CN202347109U - Negative plate for electrolytic copper powder - Google Patents
Negative plate for electrolytic copper powder Download PDFInfo
- Publication number
- CN202347109U CN202347109U CN201120477692.0U CN201120477692U CN202347109U CN 202347109 U CN202347109 U CN 202347109U CN 201120477692 U CN201120477692 U CN 201120477692U CN 202347109 U CN202347109 U CN 202347109U
- Authority
- CN
- China
- Prior art keywords
- conductive
- negative plate
- copper powder
- long
- electrolytic copper
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
技术领域 technical field
本实用新型涉及一种阴极板,尤其涉及一种电解铜粉用阴极板。 The utility model relates to a cathode plate, in particular to a cathode plate for electrolytic copper powder.
背景技术 Background technique
在铜粉电解槽中,阴极板、阳极板交错排列,按工艺要求保持一定间距。现有的阴极板有一长一短两个挂耳,长挂耳端直接与导电铜排接触导电,短挂耳端不与导电铜排接触因此不导电。由于阴极板通常较簿(4-6mm),且两挂耳之间的距离由电解槽面的宽度确定,因此,导电面积由阴极板厚度与挂耳长度决定。由于阴极板较簿,挂耳与导电铜排接触截面积小,因此导致电解过程中挂耳发烫,降低了导电效率。 In the copper powder electrolytic cell, the cathode plate and the anode plate are arranged in a staggered manner, and a certain distance is maintained according to the process requirements. The existing cathode plate has two hanging lugs, one long and one short. The end of the long hanging lug is directly in contact with the conductive copper bar for conducting electricity, and the end of the short hanging lug is not in contact with the conductive copper bar, so it is not conductive. Since the cathode plate is usually relatively thin (4-6mm), and the distance between the two hanging lugs is determined by the width of the electrolytic tank, the conductive area is determined by the thickness of the cathode plate and the length of the hanging lugs. Because the cathode plate is relatively thin, the contact cross-sectional area of the hanging lug and the conductive copper bar is small, which causes the hanging lug to become hot during the electrolysis process and reduces the conduction efficiency.
实用新型内容 Utility model content
本实用新型的目的在于提供一种挂耳不易发烫的电解铜粉用阴极板。 The purpose of this utility model is to provide a cathode plate for electrolytic copper powder with hanging lugs that are not easily heated.
本实用新型的目的是这样实现的,一种电解铜粉用阴极板,包括短挂耳和长挂耳,其特征在于:所述长挂耳为两级台阶式且其端部侧面通过与其适配的导电块和导电铜排连接。 The purpose of this utility model is achieved in this way, a cathode plate for electrolytic copper powder, including short hanging lugs and long hanging lugs, characterized in that: the long hanging lugs are two-stage stepped and the side of the end part passes through it. The matching conductive block is connected to the conductive copper bar.
所述长挂耳上设有两个连接孔且通过螺栓与所述导电块连接。 The long hanging lug is provided with two connection holes and is connected with the conductive block through bolts.
本实用新型具有如下有益效果,本实用新型将阴极板的长挂耳设计为两级台阶式且其侧面通过与其适配的导电块和导电铜排连接,增大了导电过流面积,提高了导电效率。 The utility model has the following beneficial effects. In the utility model, the long lug of the cathode plate is designed as a two-stage step type, and its side is connected with a conductive block and a conductive copper bar adapted to it, which increases the conductive overcurrent area and improves the conduction efficiency.
附图说明 Description of drawings
图1为现有阴极板结构示意图; Figure 1 is a schematic diagram of the existing cathode plate structure;
图2为本实用新型实施例结构示意图。 Figure 2 is a schematic structural diagram of an embodiment of the utility model.
具体实施方式 Detailed ways
实施例,一种电解铜粉用阴极板,阴极板1上有短挂耳和长挂耳,长挂耳为两级台阶式,长挂耳的端部侧面通过与其适配的导电块和导电铜排连接,长挂耳的端部设有两个连接孔2且通过螺栓与导电块连接。
An embodiment, a cathode plate for electrolytic copper powder, there are short lugs and long lugs on the
Claims (2)