JP5436588B2 - 高イオン導電性固体電解質材料及び焼結体、並びに、固体電解質型燃料電池 - Google Patents
高イオン導電性固体電解質材料及び焼結体、並びに、固体電解質型燃料電池 Download PDFInfo
- Publication number
- JP5436588B2 JP5436588B2 JP2012010951A JP2012010951A JP5436588B2 JP 5436588 B2 JP5436588 B2 JP 5436588B2 JP 2012010951 A JP2012010951 A JP 2012010951A JP 2012010951 A JP2012010951 A JP 2012010951A JP 5436588 B2 JP5436588 B2 JP 5436588B2
- Authority
- JP
- Japan
- Prior art keywords
- solid electrolyte
- mol
- scsz
- ion conductive
- fuel cell
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Description
導電率σ(S/cm)=(1/抵抗値R(Ω))×試験片長さL(cm)
/試験片断面積S(cm2)
また、1000℃および800℃の導電率σから、logσ vs 1/Tのアレニウスプロットにより傾きを求め、活性化エネルギーE(kJ/mol)を算出した。その結果を次の表3に示す。また図3はその裏付けデータをグラフに示したものである。
(1)試作した3種類のScSZは、いずれも導電率が8YSZの2倍程度の高い導電率を示した。11ScSZ1Aおよび10Sc1YSZの導電率はほぼ予想された数値であり、良好な焼結体が得られている。10Sc1CeSZの導電率も11ScSZ1Aの導電率(1000℃で約0.26S/cm)よりも約1割程度高い値となった。
Claims (7)
- ジルコニアを主成分とし、これにスカンジア8.5〜15モル%と、セリア1モル%とが配合固溶されると共に、スカンジアとセリアとの合計配合量が9〜15モル%の範囲に調製されていることを特徴とする高イオン導電性固体電解質材料。
- 1400℃〜1500℃の範囲内で焼成されるものであることを特徴とする請求項1に記載の高イオン導電性固体電解質材料。
- 液相法によって調製されていることを特徴とする請求項1または2に記載の高イオン導電性固体電解質材料。
- 請求項1から3のいずれか1項に記載の高イオン導電性固体電解質材料を焼結してなる焼結体。
- 固体電解質の片面に燃料極を有し、反対側面に酸素極を有する単電池セル構造を備えた固体電解質型燃料電池であって、前記固体電解質が、ジルコニアを主成分とし、これにスカンジア8.5〜15モル%と、セリア1モル%とが配合固溶されると共に、スカンジアとセリアとの合計配合量が9〜15モル%の範囲に調製された材料により構成されていることを特徴とする固体電解質型燃料電池。
- 前記固体電解質は、1400℃〜1500℃の範囲内で焼成されていることを特徴とする請求項5に記載の固体電解質型燃料電池。
- 前記固体電解質は、液相法によって調製されていることを特徴とする請求項5または6に記載の固体電解質型燃料電池。