のシュリンクラベ
ルまたはストレッチラベルがシート状に折り畳まれた状
態で連続的に繋がった長尺帯状のラベル形成基材におい
て、 その全長にわたって、幅方向に分散されるように位置を
ずらしながら、前記シュリンクラベルまたはストレッチ
ラベル毎にタックラベルを貼着したことを特徴とするラ
ベル形成基材。
1. A long band label forming base material in which a tubular shrink label or a stretch label attached to a container is continuously connected in a state of being folded into a sheet shape, and is distributed in the width direction over the entire length. A label forming base material, wherein a tack label is attached to each of the shrink labels or the stretch labels while shifting the positions so as to be performed.
JP03809198A 1998-02-04 1998-02-04 Label forming substrate Expired - Lifetime JP3992350B2 (en)