JP3781326B2 - Detection method of furnace wall damage in plasma melting furnace - Google Patents
Detection method of furnace wall damage in plasma melting furnace Download PDFInfo
- Publication number
- JP3781326B2 JP3781326B2 JP17974397A JP17974397A JP3781326B2 JP 3781326 B2 JP3781326 B2 JP 3781326B2 JP 17974397 A JP17974397 A JP 17974397A JP 17974397 A JP17974397 A JP 17974397A JP 3781326 B2 JP3781326 B2 JP 3781326B2
- Authority
- JP
- Japan
- Prior art keywords
- peripheral layer
- furnace
- outer peripheral
- electrode
- molten slag
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
【0001】
【発明の属する技術分野】
本発明は、ごみ(都市ごみ,産業廃棄物等)の焼却残渣である焼却灰や飛灰を溶融処理するプラズマ溶融炉において、その炉壁の耐火壁構造部分の侵食による損傷を検知するための方法に関するものである。
【0002】
【従来の技術】
近年、ごみ焼却炉から排出される焼却残渣たる焼却灰や飛灰(以下「灰」と略称する)の減容化及び無害化を図るため、灰の溶融固化処理法が注目され、現実に実用に供されている。灰は溶融固化することにより、その容積を1/2〜1/3に減らすことができると共に、重金属等の有害物質の溶出防止や溶融スラグの再利用、最終埋立処分場の延命等が可能になるからである。
【0003】
ところで、灰の溶融固化処理方法としては、例えば、アーク溶融炉,プラズマアーク炉,電気抵抗炉等を使用し、電気エネルギーによって灰を溶融固化する方法と、表面溶融炉,旋回溶融炉,コークスベッド炉等を使用し、燃料の燃焼エネルギーによって灰を溶融固化する方法とが実用されている。一般に、ごみ焼却設備に発電設備が併置されている場合には前者の電気エネルギーを用いる方法が採用されており、発電設備が併置されていない場合には後者の燃焼エネルギーを用いる方法が採用されている。
【0004】
図8はごみ焼却処理設備に併置した直流アーク放電黒鉛電極式のプラズマ溶融炉の一例を示したものであるが、このプラズマ溶融炉1には、灰30が灰供給装置2により灰ホッパ3から連続的に供給される。炉1には、−電極として機能する黒鉛製の主電極4を炉頂部から垂下させると共に、+極として機能する炉底電極6を炉底部に配して設けてある。両電極4,6間に直流電源装置8により供給された600〜1000KW(灰1t当たり)の直流電気によってプラズマが発生し、それによって炉1内に供給された灰30は1400〜1600℃に加熱されて、溶融状態のスラグ(以下「溶融スラグ」という)31となる。炉1の始動時には、溶融前の灰30が導電性を有しないため、スタート電極5を炉1内へ挿入してこれを+極となし、主電極4との間でスクラップ鋼材を介して通電し、灰30が溶融するのを待ち、灰30が溶融すると、その溶融スラグ31は導電性を有するため、+極をスタート電極5から炉底電極6へと切り換える。なお、炉1内には、これを還元性雰囲気とするために、窒素ガス供給装置9から窒素ガスが供給される。窒素ガスの炉1内への供給は、中空筒状をなす主電極4及びスタート電極5を通して行なわれる。また、炉底においては、炉底冷却ファン7により、炉底電極6及びその周辺部分が空冷されるようになっている。
【0005】
そして、灰30の溶融が開始されると、灰30に含まれている揮発成分や炭素成分はその一部が酸化した一酸化炭素を含むガス体34となる。このガス体34は、炉1の周壁たる炉壁1aに設けた溶融スラグ流出口10から燃焼室12に排出されて、燃焼室12において燃焼空気ファン13による燃焼用空気の供給により完全燃焼された上、排ガス冷却ファン14からの冷却空気によって冷却され、バグフィルタ15を経て誘引通風機16により煙突17から排出される。なお、バグフィルタ15で捕捉された溶融飛灰32は、溶融飛灰コンベア18により飛灰溜め19に送られる。一方、灰30に含まれている不燃性成分(鉄等の金属やガラス,砂等)は溶融状態となり、その溶融スラグ31は、溶融スラグ流出口10から連続的に溢出し、水を満したスラグ水冷槽20内に落下して水砕スラグ33となり、スラグ搬出コンベア21によってスラグ溜め22に送られる。なお、溶融炉1の停止時には、炉1内の溶融スラグ31が冷却して固化しまうのを防止するために、溶融スラグ31の底部レベルに対応して炉壁1aに設けたタップホール11により湯抜きを行い、炉1内を空にする。
【0006】
このようなプラズマ溶融炉1の周壁たる炉壁1aは、一般に、溶融スラグ31に接触する耐火壁構造部分110の外周面を水冷ジャケット120により(又は水スプレー手段や空冷手段等により)冷却するように構成してなるが、従来の代表的な炉壁構造としては、図9(A)に示す如く、耐火壁構造部分110を1600℃程度の高温に耐え得る耐火材(例えば、カーボン系,C−SiC系,SiC系,クロム系の耐火材)で構成すると共に、これを囲繞する水冷ジャケット120を鋼板製のジャケット121内に冷却水122を供給する構造のものとなし、更に耐火壁構造部分110とジャケット121との間に電気絶縁性の断熱材層130を介在させたもの(以下「従来炉壁」という)が周知である。
【0007】
【発明が解決しようとする課題】
しかし、このような従来炉壁1aにあっては、耐火壁構造部分110の侵食による損傷が問題となっている。
【0008】
すなわち、耐火壁構造部分110は、上記した如く炉1内の高温に充分耐え得る耐火材で構成されているが、高温に晒されると共に腐食性を有する溶融スラグ31が接触することから、図9(B)に示す如く、局部的に侵食され易い。かかる侵食による損傷は、特に、溶融スラグ31の液面(以下「湯面」という)に対応する高さ部分であって溶融スラグ流出口10の周辺部分において著しい。
【0009】
そして、このような耐火壁構造部分110の侵食による損傷部分(以下「侵食部分」という)114を放置したまま運転を継続すると、侵食が進行して、その侵食深さが耐火壁構造部分110の厚みを超えて、溶融炉1全体の熱破壊を起こしたり、ジャケット121が破損して、その内部水122が洩れて爆発する等の極めて危険な事態を誘発する原因となる(図9(B)鎖線参照)。したがって、耐火壁構造部分110の侵食はこれを可及的に早期に発見して、その侵食部分114を、その侵食深さが耐火壁構造部分110の厚みにまで達しない段階で、補修することが必要である。
【0010】
しかし、従来では、耐火壁構造部分110の侵食による損傷を運転中に検知する術がないため、炉壁損傷の確認は炉1の運転を停止して行なう他ないのが実情である。したがって、炉壁損傷を早期に発見するためには頻繁に運転を停止せざるを得ず、長期に亘る連続運転を行うことができなくなり、どうしても灰30の溶融処理効率が低下するといった問題が生じる。しかも、耐火壁構造部分110の表面(内周面)を視認する等によっては、耐火壁構造部分110の侵食程度を的確に判断することが困難であり、ややもすれば、侵食程度の判断を誤って適正な補修時期を逸してしまい易い。
【0011】
本発明は、このような点に鑑みてなされたもので、プラズマ溶融炉の運転を停止させることなく、炉壁における耐火壁構造部分の侵食による損傷を早期の段階で的確に検知することができる炉壁損傷検知方法を提供することを目的とするものである。
【0012】
【課題を解決するための手段】
本願請求項1の発明は、ごみ焼却灰や飛灰を溶融処理するプラズマ溶融炉の炉壁の耐火壁構造部分を、溶融スラグに接触する耐火材製の内周層と内周層の外側を囲繞する電気絶縁体とその外側を囲繞する導電性の外周層とで形成すると共に、前記内周層の厚みTaと外周層の厚みTbとがTa/Tb=(1〜3)/1となるようにし、また、前記外周層の内部の溶融スラグの湯面より僅かに下方で且つ厚さ方向に内側層側の位置に、外周層の横断面形状に沿って金属棒状体を彎曲させて形成した電極を埋設すると共に当該電極と大地間に電流計を接続し、主電極から溶融スラグ及び電極を通しての大地への通電状態を感知することにより、耐火壁構造部分の前記内周層の侵食による損傷の程度を検知するようにしたことを発明の基本構成とするものである。
また、本願請求項2の発明は、ごみ焼却灰や飛灰を溶融処理するプラズマ溶融炉の炉壁の耐火壁構造部分を、溶融スラグに接触する非導電性の耐火材製の内周層と内周層の外側を囲繞する導電性の外周層とで形成すると共に、前記内周層の厚みTaと外周層の厚みTbとがTa/Tb=(1〜3)/1となるようにし、また、前記外周層の内部の溶融スラグの湯面より僅かに下方で且つ厚さ方向に内側層側の位置に、外周層の横断面形状に沿って金属棒状体を彎曲させて形成した電極を埋設すると共に当該電極と大地間に電流計を接続し、主電極から溶融スラグ及び電極を通しての大地への通電状態を感知することにより、耐火壁構造部分の前記内周層の侵食による損傷の程度を検知するようにしたことを発明の基本構成とするものである。
【0013】
すなわち、耐火壁構造部分が侵食による損傷され、その侵食深さが内周層の厚みを超えて、溶融スラグが侵食部分から侵入して外周層に接触する事態が発生すると、溶融スラグが導電性を有することから、主電極と導電性を有する外周層との間が溶融スラグを介して通電状態となる。一方、かかる通電状態となっているか否かは、上記した如き適宜の手法により、炉運転を停止させずとも容易に確認,検知することができる。したがって、侵食が内周層の厚みを超えて外周層に達した段階で、耐火壁構造部分の損傷を的確に検知することができ、補修時期を逸するようなことがなく、連続運転を安全に行なうことができる。
【0014】
【発明の実施の形態】
以下、本発明の実施の形態を図1〜図3又は図4〜図6に基づいて詳細に説明する。
【0015】
図1〜図3は第1の実施の形態を、図4〜図6は第2の実施の形態を、夫々示したものであり、各実施の形態は、本発明を図8に示すプラズマ溶融炉1の炉壁1aに適用した例に係るものである。
【0016】
すなわち、第1の実施の形態にあっては、図1及び図2に示す如く、プラズマ溶融炉1の周壁である炉壁1aが耐火壁構造部分110の外周面を水冷ジャケット120で被覆してなる円筒形状に構成されているが、図9に示す従来炉壁と異なって、耐火壁構造部分110を、溶融スラグ31に接触する内周層111とこれを囲繞する外周層112と両層111,112間に介在された電気絶縁体113とからなる3層構造物に構成してある。
【0017】
内周層111は、従来炉壁に使用されるものと同様の耐火材で円筒状に構成されている。耐火材としては、炉1内の高温雰囲気に対して充分な耐熱性を有するもの、例えば、1600℃程度の高温に耐え得るカーボン系,C−SiC系,SiC系,マグネシアクロム系のものが使用される。なお、内周層111と外周層112との間には後述する如く電気絶縁体113が介在されることから、内周層111の構成材としては導電性の耐火材(例えば、カーボン系の耐火材)が使用されている。
【0018】
外周層112は、導電性に優れた耐火材、例えばC−SiC系、カーボン系の耐火材で円筒状に構成されており、電気絶縁体113の介在により電気的に絶縁された状態で内周層111を囲繞している。電気絶縁体113は、スピネル、Si3 N4 等の耐熱性に優れた電気絶縁材料からなる。
【0019】
ところで、内周層111と外周層112とで構成される耐火壁構造部分110の厚みは、該部分110を単一耐火材層で構成する場合と同様に、炉条件(炉の形状,大きさ等)に応じて設定されるが、内周層111の厚みTaと外周層112の厚みTbとは、通常、Ta:Tb=1〜3:1の割合となるように設定しておくことが好ましい。例えば、耐火壁構造部分110の厚みが270mmである場合には、Ta=135〜200mm,Tb=70〜135mmとしておくことが好ましい。
【0020】
また、外周層112の外周面は、従来炉壁と同様に、電気絶縁性を有する断熱層130を介在した状態で水冷ジャケット120により被覆されている。すなわち、外周層112は、その厚み方向における両側に配置された内周層111及び水冷ジャケット120の何れに対しても電気的に絶縁された状態にある。なお、水冷ジャケット120は、従来炉壁と同様に、鋼板製のジャケット121内に冷却水122を供給させる構造とされている。
【0021】
そして、外周層112には、図1及び図2に示す如く、電気絶縁体113との境界部分に配して、これに水平に沿って湾曲する棒状の電極140が埋設されている。この電極140はアースされており、そのアース部には電流指示計142が設けられている。すなわち、電極140には電流指示計142を取り付けたアース線141が接続されていて、後述する如く、直流電源装置8の陰極に接続された主電極4と導電性の外周層112との間が溶融スラグ31を介して通電状態となったときにおいて、電極140を流れる電流により電流指示計142が作動されるようになっている。なお、この例では、電流指示計142が作動されると、電極140を電流が流れたこと(つまり主電極4と外周層112との間が通電状態となったこと)を電流計指針により確認できる他、適当な安全措置が採られるようになっている。具体的には、例えば、警報が発せられると共にプラズマ溶融炉1の運転が緊急停止されるようになっている。
【0022】
而して、第1の実施の形態にあっては、本発明の方法により炉壁1aの耐火壁構造部分110の侵食による損傷が次のように検知される。
【0023】
すなわち、耐火壁構造部分110の内周部つまり内周層111は、炉1内の高温雰囲気に晒されると共に腐食性の溶融スラグ31に接触することから、主として、湯面に対応する高さ部分であって溶融スラグ流出口10の周辺部分において、局部的に侵食されるが、その侵食部分114の深さが内周層111の厚みTaを超えない状態では、主電極4と外周層112及びこれに埋設された電極140との間は通電状態とならず、電流指示計142は作動しない(図3(A)参照)。
【0024】
しかし、炉運転を継続することにより、侵食が進行して、侵食部分114の深さが内周層111の厚みTaを超えて、内外周層111、112間の電気絶縁体113をも侵食、破壊する状態となると、導電性を有する溶融スラグ31が侵食部分114に侵入して、外周層112に接触することになり、主電極4と外周層112及びこれに埋設された電極140との間が溶融スラグ31を介して通電状態となる(図3(B)参照)。その結果、かかる通電状態を適当な検知手段により検知することにより、侵食程度つまり侵食部分114の深さが内周層111の厚みTa(より正確には、内周層111と電気絶縁体113との合計厚み)に相当する寸法に達したことを的確に把握することができ、適当な安全措置をとることができる。この例では、検知手段として設けられた電流指示計142が作動し、安全措置として、警報が発せられると共にプラズマ溶融炉1が緊急停止される。
そして、運転停止後は、炉1内を点検し、侵食部分114を補修する。このとき、外周層112は侵食されておらず、耐火壁構造部分110の一部である内周層111(及び電気絶縁体113)を補修するだけであるから、補修を経済的に且つ容易に行うことができる。
【0025】
このように、本発明の方法によれば、プラズマ溶融炉の運転中において、耐火壁構造部分110の侵食程度を的確に把握することができ、つまり侵食部分114が一定深さに達しているか否かを的確に把握することができ、侵食がさほど進行していない段階で侵食確認のために不必要に炉運転を停止したり或いは侵食が危険な事態を誘発する段階まで進行しているにも拘わらず炉運転を継続したりするといった問題を生じることなく、プラズマ溶融炉1の長期に亘る安全な連続運転並びに的確な補修時期の決定による適正な保守を確保することができる。
【0026】
また、第2の実施の形態にあっては、図4及び図5に示す如く、内周層111を非導電性の耐火材(例えば、クロム系耐火材)で構成することによって、両層111,112間に上記した電気絶縁体113を介在させることなく、導電性の耐火材からなる外周層112を内周層111から電気的に絶縁させてある。また、電極140を外周層112の厚み方向における略中央部に埋設してある。これらの点、つまり内周層111を非導電性の耐火材で構成した点、両層111,112を電気絶縁体113を介在させることなく接触させた点及び電極140を外周層112の厚み方向における略中央部に埋設した点を除いて、炉壁1aを第1の実施の形態におけると同一構造となしている。なお、内周層111の厚みTaと外周層112の厚みTbとの割合も、第1の実施の形態におけると同一である。
【0027】
而して、第2の実施の形態にあっても、本発明の方法により炉壁1aの耐火壁構造部分110の侵食による損傷が、第1の実施の形態における場合と同様に検知される。
【0028】
すなわち、侵食部分114の深さが内周層111の厚みTaを超えない状態では、主電極4と外周層140及びこれに埋設された電極140との間は通電状態とならず、電流指示計142は作動しない(図6(A)参照)。しかし、侵食が進行して侵食部分114の深さが内周層111の厚みTaを超えると、導電性を有する溶融スラグ31が侵食部分114に侵入して、外周層112に接触することなり、主電極4と外周層140及びこれに埋設された電極140との間が溶融スラグ31を介して通電状態となり、電流指示計142が作動して、警報が発せられると共にプラズマ溶融炉1が緊急停止される(図6(B)参照)。
【0029】
なお、本発明は上記した各実施の形態に限定されるものではなく、本発明の基本原理を逸脱しない範囲において、適宜に改良,変更することができる。特に、主電極4と外周層112との間が通電状態にあることを感知する手段は任意であり、電極140の形状及び外周層112における埋設位置も任意である。要は、浸食部分114が外周層112の内周面に達して主電極4と外周層112との間が溶融スラグ31を介して通電状態となったことを感知できるものであればよい。例えば、耐火壁構造部分110を第1の実施の形態における如く構成した場合において、図7に示す如く、外周層112に埋設した導線144に電圧をかけておき、その変化を電流指示計143により検知することによって、通電状態を感知するようにしてもよい。或いは、導電性の内周層111と電気絶縁体113との間に電圧をかけておき、その電流変化を検知することにより通電状態を感知するようにしてもよい。
【0030】
【発明の効果】
以上の説明から容易に理解されるように、本発明によれば、炉運転を停止することなく、耐火壁構造部分がどの程度浸食されたかを的確に検知することができ、浸食が一定以上(内周層の厚み(又は内周層及び電気絶縁体の合計厚み)以上)に進行するのを確実に防止することができる。したがって、浸食が耐火壁構造部分を超えるような危険を未然に防止しつつ、炉運転を長期に亘って安全に行うことができ、灰の溶融処理を効率よく行うことができる。しかも、耐火壁構造部分の一部(内周層又は内周層及び電気絶縁体)を補修するだけでよく、外周層を含む耐火壁構造部分全体を補修する場合に比して、補修を極めて経済的に且つ容易に行うことができる。
【図面の簡単な説明】
【図1】本発明に係る方法が適用される炉壁構造の第1例を示す要部の縦断側面図である。
【図2】図1のII−II線に沿う横断平面図である。
【図3】耐火壁構造部分の浸食状態を示す図1相当の縦断側面図である。
【図4】本発明に係る方法が適用される炉壁構造の第2例を示す要部の縦断側面図である。
【図5】図4のV−V線に沿う横断平面図である。
【図6】耐火壁構造部分の浸食状態を示す図4相当の縦断側面図である。
【図7】通電状態感知手段の変形例を示す図1対応の縦断側面図である。
【図8】プラズマ溶融炉の一例を示す縦断側面図である。
【図9】従来の炉壁構造を示す要部の縦断側面図である。
【符号の説明】
1…プラズマ溶融炉、1a…炉壁、4…主電極、30…灰、31…溶融スラグ、110…耐火壁構造部分、111…内周層、112…外周層、113…電気絶縁体、114…浸食部分、120…水冷ジャケット、130…電気絶縁断熱材層、140…電極、141…アース線(アース部)、142…電流指示計。[0001]
BACKGROUND OF THE INVENTION
The present invention relates to a plasma melting furnace for melting incineration ash and fly ash, which are incineration residues of garbage (city waste, industrial waste, etc.), for detecting damage due to erosion of a fire wall structure portion of the furnace wall. It is about the method.
[0002]
[Prior art]
In recent years, in order to reduce the volume and detoxify incineration ash and fly ash (hereinafter referred to as “ash”), which are incineration residues discharged from waste incinerators, ash melt-solidification methods have attracted attention and are practically used. It is offered to. As the ash melts and solidifies, its volume can be reduced to 1/2 to 1/3, and it is possible to prevent the elution of hazardous substances such as heavy metals, reuse molten slag, and extend the life of the final landfill site. Because it becomes.
[0003]
By the way, as an ash melting and solidifying method, for example, an arc melting furnace, a plasma arc furnace, an electric resistance furnace or the like is used, and a method of melting and solidifying ash by electric energy, a surface melting furnace, a swirling melting furnace, a coke bed, etc. A method of melting and solidifying ash by the combustion energy of fuel using a furnace or the like has been put into practical use. Generally, when the power generation equipment is juxtaposed with the waste incineration equipment, the former method using electric energy is adopted, and when the power generation equipment is not juxtaposed, the latter method using combustion energy is adopted. Yes.
[0004]
FIG. 8 shows an example of a DC arc discharge graphite electrode type plasma melting furnace installed in the waste incineration facility. In this
[0005]
When the melting of the
[0006]
Such a
[0007]
[Problems to be solved by the invention]
However, in such a
[0008]
That is, the refractory
[0009]
Then, when the operation is continued while leaving the damaged portion (hereinafter referred to as “eroded portion”) 114 due to the erosion of the fire
[0010]
However, conventionally, there is no way to detect damage due to erosion of the fire
[0011]
The present invention has been made in view of the above points, and can accurately detect damage due to erosion of the fire wall structure portion in the furnace wall at an early stage without stopping the operation of the plasma melting furnace. An object of the present invention is to provide a furnace wall damage detection method.
[0012]
[Means for Solving the Problems]
In the invention of
Further, the invention of claim 2 of the present application is directed to a fire wall structure portion of a furnace wall of a plasma melting furnace for melting waste incineration ash and fly ash, and an inner peripheral layer made of a non-conductive refractory material in contact with the molten slag. A conductive outer peripheral layer surrounding the outer periphery of the inner peripheral layer, and the inner peripheral layer thickness Ta and the outer peripheral layer thickness Tb are Ta / Tb = (1-3) / 1, Further, an electrode formed by bending a metal rod-like body along the cross-sectional shape of the outer peripheral layer at a position slightly below the molten metal surface of the molten slag inside the outer peripheral layer and on the inner layer side in the thickness direction. The degree of damage due to erosion of the inner wall layer of the fire wall structure by burying and connecting an ammeter between the electrode and the ground, and sensing the state of conduction from the main electrode to the ground through the molten slag and the electrode The basic configuration of the invention is to detect the above.
[0013]
In other words, if the fire wall structure is damaged by erosion, the erosion depth exceeds the thickness of the inner peripheral layer, and molten slag enters from the eroded portion and contacts the outer peripheral layer, the molten slag becomes conductive. Therefore, between the main electrode and the outer peripheral layer having conductivity is energized via the molten slag. On the other hand, whether or not it is in the energized state can be easily confirmed and detected by the appropriate method as described above without stopping the furnace operation. Therefore, when the erosion reaches the outer layer beyond the thickness of the inner layer, it is possible to accurately detect damage to the fire wall structure, and without losing the repair time, safe operation is safe. Can be done.
[0014]
DETAILED DESCRIPTION OF THE INVENTION
Hereinafter, embodiments of the present invention will be described in detail with reference to FIGS. 1 to 3 or 4 to 6.
[0015]
FIGS. 1 to 3 show the first embodiment, and FIGS. 4 to 6 show the second embodiment, respectively. In each embodiment, the present invention is shown in FIG. This example is applied to the
[0016]
That is, in the first embodiment, as shown in FIGS. 1 and 2, the
[0017]
The inner
[0018]
[0019]
By the way, the thickness of the refractory
[0020]
The outer peripheral surface of the outer
[0021]
As shown in FIGS. 1 and 2, a rod-shaped
[0022]
Thus, in the first embodiment, damage due to erosion of the fire
[0023]
That is, the inner peripheral portion of the fire
[0024]
However, by continuing the furnace operation, erosion progresses, the depth of the eroded
After the operation is stopped, the inside of the
[0025]
Thus, according to the method of the present invention, it is possible to accurately grasp the degree of erosion of the fire
[0026]
In the second embodiment, as shown in FIGS. 4 and 5, the inner
[0027]
Thus, even in the second embodiment, damage due to the erosion of the fire
[0028]
That is, when the depth of the eroded
[0029]
The present invention is not limited to the above-described embodiments, and can be appropriately improved and changed without departing from the basic principle of the present invention. In particular, the means for sensing that the main electrode 4 and the outer
[0030]
【The invention's effect】
As can be easily understood from the above description, according to the present invention, it is possible to accurately detect how much the fire wall structure portion has been eroded without stopping the furnace operation, and erosion is above a certain level ( Proceeding to the thickness of the inner peripheral layer (or more than the total thickness of the inner peripheral layer and the electrical insulator) can be reliably prevented. Therefore, the furnace operation can be performed safely over a long period of time while preventing the danger that erosion exceeds the fire wall structure portion, and the ash melting process can be performed efficiently. Moreover, it is only necessary to repair a part of the refractory wall structure (inner peripheral layer or inner peripheral layer and electrical insulator). Compared to the case of repairing the entire refractory wall structure including the outer peripheral layer, the repair is extremely difficult. It can be done economically and easily.
[Brief description of the drawings]
FIG. 1 is a longitudinal side view of a main part showing a first example of a furnace wall structure to which a method according to the present invention is applied.
FIG. 2 is a cross-sectional plan view taken along the line II-II in FIG.
FIG. 3 is a longitudinal side view corresponding to FIG. 1 and showing an erosion state of a fire wall structure portion.
FIG. 4 is a longitudinal side view of a main part showing a second example of a furnace wall structure to which the method according to the present invention is applied.
5 is a cross-sectional plan view taken along line VV in FIG.
6 is a longitudinal side view corresponding to FIG. 4 and showing an erosion state of the fire wall structure portion. FIG.
FIG. 7 is a longitudinal side view corresponding to FIG. 1 and showing a modification of the energization state sensing means.
FIG. 8 is a longitudinal side view showing an example of a plasma melting furnace.
FIG. 9 is a longitudinal side view of a main part showing a conventional furnace wall structure.
[Explanation of symbols]
DESCRIPTION OF
Claims (2)