ES370112A1 - Un metodo de reducir las roturas del vidrio en una cinta devidrio. - Google Patents
Un metodo de reducir las roturas del vidrio en una cinta devidrio.Info
- Publication number
- ES370112A1 ES370112A1 ES370112A ES370112A ES370112A1 ES 370112 A1 ES370112 A1 ES 370112A1 ES 370112 A ES370112 A ES 370112A ES 370112 A ES370112 A ES 370112A ES 370112 A1 ES370112 A1 ES 370112A1
- Authority
- ES
- Spain
- Prior art keywords
- glass ribbon
- formation
- molten pool
- stresses during
- controlling temporary
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03B—MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03B25/00—Annealing glass products
- C03B25/04—Annealing glass products in a continuous way
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Re-Forming, After-Treatment, Cutting And Transporting Of Glass Products (AREA)
- Laminated Bodies (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US64864167A | 1967-06-26 | 1967-06-26 |
Publications (1)
Publication Number | Publication Date |
---|---|
ES370112A1 true ES370112A1 (es) | 1971-04-01 |
Family
ID=24601610
Family Applications (3)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES355118A Expired ES355118A1 (es) | 1967-06-26 | 1968-06-18 | Un metodo de disminuir los esfuerzos superficiales tempora-les en una cinta de vidrio. |
ES355119A Expired ES355119A1 (es) | 1967-06-26 | 1968-06-18 | Un aparato para estirar vidrio en hoja. |
ES370112A Expired ES370112A1 (es) | 1967-06-26 | 1969-07-31 | Un metodo de reducir las roturas del vidrio en una cinta devidrio. |
Family Applications Before (2)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES355118A Expired ES355118A1 (es) | 1967-06-26 | 1968-06-18 | Un metodo de disminuir los esfuerzos superficiales tempora-les en una cinta de vidrio. |
ES355119A Expired ES355119A1 (es) | 1967-06-26 | 1968-06-18 | Un aparato para estirar vidrio en hoja. |
Country Status (7)
Country | Link |
---|---|
US (1) | US3536463A (es) |
BE (1) | BE717163A (es) |
ES (3) | ES355118A1 (es) |
FR (1) | FR1576629A (es) |
GB (1) | GB1199835A (es) |
IL (1) | IL30170A0 (es) |
NL (1) | NL6808980A (es) |
Families Citing this family (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7248923B2 (en) * | 2003-11-06 | 2007-07-24 | Cardiac Pacemakers, Inc. | Dual-use sensor for rate responsive pacing and heart sound monitoring |
US7207193B2 (en) * | 2003-12-08 | 2007-04-24 | Corning Incorporated | Method of fabricating low-warp flat glass |
JP5327702B2 (ja) * | 2008-01-21 | 2013-10-30 | 日本電気硝子株式会社 | ガラス基板の製造方法 |
US8037716B2 (en) * | 2009-02-27 | 2011-10-18 | Corning Incorporated | Thermal control of the bead portion of a glass ribbon |
US8459062B2 (en) | 2011-09-27 | 2013-06-11 | Corning Incorporated | Apparatus and methods for producing a glass ribbon |
Family Cites Families (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US1032238A (en) * | 1908-08-29 | 1912-07-09 | John Player | Machine for drawing sheet-glass. |
NL85259C (es) * | 1951-04-21 | |||
NL206950A (es) * | 1956-04-23 | 1900-01-01 | ||
US2952097A (en) * | 1953-05-18 | 1960-09-13 | Pittsburgh Plate Glass Co | Annealing glass |
CH372138A (fr) * | 1960-05-20 | 1963-09-30 | Union Des Verreries Mecaniques | Procédé pour l'amélioration du recuit du verre en feuille et dispositif pour la mise en oeuvre de ce procédé |
NL282178A (es) * | 1961-08-18 | |||
BE621526A (es) * | 1961-08-18 | |||
BE627976A (es) * | 1962-02-05 | |||
US3318673A (en) * | 1963-02-28 | 1967-05-09 | Emhart Corp | Glassware annealing method |
US3311463A (en) * | 1963-06-03 | 1967-03-28 | Pittsburgh Plate Glass Co | Process of annealing glass sheets |
-
1967
- 1967-06-26 US US648641A patent/US3536463A/en not_active Expired - Lifetime
-
1968
- 1968-06-13 IL IL30170A patent/IL30170A0/xx unknown
- 1968-06-18 ES ES355118A patent/ES355118A1/es not_active Expired
- 1968-06-18 ES ES355119A patent/ES355119A1/es not_active Expired
- 1968-06-21 FR FR1576629D patent/FR1576629A/fr not_active Expired
- 1968-06-25 GB GB30167/68A patent/GB1199835A/en not_active Expired
- 1968-06-26 BE BE717163D patent/BE717163A/xx unknown
- 1968-06-26 NL NL6808980A patent/NL6808980A/xx unknown
-
1969
- 1969-07-31 ES ES370112A patent/ES370112A1/es not_active Expired
Also Published As
Publication number | Publication date |
---|---|
FR1576629A (es) | 1969-08-01 |
BE717163A (es) | 1968-12-27 |
US3536463A (en) | 1970-10-27 |
ES355119A1 (es) | 1969-11-16 |
ES355118A1 (es) | 1970-03-01 |
IL30170A0 (en) | 1968-08-22 |
GB1199835A (en) | 1970-07-22 |
NL6808980A (es) | 1968-12-27 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ES275957A1 (es) | Método y aparato para la producción de vidrio plano en forma de cinta | |
ES333345A1 (es) | Un metodo de fabricacion de vidrio plano. | |
ES278133A1 (es) | Un aparato para producir cinta de vidrio a partir de un baño de vidrio fundido | |
ES370112A1 (es) | Un metodo de reducir las roturas del vidrio en una cinta devidrio. | |
FR1514911A (fr) | Procédé et composition pour la fabrication de moules pour métaux | |
ES390697A1 (es) | Procedimiento para el tratamiento termico de aceros de construccion no aleados y bajos en carbono para la mejora delas caracteristicas mecanicas del material. | |
ES275960A1 (es) | Método y aparato para la fabricación de vidrio plano en forma de cinta | |
ES275958A1 (es) | Método y aparato para la fabricación de vidrio plano en forma de cinta dotada de un espesor predeterminado | |
ES310435A1 (es) | Metodo de fabricacion de vidrio plano. | |
ES323203A1 (es) | Metodo de fabricacion de vidrio plano. | |
ES290796A1 (es) | Dispositivo para la fabricación continua de vidrio en lámina | |
ES368736A1 (es) | Metodo y aparato perfeccionados para el control de tempera-tura en hornos de vidrio. | |
ES286535A1 (es) | Método y aparato de temple de vidrio | |
ES349680A1 (es) | Metodo y aparato para refrigerar planchas continuas de vi- drio en un bano de metal liquido. | |
ES390223A1 (es) | Un metodo de fabricacion de vidrio. | |
FR1176617A (fr) | Four et procédé pour le cintrage du verre | |
ES386125A1 (es) | Un metodo de producir globulos de vidrio. | |
ES231392A1 (es) | MÉTODO PARA LA FABRICACIoN DE VIDRIO PLANO TRANSPARENTE EN FORMA DE CINTA CONTINUA Y APARATO PARA SU PUESTA EN PRáCTICA. | |
ES267661A1 (es) | Procedimiento para el acondicionamiento termico del vidrio en fusiën antes de su pulido | |
ES285324A1 (es) | Un método de producir escoria en forma de fragmentos duros, sustancialmente porosos | |
FR1354320A (fr) | Procédé pour recuire le verre | |
ES294268A1 (es) | Método para preparar ésteres alquilo inferior de ácido 6, 7-di (inferior) alcoxi-4-hidroxi-3-quinolinacarboxilico | |
ES242547A1 (es) | MÉTODO DE FABRICACIoN DE CUERPOS MONOCRISTALINOS. | |
ES291795A1 (es) | Procedimiento para la fabricaciën continua de vidrio en lamina | |
FR1166577A (fr) | Procédé et dispositif pour le refroidissement de briques recuites |