[go: up one dir, main page]

JPH02297693A - Magnetic substance bar code - Google Patents

Magnetic substance bar code

Info

Publication number
JPH02297693A
JPH02297693A JP1118233A JP11823389A JPH02297693A JP H02297693 A JPH02297693 A JP H02297693A JP 1118233 A JP1118233 A JP 1118233A JP 11823389 A JP11823389 A JP 11823389A JP H02297693 A JPH02297693 A JP H02297693A
Authority
JP
Japan
Prior art keywords
magnetic
bar code
magnetic substance
substance powder
barcode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP1118233A
Other languages
Japanese (ja)
Other versions
JPH0823881B2 (en
Inventor
Hirotaka Okabe
岡部 弘高
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NEC Corp
Original Assignee
NEC Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NEC Corp filed Critical NEC Corp
Priority to JP1118233A priority Critical patent/JPH0823881B2/en
Publication of JPH02297693A publication Critical patent/JPH02297693A/en
Publication of JPH0823881B2 publication Critical patent/JPH0823881B2/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

PURPOSE:To obtain the bar code of satisfactory durability at low cost by providing recessed rectangular patterns, in which magnetic substance powder is respectively embedded, in arrangement with intervals and width, which are determined in advance, on the plate surface of a non-magnetic resin plate. CONSTITUTION:On the plate surface of a non-magnetic resin plate 1, as the female mold of the bar code, plural rectangular patterns 2 are provided in the recessed shapes in the arrangement with the intervals and width which are determined in advance. Next, magnetic substance powder 3 is embedded in the recessed parts of the rectangular patterns 2 and liquid-state adhesive agent is immersed. Then, the magnetic substance powder 3 is fixed in the recessed parts of the patterns. Since permeability can be freely adjusted for the magnetic substance powder 3 by mixing various magnetic substances, the permeability can be set to an optimum value in correspondence to a magnetic sensor used for reading. Thus, the bar code of the satisfactory durability can be formed at low cost.

Description

【発明の詳細な説明】 〔産業上の利用分野〕 本発明は磁性体を用いたバーコードに関するものである
DETAILED DESCRIPTION OF THE INVENTION [Field of Industrial Application] The present invention relates to a barcode using a magnetic material.

〔従来の技術〕[Conventional technology]

近年、物流管理のOA化、FA化にコンピュータが広く
導入されており1例えば大規模小売店舗における商品の
販売管理や製造工程における部品や製品の生産管理に広
く使われている。その入力用端末機器として印刷バーコ
ードを光学的に読み取る装置が多く利用され、商品や部
品には印刷された帯状パターン(光学式バーコード)が
付加されている。この光学式バーコードは、比較的離れ
た距離から読取りができる利点を持つが、欠点として読
取り而りの汚れ(例えば付着したゴミ)に弱く、耐久性
にも劣る。特に、汚染の危険性の高い製造工程等では従
来の光学式バーコードを使うことができなかった。
In recent years, computers have been widely introduced for OA and FA in logistics management, and are widely used, for example, for managing product sales in large-scale retail stores and for managing the production of parts and products in manufacturing processes. Devices that optically read printed barcodes are often used as input terminal devices, and printed strip patterns (optical barcodes) are added to products and parts. This optical barcode has the advantage that it can be read from a relatively long distance, but has the disadvantage that it is susceptible to dirt (for example, attached dust) during reading and is inferior in durability. In particular, conventional optical barcodes cannot be used in manufacturing processes where there is a high risk of contamination.

一方、近年汚れに強いバーコードとして、金属板上に凹
状又は凸状に刻印された複数の矩形パターンを有する刻
印バーコードが知られている(昭和62年日本応用磁気
学会学術講演概要集p、307)。
On the other hand, in recent years, an engraved barcode that has a plurality of rectangular patterns engraved in concave or convex shapes on a metal plate has become known as a stain-resistant barcode (1988 Japanese Society of Applied Magnetics, Academic Lecture Abstracts, p. 307).

この刻印バーコードの構成を第3図(a)、(b)に示
す。
The structure of this stamped barcode is shown in FIGS. 3(a) and 3(b).

(a)はqZ而面、(b)は断面図である。図において
、鉄板4のLに、矩形パターン2が刻印されている。
(a) is a qZ plane, and (b) is a cross-sectional view. In the figure, a rectangular pattern 2 is stamped on L of the iron plate 4.

この刻印バーコードは、61気を用いて読み取ること力
S H’f能である。即ち、直流磁界又は交流磁界を鉄
板4に印加すると、鉄板4」;の矩形パターン2によっ
て印加された磁界が歪められる。その歪みは磁気センサ
で検出できるので、磁気センサの出力から鉄板4]二の
パターンを検出できる。即ちバーコードを検出できる。
This engraved barcode can be read using 61 degrees of power. That is, when a DC magnetic field or an AC magnetic field is applied to the iron plate 4, the applied magnetic field is distorted by the rectangular pattern 2 of the iron plate 4''. Since the distortion can be detected by a magnetic sensor, the pattern of the iron plate 4] can be detected from the output of the magnetic sensor. That is, barcodes can be detected.

磁界は汚れの影響を受けないので、刻印バーコードは汚
れに影響されず番こ読取り可能である。また、板上の凹
凸ノ(ターンは光学式バーコードに沈入耐久性に富んで
いる。
Since the magnetic field is not affected by dirt, engraved barcodes can be read without being affected by dirt. In addition, the irregularities (turns) on the board sink into the optical barcode and are highly durable.

〔発明が解決しようとする課題〕[Problem to be solved by the invention]

ところが、刻印バーコードは耐久性に富むが、加工が非
常に難しいという問題点を持っている。
However, although engraved barcodes are highly durable, they have the problem of being extremely difficult to process.

即ち、バーコードは、バーコード全体の幅を数−以内に
抑えるためにバーの最小輻を0.1m〜0.5画と小さ
くする必要がある。しかし、刻印の精度は。
That is, in order to suppress the width of the entire barcode to within a few centimeters, the barcode must have a minimum bar width of 0.1 m to 0.5 strokes. However, the accuracy of the engraving is.

通常の工作機械を用いた場合、加工精度は0.3 m程
度が限界であり、0.5αIの溝幅でも工作に長6s時
間を要するので、刻印バーコード自体が非常に高価なも
のとなり、実用性に乏しくなると0う欠点があった。
When using a normal machine tool, the machining accuracy is limited to about 0.3 m, and even a groove width of 0.5αI takes a long time of 6 seconds, making the engraved barcode itself very expensive. There was a drawback that it became impractical.

本発明の[1的は、このような従来の欠点を除去せしめ
て、容易に工作が可能な磁性体バーコードを提供するこ
とにある。
One object of the present invention is to eliminate such conventional drawbacks and provide a magnetic barcode that can be easily worked.

〔課題を解決するための手段〕[Means to solve the problem]

上記目的を達成するため、本発明の磁性体バーコードに
おいては、非磁性樹脂板の板面に予め定められた間隔と
幅とによる配列でそれぞれ磁性体粉が埋め込まれた凹状
の矩形パターンを有するものである。
In order to achieve the above object, the magnetic barcode of the present invention has a concave rectangular pattern in which magnetic powder is embedded in an array with a predetermined interval and width on the surface of a non-magnetic resin plate. It is something.

〔作用〕[Effect]

本発明の磁性体バーコードでは、金属板の代わりに磁性
体粉と非磁性樹脂とを用いているので]二作が容易であ
る。また、非磁性樹脂部を射出成形によって作成するこ
とで、太線生産も容易である。
In the magnetic barcode of the present invention, magnetic powder and non-magnetic resin are used instead of a metal plate, so it is easy to create two barcodes. Furthermore, by producing the non-magnetic resin portion by injection molding, thick wire production is also easy.

また、磁性体粉は、種々の磁性体を混ぜることによって
、透磁率を自由に調節できるので、読取りに用いる磁気
センサに応じて透磁率を最適値に設定することが+i(
能である。
In addition, the magnetic permeability of magnetic powder can be freely adjusted by mixing various magnetic substances, so it is possible to set the magnetic permeability to an optimal value according to the magnetic sensor used for reading.
It is Noh.

〔実施例〕〔Example〕

次に第1図と第2図を参照して本発明の実施例について
説明する。各々(a)は平面図、(b)は断面図である
。第1図(a)において、非磁性樹脂板1の板面にバー
コードの雌型として、非磁性樹脂板1の板面に予め定め
られた間隔と幅とによる配列で複数の矩形パターン2を
第1図(b)のように凹状に設け1次に、矩形パターン
2の凹部内に磁性体粉3を埋め込むと共に、液体状接着
剤を浸み込ませ。
Next, an embodiment of the present invention will be described with reference to FIGS. 1 and 2. (a) is a plan view, and (b) is a cross-sectional view. In FIG. 1(a), a plurality of rectangular patterns 2 are formed on the surface of the non-magnetic resin plate 1 in an arrangement with predetermined intervals and widths as female barcode patterns. As shown in FIG. 1(b), the rectangular pattern 2 is provided in a concave shape.Firstly, magnetic powder 3 is embedded in the concave portion of the rectangular pattern 2, and liquid adhesive is soaked therein.

磁性体粉3をパターンの凹部内に固定する。磁性体粉3
と液体状接着剤とは、磁性体粉3とバインダを混合した
もので代用することも可能である。
Magnetic powder 3 is fixed within the recesses of the pattern. Magnetic powder 3
The liquid adhesive may be replaced by a mixture of the magnetic powder 3 and a binder.

このようにして作った磁性体バーコードを刻印バーコー
ド読み取り用磁気センサで読み取ったところ、刻印バー
コードと同様に、良好な読取りが可能であった− 第2図は非磁性樹脂板1に形成された矩形パターン2の
凹部内に、磁性体粉3を溶かし込んだ樹脂を流し込むと
共に、同図(b)のように非磁性樹脂板1の板面に磁性
体粉3を一定の膜厚で盛り上げて固めた実施例である。
When the magnetic barcode made in this way was read with a magnetic sensor for reading engraved barcodes, it was possible to read it as well as the engraved barcodes. The resin containing the magnetic powder 3 dissolved therein is poured into the recesses of the rectangular pattern 2, and the magnetic powder 3 is applied to the surface of the non-magnetic resin plate 1 at a constant thickness as shown in FIG. This is an example in which it was raised and solidified.

第2図の実施例においては、非磁性樹脂板1の裏から磁
気センサで矩形パターン2を読み取ることができる。し
かも、非磁性樹脂板1が矩形パターン2の保護膜を兼ね
るという効果もあわせて得られる。第2図の実施例にお
いても、刻印バーコード用磁気センサで良好な読取りが
可能であった。
In the embodiment shown in FIG. 2, the rectangular pattern 2 can be read from the back side of the non-magnetic resin plate 1 with a magnetic sensor. Moreover, the effect that the non-magnetic resin plate 1 also serves as a protective film for the rectangular pattern 2 can also be obtained. In the example shown in FIG. 2 as well, good reading was possible with the magnetic sensor for stamped barcodes.

〔発明の効果〕〔Effect of the invention〕

以−1−のように本発明によれば、塗装などの処理を含
めた汚れの影響を受けず、しかも耐久性に優れたバーコ
ードを容易に、即ち安価に提供することができる効果を
有する。
As described in -1- above, the present invention has the effect of easily providing barcodes that are not affected by stains, including treatments such as painting, and have excellent durability, that is, at low cost. .

【図面の簡単な説明】[Brief explanation of the drawing]

第1図(a)は本発明の第1の実施例を示す平面図、(
b)は断面図、第2図(a)は本発明の第2の実施例を
示す平面図、(b)は断面図、第3図(a)は従来技術
のバーコードの平面図、(b)は断面図である。 1・・非磁性樹脂板    2・・・矩形パターン3・
・・磁性体粉
FIG. 1(a) is a plan view showing a first embodiment of the present invention;
b) is a sectional view, FIG. 2(a) is a plan view showing the second embodiment of the present invention, FIG. 3(b) is a sectional view, and FIG. b) is a sectional view. 1. Non-magnetic resin plate 2. Rectangular pattern 3.
・Magnetic powder

Claims (1)

【特許請求の範囲】[Claims] (1)非磁性樹脂板の板面に予め定められた間隔と幅と
による配列でそれぞれ磁性体粉が埋め込まれた凹状の矩
形パターンを有することを特徴とする磁性体バーコード
(1) A magnetic barcode characterized by having a concave rectangular pattern in which magnetic powder is embedded in an arrangement with a predetermined interval and width on the surface of a non-magnetic resin plate.
JP1118233A 1989-05-11 1989-05-11 Magnetic bar code Expired - Lifetime JPH0823881B2 (en)