CN1586912A - Process for producing building material and artificial yuhua pebble - Google Patents
Process for producing building material and artificial yuhua pebble Download PDFInfo
- Publication number
- CN1586912A CN1586912A CN 200410070790 CN200410070790A CN1586912A CN 1586912 A CN1586912 A CN 1586912A CN 200410070790 CN200410070790 CN 200410070790 CN 200410070790 A CN200410070790 A CN 200410070790A CN 1586912 A CN1586912 A CN 1586912A
- Authority
- CN
- China
- Prior art keywords
- add
- artificial
- mold
- cured
- mould
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention relates to the technological process of making building material and artificial Yuhua pebble, and features that after the material for building material and artificial Yuhua pebble is prepared, the building material and artificial Yuhua pebble is made through injection molding. The technological process is short, low in cost and environment friendly, and the product is high in artistic value.
Description
Technical field
The present invention relates to the making construction method of building materials or artificial Yuhuatai colorful pebble, belong to water mould, imitation yuhua-stone material and goods field.
Existing Yuhuatai colorful pebble is the building materials and ornaments product, can't change material and product-use, so goods are on sense organ, works with great care not as Counterfeit Item, and color is soft and moist, imitated vestige.
The purpose of this invention is to provide the process for making of building materials or artificial rain flower stone material and goods, goods obviously are better than existing goods, and the Counterfeit Item duration is short, and cost is low; Not being subjected to the restriction in environment, space, kind, specification, color, classification, traditional handicraft, material, environmental protection, market, is to have material and the goods of viewing and admiring, collect, develop value.
1) simulation:
(1) system plaster cast: gypsum is added 801 glue, mix well, water and be filled in, after solidifying it is engraved as the model that adheres to specification than in big 0.5~10 centimeter sylphon of model by the mixing of 100: 40~70 ratio;
(2) polishing: the corase grind machine, finish grind by hand, to the light cleaning;
(3) go up cured: the floor is cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the model, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
2) system plane soft or hard mould:
(1) system sylphon: vary in size according to model, make the sylphon of different size;
(2) system soft mold: silicon rubber is added curing agent, mix well in 100: 5~20 ratio mixing, brush was being gone up on that cured half model;
(3) drying: dried in the shade slow curing 2~24 hours 1~2 hour;
(4) system hard mold: resin is added ketone slurry add and buy liquid and add talcum powder, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, brush do not water gypsum mold half soft mold on, spread two layers of fine glass fibre cloth, again above-mentioned hybrid resin is brushed at fine glass fibre cloth, layer overlay thick glass fibre cloth waters above-mentioned hybrid resin and is filled on the thick glass fibre cloth till flood over half 0,5~10 centimeters of thick glass fibre cloth;
(5) drying: dried in the shade 10~30 minutes;
(6) die sinking tool: open box, remove tabula rasa, take out the model of the inside;
(7) go up cured: the floor is cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the soft or hard mould inner wall, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly;
3) system imitation yuhua-stone material: transparent resin is added diluent add curing agent and add required color=100: 10~30: 10~30: 10~30.
4) system imitation yuhua-stone material and goods:
(1) mould: soft mold is put in the hard mold;
(2) goods: transparent resin is added diluent add curing agent and add required color, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, with syringe or other vessel, inject or water and be filled in soft mold or soft or hard mould or hard mold or the gypsum mold, buckle the pressing mold tool, with the limit that a plurality of clips are clamped mould, above-mentioned hybrid resin can't be leached;
(3) drying: dry in the shade to just solidifying;
(4) die sinking tool: open mould, take out early-products:
(5) engraving: early-products is engraved as the goods that adhere to specification;
(6) cool off: goods are placed in the cold water soaked 30 minutes~1 hour;
(7) polishing: the corase grind machine, finish grind by hand, to the light cleaning;
With building materials or the artificial granite stone that above-mentioned process for making is finished, it is exquisite, elegant in appearance to do manual work, and is that the utmost point has material and the goods of viewing and admiring, develop value.
The specific embodiment:
Introduce the step of making building materials or granolith stone material and goods of process provided by the present invention below.
Building materials artificial granite stone profile: length * wide * thick=50 centimeter * 50 centimeters * 2 centimeters
Basic pattern is a granite.
1) simulation:
(1) system plaster cast: gypsum is added 801 glue, mix well, water and be filled in, after solidifying it is engraved as the model that adheres to specification than in big 0.5~10 centimeter sylphon of model by the mixing of 100: 40~70 ratio;
(2) polishing: with the sand polishing, from thick number to thin number, to the light cleaning;
(3) go up cured: the floor is cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the model, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
2) system plane soft or hard mould:
(1) system sylphon: vary in size according to model, make the sylphon of different size;
(2) system soft mold: silicon rubber is added curing agent, mix well in 100: 5~20 ratio mixing, brush was being gone up on that cured half model;
(3) drying: dried in the shade slow curing 2~24 hours 1~2 hour;
(4) system hard mold: resin is added ketone slurry add and buy liquid and add talcum powder, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, brush do not water gypsum mold half soft mold on, spread two layers of fine glass fibre cloth, again above-mentioned hybrid resin is brushed at fine glass fibre cloth, layer overlay thick glass fibre cloth waters above-mentioned hybrid resin and is filled on the thick glass fibre cloth till flood over half 0,5~10 centimeters of thick glass fibre cloth;
(5) drying: dried in the shade 10~30 minutes;
(6) go up cured: analyse ground cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the soft or hard mould inner wall, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
3) system imitation yuhua-stone material: transparent resin is added diluent add curing agent and add required color=100: 10~30: 10~30: 10~30.
4) system imitation yuhua-stone material and goods:
(1) mould: soft mold is put in the hard mold;
(2) goods: transparent resin is added diluent add curing agent and add required color, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, use vessel, water and be filled in soft mold or soft or hard mould or hard mold or the gypsum mold, buckle the pressing mold tool, with the limit that a plurality of clips are clamped mould, above-mentioned hybrid resin can't be leached;
(3) drying: dry in the shade to just solidifying:
(4) die sinking tool: open mould, take out early-products;
(5) engraving: early-products is engraved as the goods that adhere to specification;
(6) cool off: goods are placed in the cold water soaked 30 minutes~1 hour;
(8) polishing: the corase grind machine, finish grind by hand, to the light cleaning;
(9) go up coloring agent; Above-mentioned mixed transparent resin is sprayed on the goods, till satisfied;
(10) japanning: blowing varnish is sprayed repeatedly to goods, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
Claims (9)
1, the process for making of building materials or artificial Yuhuatai colorful pebble, its particular-trade are to carry out according to the following steps:
1) simulation:
(1) system plaster cast: gypsum is added 801 glue, mix well, water and be filled in, after solidifying it is engraved as the model that adheres to specification than in big 0.5~10 centimeter sylphon of model by the mixing of 100: 40~70 ratio;
(2) polishing: with the sand polishing, from thick number to thin number, to the light cleaning;
(3) go up cured: the floor is cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the model, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
2) system plane soft or hard mould:
(1) system sylphon: vary in size according to model, make the sylphon of different size;
(2) system soft mold: silicon rubber is added curing agent, mix well in 100: 5~20 ratio mixing, brush was being gone up on that cured half model;
(3) drying: dried in the shade slow curing 2~24 hours 1~2 hour;
(4) system hard mold: resin is added ketone slurry add and buy liquid and add talcum powder, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, brush do not water gypsum mold half soft mold on, spread two layers of fine glass fibre cloth, again above-mentioned hybrid resin is brushed at fine glass fibre cloth, layer overlay thick glass fibre cloth waters above-mentioned hybrid resin and is filled on the thick glass fibre cloth till flood over half 0,5~10 centimeters of thick glass fibre cloth;
(5) drying: dried in the shade 10~30 minutes;
(6) go up cured: analyse ground cured or mould is cured or the spray of table leather board is cured, brush or be sprayed on the soft or hard mould inner wall, dried in the shade 15~20 minutes, this step need be carried out 2~3 times repeatedly.
3) system imitation yuhua-stone material: transparent resin is added diluent add curing agent and add required color=100: 10~30: 10~30: 10~30.
4) system imitation yuhua-stone material and goods:
(1) mould: soft mold is put in the hard mold;
(2) goods: transparent resin is added diluent add curing agent and add required color, ratio mixing in 100: 10~30: 10~30: 10~30 is mixed well, use vessel, water and be filled in soft mold or soft or hard mould or hard mold or the gypsum mold, buckle the pressing mold tool, with the limit that a plurality of clips are clamped mould, above-mentioned hybrid resin can't be leached;
(3) drying: dry in the shade to just solidifying;
(4) die sinking tool: open mould, take out early-products;
(5) engraving: early-products is engraved as the goods that adhere to specification;
(6) cool off: goods are placed in the cold water soaked 30 minutes~1 hour;
(7) polishing: the corase grind machine, finish grind by hand, to the light cleaning.
2, model: the preparation method of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described cast material is that wood, 801 glue add the shape that land plaster=100: 40~70 or foundry loam, rubber sculpture become designing requirement.
3, main body bonding: the preparation method of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described binding material is that 302 glue or 502 glue add talcum powder and add saw wood ash=100: 10~30: 10~30.
4, moulding: the method for manufacturing technology of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described Modeling Material is reinforcing bar or steel pipe or iron wire or iron pipe or iron nail or fastener or copper wire or copper pipe.
5, putty: building materials according to claim 1 or artificial Yuhuatai colorful pebble process for making, it is characterized in that described putty material is that transparent resin adds diluent and adds curing agent and add talcum powder and add required color=100: 10~30: 10~30: 10~30: 10~30 or atom ash and add curing agent and add required color=100: 10~30: 10~30.
6, soft mold: the process for making of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described soft model material is that silicon rubber adds curing agent=100: 5~20.
7, hard mold and hollow mould: the process for making of building materials according to claim 1 or artificial Yuhuatai colorful pebble, it is characterized in that described hard mold and hollow mould material are that resin adds ketone slurry and adds and buy liquid and add talcum powder=100: 10~30: 10~30: 10~30 and add two layers of fine glass fibre cloth, one deck thick glass fibre cloth.
8, imitation yuhua-stone: the process for making of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described Yuhuatai colorful pebble material is that resin adds ketone slurry and adds talcum powder and add saw wood ash and add required color=100: 10~30: 10~30: 10~30: 10~30: 10~30.
9, go up coloring agent: the preparation method of building materials according to claim 1 or artificial Yuhuatai colorful pebble is characterized in that described coloring agent material is that transparent resin adds diluent and adds curing agent and add required color.