CN1325413C - 用磷渣生产微晶玻璃饰板的方法 - Google Patents
用磷渣生产微晶玻璃饰板的方法 Download PDFInfo
- Publication number
- CN1325413C CN1325413C CNB2005100032056A CN200510003205A CN1325413C CN 1325413 C CN1325413 C CN 1325413C CN B2005100032056 A CNB2005100032056 A CN B2005100032056A CN 200510003205 A CN200510003205 A CN 200510003205A CN 1325413 C CN1325413 C CN 1325413C
- Authority
- CN
- China
- Prior art keywords
- gas
- phosphorus slag
- plaque
- standby
- materials
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (5)