[go: up one dir, main page]

CN2433493Y - 一种耐磨弯管 - Google Patents

一种耐磨弯管 Download PDF

Info

Publication number
CN2433493Y
CN2433493Y CN 00215169 CN00215169U CN2433493Y CN 2433493 Y CN2433493 Y CN 2433493Y CN 00215169 CN00215169 CN 00215169 CN 00215169 U CN00215169 U CN 00215169U CN 2433493 Y CN2433493 Y CN 2433493Y
Authority
CN
China
Prior art keywords
cast layer
bent tube
abrasion
antifriction alloy
layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 00215169
Other languages
English (en)
Inventor
曲树蓁
卢继忠
杨兴强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN 00215169 priority Critical patent/CN2433493Y/zh
Application granted granted Critical
Publication of CN2433493Y publication Critical patent/CN2433493Y/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本实用新型提供了一种用于工业路的耐磨弯管,它包括一层钢弯管外管(1),其改进之处在于在外管(1)内具有一层钢弯管内管(2),在外管(1)和内管(2)之间具有一层浇铸的抗磨合金白口铁浇铸层(3)。这种结构的耐磨弯管的内管(2)磨损后,其抗磨合金白口铁浇铸层(3)具有良好的耐磨性能,它具有重量轻、制造工艺简单、成本低的优点。

Description

一种耐磨弯管
本实用新型涉及一种用于工业管路的耐磨管,特别是耐磨弯管。
目前,在公知的用于工业管路的耐磨弯管中,有铸石耐磨复合弯管,它具有一层钢管弯管外管,在外管内复合一层铸石管耐磨内管,这种结构的耐磨弯管具有良好的耐磨性能,其不足之处是其重量大,复合工艺复杂,制造成本高。
本实用新型的目的在于提供一种耐磨弯管,以克服公知技术之不足。
本实用新型是这样实现的:一种耐磨弯管,它包括一层钢弯管外管(1),其改进之处在于在外管(1)内具有一层钢弯管内管(2),在外管(1)和内管(2)之间具有一层浇铸的抗磨合金白口铁浇铸层(3)。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是钼钒白口铸铁浇铸层。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是锰钼铜钒白口铸铁浇铸层。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是铬镍铸铁浇铸层。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是高铬铸铁浇铸层。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是铬28浇铸层。
本实用新型耐磨弯管,可以是抗磨合金白口铁浇铸层(3)是铬15钼3浇铸层。
本实用新型提供的耐磨弯管,其内管(2)被磨损后抗磨合金白口铁浇铸层(3)具有良好的耐磨性能,它具有重量轻、制造工艺简单、成本低的优点。
图1:本实用新型耐磨弯管一种结构的主视剖视图。
参照附图结合实施例对本实用新型作进一步说明。
实施例1,图1给出了本实用新型一种具体结构,参阅图1,一种耐磨弯管,它包括一层钢弯管外管(1),在外管(1)内具有一层钢弯管内管(2),在外管(1)和内管(2)之间具有一层浇铸的抗磨合金白口铁浇铸层(3)。抗磨合金白口铁浇铸层(3)可以是钼钒白口铸铁浇铸层;抗磨合金白口铁浇铸层(3)可以是锰钼铜钒白口铸铁浇铸层;抗磨合金白口铁浇铸层(3)可以是铬镍铸铁浇铸层;抗磨合金白口铁浇铸层(3)可以是高铬铸铁浇铸层;抗磨合金白口铁浇铸层(3)也可以是铬28浇铸层;抗磨合金白口铁浇铸层(3)还可以是铬15钼3浇铸层。抗磨合金白口铁具有良好的耐磨性,但其机械性能差,不易焊接。这种结构的耐磨弯管其外管(1)具有良好的机械性能,其内管(2)在浇铸过程起到了内模的作用,在管路运行过程内管(2)磨损后抗磨合金白铁浇铸层(3)具有良好的耐磨性能。它具有重量轻,制造工艺简单、成本低的优点。

Claims (7)

1、一种耐磨弯管,它包括一层钢弯管外管(1),其特征在于在外管(1)内具有一层钢弯管内管(2),在外管(1)和内管(2)之间具有一层浇铸的抗磨合金白口铁浇铸层(3)。
2、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是钼钒白口铸铁浇铸层。
3、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是锰钼铜钒白口铸铁浇铸层。
4、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是铬镍铸铁浇铸层。
5、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是高铬铸铁浇铸层。
6、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是铬28浇铸层。
7、根据权利要求1所述的耐磨弯管,其特征在于抗磨合金白口铁浇铸层(3)是铬15钼3浇铸层。
CN 00215169 2000-06-14 2000-06-14 一种耐磨弯管 Expired - Fee Related CN2433493Y (zh)