DE914571C - Process for avoiding seizure of screw connections that are stressed at higher temperatures - Google Patents
Process for avoiding seizure of screw connections that are stressed at higher temperaturesInfo
- Publication number
- DE914571C DE914571C DEM15374A DEM0015374A DE914571C DE 914571 C DE914571 C DE 914571C DE M15374 A DEM15374 A DE M15374A DE M0015374 A DEM0015374 A DE M0015374A DE 914571 C DE914571 C DE 914571C
- Authority
- DE
- Germany
- Prior art keywords
- higher temperatures
- screw connections
- stressed
- seizure
- nitriding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur Vermeidung des Fressens von bei höheren Temperaturen beanspruchten Schraubverbindungen Schraulyverbindungen, die höheren Temperaturen ausgesetzt sind, neigen durch Verzunderung, Erniedrigung der Werkstoffhärte usw. zum Fressen, so daß sich die Schrauben nicht mehr lösen lassen. Um dieses Fressen zu vermieiden, werden verschiedene Mittel angewendet, die zwei Eigenschaften haben müssen,. Erstens sollen sie eine unmittelbare metallische Berührung verhindern und zweitens nach Möglichkeit eine schmierende Wirkung haben,. Bekannt ist z. B. das Nitrieren als Mittel zur Verringerung der Freßgefahr. Das Nitrieren hat jedoch folgende Nachteile: t. Es müssen besondere zum Nitrieren geeignete Stähle verwendet werden, d.iie hohe Werkstoffkosten verursachen; a. die ,metallische Berührung der Gewindeflanken von Bolzen und Mutter wird nicht verhindert, es wird lediglich die Freßneigung durch Veränderung der Oberflächenschicht beim Nitrieren vermindert; 3. das Nitrieren wird bei Temperaturen unter 58o° durchgeführt; bei Teilen, die höhere Temperaturen auszuhalten haben, würde sich die Nitrierschicht in ungünstigef Weise umwandeln, bzw. es würde der Stickstoff in das Innere des Werkstoffes weiterdiffundieren, so, daß die Nitrierwirkung verlorengeht..Method of avoiding seizure at higher temperatures screw connections stressed screw connections, the higher temperatures are exposed to, tend due to scaling, lowering of the material hardness, etc. to eat, so that the screws can no longer be loosened. About this eating To avoid it, various means are used which have two properties have to,. First, they should prevent direct metallic contact and secondly, if possible, have a lubricating effect. Is known z. B. that Nitriding as a means of reducing the risk of seizure. However, nitriding has the following Cons: t. Special steels suitable for nitriding must be used, d. they cause high material costs; a. the metallic contact of the thread flanks bolts and nuts are not prevented, only the tendency to seize is prevented Change in the surface layer during nitriding reduced; 3. the nitriding is carried out at temperatures below 58o °; for parts that can withstand higher temperatures the nitrided layer would change in an unfavorable way, or it would the nitrogen diffuses further into the interior of the material, so that the nitriding effect get lost..
Das Nitrieren verhindert also weder die metallische Berührung, noch ergibt es eine schmierende Wirkung. Dias Einbringen eines Schmiermittels zwischen die Gewindeflanken ist an sich 'bekannt. Die Geeignetheit des Mittels äst abhängig von seiner Struktur. Das bekannte Graphit hat, mit Öl gemischt, bereits eine Struktur, die den vorgenannten Forderungen ganz gut entspricht. Weiter sind einige Salze, die ähnliche Eigenschaften haben, z. B. Molybdändisulfit, bekannt, die ebenfalls verwendet werden.Nitriding doesn’t prevent metallic contact, either it gives a lubricating effect. Slides the introduction of a lubricant between the thread flanks is known per se '. The suitability of the remedy aest depending on its structure. The well-known graphite, mixed with oil, already has a structure that meets the aforementioned requirements quite well. Are further some salts that have similar properties e.g. B. Molybdenum disulfite, known which are also used.
Es hat sich nun gezeigt, duß bei einem Bestreichen der Gewinde vor der Verbindung mit einer Aufschwemmung von Bleiglätte gemäß der Erfindung besonders gute Ergebnisse erzielt werden. Bleiglätte besitzt eine Struktur, die sehr gute Schmiereigenschaften hat. Durch dieses Mittel wird jegliches Fressen im Gewinde auch nach lang andauernder Beanspruchung bei hohen Temperaturen sicher verhindert. Die Bleiglätte hat sich nicht nur bei den üblichen warmfesten Stählen bewährt, sondern auch bei hoch dauerstandfesten hitzebeständigen austenitischen Stählen, die wegen ihrer Weichheit eine besondere Freßneägung haben. Als Aufschwgmmittel für die Bleiglätte kann ein beliebiges hierzu geeignetes Mittel verwendet werden. Eine Aufschwemmung in Wasser hat sich als sehr vorteilhaft erwiesen,.It has now been shown that the thread must first be coated the connection with a flooding of black lead according to the invention in particular good results can be achieved. Metallic lead has a structure that is very good Has lubricating properties. This means that any seizure in the thread is eliminated reliably prevented even after prolonged exposure to high temperatures. The litharge has not only proven itself with the usual creep-resistant steels, but even in the case of high-strength, heat-resistant austenitic steels, which are due to their softness have a special eating tendency. As a buoyancy aid for the black lead any suitable means can be used. A suspension in water has been found to be very beneficial.
Mittels der Bleiglätte können außerdem die Hohlräume zwischen Bolzengewinde und Mutter ausgefüllt werden, so daß korrodierende oder oxydierende Medien nicht .eindringen können..By means of the black lead, the cavities between the bolt threads can also be opened and nut are filled out so that corrosive or oxidizing media do not .can penetrate ..
Claims (1)