[go: up one dir, main page]

CN202259531U - Accumulator plate curing kiln - Google Patents

Accumulator plate curing kiln Download PDF

Info

Publication number
CN202259531U
CN202259531U CN2011203531485U CN201120353148U CN202259531U CN 202259531 U CN202259531 U CN 202259531U CN 2011203531485 U CN2011203531485 U CN 2011203531485U CN 201120353148 U CN201120353148 U CN 201120353148U CN 202259531 U CN202259531 U CN 202259531U
Authority
CN
China
Prior art keywords
main chamber
air
air inlet
concubine
air outlet
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Lifetime
Application number
CN2011203531485U
Other languages
Chinese (zh)
Inventor
彭正雄
朱新华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU JINFAN POWER TECHNOLOGY CO LTD
Original Assignee
JIANGSU JINFAN POWER TECHNOLOGY CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU JINFAN POWER TECHNOLOGY CO LTD filed Critical JIANGSU JINFAN POWER TECHNOLOGY CO LTD
Priority to CN2011203531485U priority Critical patent/CN202259531U/en
Application granted granted Critical
Publication of CN202259531U publication Critical patent/CN202259531U/en
Anticipated expiration legal-status Critical
Expired - Lifetime legal-status Critical Current

Abstract

The utility model relates to a battery polar plate curing kiln, main chamber including the elongated, including a plurality of solidification unit in the main chamber, every solidification unit includes the loco that is linked together with the main chamber, be provided with the humidification device that heats in the loco, the bottom of main chamber is provided with the air intake, the lateral part of main chamber is provided with the air-supply line, the one end of air-supply line is connected with the air intake, the air outlet of fan is connected to the other end of air-supply line, the fan setting is outside in the main chamber, be provided with the air outlet on the loco, air outlet department is provided with out the tuber pipe, the air intake. The utility model is suitable for a solidify battery plate, its solidification quality that can improve battery plate.

Description

The battery polar plate solidification kiln
Technical field
The utility model relates to the technical field of battery polar plate solidification drying equipment, is meant a kind of deep-wall type battery polar plate solidification kiln especially.
Background technology
In the production process of accumulator plate; It is that the pole plate that has just coated is cured drying that one procedure is arranged; By fork truck which floor the pole plate frame stacked and deliver in the solidying kiln, pole plate is cured under certain temperature, higher humidity, if temperature does not reach requirement; Too high meeting makes the lead plaster embrittlement on the pole plate, drops easily; Cross and low the pole plate drying is not passed through, water content exceeds standard, if humidity does not reach requirement, the pole plate of production just has crackle, the requirement that the discharge capacity of assembling back battery does not just reach regulation.Therefore, the uniformity of humiture is particularly important to the quality of pole plate, and humiture evenly is to lean on the uniformity of wind circulation to reach.Solidying kiln scheme as shown in Figure 4, common: an air channel is respectively made on two limits about solidying kiln, Yi Bian air-out; Air intake on one side, negative pressure air channel 1 is drawn into concubine 2 with the air in the main chamber 7, through heater 3 air heat; Under the effect of blower fan 4; Blow to malleation air channel 5 to the air after the heating, hot-air blows to main chamber 7 through the slit between the cloth wind screen 6, finally forms a systemic circulation.Wherein the space size of the size of air quantity, main chamber has determined the uniformity of circulated air.And institute's required airflow will change, and needed wind speed is slower when solidifying, only need be pneumatic, and needed wind speed will reach more than the 2.5m/s when drying, and this is the requirement of technology, can not change.The space that only changes, the space is more little, and the uniformity is just high more.But little by existing structure receipts, cost performance is just very low.
The utility model content
The utility model technical problem to be solved is: provide a kind of humiture the relatively even and higher battery polar plate solidification kiln of area utilization.
For addressing the above problem, the technical scheme that the utility model adopts is: the battery polar plate solidification kiln comprises the main chamber of sleeve configuration; Comprise several solidified cells in the said main chamber, each solidified cell comprises the concubine that is connected with the main chamber, is provided with warming and wetting apparatus in the concubine; The bottom of main chamber is provided with air inlet, and the sidepiece of main chamber is provided with blast pipe, and an end of blast pipe is connected with air inlet; The other end of blast pipe connects the air outlet of blower fan, and blower fan is arranged on the outside, main chamber, and concubine is provided with air outlet; The air outlet place is provided with discharge pipe, and the other end of discharge pipe connects the air inlet of blower fan.
The bottom of said main chamber is provided with line slideway, and line slideway is provided with the pole plate frame.
Said each solidified cell also comprises the flow-stopping plate that is arranged on main chamber and the below that is communicated with the place of concubine.
The beneficial effect of the utility model is: above-mentioned battery polar plate solidification kiln, it is simple in structure, easy to use, with low cost.It can make the circulated air in the main chamber more even, thus make in the main chamber humiture relatively evenly and also area utilization higher, thereby can improve the quality of polar plate solidification.
Description of drawings
Fig. 1 is the main TV structure sketch map of the utility model battery polar plate solidification kiln;
Fig. 2 is the plan structure sketch map of Fig. 1;
Fig. 3 is the sectional structure sketch map of A-A part among Fig. 2;
Fig. 4 is the structural representation of the present employed battery polar plate solidification kiln described in the background technology;
Among Fig. 1 to Fig. 3: 1, main chamber, 2, line slideway, 3, the pole plate frame, 4, concubine, 5, flow-stopping plate, 6, air inlet, 7, blast pipe, 8, blower fan, 9, air outlet, 10, discharge pipe, 11, the air inlet cover plate;
Among Fig. 4: 1, negative pressure air channel, 2, concubine, 3, heater, 4, blower fan, 5, the malleation air channel, 6, cloth wind screen, 7, the main chamber.
Embodiment
Through specific embodiment the utility model battery polar plate solidification kiln is done further to describe in detail below.
Like Fig. 1, Fig. 2, shown in Figure 3, the battery polar plate solidification kiln comprises the main chamber 1 of sleeve configuration; Comprise two rows, four row totally eight solidified cells in the main chamber 1, the bottom of main chamber 1 is provided with four row line slideways 2, and per two row line slideways 2 are provided with pole plate frame 3; Each solidified cell comprises the concubine 4 that is connected with main chamber 1, is provided with the warming and wetting apparatus (not shown) in the concubine 4, and the top of main chamber 1 is provided with flow-stopping plate 5; Flow-stopping plate 5 is provided with the exhaust vent (not shown), and the effect of flow-stopping plate 5 is to prevent that condensed water from directly dropping on the pole plate and cause pole plate to sustain damage, and the bottom of main chamber 1 is provided with air inlet 6; Air inlet 6 places are provided with air inlet cover plate 11, are provided with porosely in the air inlet cover plate 11, and the sidepiece of main chamber 1 is provided with blast pipe 7; One end of blast pipe 7 is connected with air inlet 6; The other end of blast pipe 7 connects the air outlet of blower fan 8, and blower fan 8 is arranged on 1 outside, main chamber, and concubine 4 is provided with air outlet 9; Air outlet 9 places are provided with discharge pipe 10, and the other end of discharge pipe 10 connects the air inlet of blower fan 8.
The operation principle of the utility model is: through the work of blower fan 8; Air in the main chamber 1 gets into concubine 4 after via the exhaust vent on the drainage plate, behind the heating of warming and wetting apparatus, humidification, gets into blower fans 8 through air outlet 9; Air outlet 9 by blower fan 8 is discharged; Air inlet 6 via blast pipe 71 bottom from the main chamber gets into main shaft, make thus to form some strands of circulated airs in the whole main chamber 1, so the circulation wind energy evenly distributes in the main chamber 1.Because the air inlet 6 entering main chambers 1 of circulated air 1 bottom, make the circulated air on width two side directions of main chamber 1 also more even, thereby improved the quality of polar plate solidification from the main chamber.In addition, employing line slideway 2 is carried pole plate with cooperating of pole plate frame 3, makes pole plate frame 3 need not stack with fork truck, only need push ahead along line slideway 2 to get final product, and can save fork truck equipment and full-time Forklift Worker, has practiced thrift the production cost of enterprise.Eight solidified cells are two rows, four row to be arranged, and makes the adjacent solidified cell can a shared face wall, thereby the space is practiced thrift more, manufacturing cost is lower and save energy consumption.
The above embodiments are the principle and the effect thereof of illustrative the invention only, and the embodiment of part utilization, but not is used to limit the utility model; Should be pointed out that for the person of ordinary skill of the art under the prerequisite that does not break away from the utility model creation design, can also make some distortion and improvement, these all belong to the protection range of the utility model.

Claims (4)

1. battery polar plate solidification kiln comprises the main chamber of sleeve configuration it is characterized in that: comprise several solidified cells in the said main chamber; Each solidified cell comprises the concubine that is connected with the main chamber, is provided with warming and wetting apparatus in the concubine, and the bottom of main chamber is provided with air inlet; The sidepiece of main chamber is provided with blast pipe, and an end of blast pipe is connected with air inlet, and the other end of blast pipe connects the air outlet of blower fan; Blower fan is arranged on the outside, main chamber; Concubine is provided with air outlet, and the air outlet place is provided with discharge pipe, and the other end of discharge pipe connects the air inlet of blower fan.
2. battery polar plate solidification kiln according to claim 1 is characterized in that: the bottom of said main chamber is provided with line slideway, and line slideway is provided with the pole plate frame.
3. battery polar plate solidification kiln according to claim 1 and 2 is characterized in that: said each solidified cell also comprises the flow-stopping plate that is arranged on main chamber and the below that is communicated with the place of concubine.
4. battery polar plate solidification kiln according to claim 1 and 2 is characterized in that: the air inlet place of said main chamber is provided with the air inlet cover plate, is provided with porose in the air inlet cover plate.
CN2011203531485U 2011-09-20 2011-09-20 Accumulator plate curing kiln Expired - Lifetime CN202259531U (en)