FI119943B - For forming a paper or board machine - Google Patents
For forming a paper or board machine Download PDFInfo
- Publication number
- FI119943B FI119943B FI20055212A FI20055212A FI119943B FI 119943 B FI119943 B FI 119943B FI 20055212 A FI20055212 A FI 20055212A FI 20055212 A FI20055212 A FI 20055212A FI 119943 B FI119943 B FI 119943B
- Authority
- FI
- Finland
- Prior art keywords
- wire
- web
- forming unit
- web forming
- unit according
- Prior art date
Description
Paperi- tai kartonkikoneen rainanmuodostusyksikköPaper or board forming machine forming unit
Keksinnön kohteena on paperi- tai kartonkikoneen rainanmuodostusyksikkö, joka 5 käsittää perälaatikon ja viiran, joka on sovitettu liukumaan perälaatikon ensimmäisen ja toisen liukupinnan yli, joiden välissä sijaitsee perälaatikon huuliaukko, ja jossa viira ja toinen liukupinta rajaavat väliinsä muodostusalueen, joka ottaa vastaan huuliaukosta syötettävän massasuspensiovirtauksen.The invention relates to a paper or board machine web forming unit comprising a headbox and a wire adapted to slide over the first and second sliding surfaces of the headbox, between which the lip opening of the headbox is disposed, and the wire and the second sliding surface delimiting the forming area.
10 Keksinnön kohteena on myös menetelmä monikerrosrainan valmistamiseksi, jossa menetelmässä muodostetaan ainakin kaksi rainan kerrosta erillisissä rainanmuo-dostusyksiköissä ja liitetään erikseen muodostetut kerrokset toisiinsa.The invention also relates to a method of producing a multilayer web, comprising forming at least two web layers in separate web forming units and joining the separately formed layers to one another.
Julkaisu US 4,308,097 kuvaa rainanmuodostusyksikön, joka käsittää kaarevan 15 puristuskengän, jossa on liukupinta ja siinä syöttöaukko kuitususpension syöttämiseksi liukupinnalle, sekä viiran ja välineet viiran liuottamiseksi liukupinnan ohi. Syöttöaukosta alavirtaan oleva liukupinnan osa on pienen välimatkan päässä ohitse liukuvasta viirasta ja syöttöaukosta ylävirtaan oleva liukupinnan osa ulottuu syöttöaukon kohdalla lähemmäs viiraa kuin alavirtaan oleva osa. Viira ja syöttö-20 aukosta alavirtaan oleva liukupinnan osa rajaavat väliinsä kiilamaisesti suppenevan muodostusalueen. Kompaktin ja pieneen tilaan mahtuvan rakenteen aikaansaamiseksi syöttökanavassa on juuri ennen syöttöaukkoa jyrkkä mutka, jonka seurauksena virtauksella on syöttöaukon kohdalla pienempi kaarevuussäde kuin sitä seuraavalla muodostusalueella. Tällöin on vaarana, että suurilla ajonopeuksilla 25 muodostusalueella syntyy päävirtauksen suuntaan nähden poikittaisia sekundääri-virtauksia. Ne voivat johtaa epähomogeeniseen kuitujakautumaan ja äärimmäisissä tapauksissa kavitaatioon. Saman patentinhaltijan myöhemmässä patentissa US 4,416,730 nämä ongelmat on ratkaistu siirtämällä syöttöaukosta ylävirtaan oleva liukupinta viiran vastakkaiselle puolelle, jolloin syöttökanavasta on voitu tehdä 30 lineaarinen. Samalla on kuitenkin menetetty alkuperäisen ratkaisun etuna ollut kompakti rakenne sekä täysin suljettuja tuettu virtaus.US 4,308,097 discloses a web forming unit comprising a curved press shoe 15 having a sliding surface and an inlet for feeding a fiber suspension to the sliding surface, and a wire and means for dissolving the wire past the sliding surface. The portion of the sliding surface downstream of the inlet is at a short distance from the sliding wire and the portion of the sliding surface upstream of the inlet extends closer to the wire than the portion downstream of the inlet. The wire and a portion of the sliding surface downstream of the feed 20 orifice define a wedge-tapered forming area therebetween. In order to provide a compact and compact space structure, the feed channel has a steep bend just before the inlet, as a result of which the flow has a smaller radius of curvature at the inlet than in the subsequent forming region. There is a risk that, at high travel speeds 25, secondary currents transverse to the direction of the main flow will be generated. They can lead to inhomogeneous fiber distribution and, in extreme cases, cavitation. In later patent US 4,416,730 by the same patentee, these problems are solved by moving the sliding surface upstream of the inlet to the opposite side of the wire, whereby the inlet can be made linear. At the same time, however, the compact design that was the advantage of the original solution, as well as the fully enclosed supported flow, are lost.
22
Syöttöaukkoa edeltävän jyrkän mutkan vuoksi julkaisun US 4,308,097 perälaatik-ko ei kovin hyvin sovellu suursakeusmassoille. Julkaisussa US 3,846,230 opetetaan, että suursakeusmassan turbulenssin tulisi antaa vaimentua perälaatikon syöt-tökanavassa ennen kuin massa syötetään viiralle. Tätä varten suursakeusperälaa-5 tikko tulee varustaa niin pitkällä syöttökanavalla, että kuitupartikkelit ehtivät muodostaa lujan kolmiulotteisen verkkorakenteen ennen kuiturainan saostamista viiralle.Due to the steep bend before the inlet, the headbox of US 4,308,097 is not very suitable for high consistency masses. US 3,846,230 teaches that turbulence of high consistency pulp should be allowed to dampen in the headbox feed channel before the pulp is fed to the wire. For this purpose, the high-consistency stern-5 needle should be provided with such a long feed channel that the fiber particles can form a solid three-dimensional mesh structure before the fiber web is deposited on the wire.
Julkaisusta WO 00/52261 tunnetaan alussa esitettyä tyyppiä oleva rainanmuodos-10 tusyksikkö, joka on tarkoitettu suursakeusmassoille. Perälaatikko painetaan viiraa vasten ja massasuspensio syötetään perälaatikon huuliaukosta muodostusalueelle, joka rajoittuu pidennetyn ylähuulen ja sen yli liukuvan viiran väliin. Huulisuihku on avoin, sillä alahuulen ja viiran välinen kontakti päättyy ennen kohtaa, jossa massasuspensiosuihku osuu viiraan. Tyhjä tila alahuulen kärjen ja huulisuihkun 15 iskeytymiskohdan välissä synnyttää helposti ylimääräisiä pyörrevirtauksia.WO 00/52261 discloses a web forming unit of the type disclosed above for high consistency masses. The headbox is pressed against the wire and a pulp suspension is introduced from the lip opening of the headbox into the forming region bordering the elongated upper lip and the wire sliding over it. The lip shower is open since the contact between the lower lip and the wire ends before the point where the pulp suspension spray hits the wire. The empty space between the lower lip tip and the lip jet 15 impact points easily generates additional eddy currents.
Tunnetuissa ratkaisuissa on ongelmana, että suurilla massan syöttöpaineilla on vaarana, että viira irtoaa liukupinnan ohjauksesta muodostusvyöhykkeen alueella. Toiminta häiriintyy ja rainan rakenne kärsii, jos massa pääsee virtaamaan viiran 20 kulkusuuntaan nähden vastavirtaan tai jos muodostusalueen loppuosa ei ole kunnolla tiivistetty.The known solutions have the problem that high pulp feed pressures run the risk of loosening the wire from the sliding surface control in the forming zone. Operation is disrupted and the web structure suffers if the pulp is allowed to flow upstream of the web 20 or if the rest of the forming region is not properly sealed.
Keksinnön päämääränä on ratkaista tunnettuun tekniikkaan liittyvät ongelmat. Erityisesti päämääränä on kompakti rainanmuodostusyksikkö, joka soveltuu käy-25 tettäväksi suurilla massan sakeuksilla. Lisätavoitteena on rainanmuodostusyksikkö, jota voidaan käyttää monikerrosrainan yksittäisten kerroksien tuottamiseen sakeasta massasta.The object of the invention is to solve the problems of the prior art. In particular, the object is a compact web forming unit suitable for use at high pulp consistency. A further object is a web forming unit that can be used to produce individual layers of a multilayer web from a thick pulp.
Näihin ja myöhemmin selviäviin päämääriin pääsemiseksi keksinnön mukaiselle 30 rainanmuodostusyksikölle on tunnusomaista se, mitä on esitetty patenttivaatimuksen 1 tunnusmerkkiosassa.To achieve these and later objects, the web forming unit 30 of the invention is characterized by what is stated in the characterizing part of claim 1.
33
Keksinnön mukaisessa ratkaisussa perälaatikon alueella on kaksi taivutuspistettä, joiden kohdalla viiran kulkusuunta muuttuu verrattuna sen taivutuspistettä edeltävään suoraan tai kaarevaan kulkuun. Ensimmäinen taivutuspiste voi olla esimerkiksi ensimmäisen liukupinnan jättöreunan kohdalla, jossa viiran kulkusuuntaa 5 muutetaan taivutuskuiman a verran, jonka suuruus on edullisesti 1-5°. Toinen taivutuspiste on edullisesti toisen liukupinnan jättöreunan kohdalla, jossa viiran kulkusuuntaa muutetaan taivutuskuiman β verran, jonka suuruus on edullisesti 1-8°.In the solution according to the invention, there are two bending points in the headbox region at which the direction of travel of the wire changes relative to its straight or curved passage before its bending point. The first bending point may be, for example, at the leading edge of the first sliding surface, in which the direction of movement of the wire 5 is changed by a bending angle α, preferably of the order of 1-5 °. Preferably, the second bending point is located at the trailing edge of the second sliding surface, where the direction of travel of the wire is changed by a bending temperature β of preferably 1-8 °.
Ensimmäisen taivutuspisteen kohdalla viira kiristyy ensimmäisen liukupinnan 10 jättöreunaa vasten tiivistäen muodostusalueen sisääntulon niin, että huulikanavas-ta purkautuva massasuspensio ei pääse tunkeutumaan vastavirtaan viiran ja ensimmäisen liukupinnan väliin. Toisen taivutuspisteen kohdalla viira kiristyy toisen liukupinnan jättöreunaa kohti tiivistäen muodostusalueen ulostulon niin, että paine muodostusalueella saadaan pysymään halutuissa rajoissa. Taivutuspisteet on va-15 rustettu pyöristetyllä reunalla, jolla on suhteellisen pieni kaarevuussäde.At the first bending point, the wire is tensioned against the trailing edge of the first sliding surface 10, sealing the entrance of the forming area so that the pulp suspension discharged from the lip duct cannot penetrate upstream between the wire and the first sliding surface. At the second bending point, the wire is tensioned toward the trailing edge of the second sliding surface, sealing the exit of the forming zone so that the pressure in the forming zone is maintained within the desired range. Bending points are provided with a rounded edge with a relatively small radius of curvature.
Edullisesti toinen liukupinta on kaareva siten, että sen kaarevuussäde on 200-1000 mm. Ensimmäinen liukupinta voi olla suora tai kaareva.Preferably, the second sliding surface is curved with a radius of curvature of 200-1000 mm. The first sliding surface may be straight or curved.
20 Edullisesti perälaatikon geometria on sellainen, että huulikanavasta purkautuva massasuspensiosuihku kohtaa viiran 20-70° kulmassa.Preferably, the geometry of the headbox is such that a pulp suspension jet discharging from the lip channel meets the wire at an angle of 20-70 °.
Sakeamassaperälaatikoille on tyypillistä, että massaliete ensin fluidisoidaan hyvin, minkä jälkeen turbulenssin annetaan vaimentua samalla kun estetään suurten kui-25 tuflokkien muodostuminen. Kuituflokkien muodostumisen estämiseksi huulikana-va voidaan varustaa sinänsä tunnettuun tapaan erilaisilla syvennyksillä, ulokkeilla tai mutkilla, jotka synnyttävät virtauksessa pienen mittakaavan turbulenssia. Vaihtoehtoisesti huulikanava voi olla sileäseinäinen, jolloin seinämäkitka aiheuttaa riittävästi pienen mittakaavan turbulenssia erityisesti silloin, kun virtauskanavan 30 korkeus on pieni.It is typical of thick pulp boxes that the pulp slurry is first well fluidized, after which turbulence is allowed to dampen while preventing the formation of large fiber blocks. In order to prevent the formation of fiber flocs, the lip canal may be provided, in a manner known per se, with various recesses, projections or bends that create small-scale turbulence in the flow. Alternatively, the lip channel may be smooth-walled, whereby the wall friction causes sufficiently small-scale turbulence, especially when the height of the flow channel 30 is small.
44
Perinteisillä avoimeen huulisuihkuun perustuvilla sakeamassaformereilla on vaikea saada aikaan rainaa, jolla on hyvät tason suuntaiset lujuusominaisuudet. Keksinnön mukaisessa formerissa ongelma voidaan ratkaista järjestämällä viiran ja massasuspensiovirtauksen nopeudet erilaisiksi. Kun viiran nopeus säädetään olen-5 naisesti suuremmaksi kuin huulikanavasta purkautuvan massasuspensiovirtauksen nopeus, kuitukerros saadaan venymään ja ohenemaan muodostusalueella. Kiinteän liukupinnan ja liikkuvan viiran välissä massasuspension kuidut asettuvat enenevässä määrin virtauksen suuntaisesti, mikä parantaa rainan tason suuntaisia lujuusominaisuuksia.Conventional open lip spray based bulk formulators find it difficult to obtain a web having good planar strength properties. In the former according to the invention, the problem can be solved by arranging different velocities of wire and pulp suspension flow. By adjusting the wire velocity to substantially greater than the velocity of the pulp suspension flow from the lip duct, the fiber layer is made to stretch and thinner in the forming region. Between the fixed sliding surface and the movable wire, the fibers of the pulp suspension are increasingly aligned with the flow, which improves the strength properties parallel to the web plane.
1010
Keksinnön kohteena on myös menetelmä monikerrosrainan valmistamiseksi, jossa menetelmässä muodostetaan ainakin kaksi rainan kerrosta erillisissä rainanmuo-dostusyksiköissä ja liitetään erikseen muodostetut rainan kerrokset toisiinsa. Menetelmälle on tunnusomaista, että ainakin yksi rainan kerroksista muodostetaan 15 käyttäen keksinnön mukaista rainanmuodostusyksikköä.The invention also relates to a method of producing a multilayer web, comprising forming at least two web layers in separate web forming units and joining separately formed web layers. The method is characterized in that at least one of the web layers is formed using a web forming unit according to the invention.
Keksinnön avulla voidaan tuottaa riittävän hyviä kartonki- ja paperilaatuja olennaisesti nykyistä matalammilla pääoma- ja käyttökustannuksilla. Ratkaisu soveltuu korkeille perälaatikkosakeuksille aina 5 % sakeuteen asti, mutta sitä voidaan 20 käyttää myös normaalilla 0,5-2 % sakeusalueella korvaamaan avoimeen huulisuihkuun perustuvia formerikonsepteja. Koeajojen perusteella rainanmuodos-tusyksikön ensisijainen käyttökohde näyttäisi olevan yksi- tai monikerroksiset kartonki laadut, joiden neliömassa on 100-200 g/m2.The invention enables the production of sufficiently good grades of paperboard and paper with substantially lower capital and operating costs. The solution is suitable for high headbox consistencies up to 5% consistency, but it can also be used in the normal 0.5-2% consistency range to replace open lip shower former concepts. On the basis of the test runs, the primary use of the web forming unit would appear to be single or multilayer board grades having a basis weight of 100-200 g / m2.
25 Seuraavaksi keksintöä selostetaan yksityiskohtaisesti viittaamalla oheisten piirustusten kuvioihin, joiden yksityiskohtiin keksintöä ei kuitenkaan ole tarkoitus ahtaasti rajoittaa.In the following, the invention will be described in detail with reference to the figures in the accompanying drawings, in which details, however, are not intended to be narrowly limited.
Kuvio 1 esittää kaaviollisestä keksinnön mukaisen rainanmuodostusyksikön ra-30 kennetta.Figure 1 shows schematically the structure of a web forming unit according to the invention.
55
Kuvio 2 on sivukuva tekniikan tason mukaisesta kaksikerrosformerista.Fig. 2 is a side view of a prior art two-layer formatter.
Kuvio 3 on sivukuva kaksikerrosformerista, jossa rainan pintakerros muodostetaan käyttäen keksinnön mukaista rainanmuodostusyksikköä.Fig. 3 is a side view of a two-layer forming machine in which the surface layer of the web is formed using a web forming unit according to the invention.
55
Kuvio 4 on sivukuva kaksikerrosformerista, jossa rainan molemmat kerrokset muodostetaan käyttäen keksinnön mukaista rainanmuodostusyksikköä.Fig. 4 is a side view of a two-layer formatter in which both layers of the web are formed using a web forming unit according to the invention.
Kuvio 5 on sivukuva kolmikerrosformerista, jossa rainan keskikerros muodoste-10 taan käyttäen keksinnön mukaista rainanmuodostusyksikköä.Fig. 5 is a side view of a three-layer forming machine in which the middle layer of the web is formed using a web forming unit according to the invention.
Kuvio 6 on sivukuva kolmikerrosformerista, jossa rainan kaikki kerrokset muodostetaan käyttäen keksinnön mukaista rainanmuodostusyksikköä.Fig. 6 is a side view of a three-layer forming machine in which all layers of the web are formed using a web forming unit according to the invention.
15 Kuvio 7 esittää muunnoksen kuvion 6 kolmikerrosformerista.Fig. 7 shows a modification of the three-layer mold of Fig. 6.
Kuvio 1 on periaatekuva keksinnön mukaisesta rainanmuodostusyksiköstä, joka käsittää perälaatikon 10 ja viiran 13, joka on sovitettu liukumaan perälaatikon liukupintojen 15 ja 16 yli samanaikaisesti kun massasuspensio syötetään liukupin-20 tojen 15 ja 16 välissä sijaitsevasta huuliaukosta 12 muodostusviiralle 13.Fig. 1 is a plan view of a web forming unit according to the invention comprising a head box 10 and a wire 13 adapted to slide over the head box sliding surfaces 15 and 16 while feeding a pulp suspension from the lip opening 12 between the slide pins 20 and 16.
Ennen huuliaukkoa 12 viira 13 liukuu pitkin ensimmäisen liukupinnan 15 kaarevaa pintaa. Toinen liukupinta 16 on vedetty sisäänpäin ensimmäiseen liukupintaan 15 nähden siten, että perälaatikon viiraa 13 vastaan tulevaan pintaan muodostuu 25 sisennys, joka sisältää huuliaukon 12. Huuliaukon 12 jälkeen viira 13 liukuu pienen välimatkan päässä toisesta liukupinnasta 16. Viira 13 ja toinen liukupinta 16 rajaavat väliinsä muodostusalueen 17, joka ottaa vastaan huuliaukosta 12 purkautuvan massasuspensiovirtauksen. Massasuspension syöttöpaine ja viiran 13 kireys saavat aikaan veden poistumista viiran 13 läpi. Massasuspensio poistuu muodos-30 tusalueelta 17 rainan W muodossa.Prior to lip opening 12, wire 13 slides along the curved surface of first sliding surface 15. The second sliding surface 16 is retracted inward with respect to the first sliding surface 15 so that a recess 25 is formed on the surface facing the wire 13 of the headbox, including a lip opening 12. After the lip opening 12, the wire 13 slides a short distance from the second sliding surface 16. 17 receiving a mass suspension flow from the lip opening 12. The feed pressure of the pulp suspension and the tension of the wire 13 cause the water to drain through the wire 13. The pulp suspension leaves the formation 30 region 17 in the form of web W.
66
Huuliaukkoa 12 edeltävä huulikanava 11 on olennaisesti lineaarinen suhteellisen pitkältä matkalta. Ennen huulikanavan 11 lineaarista osuutta massasuspensio on fluidisoitu sinänsä tunnettuun tapaan. Huulikanava 11 voi olla sileäseinäinen tai se voi olla sinänsä tunnettuun tapaan varustettu pienillä mutkilla, ulokkeilla tai sy-5 vennyksillä 18, jotka saavat virtauksessa aikaan pienen mittakaavan turbulenssia. Huulikanavasta 11 huuliaukon 12 kautta viiralle 13 purkautuva massasuspen-siovirtaus osuu viiraan 13 tulokulmassa, jonka suuruus on 20-70°. Edullisesti viiran 13 nopeus Vw on säädetty suuremmaksi kuin massasuspensiosuihkun nopeus Vs, jolloin massasuspensiokerros venyy ja ohenee muodostusalueella 17. Säätä-10 mällä viiran nopeuden Vw ja massasuspension nopeuden Vs suhdetta voidaan vaikuttaa kuitujen orientaatioon rainassa ja sitä kautta rainan lujuusominaisuuksiin.The lip passageway 11 preceding lip opening 12 is substantially linear over a relatively long distance. Prior to the linear portion of the lip duct 11, the pulp suspension is fluidized in a manner known per se. The lip duct 11 may be smooth-walled or may, in a manner known per se, be provided with small bends, projections, or recesses 18 that cause small-scale turbulence in the flow. The mass suspension flow discharged from the lip duct 11 through the lip opening 12 onto the wire 13 hits the wire 13 at an inlet angle of 20-70 °. Advantageously, the velocity Vw of the wire 13 is set higher than the velocity Vs of the pulp suspension jet, whereby the pulp suspension layer is stretched and thinned within the forming region 17. By adjusting the ratio of wire velocity Vw to pulp suspension Vs.
Ensimmäinen liukupinta 15 voi olla kaareva kuten kuviossa 1 tai se voi olla suora. 15 Liukupinnan 15 jättöreuna muodostaa taivutuspisteen A, jossa viiran 13 kulkusuunta muuttuu kulman a verran. Viiran kulkusuunnan muutos tiivistää muo-dostusalueen 17 tulopuolen niin, että massasuspensio ei pääse tunkeutumaan vastavirtaan viiran 13 ja ensimmäisen liukupinnan 15 väliin.The first sliding surface 15 may be curved as in Figure 1 or it may be straight. The leaving edge of the sliding surface 15 forms a bending point A, in which the direction of travel of the wire 13 changes by an angle a. change the running direction of the wire seals fas-dostusalueen 17 of the input side, so that the pulp suspension does not penetrate between the upstream of the wire 13 and the first sliding surface 15.
20 Toinen liukupinta 16 on kaareva siten, että sen kaarevuussäde R on 200-1000 mm. Kaarevuussäde R voi olla vakio liukupinnan 16 koko pituudella tai se voi olla erilainen liukupinnan 16 eri osissa. Toisen liukupinnan 16 jättöreuna muodostaa taivutuspisteen B, jossa viiran 13 kulkusuunta muuttuu kulman β verran. Kulman β suuruus on edullisesti 1-8°. Tämä toinen viiran kulkusuunnan muutos tiivistää 25 muodostusalueen 17 jättöpuolen.The second sliding surface 16 is curved such that its radius of curvature R is 200-1000 mm. The radius of curvature R may be constant over the entire length of the slide surface 16 or it may be different at different portions of the slide surface 16. The leaving edge of the second sliding surface 16 forms a bending point B where the direction of travel of the wire 13 changes by an angle β. The angle β is preferably from 1 to 8 °. This second change in the direction of travel of the wire seals the leaving side of the forming region 17.
Formerirakenteella, jossa viiran 13 kulkusuunta muuttuu hieman sekä sen tullessa muodostusalueelle 17 että sen poistuessa muodostusalueelta 17, voidaan tehokkaasti tiivistää massasuspension tuonti perälaatikosta 10 viiralle 13. Lisäksi viira 30 käyttäytyy stabiilimmin ja saavutetaan hyvä rainan formaatio myös suuremmilla 7 sakeuksilla. Myös rainan lujuus suuremmilla sokeuksilla pysyy lähes samalla tasolla kuin alhaisemmilla sakeuksilla.The molded structure, in which the direction of travel of the wire 13 changes slightly as it enters and exits the forming zone 17, can efficiently seal the introduction of the pulp suspension from the headbox 10 to the wire 13. In addition, the wire 30 behaves more stably and good web formation is achieved. Also, the web strength at higher blinds remains almost at the same level as at lower consistency.
Kuvion 1 mukainen rainanmuodostusyksikkö soveltuu erityisen hyvin käytettä-5 vaksi suurilla 2-5 % massan sakeuksilla, mutta mikään ei estä käyttämästä sitä myös normaaleilla 0,5-2 % sakeuksilla. Rainanmuodostusyksikkö soveltuu erinomaisesti paksujen paperi- ja kartonkilajien valmistukseen. Sitä voidaan myös käyttää monikerrosrainan yksittäisten kerroksien muodostamiseen, kuten seuraa-vaksi tullaan esittämään.The web forming unit of Figure 1 is particularly well-suited for use at high 2-5% pulp consistency, but nothing prevents it from being used at normal 0.5-2% pulp consistency as well. The web forming unit is ideally suited for the production of thick grades of paper and board. It can also be used to form individual layers of a multilayer web, as will be described below.
1010
Kuviossa 2 on esitetty tekniikan tason mukainen kaksikerrosformeri. Se käsittää alaviirayksikön, jossa muodostetaan rainan pohjakerros, ja yläviirayksikön, jossa muodostetaan rainan pintakerros, sekä välineet rainojen liittämiseksi toisiinsa. Alaviirayksikkö käsittää ensimmäisen perälaatikon 8 ja alaviiran 20, joka kulkee 15 ohjaustelojen 21 ohjaamana ja muodostaa päättymättömän silmukan. Laimennettu massasuspensio syötetään perälaatikosta 8 avoimena suihkuna alaviiralle 20, jonka tasoviiraosuudella siitä poistetaan vettä viiran 20 läpi rainan pohjakerroksen muodostamiseksi. Yläviirayksikkö käsittää toisen perälaatikon 9 ja yläviiran 30, joka telojen 31,32 ohjaamana muodostaa päättymättömän silmukan, joka sivuaa 20 alaviiraa 20. Laimennettu massasuspensio syötetään toisesta perälaatikosta 9 avoimena suihkuna yläviiran 30 tasoviiraosuudelle, jossa siitä poistetaan vettä rainan pintakerroksen muodostamiseksi. Muodostettu raina johdetaan tämän jälkeen alaviiralla 20 olevan pohjakerroksen päälle ja kerrokset liitetään toisiinsa huopautustelan 32 avulla. Alaviiran 8 tasoviiraosuuden lopussa yhdistetty raina 25 siirretään sieppotelan 50 avulla puristinosalle. Molemmat perälaatikot 8 ja 9 ovat perinteisiä laimean massan perälaatikoita, joissa massasuspension sakeus on alueella 0,5-1,0 %.Figure 2 shows a prior art double-layer formatter. It comprises a lower wire unit for forming a web base layer and an upper wire unit for forming a web surface layer and means for connecting the webs to one another. The bottom wire unit comprises a first headbox 8 and a bottom wire 20, which is guided by guide rollers 21 and forms an endless loop. The diluted pulp suspension is fed from the headbox 8 as an open jet to the lower wire 20, the flat wire portion of which is dewatered through the wire 20 to form the bottom layer of the web. The upper wire unit comprises a second headbox 9 and an upper wire 30 which, guided by rolls 31,32, forms an endless loop which touches the lower wire 20. The diluted pulp suspension is fed from the second headbox 9 as an open jet to dewater the web. The formed web is then guided over the bottom layer on the bottom wire 20 and the layers are joined together by a felt roll 32. At the end of the flat wire portion of the lower wire 8, the connected web 25 is moved by a catch roll 50 to the press section. Both headboxes 8 and 9 are conventional dilute mass headboxes having a consistency of the pulp suspension in the range of 0.5-1.0%.
Kuviossa 3 on esitetty kaksikerrosformeri, jossa yläviirayksikkö on korvattu ku-30 viota 1 vastaavalla rainanmuodostusyksiköllä. Alaviirayksikkö on samanlainen kuin kuviossa 2. Yläviirayksikkö käsittää perälaatikon 10, jota painetaan viiraa 30 8 vasten. Viira 30 liukuu aluksi pitkin ensimmäistä liukupintaa 15 ja huuliaukon 12 jälkeen se etenee pienen välin päässä toisesta liukupinnasta 16. Viiran 30 ja toisen liukupinnan 16 väliin jää muodostusaiue, jolla massasuspensiosta poistuu vettä viiran 30 läpi syöttöpaineen ja viiran 30 kireyden seurauksena. Perälaatikosta 10 5 syötettävän massan sakeus on edullisesti alueella 2-5 %. Tällöin yläviirasilmukan 30 tasoviiraosuus, joka tarvitaan halutun kuiva-ainepitoisuuden saavuttamiseksi, voi olla merkittävästi lyhyempi kuin kuvion 2 perinteisessä yläviirayksikössä.Fig. 3 shows a double-layer reformer in which the top wire unit is replaced by a forming unit corresponding to Fig. 1. The lower wire unit is similar to Figure 2. The upper wire unit comprises a head box 10 which is pressed against the wire 30 8. The wire 30 initially initially slides along the first sliding surface 15 and, after the lip opening 12, advances at a short distance from the second sliding surface 16. A forming region remains between the wire 30 and the second sliding surface 16 to drain water from the pulp suspension through the feed pressure and wire tension. The consistency of the pulp fed from the headbox 10 5 is preferably in the range of 2-5%. In this case, the flat wire portion of the upper wire loop 30 required to achieve the desired dry matter content may be significantly shorter than in the conventional upper wire unit of Figure 2.
Kuvion 4 kaksikerrosfonnerissa myös alaviirayksikkö käsittää keksinnön mukai-10 sen formeriratkaisun, jossa kaarevilla liukupinnoilla 15,16 varustettu perälaatikko 10 on painettu alaviiraa 10 vasten. Näin rainan molemmat kerrokset voidaan muodostaa käyttäen keksinnön mukaisia rainanmuodostusyksiköita.Also, in the bilayer fender of Figure 4, the bottom wire assembly 10 comprises a former arrangement according to the invention in which the headbox 10 with curved sliding surfaces 15,16 is pressed against the bottom wire 10. Thus, both layers of the web can be formed using web forming units according to the invention.
Kuviossa 5 on esitetty monikerrosformeri, jossa rainan pohjakerros ja pintakerros 15 muodostetaan matalan sakeuden massasta perinteisellä tekniikalla ja keskikerros muodostetaan korkean sakeuden massasta käyttäen keksinnön mukaista rainan-muodostusyksikköä. Rainan pohjakerroksen muodostamiseksi syötetään laimea massasuspensio avoimena suihkuna tavanomaisesta perälaatikosta 8 alaviiralle 30. Rainan keskikerroksen muodostamiseksi syötetään sakea massasuspensio perälaa-20 tikosta 10 ensimmäiselle yläviiralle 30, joka on sovitettu liukumaan pitkin perä-laatikon liukupintoja 15 ja 16 kuten edellä kuvion 1 yhteydessä on selostettu. Rainan pintakerroksen muodostamiseksi syötetään laimea massasuspensio avoimena suihkuna toisesta tavanomaisesta perälaatikosta 9 toiselle yläviiralle 40. joka kulkee ohjaustelojen 41,42 ohjaamana muodostaen päättömän silmukan. Ensimmäi-25 nen yläviira 30 ja toinen yläviira 40 johdetaan yhteen kaksiviiravyöhykkeen aikaansaamiseksi, jossa rainan keski- ja pintakerros liitetään yhteen. Tämän jälkeen yhdistetty raina johdetaan alaviiralla 20 olevan rainan pohjakerroksen päälle ja rainan kaikki kerrokset liitetään yhteen huopautustelan 42 avulla kaksiviira-vyöhykkeessä, jonka alaviira 20 ja toinen yläviira 40 yhdessä muodostavat.Figure 5 illustrates a multilayer forming machine in which the bottom layer and the top layer 15 of the web are formed from a low consistency mass by conventional technique and the middle layer is formed from a high consistency mass using a web forming unit according to the invention. To form the bottom layer of the web, a dilute pulp suspension is fed as an open jet from the conventional headbox 8 to the lower wire 30. To form the middle web layer, a thick pulp suspension from the headboard 20 to the first upper wire 30 is arranged to slide along the headbox sliding surfaces 15 and 16. To form the surface layer of the web, a dilute pulp suspension is fed as an open jet from one conventional headbox 9 to another upper wire 40. which is guided by the guide rollers 41,42 to form an endless loop. The first top-25 wire and the second top-wire 40 are guided together to provide a two-wire zone in which the middle and surface layers of the web are joined. The composite web is then guided over the bottom layer of the web on the lower wire 20 and all layers of the web are joined together by a felt roll 42 in the two-wire zone formed by the lower wire 20 and the second upper wire 40 together.
30 930 9
Kuviossa 6 on esitetty monikerrosformeri, joka käsittää kolme keksinnön mukaista rainanmuodostusyksikköä. Kukin rainan kolmesta kerroksesta muodostetaan sakeasta massasta käyttäen keksinnön mukaista sakeamassaperälaatikkoa 10, joka on painettu vastaavaa viiraa 20, 30 tai 40 vasten. Tämän jälkeen ensimmäiselle 5 yläviiralle 30 muodostettu rainan keskikerros yhdistetään alaviiralla 20 olevaan rainan pohjakerrokseen ja lopuksi toiselle yläviiralle 40 muodostettu rainan pintakerros liitetään alaviiralla 20 jo olevien rainan kerroksien päälle.Fig. 6 shows a multilayerformer comprising three web forming units according to the invention. Each of the three layers of the web is formed from a thick pulp using a thick pulp base box 10 according to the invention printed on a respective wire 20, 30 or 40. The middle web layer formed on the first 5 upper wire 30 is then connected to the bottom layer of the web 20 on the lower wire 20 and finally the web top layer formed on the second upper wire 40 is joined to the already existing web layers on the lower wire 20.
Kuvio 7 on esitetty vaihtoehtoinen ratkaisu, jossa ensimmäiselle yläviiralle 30 10 muodostettu rainan keskikerros ja toiselle yläviiralle 40 muodostettu rainan pintakerros liitetään ensin toisiinsa mainittujen viirojen muodostamassa kaksiviira-vyöhykkeessä ja vasta tämän jälkeen nämä kerrokset yhdistetään alaviiralla 20 olevaan rainan pohjakerrokseen.Fig. 7 shows an alternative solution in which the middle web layer formed on the first top fabric 30 and the web top layer formed on the second top fabric 40 are first joined together in the biaxial zone formed by said wires, and then these layers are joined to the bottom layer web.
15 Keksinnön monet eri muunnokset ovat mahdollisia seuraavaksi esitettävien patenttivaatimuksien määrittelemän suojapiirin puitteissa.Many variations of the invention are possible within the scope defined by the following claims.
Claims (10)