ES348062A1 - Procedimiento para el afino de metal en una instalacion de colada continua. - Google Patents
Procedimiento para el afino de metal en una instalacion de colada continua.Info
- Publication number
- ES348062A1 ES348062A1 ES348062A ES348062A ES348062A1 ES 348062 A1 ES348062 A1 ES 348062A1 ES 348062 A ES348062 A ES 348062A ES 348062 A ES348062 A ES 348062A ES 348062 A1 ES348062 A1 ES 348062A1
- Authority
- ES
- Spain
- Prior art keywords
- metal
- slag
- mould
- stream
- refining
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
- 239000002184 metal Substances 0.000 title abstract 4
- 229910052751 metal Inorganic materials 0.000 title abstract 4
- 238000005266 casting Methods 0.000 title 1
- 238000007670 refining Methods 0.000 title 1
- 239000002893 slag Substances 0.000 abstract 5
- RYGMFSIKBFXOCR-UHFFFAOYSA-N Copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 abstract 1
- 238000009749 continuous casting Methods 0.000 abstract 1
- 229910052802 copper Inorganic materials 0.000 abstract 1
- 239000010949 copper Substances 0.000 abstract 1
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22B—PRODUCTION AND REFINING OF METALS; PRETREATMENT OF RAW MATERIALS
- C22B9/00—General processes of refining or remelting of metals; Apparatus for electroslag or arc remelting of metals
- C22B9/16—Remelting metals
- C22B9/18—Electroslag remelting
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B22—CASTING; POWDER METALLURGY
- B22D—CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
- B22D11/00—Continuous casting of metals, i.e. casting in indefinite lengths
- B22D11/10—Supplying or treating molten metal
- B22D11/11—Treating the molten metal
Landscapes
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Chemical & Material Sciences (AREA)
- Manufacturing & Machinery (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Continuous Casting (AREA)
- Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces (AREA)
- Furnace Details (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
FR90258A FR1513573A (fr) | 1967-01-06 | 1967-01-06 | Procédé et dispositif pour l'affinage du métal dans une installation de coulée continue |
Publications (1)
Publication Number | Publication Date |
---|---|
ES348062A1 true ES348062A1 (es) | 1969-06-16 |
Family
ID=8623498
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
ES348062A Expired ES348062A1 (es) | 1967-01-06 | 1967-12-07 | Procedimiento para el afino de metal en una instalacion de colada continua. |
Country Status (7)
Country | Link |
---|---|
US (1) | US3517727A (es) |
BE (1) | BE706892A (es) |
DE (1) | DE1608082C3 (es) |
ES (1) | ES348062A1 (es) |
FR (1) | FR1513573A (es) |
GB (1) | GB1198290A (es) |
SE (1) | SE327261B (es) |
Families Citing this family (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3669178A (en) * | 1969-06-09 | 1972-06-13 | Continental Ore Corp | Direct reduction process and simultaneous continuous casting of metallic materials in a crucible to form rods |
FR2325727A1 (fr) * | 1975-09-26 | 1977-04-22 | Servimetal | Flux pour l'elimination des metaux alcalins et alcalino-terreux de l'aluminium et de ses alliages et procedes de mise en oeuvre |
JPS599170B2 (ja) * | 1976-06-11 | 1984-02-29 | 株式会社クボタ | スカム吸引方法とその装置 |
FR2460171A1 (fr) * | 1979-06-29 | 1981-01-23 | Inst Elektroswarki Patona | Procede d'elaboration, sous laitier electroconducteur, de lingots a section pleine et installation pour la mise en oeuvre dudit procede |
FR2522551A1 (fr) * | 1982-03-05 | 1983-09-09 | Lorraine Laminage | Procede et dispositif d'alimentation et de regulation de la couche de poudre de lubrification dans une lingotiere de coulee continue |
AT399463B (de) * | 1987-03-03 | 1995-05-26 | Inteco Int Techn Beratung | Verfahren zum elektroschlacke-stranggiessen von stählen und legierungen |
AT406384B (de) * | 1996-01-29 | 2000-04-25 | Inteco Int Techn Beratung | Verfahren zum elektroschlacke-strangschmelzen von metallen |
Family Cites Families (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US2375107A (en) * | 1941-06-26 | 1945-05-01 | Kellogg M W Co | Method and apparatus for the continuous production of metal |
US2369233A (en) * | 1943-01-26 | 1945-02-13 | Kellogg M W Co | Method and apparatus for producing metal |
FR1264474A (fr) * | 1959-11-19 | 1961-06-23 | Renault | Procédé de fusion à électrode consommable sous laitier et à coulée continue |
US3344839A (en) * | 1963-11-28 | 1967-10-03 | Soudure Electr Autogene | Process for obtaining a metallic mass by fusion |
US3411566A (en) * | 1967-02-20 | 1968-11-19 | Astrov Evgeny Ivanovitch | Device for supplying powdered material into a mold of a continuous casting machine |
-
1967
- 1967-01-06 FR FR90258A patent/FR1513573A/fr not_active Expired
- 1967-11-22 BE BE706892D patent/BE706892A/xx unknown
- 1967-12-05 GB GB55361/67A patent/GB1198290A/en not_active Expired
- 1967-12-06 SE SE16755/67A patent/SE327261B/xx unknown
- 1967-12-07 ES ES348062A patent/ES348062A1/es not_active Expired
- 1967-12-27 US US693954A patent/US3517727A/en not_active Expired - Lifetime
-
1968
- 1968-01-04 DE DE1608082A patent/DE1608082C3/de not_active Expired
Also Published As
Publication number | Publication date |
---|---|
DE1608082B2 (de) | 1973-03-15 |
SE327261B (es) | 1970-08-17 |
BE706892A (es) | 1968-04-01 |
GB1198290A (en) | 1970-07-08 |
DE1608082C3 (de) | 1973-10-31 |
DE1608082A1 (de) | 1972-03-02 |
US3517727A (en) | 1970-06-30 |
FR1513573A (fr) | 1968-02-16 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
GB496151A (en) | A method and apparatus for the continuous casting of metal pipes or tubes | |
GB993086A (en) | Process for the horizontal continuous casting of molten metal | |
ES432401A1 (es) | Metodo y dispositivo para la colada continua horizontal de metales. | |
ES348062A1 (es) | Procedimiento para el afino de metal en una instalacion de colada continua. | |
GB1240566A (en) | Apparatus for the production of hollow ingots of metal by electro-slag refining | |
GB1149788A (en) | Improvements in or relating to the treatment of readily oxidisable metals during casting | |
GB1277765A (en) | Apparatus for casting hollow ingots by electroslag remelting of a consumable electrode | |
GB752271A (en) | Improvements in moulds for use in the continuous casting of metals and particularly steel | |
FR1476181A (fr) | Lingotière pour la coulée continue des métaux, et procédé de fabrication de cette lingotière | |
GB829957A (en) | Improvements relating to ingot moulds and to continuous casting processes utilizing such moulds | |
ES329933A1 (es) | Perfeccionamientos en maquinas para la colada continua de metales. | |
FR1486339A (fr) | Procédé d'amenée du lubrifiant dans la coulée continue de métaux en lingotières fixes | |
GB1034593A (en) | Apparatus for the continuous casing of metals under vacuum | |
GB1219707A (en) | An installation for making ingots | |
GB1313009A (en) | Device for casting metals | |
FR1454981A (fr) | Tour d'affinage du cuivre et de ses alliages | |
SU143518A1 (ru) | Способ заполнени форм | |
GB1238694A (es) | ||
ES277284A1 (es) | Procedimiento y aparato para el fundido continuo de lingotes de metal | |
JPS5561368A (en) | Casting method of thin-walled casting | |
JPS5728655A (en) | Continuous casting method of steel | |
JPS57149056A (en) | Method and device for electroslag remelting | |
ES368613A1 (es) | Un metodo y su correspondiente aparato para el moldeo en continuo de metal fundido. | |
JPS5611140A (en) | Cooling method of mold for continuous horizontal casting | |
FR1496241A (fr) | Procédé de coulée continue de métaux dans des lingotières fixes en graphite suivie d'un refroidissement direct |