DE661174C - Process for the production of pure clay - Google Patents
Process for the production of pure clayInfo
- Publication number
- DE661174C DE661174C DEE45738D DEE0045738D DE661174C DE 661174 C DE661174 C DE 661174C DE E45738 D DEE45738 D DE E45738D DE E0045738 D DEE0045738 D DE E0045738D DE 661174 C DE661174 C DE 661174C
- Authority
- DE
- Germany
- Prior art keywords
- alumina
- aluminum
- production
- acid
- temperatures
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
Verfahren zur Herstellung reiner Tonerde Die Erfindung betrifft ein Verfahren zur Herstellung reiner Tonerde über Aluminiumsulfite.Process for the production of pure alumina The invention relates to a Process for the production of pure alumina using aluminum sulphites.
Es ist bei einem Verfahren zur Vorbereitung tonerdehaltiger Mineralien für den Aufschluß mittels schwefeliger Säure, insbesondere zwecks Gewinnung von Tonerde, bekannt, diie Mineralien zum Zwecke ihrer Zersetzung, jedoch nicht zur Bildung von Aluminaten, mit Schwefelverbindungen der Alkalien oder Erdalkalien oder mit einem gleichwertigen Gemisch von schwefelsauren Alkalien oder Erdalkalien und Kohle in zur Aluminatbildung ungenügenden Mengen und ebenso bei hierzu nicht ausreichenden Temperaturen zu erhitzen. Der wesentlicheZweck dieses alten Vorschlages besteht also darin, die tonerdehaltigen Mineralien für die Aufschließung mittels schwefeliger Säure vorzubereiten, und nicht darin, eine Umwandlung in ein Aluminat hervorzurufen. Nach dem Glühen bei einer Temperatur, die wesentlich unter der Bildungstemperatur der Aluminate Biegt, sollen die tonerdehaltigen Verbindungen bei dem bekannten Verfahren seine solche Beschaffenheit haben, daß sie von schwefeliger Säure leichter angegriffen werden.It is in a process of preparing alumina minerals for digestion by means of sulphurous acid, in particular for the purpose of obtaining Alumina, known to use minerals for the purpose of their decomposition, but not for Formation of aluminates, with sulfur compounds of alkalis or alkaline earths or with an equivalent mixture of sulfuric acid alkalis or alkaline earths and Coal in insufficient quantities for the formation of aluminate and also in insufficient quantities for this purpose To heat temperatures. The main purpose of this old proposal is So in it, the alumina-containing minerals for the digestion by means of sulphurous To prepare acid, not to cause conversion to an aluminate. After annealing at a temperature substantially below the formation temperature the aluminate bends, the alumina-containing compounds are said to be in the known process are of such a nature that they are more easily attacked by sulphurous acid will.
Das erhaltene Glühprodukt wird mit Wasser behandelt, um durch Auslaugen sämtliche Alkalisalze zu extrahieren, so daß sie wieder verwendet 1Werden können. Demnach ist der Rückstand des bekannten Erzeugnisses von Alkalisalzen vollkommen frei. Daher kann sich ein unlösliches ternäres Alkalialuminiumsilicat nicht gebildet haben. Nach dem bebekannten Verfahren wird die im Kaolin befindliche Tonerde nur zu etwa 8o % aufgeschlossen. Außerdem ist sie mit großen Mengen Kieselsäure verunreinigt.The obtained glow product is treated with water to by leaching to extract all alkali salts so that they can be reused. Accordingly, the residue of the known product of alkali salts is complete free. Therefore, an insoluble ternary alkali aluminum silicate cannot be formed to have. According to the known method, the clay in the kaolin is only about 8o% open-minded. It is also contaminated with large amounts of silica.
Es ist bereits vorgeschlagen worden, vorher ;geglühten Ton und Kaolin mittels überschüssiger wässeriger schwefeliger Säure bei höherer Temperatur unter Druck zu behandeln. Derartige Verfahren führen aber lediglich zu Tonerdeausbeuten, die unter 8 5 % liegen; außerdem brauchen sie, wenn man die genannte Höchstausbeute erreichen will, eine sehr lange Reaktionszeit, etwa 2o Stunden.It has already been suggested previously; calcined clay and kaolin by means of excess aqueous sulphurous acid at a higher temperature Handle pressure. Such processes only lead to alumina yields, which are below 8 5%; also need them when you get the said maximum yield want to achieve a very long reaction time, about 20 hours.
Nach der Erfindung werden die Mängel der bekannten Verfahren dadurch beseitigt, daß man Aluminiumsilicate; wie Kaoline und Tone, bei Temperaturen von 5oo bis 8oo° C mit Alkaliverbändungen, .die in Gegenwart von Silicaten bei diesen Temperaturen ihren Säurerest leicht abspalten, wie Carbonaten und Sulfiten, zwecks Bildung einer ternären Verbindung, Na@0 # A1203 # 2 Si 0., glüht und erst diese Verbindung, nicht aber unmittelbar die Tone und Kaoline selbst mit schwefeliger Säure behandelt.According to the invention, the shortcomings of the known processes are eliminated by using aluminum silicates; such as kaolins and clays, at temperatures from 500 to 800 ° C with alkali compounds, which easily split off their acid residue in the presence of silicates at these temperatures, such as carbonates and sulfites, for the purpose of forming a ternary compound, Na @ 0 # A1203 # 2 Si 0 ., glows and first treats this compound, but not directly the clays and kaolins themselves with sulphurous acid.
DiebeiderangegebenenTemperaturgebildote
Beispiel Es werden 5 g Kaolin mit 1,5449 reiner Soda gut gemischt
und bei 65o° 25 Minuten lang geglüht. Das Kaolin hat die Zusammensetzung 37 % A12
0s, 58 % SiO2, i,5 % Fe. 03. Die verwendete Sodamenge macht 8o oio der theoretischen
Menge aus. Nach dem Erkalten wird das nichtgesinterte Glühprodukt, die. tern.äre
Verbindung, zerrieben, dann mit 95 ccm einer io%igen wässerigen schwefeligen Säure
verrührt und in einer Druckflasche 1/2 bis i Stunde auf i oo° C erhitzt. Während
des Erhitzens scheidet sich ein gallertartiger Niederschlag von Kieselsäure aus.
Von der unlöslichen Kieselsäure läßt sich die Lösung gut abfiltrieren; der Niederschlag
:,wird mit schwefeliger Säure nachgewaschen -und hierauf das Filtrat kurze Zeit
zum Kochen
Zur Herstellung von Aluminiumsalzen kann das Glühprodukt auch mit anderen anorganischen Säuren auf dem Wasserbad- abgeraucht werden.The annealing product can also be used to produce aluminum salts other inorganic acids can be smoked on the water bath.
Das Verhältnis der Soda zur Kaolinsubstanz soll möglichst i : i sein; man erhält bei gewissen Kaolinsorten jedoch auch mit weniger als der theoretisch notwendigen Menge Soda einen quantitativen Aufschluß, da durch die Nachbehandlung mit schwefeliger Säure im Autoklaven etwa 3o % des Kaolins allein aufgeschlossen werden.The ratio of soda to kaolin should be as much as possible i: i; with certain types of kaolin, however, one also obtains less than that theoretically necessary amount of soda a quantitative digestion, because of the aftertreatment With sulphurous acid in the autoclave about 3o% of the kaolin alone is digested will.
Die beider Reaktian zum Schluß anfallenden Alkalisulfite lassen sich ähnlich wie Soda an Stelle dieser wieder verwenden.The alkali sulphites obtained at the end of both reactants can be similar to using soda again in place of this.
Claims (1)