JP3766682B2 - Nanotube probe - Google Patents
Nanotube probe Download PDFInfo
- Publication number
- JP3766682B2 JP3766682B2 JP17310699A JP17310699A JP3766682B2 JP 3766682 B2 JP3766682 B2 JP 3766682B2 JP 17310699 A JP17310699 A JP 17310699A JP 17310699 A JP17310699 A JP 17310699A JP 3766682 B2 JP3766682 B2 JP 3766682B2
- Authority
- JP
- Japan
- Prior art keywords
- nanotube
- probe
- holder
- ultrafine particles
- tip
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
【0001】
【発明の属する技術分野】
本発明はカーボンナノチューブ、BCN系ナノチューブ、BN系ナノチューブ等のナノチューブを探針として物質の表面信号を操作するナノチューブプローブに関し、更に詳細には、ナノチューブの先端に超微粒子やフラーレン等をセンサー部として設け、この所定構造のセンサー部により物質の表面信号を再現性よく高分解能に操作できるナノチューブプローブに関する。
【0002】
【従来の技術】
従来、試料表面を高倍率に観察する顕微鏡として電子顕微鏡があったが、真空中でなければ電子ビームが飛ばないために実験技術上で種々の問題があった。ところが、近年、大気中でも表面を原子レベルで観察できる走査型プローブ顕微鏡技術が開発されるに到った。プローブの最先端にある探針を試料表面に原子サイズまで極微接近させると、個々の試料原子からの物理的・化学的作用を探針で検出し、探針を表面上に走査させながら検出信号から試料表面像を現出させる顕微鏡である。
【0003】
これらの顕微鏡の中でも特によく利用されるものは、走査型トンネル顕微鏡(STMとも略称する)と原子間力顕微鏡(AFMとも略称する)である。STMでは研磨金属針などの導電性探針が用いられ、AFMではシリコン製ピラミッドを探針としたカンチレバーを用いて表面信号を検出している。これらに共通した問題は、探針の先端を超微細に先鋭加工できないために物質表面の原子レベルでの微細構造を高分解能に検出できないと云うことであった。
【0004】
例えば、図15は従来のシリコン製のAFM用カンチレバーである。このカンチレバー50の後方はサブストレート52に固定され、前方にはピラミッド状探針54が形成されている。このピラミッド状探針54の先端には極細の先鋭部56が形成され、この先鋭部56が物質表面に近接して表面情報を検出する。このAFM用カンチレバーは半導体プレーナ技術により製造されるが、如何に先鋭部をシャープに形成したとしても、原子サイズと比較すればかなり大きなものになる。従って、表面情報が原子サイズで変化する場合には、上記探針を用いても表面情報を原子レベルにまで高精度に検出することには限界があった。
【0005】
そこで、近年になってカーボンナノチューブを探針に利用しようとするアイデアが出現した。カーボンナノチューブは導電性であるため、トンネル電流を検出するSTMにはもちろん、原子間力を検出するAFMにも利用できる。J.Am.Chem.Soc.120巻(1998年)603頁に、生物システムを映像化する高分解能プローブとしてカーボンナノチューブ探針が提案されている。しかし、カーボン混合物中からカーボンナノチューブだけをどのように収集するか、またどのようにしてホルダーにカーボンナノチューブを固定するのかについては全く未解決であった。
【0006】
また、プローブ顕微鏡分野とは異なるが、近年、コンピュータのメモリ容量が増大するにつれ、メモリ装置がフロッピーディスク装置からハードディスク装置へ、更に高密度ディスク装置へと進化しつつある。小さな空間に更に高密度に情報を詰め込むと、1情報当たりのサイズが小さくなるため、その入出力用の探針もより微細なものが必要になってくる。従来の磁気ヘッド装置では一定以上に小さくすることは不可能であった。CD装置などの電子装置でもその入出力用プローブの超微小化が要望されていた。
【0007】
この磁気ヘッドに替わるものとして、図16に示す磁気プローブが考えられていた。この磁気プローブは、前記ピラミッド状探針54の先鋭部56に蒸着法により強磁性金属膜58を形成して構成される。しかし、この強磁性金属膜58は多結晶膜であるから、多数の磁気的ドメイン60が複合的に配置した膜構造となっている。
【0008】
図17はこの磁気プローブで対象物質の磁気情報を検出する場合の説明図である。この磁気プローブを対象物質62の表面に近接させると、磁気力は逆二乗則で作用する長距離力であるから、各々の磁気的ドメインが1/z2に比例した強度で磁気情報を検出する。結果的にそれらの合成信号が磁気的表面情報となるため、磁気情報を高分解能に検出することは極めて困難である。問題点は、先鋭部自体が原子レベルではかなり巨大であること、また多数の磁気的ドメインから構成されることである。
【0009】
従って、この磁気プローブとして前述したカーボンナノチューブを利用することが当然考えられる。しかし、カーボンナノチューブにどうやって強磁性体を担持させるかという技術はまだできていない。更に、カーボンナノチューブの精製技術やホルダーへの固定化技術については全く未解決であることは前述と同様であった。
【0010】
本発明者等は、これらの問題点のうち微小化技術に解決策を与える3件の特許出願をなした。即ち、特願平10−280431号では電気泳動法によりナノチューブの精製方法を与え、特願平10−376642号ではコーティング膜によるナノチューブの固定化技術を提案し、特願平10−378548号では熱融着によるナノチューブの固定化技術を完成した。
【0011】
【発明が解決しようとする課題】
本発明者等は更にナノチューブプローブの研究を進める中で、ナノチューブを探針としてSTM,AFMや磁気プローブ等に応用した場合に、同一物質表面に対して得られる信号が使用するナノチューブによって変動するという欠点があることに気づいた。これは、表面信号を感知するナノチューブの先端部の物理構造あるいは電子構造がナノチューブ毎にバラバラであることを意味している。言い換えると、使用されるナノチューブのサイズがバラバラであることである。電子顕微鏡内でナノチューブを選別してホルダーに固定しているが、電子顕微鏡像ではサイズや電子構造を含めて同一構造のナノチューブであるかどうかを判別することは困難である。
【0012】
従って、本発明の第1目的は、先端部の物理構造や電子構造を同一にしたナノチューブおよびその製造方法を提供することである。
本発明の第2目的は、先端部を同一化した前記ナノチューブをホルダーに固定することにより、対象物質の表面情報を高精度に再現できるナノチューブプローブを提供することである。
【0013】
【課題を解決するための手段】
本発明は上記課題及び目的を達成するためになされたものである。
請求項1の発明は、ナノチューブの先端にセンサー部を設けたことを特徴とするナノチューブである。
請求項2の発明は、前記センサー部が超微粒子のナノチューブである。
請求項3の発明は、前記超微粒子が強磁性金属超微粒子のナノチューブである。
請求項4の発明は、前記センサー部がフラーレンのナノチューブである。
【0014】
請求項5の発明は、基板上に金属の薄膜を形成し、この金属薄膜を加熱して金属超微粒子化し、この金属超微粒子上に炭素化合物ガスを流通させながら加熱して炭素化合物を分解させ、超微粒子を押し上げながら炭素成分がその根本にカーボンナノチューブを形成することを特徴とするナノチューブの製造方法である。
請求項6の発明は、ナノチューブの所要部を切断し、その切断面にフラーレンを結合させることを特徴とするナノチューブの製造方法である。
請求項7の発明は、ナノチューブの閉口または開口した先端面にフラーレンを結合させるナノチューブの製造方法である。
【0015】
請求項8の発明は、先端にセンサー部を設けたナノチューブの基端部をホルダーに固定したことを特徴とするナノチューブプローブである。
請求項9の発明は、前記センサー部が超微粒子のナノチューブプローブである。
請求項10の発明は、前記超微粒子が強磁性金属超微粒子のナノチューブプローブである。
請求項11の発明は、前記センサー部がフラーレンのナノチューブプローブである。
請求項12の発明は、請求項5により形成されたナノチューブの基端部をホルダーに固定することを特徴とするナノチューブプローブの製造方法である。
請求項13の発明は、請求項6又は7により形成されたナノチューブの基端部をホルダーに固定することを特徴とするナノチューブプローブの製造方法である。
【0016】
【発明の実施の形態】
本発明者等はナノチューブ探針の先端部の物理構造や電子構造を同一化するために鋭意研究した結果、ナノチューブの先端にサイズや構造の決まったセンサー部を別個形成することにより、ナノチューブの構造が多少変動してもセンサー部の同一性を保証できる技術を完成するに到った。センサー部が同一である限りその物質構造や電子構造は同一であり、対象物質の表面情報を高精度に再現することが可能となる。
【0017】
本発明者等は、既定のサイズや物質構造を有したセンサー部として、超微粒子やサッカーボール状物質であるフラーレンが適当であるとの認識に到達した。
【0018】
超微粒子は粒径が数十nm以下のクラスター状の原子集団を云い、金属超微粒子、金属酸化物超微粒子、シリコン超微粒子、SiC超微粒子など多種類の超微粒子が製造されている。その製造方法および製造条件によって、単結晶状または単結晶性の強い多結晶状で、各種の粒径の超微粒子が製造できることが分かっている。従って、製法と条件を特定すれば、電子構造が同一で単一ドメインを有した特定粒径の超微粒子を製造することができる。この特定構造の超微粒子をナノチューブの先端に固定することによって、高再現性能を有して超微粒子により対象物質の表面情報を読み取ったり、対象物質表面に情報を書きこんだりすることが可能になる。
【0019】
この超微粒子ナノチューブプローブは、従来から存するプローブ顕微鏡、例えば走査型トンネル顕微鏡、原子間力顕微鏡、摩擦力顕微鏡、磁気力顕微鏡、化学力顕微鏡などの探針プローブとして利用できる。それぞれの用途に応じて、特有の物理的・化学的作用を検知する超微粒子をナノチューブの先端に固定すれば、対象物質の物理的・化学的な表面情報を得ることができる。
【0020】
例えば、超微粒子としてFe、Co、Ni等の強磁性金属超微粒子を利用すれば、対象物質表面の磁気を感知するから、その磁性表面構造を読み取ることができる。逆に、この強磁性金属超微粒子を磁気ヘッドとして利用すれば、対象物質表面に磁気情報を書きこむことが可能となり、入出力用プローブとすることができる。入出力できる磁気情報の単位サイズは超微粒子のサイズに依存し、数nm以下、更には1nm以下にまで小さくすることができ、超高密度化を図ることが可能となる。
このように超微粒子は極めて小さいので、微小物体の磁性測定に有効である。例えば、生物細胞内の磁性測定にはFe2O3やFe2O4等の酸化鉄超微粒子を用いることができ、ナノチューブプローブとすることにより、細胞内の測定位置を自在に極微調整することができる。
【0021】
また、触媒作用を有する超微粒子をセンサー部として用いれば、ナノチューブプローブを触媒用プローブとして活用することができる。例えば、Ni超微粒子は1,3−シクロオクタジエンの水素化触媒として利用できるし、Cu−ZnO超微粒子はメタノール合成触媒として利用できる。これらの超微粒子を粉体として単に分散配置させるのではなく、ナノチューブに固定することにより、触媒配置を正確に調整でき、触媒効率の高度化を図ることができる。また、触媒反応測定用のプローブとすることもできる。
【0022】
超微粒子をナノチューブの先端に固定する方法として、現在のところ二つの方法がある。一つ目は、ナノチューブと超微粒子を別個に製造しておき、ナノチューブの先端面或いは先端を切断した切断面に超微粒子を極微接近させて原子間力により結合させる方法である。またはナノチューブの先端面や切断面の2重結合を光照射・化学反応などで開いて、その結合の手に超微粒子を化学結合させる方法もある。その結合部に電子ビーム照射やレーザービーム照射して融着により結合を強化することもできる。これらの一連の操作は電子顕微鏡内で直接観察しながら行なうことができる。
二つ目は、ナノチューブと超微粒子を同時又は前後に結晶成長させる方法である。この方法には半導体技術に用いられている化学的気相成長法(CVD法)などの各種の方法が利用できる。例えば、基板上に超微粒子を成長させ、次にその表面付近に炭素化合物ガスを流通させると、熱分解により炭素分子が超微粒子の根本部分に成長してカーボンナノチューブとして成長し、その先端に超微粒子を担持することになる。
【0023】
センサー部としてフラーレンを用いることができる。フラーレンはサッカーボール状物質、即ち球殻分子の総称で、1985年にグラファイトを高エネルギーレーザーで照射して得られた蒸気冷却物の中に第1号のC60が発見された。現在では原子数70〜100の高級フラーレン、それ以上の巨大フラーレンも発見され、これらの合成法も確立している。これらのフラーレンは、炭素のsp2軌道が作る五員環と六員環で構成されており、中には七員環を含むものも発見されている。
【0024】
フラーレンを図形として理論的に考えた場合に、オイラーの多面体定理から、五員環は12個含まれ、六員環は全原子の数によって変化することが分かっている。また、12個の五員環は隣接しないという孤立五員環則が数学的に満たされると考えられている。これらの数学的規則から考察すると、高級フラーレンにはC70、C76、C78等があり、巨大フラーレンにはC240、C540、C960等が存在することが分かる。また、実験的にもそれらの存在が確認されている。
【0025】
フラーレンは炭素ススの中に大量に含まれていることが確認されている。従って、特定構造のフラーレンの製造方法は、ススの製造法とススからの特定フラーレンの分離法からなる。フラーレンのススの製造法には抵抗加熱法やアーク放電法等があるが、直流アーク放電法が多く利用される。即ち、グラファイト電極間に直流電圧を印加してアーク放電を起こさせると、生成されるススの中に各種炭素数のフラーレンが混在するのである。次に、このススをクロマトグラフィの技術で分離する。特に液体クロマトグラフィやカラムクロマトグラフィを用いれば特定炭素原子数のフラーレンを容易に分離することができる。
【0026】
例えば、ポリスチレン系のカラムを用い、展開溶液をベンゼンや二硫化炭素として、高速液体クロマトグラフを行うことにより、C76、C78、C82、C84、C90、C96等のフラーレンを分離することができる。原子数が決まったフラーレンは異性体の区別を除けば同一の電子構造をとると考えてよい。また、最近では、同一サイズのフラーレンを構造異性体毎に分離することも可能になってきた。この段階まで行けば、電子状態が同一である特定構造のフラーレンを大量に製造することができる。このサイズや構造の決まったフラーレンをナノチューブ先端に固定することにより、ナノチューブの異同に関係なく対象物質の表面構造を高精度に再現可能に読み取ることができ、また情報を対象表面に書き込むことも可能になる。
【0027】
金属を内包したフラーレンを製造することもできる。例えば、グラファイト粉末と金属酸化物を適当な割合で混合し、この混合物にグラファイトセメントを加えて棒状電極の形に成形する。この棒状電極をアルゴン雰囲気中でゆっくり加熱して、最終的に1200℃で10時間くらい加熱すると電極として完成する。この電極を用いてアーク放電させ、得られたススを溶媒抽出して特定構造のフラーレンを分離する。このフラーレンの中には金属原子が閉じこめられている。金属原子としてはLa、Y、Sc等があるが、金属酸化物を変更することによって、所望の金属原子をフラーレン中に包含させることができる。
【0028】
この特定構造のフラーレンをナノチューブに固定するには次のような方法がある。まず、ナノチューブとフラーレンを別個に製造しておく。次に、ナノチューブの先端を切断して、その切断面にフラーレンを極微接近させて原子間力により結合させる。この結合部に電子ビーム照射やレーザービーム照射して結合を強化することもできる。これらの一連の操作は電子顕微鏡内で実観察しながら行われる。
【0029】
こうして完成したナノチューブは、ナノチューブに多少のサイズのバラツキがあっても、物質表面を観測するセンサー部は特定構造のフラーレンであるから、同一対象表面からは同一の信号を高精度に再現することができる。従って、ナノチューブの構造のバラツキに影響されずに、高精度に物質表面を測定・操作できるナノチューブプローブを提供できる。
【0030】
このフラーレンナノチューブプローブは、従来から存するプローブ顕微鏡、例えば走査型トンネル顕微鏡、原子間力顕微鏡、摩擦力顕微鏡、磁気力顕微鏡、化学力顕微鏡などの探針プローブとして利用できる。それぞれの用途に応じて、特有の物理的・化学的作用を検知するフラーレンをナノチューブの先端に固定すれば、対象物質の物理的・化学的な表面情報を得ることができる。
【0031】
また、特定の物理的・化学的情報を検知する原子をフラーレンに内包し、この原子内包フラーレンをナノチューブに固定すれば、対象表面の特定情報を検出することができる。例えば、Fe、Co、Niのような強磁性金属原子を内包させると、前述した超微粒子と同様に、対象表面の磁気構造を検出できる。又逆に、対象物質表面が磁気記録媒体であれば、このフラーレンナノチューブプローブを用いて特定情報を書き込むこともできる。
【0032】
本発明で用いられるナノチューブは、カーボンナノチューブ、BCN系ナノチューブ、BN系ナノチューブ等のナノチューブである。その中でもカーボンナノチューブ(以下、CNTとも称する)が最初に発見された。従来、カーボンの安定な同素体としてダイヤモンド、グラファイトおよび非晶質カーボンが知られていた。ところが、1991年に直流アーク放電によって生成される陰極堆積物の中に、筒状構造のカーボンナノチューブの存在が認められた。
【0033】
このカーボンナノチューブの発見に基づいてBCN系ナノチューブが合成された。例えば、非晶質ホウ素とグラファイトの混合粉末をグラファイト棒に詰め込み、窒素ガス中で蒸発させる。また、焼結BN棒をグラファイト棒に詰め込み、ヘリウムガス中で蒸発させる。更に、BC4Nを陽極、グラファイトを陰極にしてヘリウムガス中でアーク放電させる。これらの方法でカーボンナノチューブ中のC原子が一部B原子とN原子に置換したBCN系ナノチューブが合成されたり、BN層とC層が同心状に積層した多層ナノチューブが合成される。
【0034】
またごく最近では、BN系ナノチューブが合成された。これはC原子をほとんど含有しないナノチューブである。例えば、カーボンナノチューブとB2O3粉末をるつぼの中に入れて窒素ガス中で加熱する。この結果、カーボンナノチューブ中のC原子のほとんどがB原子とN原子に置換されたBN系ナノチューブに変換できる。勿論、これら以外の種々のナノチューブも利用できる。
【0035】
本発明のナノチューブプローブを製造するには二つの方法がある。一つ目は、ナノチューブにセンサー部を固定し、その後このセンサー部付きナノチューブの基端部をホルダーに固定する方法である。二つ目は、ナノチューブの基端部を先にホルダーに固定して、その後センサー部をナノチューブの先端部に固定する方法である。
【0036】
ナノチューブをセンサー部に固定するには、配置されたナノチューブの先端にセンサー部を固定する(又は結晶成長させる)場合、配置されたセンサー部にナノチューブを固定する(又は結晶成長させる)場合がある。特に後者では、超微粒子を形成して超微粒子を押し上げながらナノチューブを形成する場合も含まれる。
【0037】
ナノチューブの基端部をホルダーに固定するには二つの方法がある。一つ目は、電界印加またはファンデルワールス力によりナノチューブをホルダー面上に転移させ、ナノチューブの先端部を突出させた状態で、ホルダー面に接触した基端部をコーティング膜により被覆固定する方法である。二つ目は、電界印加またはファンデルワールス力によりナノチューブをホルダー面に転移させ、ホルダー面に接触したナノチューブの基端部をホルダー面に熱融着させる方法である。
【0038】
センサー付きナノチューブの形成とそのホルダーへの取り付けを同時に行うこともできる。具体的には、カンチレバーのシリコンピラミッドの表面に金属膜を形成し、更に加熱して金属膜を金属超微粒子にし、続いて炭素化合物ガスを流通させて金属超微粒子を押し上げるようにカーボンナノチューブを形成する。こうすればカンチレバーのピラミッドにセンサー付きナノチューブを一気に形成することになり、製造工程の簡易化を図ることができる。炭素化合物の中でも炭化水素が好ましい。
【0039】
【実施例】
[実施例1:超微粒子付きナノチューブの形成]
図1(A)〜(D)は超微粒子付きナノチューブの中で、特に超微粒子付きカーボンナノチューブの形成方法の工程図である。図1(A)の酸化鉄を表面に持つシリコン基板2の表面に厚さ10nmのNiの金属膜4を蒸着法で形成する(図1(B))。これを直径28mmで長さが50cmの円筒容器に入れ、Heガスを50sccmの流量で流しながら真空度を60mTorrに保持する。毎分120℃の温度上昇率で800℃まで加熱して1時間熱処理すると、図1(C)に示すように、シリコン基板2上でNiの金属膜4が多数のNiの超微粒子6に変化し、その直径は約20nmである。次に、真空を壊すことなく、60mTorrの真空度を保持しながら、C6H6ガスを10sccmの流量で1時間流すと、Ni超微粒子6の脱水素触媒反応により、Ni超微粒子6の下端に炭素原子が蓄積してカーボンナノチューブ8が形成される。このカーボンナノチューブ8はNi超微粒子6を押し上げながら成長し、超微粒子付きカーボンナノチューブ10が形成される。
【0040】
図2は超微粒子付きカーボンナノチューブ10の断面図である。カーボンナノチューブ8の直径dは15〜150nmに分布し、平均は45nmであった。Niの超微粒子6の直径Dは前記直径dよりやや大きいが、直径Dを小さくするには、Ni金属膜4の厚さを薄くしたり、超微粒子化するための加熱処理時間を短くする等の方法がある。
【0041】
図3は超微粒子付きカーボンナノチューブ10をAFM用カンチレバー12のピラミッド14に転移させる工程図である。この場合、ピラミッド14が超微粒子付きカーボンナノチューブ10の取り付け用のホルダーになる。超微粒子付きカーボンナノチューブ10を形成したシリコン基板2とカンチレバー12間に直流電源16により直流電界を形成し、この静電界力により超微粒子付きカーボンナノチューブ10をピラミッド14に飛跳転移させる。この場合、超微粒子6が先端に突出し、カーボンナノチューブ8の軸がカンチレバー12にほぼ垂直になり、その基端部8aがピラミッド14に接合するように調整される。これらの操作は電子顕微鏡の中で直接観察しながら行われる。直流電源16の電極の向きはナノチューブの帯電性に応じて調整される。
【0042】
図4は超微粒子付きカーボンナノチューブ10をピラミッド14に固定する工程図である。カーボンナノチューブ8の基端部8aを電子ビーム16で照射すると、基端部8aが変成して融着部8bとなり、ピラミッド14に熱融着で固定される。
【0043】
図5はNi超微粒子6の磁化工程図である。この試料では、ナノチューブ直径dは25nm、Ni超微粒子直径Dは35nm、先端長Lは400nmである。このNi超微粒子6に対し、10msの間だけ12.5テスラのパルス磁場Bを加えて磁化する。Ni超微粒子6は単一ドメインの強磁性体であり、このパルス磁化によって単一磁化ドメインを持った高分解能磁気検出用のナノチューブプローブ16として活用できるようになる。
【0044】
図6は高分解能磁気検出用のナノチューブプローブの使用状態図であり、このナノチューブプローブ16を用いて磁気記録媒体18の表面磁気情報20を測定する。超微粒子6の表面への接近距離ADは50〜100nmが好ましいが、ファンデルワールス力の影響を避けるために80nmに設定された。
【0045】
図7はコンピュータに表示された磁気記録媒体18の磁気像である。走査対象は20μm×20μmの領域で、磁気トラックの間隔は1.5μmである。このように、本発明のナノチューブプローブ16によって、表面磁気構造が詳細に現出できることが分かった。逆に、このナノチューブプローブ16を用いて磁気記録媒体に対し磁気情報を書き込むこともできる。図示しない電子装置によりNi超微粒子6に磁気信号を与えながら磁気記録媒体表面を走査すると、次々と磁気信号が書き込まれて行くことになる。
【0046】
図8はナノチューブ8をホルダーに固定する他の方法を示す工程図である。この場合、ホルダーはピラミッド14であり、ナノチューブ8とカンチレバー12間に電源22を介して電流を流し、基端部8aを融着部8bに変成させてピラミッドに固定する。
【0047】
図9は更に他の固定方法を示す工程図である。電子顕微鏡内には不純物として炭素化合物が含まれている。従って、ナノチューブ近傍を電子ビーム16により照射すると炭素化合物が分解し、ナノチューブ8の基端部8a上に炭素皮膜であるコーティング膜24が堆積形成される。このコーティング膜24によりカーボンナノチューブ8はピラミッド14に強固に固定される。コーティング膜24の形成方法には、上記方法以外に物理蒸着法や化学蒸着法(CVD法)などの公知の各種方法が利用できる。このコーティング膜法では、カーボンナノチューブ8の先端部上にもコーティング膜を形成できるから、カーボンナノチューブ8を太くすることによって共振を抑制でき、精度向上の効果を有する。
【0048】
図10は本発明に係る前記ナノチューブプローブ16を原子間力顕微鏡(AFM)
に適用した構成図である。ナノチューブプローブ16の先端にある超微粒子が試料面に当接し、試料表面情報を正確に読み取ることができる。このナノチューブプローブ16は図示しないホルダーセット部に着脱自在に固定される。探針の交換時にはプローブ16の全体が交換される。この場合に、探針はセンサー部付きナノチューブである。試料26はピエゾ素子からなる走査駆動部28によりXYZ方向に駆動される。30は半導体レーザー装置、32は反射ミラー、33は二分割光検出器、34はXYZ走査回路、35はAFM表示装置、36はZ軸検出回路である。
【0049】
試料26をナノチューブプローブ16に対し所定の斥力位置になるまでZ軸方向に接近させ、その後、Z位置を固定した状態で走査回路34で走査駆動部28をXY方向に走査する。このとき、表面原子の凹凸でカンチレバー12が撓み、反射したレーザービームLBが二分割光検出器33に位置変位して入射する。上下の検出器33a、33bの光検出量の差からZ軸方向の変位量をZ軸検出回路36で算出し、この変位量を原子の凹凸量としてAFM表示装置35に表面原子像を表示する。この装置では、試料26をXYZ走査する構成にしているが、プローブ16をXYZ走査しても構わない。
【0050】
図11は本発明に係るナノチューブプローブを適用した走査型トンネル顕微鏡(STM)の構成図である。超微粒子付きナノチューブ10を探針として平板状のホルダー15に固着してナノチューブプローブ16を構成する。固定法は融着法、コーティング膜法またその他方法でもよい。このホルダー15をホルダーセット部17の切り溝17aに嵌合してバネ圧で着脱自在に固定する。Xピエゾ28x、Yピエゾ28y、Zピエゾ28zからなる走査駆動部28はホルダーセット部17をXYZの3次元方向に伸縮走査してナノチューブプローブ16の試料26に対する走査を実現する。37はバイアス電源、38はトンネル電流検出回路、39はZ軸制御回路、40はSTM表示装置、41はXY走査回路である。
【0051】
各XY位置においてトンネル電流が一定になるようにZ軸制御回路でナノチューブプローブ16をZ方向に伸縮制御し、この移動量がZ軸方向の凹凸量になる。ナノチューブプローブ16をXY走査するに従いSTM表示装置40に試料26の表面原子像が表示される。本発明ではナノチューブプローブを交換する場合には、ホルダー15をホルダーセット部17から取り外してプローブ16として一体で交換する。
【0052】
図12はC60というフラーレンの拡大図である。このフラーレンは12個の五角形と20個の六角形から構成され、五角形は相互に隣接しないと云う孤立五員環則が成立している。更に大きなフラーレンでは六角形の数が増大することが分かっている。このフラーレンをセンサー部としてナノチューブの先端に固定すれば、高分解能を有したナノチューブプローブを形成できる。
【0053】
図13(A)〜(B)はフラーレンをセンサー部としたナノチューブプローブの製造工程図である。工程(A)のナノチューブ8は、CNT系ナノチューブ、BCN系ナノチューブ、BN系ナノチューブ等のいずれのナノチューブであってもよい。工程(B)でナノチューブ8の所要部、主には先端部を切断する。工程(C)で、切断面8cにフラーレン7をファンデルワールス力で接着させて、フラーレン付きナノチューブ11を形成する。この接着を強力にするために、電子ビーム照射や電流加熱により両者を結合部で融着させることもできる。
【0054】
図14はフラーレン付きナノチューブの他の形成方法を示している。ナノチューブ8の先端は通常は閉じており、この閉口した先端面において、光励起や触媒などを利用してその二重結合を開く。同様にフラーレンの二重結合も開き、両者の結合の手を結ぱせることによって、フラーレン付きナノチューブ11を形成できる。この方法は先端が開口したナノチューブに対しても適用できる。ここで開口したとは、切断して開口させた場合と、自然状態で開口している場合の両者を含む。
【0055】
このフラーレン付きナノチューブ11の基端部を図示しないホルダーに固定して、ナノチューブプローブを構成できる。固定方法には前述したコーティング膜法や融着法などが利用できる。このようにすれば、ナノチューブ8の太さや構造が多少変わっても、フラーレン7さえ同一の構造であれば、同一の対象表面からは常に同一の信号を高精度に再現することができる。
【0056】
本発明は上記実施例に限定されるものではなく、本発明の技術的思想を逸脱しない範囲における種々の変形例、設計変更などをその技術的範囲内に包含するものである。
【0057】
【発明の効果】
請求項1の発明によれば、新規な構造のナノチューブを提供でき、各種の物質表面に感応するナノチューブを提供できる。
請求項2の発明によれば、特定構造の超微粒子をセンサー部として利用でき、ナノチューブの異同に関係なく、高精度に物質表面に感応するナノチューブを提供できる。
請求項3の発明によれば、対象物質の磁気構造に感応するナノチューブを提供でき、また対象物質に磁気書き込みできるナノチューブ提供できる。
請求項4の発明によれば、特定構造のフラーレンをセンサー部として利用でき、ナノチューブの異同に関係なく、高精度に物質表面に感応するナノチューブを提供できる。
請求項5の発明によれば、金属超微粒子を先端に形成したカーボンナノチューブを安価に量産することができる。
請求項6及び7の発明によれば、フラーレンを先端に形成したナノチューブを安価に量産することができる。
【0058】
請求項8の発明によれば、センサー部をナノチューブ先端に固定するから、ナノチューブの異同に関係なく、高精度に物質の表面情報を入出力したり、操作できるナノチューブプローブを提供できる。
請求項9の発明によれば、センサー部が超微粒子であるから、同一構造の超微粒子を用いて対象物質の表面情報を読みとり、また書き込んだりできるナノチューブプローブを提供できる。
請求項10の発明によれば、強磁性金属超微粒子を用いることにより、対象物質の表面磁気情報を読み取ったり、また磁気情報を書き込んだりできるナノチューブプローブを提供できる。
【0059】
請求項11の発明によれば、大量に存するフラーレンを活用して、安価にしかも大量に高分解能のナノチューブプローブを提供できる。
請求項12の発明によれば、超微粒子をセンサー部とするナノチューブプローブを安価にしかも大量に量産できる製造方法を提供できる。
請求項13の発明によれば、フラーレンをセンサー部とするナノチューブプローブを安価にしかも大量に量産できる製造方法を提供できる。
【図面の簡単な説明】
【図1】図1(A)〜(D)は超微粒子付きカーボンナノチューブの形成方法の工程図である。
【図2】図2は超微粒子付きカーボンナノチューブの断面図である。
【図3】図3は超微粒子付きカーボンナノチューブをホルダーの一種であるAFM用カンチレバーのピラミッドに転移させる工程図である。
【図4】図4は超微粒子付きカーボンナノチューブをピラミッドに強固に固定する工程図である。
【図5】図5はNi超微粒子の磁化工程図である。
【図6】図6は高分解能磁気検出用のナノチューブプローブの使用状態図である。
【図7】図7はコンピュータに表示された磁気記録媒体の磁気像である。
【図8】図8はナノチューブをホルダーに電流により熱融着固定する工程図である。
【図9】図9はコーティング膜による固定方法を示す工程図である。
【図10】図10は本発明に係るナノチューブプローブを原子間力顕微鏡(AFM)に適用した構成図である。
【図11】図11は本発明に係るナノチューブプローブを走査型トンネル顕微鏡(STM)に適用した構成図である。
【図12】図12はC60というフラーレンの拡大図である。
【図13】図13(A)〜(B)はフラーレンをセンサー部としたナノチューブプローブの製造工程図である。
【図14】図14は他の製造方法によるフラーレン付きナノチューブの構成図である。
【図15】図15は従来のシリコン製のAFM用カンチレバーの概念図である。
【図16】図16は従来考えられた磁気プローブの説明図である。
【図17】図17はこの従来磁気プローブで対象物質の磁気情報を検出する場合の説明図である。
【符号の説明】
2は酸化膜を表面に持つシリコン基板、4は金属膜、6は超微粒子、7はフラーレン、8はナノチューブ又はカーボンナノチューブ、8aは基端部、8bは融着部、8cは切断面、10は超微粒子付きカーボンナノチューブ、11はフラーレン付きナノチューブ、12はAFM用カンチレバー、14はピラミッド、15はホルダー、16はナノチューブプローブ、17はホルダーセット部、17aは切り溝、18は磁気記録媒体、20は磁気情報、22は電源、24はコーティング膜、28は走査駆動部、28xはXピエゾ、28yはYピエゾ、28zはZピエゾ、30は半導体レーザー装置、32は反射ミラー、33は2分割光検出器、34はXYZ走査回路、35はAFM表示装置、36はZ軸検出回路、37はバイアス電源、38はトンネル電流検出回路、39はZ軸制御回路、40はSTM表示装置、41はXY走査回路、50はカンチレバー、52はサブストレート、54はピラミッド状探針、56は先鋭部、58は金属膜、60は磁気的ドメイン、62は対象物質、LBはレーザービームである。[0001]
BACKGROUND OF THE INVENTION
The present invention relates to a nanotube probe for manipulating a surface signal of a substance using a nanotube such as a carbon nanotube, a BCN-based nanotube, or a BN-based nanotube as a probe. The present invention relates to a nanotube probe capable of manipulating a surface signal of a substance with high reproducibility and high resolution by a sensor unit having a predetermined structure.
[0002]
[Prior art]
Conventionally, there has been an electron microscope as a microscope for observing the surface of a sample at a high magnification. However, since the electron beam does not fly unless it is in a vacuum, there are various problems in the experimental technique. However, in recent years, a scanning probe microscope technique that can observe the surface at an atomic level even in the atmosphere has been developed. When the probe at the tip of the probe is brought close to the sample surface to the atomic size, the physical and chemical action from each sample atom is detected by the probe, and the detection signal is detected while scanning the probe on the surface. It is the microscope which makes the sample surface image appear from.
[0003]
Among these microscopes, a scanning tunnel microscope (abbreviated as STM) and an atomic force microscope (abbreviated as AFM) are particularly frequently used. In STM, a conductive probe such as a polished metal needle is used. In AFM, a surface signal is detected using a cantilever having a silicon pyramid as a probe. A problem common to them is that the fine structure at the atomic level of the material surface cannot be detected with high resolution because the tip of the probe cannot be sharpened.
[0004]
For example, FIG. 15 shows a conventional silicon AFM cantilever. The back of the
[0005]
In recent years, an idea to use carbon nanotubes as a probe has appeared. Since carbon nanotubes are conductive, they can be used not only for STM for detecting tunneling current but also for AFM for detecting atomic force. J. et al. Am. Chem. Soc. 120 (1998), page 603, a carbon nanotube probe has been proposed as a high-resolution probe for imaging biological systems. However, how to collect only the carbon nanotubes from the carbon mixture and how to fix the carbon nanotubes to the holder have not yet been solved.
[0006]
Although the field is different from the probe microscope field, in recent years, as the memory capacity of a computer increases, the memory device is evolving from a floppy disk device to a hard disk device and further to a high-density disk device. If information is packed in a small space at a higher density, the size per one information becomes smaller, and thus a finer probe for input / output is required. In the conventional magnetic head device, it was impossible to make it smaller than a certain value. There has also been a demand for miniaturization of input / output probes for electronic devices such as CD devices.
[0007]
As an alternative to this magnetic head, the magnetic probe shown in FIG. 16 has been considered. This magnetic probe is configured by forming a
[0008]
FIG. 17 is an explanatory diagram when the magnetic information of the target substance is detected by this magnetic probe. When this magnetic probe is brought close to the surface of the
[0009]
Therefore, it is naturally considered to use the above-described carbon nanotube as the magnetic probe. However, the technology of how to support the ferromagnetic material on the carbon nanotube has not yet been established. Furthermore, the carbon nanotube refining technology and the immobilization technology to the holder are completely unsolved as described above.
[0010]
The inventors have filed three patent applications that provide solutions to the miniaturization technology among these problems. That is, Japanese Patent Application No. 10-280431 provides a method for purifying nanotubes by electrophoresis, Japanese Patent Application No. 10-376642 proposes a technique for immobilizing nanotubes with a coating film, and Japanese Patent Application No. 10-378548 is a thermal process. We have completed the technology for fixing nanotubes by fusion.
[0011]
[Problems to be solved by the invention]
While the present inventors are further researching the nanotube probe, when the nanotube is applied to an STM, AFM, magnetic probe, etc. using the nanotube as a probe, the signal obtained for the same material surface varies depending on the nanotube used. I noticed there was a flaw. This means that the physical structure or electronic structure of the tip of the nanotube that senses the surface signal is different for each nanotube. In other words, the sizes of the nanotubes used are different. Nanotubes are selected and fixed to the holder in the electron microscope, but it is difficult to determine whether the nanotubes have the same structure including size and electronic structure from the electron microscope image.
[0012]
Accordingly, a first object of the present invention is to provide a nanotube having the same physical structure and electronic structure at the tip and a method for producing the same.
The second object of the present invention is to provide a nanotube probe capable of reproducing the surface information of the target substance with high accuracy by fixing the nanotubes having the same tip part to a holder.
[0013]
[Means for Solving the Problems]
The present invention has been made to achieve the above objects and objects.
The invention of claim 1 is a nanotube characterized in that a sensor portion is provided at the tip of the nanotube.
According to a second aspect of the present invention, the sensor unit is a nanoparticle nanotube.
According to a third aspect of the present invention, the ultrafine particles are ferromagnetic metal nanoparticle nanotubes.
According to a fourth aspect of the present invention, the sensor unit is a fullerene nanotube.
[0014]
In the invention of claim 5, a metal thin film is formed on a substrate, the metal thin film is heated to form ultrafine metal particles, and the carbon compound gas is decomposed by heating while flowing a carbon compound gas over the ultrafine metal particles. The method for producing a nanotube is characterized in that a carbon component forms a carbon nanotube at its root while pushing up ultrafine particles.
The invention according to
The invention according to claim 7 is a method for producing a nanotube in which fullerene is bonded to the closed or opened end face of the nanotube.
[0015]
The invention according to
According to a ninth aspect of the present invention, the sensor unit is an ultrafine particle nanotube probe.
The invention of
In the invention of
According to a twelfth aspect of the present invention, there is provided a method for producing a nanotube probe, wherein the base end portion of the nanotube formed according to the fifth aspect is fixed to a holder.
A thirteenth aspect of the present invention is a method for manufacturing a nanotube probe, characterized in that the base end portion of the nanotube formed according to the sixth or seventh aspect is fixed to a holder.
[0016]
DETAILED DESCRIPTION OF THE INVENTION
As a result of diligent research in order to make the physical structure and electronic structure of the tip of the nanotube probe the same, the inventors have formed a nanotube structure by separately forming a sensor part with a fixed size and structure at the tip of the nanotube. As a result, we have completed a technology that can guarantee the identity of the sensor unit even if it fluctuates slightly. As long as the sensor parts are the same, the material structure and the electronic structure are the same, and the surface information of the target material can be reproduced with high accuracy.
[0017]
The present inventors have reached the recognition that ultrafine particles or fullerene, which is a soccer ball-like substance, is suitable as a sensor unit having a predetermined size and material structure.
[0018]
An ultrafine particle refers to a cluster-like atomic group having a particle size of several tens of nm or less, and various types of ultrafine particles such as metal ultrafine particles, metal oxide ultrafine particles, silicon ultrafine particles, and SiC ultrafine particles are manufactured. It has been found that, depending on the production method and production conditions, ultrafine particles having various particle sizes can be produced in a single crystal form or a polycrystalline form having a strong single crystallinity. Therefore, if the production method and conditions are specified, ultrafine particles having a specific particle diameter having the same electronic structure and a single domain can be produced. By fixing the ultrafine particles of this specific structure to the tip of the nanotube, it is possible to read the surface information of the target substance with the ultrafine particles and write information on the target substance surface with high reproducibility. .
[0019]
The ultrafine particle nanotube probe can be used as a probe probe for a conventional probe microscope such as a scanning tunnel microscope, an atomic force microscope, a friction force microscope, a magnetic force microscope, or a chemical force microscope. If the ultrafine particles for detecting a specific physical and chemical action are fixed to the tip of the nanotube according to each application, the physical and chemical surface information of the target substance can be obtained.
[0020]
For example, if ferromagnetic metal ultrafine particles such as Fe, Co, and Ni are used as ultrafine particles, the magnetic surface structure can be read because the magnetism on the surface of the target substance is sensed. On the other hand, if this ferromagnetic metal ultrafine particle is used as a magnetic head, magnetic information can be written on the surface of the target material, and an input / output probe can be obtained. The unit size of magnetic information that can be input and output depends on the size of the ultrafine particles, and can be reduced to several nm or less, and further to 1 nm or less, and it is possible to achieve ultrahigh density.
In this way, the ultrafine particles are extremely small and are effective in measuring the magnetic properties of a minute object. For example, for measuring magnetic properties in living cells, Fe 2 O 3 Or Fe 2 O 4 The ultrafine particles of iron oxide can be used, and the measurement position in the cell can be finely adjusted freely by using a nanotube probe.
[0021]
If ultrafine particles having a catalytic action are used as the sensor part, the nanotube probe can be used as a catalyst probe. For example, Ni ultrafine particles can be used as a hydrogenation catalyst for 1,3-cyclooctadiene, and Cu-ZnO ultrafine particles can be used as a methanol synthesis catalyst. Rather than simply disperse and arrange these ultrafine particles as powder, the catalyst arrangement can be adjusted accurately and the catalyst efficiency can be enhanced by fixing to the nanotubes. It can also be used as a probe for catalytic reaction measurement.
[0022]
There are currently two methods for fixing ultrafine particles to the tips of nanotubes. The first is a method in which nanotubes and ultrafine particles are produced separately, and the ultrafine particles are brought very close to the front end surface of the nanotube or a cut surface obtained by cutting the front end and bonded by atomic force. Alternatively, there is a method in which a double bond between the tip surface and the cut surface of the nanotube is opened by light irradiation, a chemical reaction, etc., and ultrafine particles are chemically bonded to the bond. The bonding can be strengthened by fusing by irradiating the bonding portion with an electron beam or laser beam. These series of operations can be performed while directly observing in an electron microscope.
The second is a method of crystal growth of nanotubes and ultrafine particles simultaneously or before and after. Various methods such as chemical vapor deposition (CVD) used in semiconductor technology can be used for this method. For example, when ultrafine particles are grown on a substrate and then a carbon compound gas is circulated in the vicinity of the surface, carbon molecules grow at the root of the ultrafine particles by thermal decomposition and grow as carbon nanotubes. It will carry fine particles.
[0023]
Fullerene can be used as the sensor unit. Fullerene is a generic name for soccer ball-like materials, ie, spherical shell molecules. In 1985, the first C in the steam-cooled material obtained by irradiating graphite with a high-energy laser. 60 Was discovered. At present, higher fullerenes having 70 to 100 atoms and larger fullerenes having more than 70 atoms have been discovered, and their synthesis methods have also been established. These fullerenes are carbon sp 2 It is composed of a five-membered ring and a six-membered ring created by orbits, and some of them contain seven-membered rings.
[0024]
When fullerene is theoretically considered as a figure, Euler's polyhedral theorem shows that 12 five-membered rings are included and the six-membered ring varies with the number of all atoms. Moreover, it is thought that the isolated five-membered ring rule that 12 five-membered rings are not adjacent is satisfied mathematically. Considering these mathematical rules, the higher fullerenes have C 70 , C 76 , C 78 Etc., and the giant fullerene is C 240 , C 540 , C 960 Etc. exist. Their existence has also been confirmed experimentally.
[0025]
It has been confirmed that fullerenes are contained in large amounts in carbon soot. Accordingly, the method for producing fullerene having a specific structure comprises a method for producing soot and a method for separating specific fullerene from soot. The fullerene soot production method includes a resistance heating method and an arc discharge method, and a direct current arc discharge method is often used. That is, when a DC voltage is applied between the graphite electrodes to cause arc discharge, fullerenes having various carbon numbers are mixed in the generated soot. The soot is then separated by chromatographic techniques. In particular, fullerene having a specific number of carbon atoms can be easily separated by using liquid chromatography or column chromatography.
[0026]
For example, by performing high performance liquid chromatography using a polystyrene column and developing solution as benzene or carbon disulfide, C 76 , C 78 , C 82 , C 84 , C 90 , C 96 And fullerenes can be separated. It can be considered that fullerenes having a predetermined number of atoms have the same electronic structure except for isomers. Recently, it has also become possible to separate fullerenes of the same size into structural isomers. If it goes to this stage, the fullerene of the specific structure with the same electronic state can be manufactured in large quantities. By fixing the fullerene of this size and structure to the tip of the nanotube, the surface structure of the target substance can be read with high accuracy and reproducibility regardless of the difference in the nanotube, and information can be written on the target surface. become.
[0027]
A fullerene containing a metal can also be produced. For example, graphite powder and metal oxide are mixed at an appropriate ratio, and graphite cement is added to this mixture to form a rod-shaped electrode. When this rod-shaped electrode is slowly heated in an argon atmosphere and finally heated at 1200 ° C. for about 10 hours, the electrode is completed. Using this electrode, arc discharge is performed, and the obtained soot is extracted with a solvent to separate fullerene having a specific structure. A metal atom is confined in the fullerene. Examples of the metal atom include La, Y, and Sc. By changing the metal oxide, a desired metal atom can be included in the fullerene.
[0028]
There are the following methods for fixing the fullerene having the specific structure to the nanotube. First, nanotubes and fullerenes are produced separately. Next, the tip of the nanotube is cut, and fullerene is brought close to the cut surface and bonded by atomic force. The coupling can be strengthened by irradiating the coupling portion with an electron beam or a laser beam. These series of operations are performed while actually observing in an electron microscope.
[0029]
The completed nanotubes can reproduce the same signal with high accuracy from the same target surface because the sensor part that observes the material surface is a fullerene with a specific structure even if the nanotubes have some size variation. it can. Therefore, it is possible to provide a nanotube probe that can measure and manipulate a material surface with high accuracy without being affected by variations in the structure of the nanotube.
[0030]
The fullerene nanotube probe can be used as a probe probe for a conventional probe microscope such as a scanning tunnel microscope, an atomic force microscope, a friction force microscope, a magnetic force microscope, or a chemical force microscope. If a fullerene for detecting a specific physical / chemical action is fixed to the tip of the nanotube according to each application, physical / chemical surface information of the target substance can be obtained.
[0031]
Further, if atoms for detecting specific physical / chemical information are included in fullerene, and the atomic-encapsulated fullerene is fixed to the nanotube, the specific information on the target surface can be detected. For example, when a ferromagnetic metal atom such as Fe, Co, or Ni is included, the magnetic structure of the target surface can be detected as in the case of the ultrafine particles described above. Conversely, if the surface of the target substance is a magnetic recording medium, specific information can be written using this fullerene nanotube probe.
[0032]
The nanotubes used in the present invention are nanotubes such as carbon nanotubes, BCN-based nanotubes, and BN-based nanotubes. Among them, carbon nanotubes (hereinafter also referred to as CNT) were first discovered. Conventionally, diamond, graphite, and amorphous carbon have been known as stable allotropes of carbon. However, in 1991, the presence of cylindrical carbon nanotubes was recognized in the cathode deposit produced by DC arc discharge.
[0033]
Based on the discovery of this carbon nanotube, a BCN-based nanotube was synthesized. For example, a mixed powder of amorphous boron and graphite is packed in a graphite rod and evaporated in nitrogen gas. Further, the sintered BN bar is packed in a graphite bar and evaporated in helium gas. In addition, BC 4 Arc discharge is performed in helium gas using N as an anode and graphite as a cathode. By these methods, a BCN-based nanotube in which C atoms in the carbon nanotube are partially substituted with B atoms and N atoms is synthesized, or a multi-layer nanotube in which the BN layer and the C layer are concentrically laminated is synthesized.
[0034]
Very recently, BN-based nanotubes have been synthesized. This is a nanotube containing almost no C atoms. For example, carbon nanotubes and B 2 O 3 Place the powder in a crucible and heat in nitrogen gas. As a result, most of the C atoms in the carbon nanotube can be converted into a BN nanotube in which B atoms and N atoms are substituted. Of course, various other nanotubes can be used.
[0035]
There are two methods for producing the nanotube probes of the present invention. The first method is to fix the sensor part to the nanotube, and then fix the base end part of the nanotube with the sensor part to the holder. The second method is to fix the base end of the nanotube to the holder first, and then fix the sensor to the tip of the nanotube.
[0036]
In order to fix the nanotube to the sensor unit, the sensor unit may be fixed to the tip of the arranged nanotube (or crystal growth), or the nanotube may be fixed to the arranged sensor unit (or crystal grown). In particular, the latter includes the case of forming the nanotubes while forming the ultrafine particles and pushing up the ultrafine particles.
[0037]
There are two methods for fixing the base end of the nanotube to the holder. The first is a method in which the nanotube is transferred onto the holder surface by applying an electric field or van der Waals force, and the base end portion contacting the holder surface is covered and fixed with a coating film in a state where the tip end portion of the nanotube is projected. is there. The second is a method in which the nanotube is transferred to the holder surface by applying an electric field or van der Waals force, and the base end of the nanotube in contact with the holder surface is thermally fused to the holder surface.
[0038]
It is also possible to simultaneously form a sensor-attached nanotube and attach it to a holder. Specifically, a metal film is formed on the surface of the silicon pyramid of the cantilever, and further heated to form the metal film into ultrafine metal particles, and then carbon nanotubes are formed to push up the ultrafine metal particles by passing a carbon compound gas. To do. In this way, the sensor-equipped nanotubes are formed at once in the cantilever pyramid, and the manufacturing process can be simplified. Of the carbon compounds, hydrocarbons are preferred.
[0039]
【Example】
[Example 1: Formation of nanotube with ultrafine particles]
1A to 1D are process diagrams of a method for forming carbon nanotubes with ultrafine particles, among the nanotubes with ultrafine particles. A Ni metal film 4 having a thickness of 10 nm is formed by vapor deposition on the surface of a
[0040]
FIG. 2 is a cross-sectional view of the
[0041]
FIG. 3 is a process diagram for transferring the
[0042]
FIG. 4 is a process diagram for fixing the
[0043]
FIG. 5 is a magnetization process diagram of the Ni
[0044]
FIG. 6 is a use state diagram of a nanotube probe for high-resolution magnetic detection, and the surface
[0045]
FIG. 7 is a magnetic image of the
[0046]
FIG. 8 is a process diagram showing another method for fixing the
[0047]
FIG. 9 is a process diagram showing still another fixing method. The electron microscope contains a carbon compound as an impurity. Therefore, when the vicinity of the nanotube is irradiated with the
[0048]
FIG. 10 shows an atomic force microscope (AFM) for the
It is the block diagram applied to. Ultrafine particles at the tip of the
[0049]
The
[0050]
FIG. 11 is a configuration diagram of a scanning tunneling microscope (STM) to which the nanotube probe according to the present invention is applied. A
[0051]
The Z-axis control circuit controls the expansion and contraction of the
[0052]
FIG. 12 shows C 60 It is an enlarged view of fullerene. This fullerene is composed of 12 pentagons and 20 hexagons, and the isolated five-membered ring rule is established that the pentagons are not adjacent to each other. Larger fullerenes have been found to increase the number of hexagons. If this fullerene is fixed to the tip of the nanotube as a sensor part, a nanotube probe with high resolution can be formed.
[0053]
FIGS. 13A to 13B are manufacturing process diagrams of a nanotube probe using fullerene as a sensor part. The
[0054]
FIG. 14 shows another method for forming fullerene-attached nanotubes. The tip of the
[0055]
A nanotube probe can be constructed by fixing the base end of the fullerene-attached
[0056]
The present invention is not limited to the above embodiments, and includes various modifications, design changes, and the like within the technical scope without departing from the technical idea of the present invention.
[0057]
【The invention's effect】
According to the first aspect of the present invention, a nanotube having a novel structure can be provided, and a nanotube sensitive to the surface of various substances can be provided.
According to the invention of
According to the invention of claim 3, it is possible to provide a nanotube that is sensitive to the magnetic structure of the target substance, and to provide a nanotube that can be magnetically written to the target substance.
According to the invention of claim 4, fullerene having a specific structure can be used as a sensor part, and a nanotube sensitive to the surface of a substance can be provided with high accuracy regardless of the difference in nanotube.
According to the invention of claim 5, it is possible to mass-produce carbon nanotubes formed with metal ultrafine particles at the tip at low cost.
According to the inventions of
[0058]
According to the invention of
According to the ninth aspect of the present invention, since the sensor portion is an ultrafine particle, it is possible to provide a nanotube probe that can read and write surface information of a target substance using ultrafine particles having the same structure.
According to the invention of
[0059]
According to the invention of
According to the twelfth aspect of the present invention, it is possible to provide a manufacturing method capable of mass-producing nanotube probes having ultrafine particles as sensor portions at low cost.
According to the invention of claim 13, it is possible to provide a manufacturing method capable of mass-producing a nanotube probe using fullerene as a sensor part at a low cost.
[Brief description of the drawings]
FIG. 1A to FIG. 1D are process diagrams of a method for forming carbon nanotubes with ultrafine particles.
FIG. 2 is a cross-sectional view of a carbon nanotube with ultrafine particles.
FIG. 3 is a process diagram for transferring carbon nanotubes with ultrafine particles to a pyramid of an AFM cantilever which is a kind of holder.
FIG. 4 is a process diagram for firmly fixing a carbon nanotube with ultrafine particles to a pyramid.
FIG. 5 is a magnetization process diagram of Ni ultrafine particles.
FIG. 6 is a use state diagram of a nanotube probe for high resolution magnetic detection.
FIG. 7 is a magnetic image of a magnetic recording medium displayed on a computer.
FIG. 8 is a process diagram for fixing a nanotube to a holder by heat fusion with an electric current.
FIG. 9 is a process diagram showing a fixing method using a coating film.
FIG. 10 is a configuration diagram in which a nanotube probe according to the present invention is applied to an atomic force microscope (AFM).
FIG. 11 is a configuration diagram in which the nanotube probe according to the present invention is applied to a scanning tunneling microscope (STM).
FIG. 12 is an enlarged view of C60 fullerene.
FIGS. 13A to 13B are manufacturing process diagrams of a nanotube probe using fullerene as a sensor part.
FIG. 14 is a configuration diagram of fullerene-attached nanotubes produced by another manufacturing method.
FIG. 15 is a conceptual diagram of a conventional silicon AFM cantilever.
FIG. 16 is an explanatory diagram of a conventionally considered magnetic probe.
FIG. 17 is an explanatory diagram when magnetic information of a target substance is detected by this conventional magnetic probe.
[Explanation of symbols]
2 is a silicon substrate having an oxide film on the surface, 4 is a metal film, 6 is ultrafine particles, 7 is fullerene, 8 is a nanotube or carbon nanotube, 8 a is a base end, 8 b is a fused portion, 8 c is a cut surface, 10 Is a carbon nanotube with ultrafine particles, 11 is a nanotube with fullerene, 12 is a cantilever for AFM, 14 is a pyramid, 15 is a holder, 16 is a nanotube probe, 17 is a holder set portion, 17 a is a groove, 18 is a magnetic recording medium, 20 Is a magnetic information, 22 is a power supply, 24 is a coating film, 28 is a scanning drive unit, 28x is an X piezo, 28y is a Y piezo, 28z is a Z piezo, 30 is a semiconductor laser device, 32 is a reflection mirror, and 33 is a split light. Detector, 34 is an XYZ scanning circuit, 35 is an AFM display device, 36 is a Z-axis detection circuit, 37 is a bias power supply, and 38 is a top Channel current detection circuit, 39 is a Z-axis control circuit, 40 is an STM display device, 41 is an XY scanning circuit, 50 is a cantilever, 52 is a substrate, 54 is a pyramidal probe, 56 is a sharpened portion, 58 is a metal film,
Claims (5)