CN1266455A - Use of phosphorylated cellulose in detergent compositions - Google Patents
Use of phosphorylated cellulose in detergent compositions Download PDFInfo
- Publication number
- CN1266455A CN1266455A CN 98808030 CN98808030A CN1266455A CN 1266455 A CN1266455 A CN 1266455A CN 98808030 CN98808030 CN 98808030 CN 98808030 A CN98808030 A CN 98808030A CN 1266455 A CN1266455 A CN 1266455A
- Authority
- CN
- China
- Prior art keywords
- water
- cellulose
- phosphoric acid
- weight
- mierocrystalline cellulose
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention pertains to the use of a water-soluble phosphorylated cellulose which is obtained by dissolving cellulose in a phosphoric acid-containing solvent to produce a solution 94-100 wt.% which is composed of the constituents cellulose, phosphoric acid and/or its anhydrides, and water, in detergent compositions. The use concerns utilisation both in detergents for textiles and in dishwashing detergents.
Description
The present invention relates to the purposes of water-soluble phosphorus acid cellulose in cleaning composition.
At US-A-2, the preparation of water soluble cellulose has been discussed in 759,924, and has been taked in the alcohol that dissolves each other with it with phosphoric acid and P
2O
5The cellulosic form of esterification solution-treated.This reaction occurs in multiphase system, needs carefully to guarantee that the particle cellulose powder is not dissolved in the reaction mixture.Although point out, the product that obtains like this can be used for textile industry, for example,, find as detergent additive, under certain conditions, because too high partial cross-linking may cause gelation when known product is soluble in water.As a result, as if these products of discussing in the said document are not suitable for cleaning composition commonly used.
The present invention provides a kind of water-soluble phosphorus acid cellulose that is used for cleaning composition now, can cause any gelation hardly when it is soluble in water.
The invention reside in by cellulose dissolution is obtained be used for saving the water-soluble phosphorus acid cellulose of the known application of mentioning in the solvent of phosphoric acid, the 94-100% weight in the aqueous solution that obtains is grouped into by Mierocrystalline cellulose, phosphoric acid and/or one-tenth such as phosphoric anhydride and water.
Should be noted that, solvent by Mierocrystalline cellulose being dissolved in phosphoric acid is with preparation water-soluble phosphorus acid cellulose, the 94-100% weight of the solution that obtains is grouped into by Mierocrystalline cellulose, phosphoric acid and/or one-tenth such as phosphoric anhydride and water, and this aqueous solution is known from unpub WO 97 30090.But, in said document, do not mention the potential application of water-soluble phosphorus acid cellulose in cleaning composition.
Phosphoric acid one speech is meant all mineral acids of phosphorus and their mixture.Ortho-phosphoric acid is phosphoric acid, i.e. H
3PO
4, its anhydrous equivalent is Vanadium Pentoxide in FLAKES (P
2O
5).Except ortho-phosphoric acid and Vanadium Pentoxide in FLAKES,, also has the phosphoric acid of ability between five phosphorus oxide and ortho-phosphoric acid of a series of combination water, for example Tripyrophosphoric acid (H according to the water yield in the system
6P
4O
13, PPA).
When the preparation phosphorylated cotton, in solution, except water, phosphoric acid and/or phosphoric anhydride, Mierocrystalline cellulose and/or phosphoric acid and cellulosic reactor product, also there is other material.This solution can be by with four kinds of compositions: the mineral acid of Mierocrystalline cellulose, water, phosphorus comprises that its acid anhydride and other composition mix and makes." other composition " can be to help cellulose solution, the solvent except that phosphoric acid or batching (additive), for example reagent of anti-as far as possible cellulose degradation or dyestuff etc.Phosphorus is incorporated into Mierocrystalline cellulose and is also included within the composition of the 94-100% weight that constitutes solution.Under the situation of Mierocrystalline cellulose bonded phosphorus, the cellulosic % weight ratio that is listed in the solution in the patent specification is relevant with the amount of calculating according to Mierocrystalline cellulose.This also is applicable to the amount of the phosphorus of mentioning in a similar manner in this specification sheets.
US 3,424, disclose in the home-use aqueous detergent in 545 and used phosphorylated cotton.Obtain phosphorylated cotton with containing urea and ortho-phosphoric solution impregnation " band Indians head portrait " fiber.The water-fast phosphorylated cotton that obtains finds to have the effect of softening water in the time of in being used in above-mentioned washing composition.But, do not find to use this phosphorylated cotton that known water-softening agent is had any improved action.
Solvent by Mierocrystalline cellulose being dissolved in phosphoric acid is with preparation water-soluble phosphorus acid cellulose, the 94-100% weight of the aqueous solution that obtains is grouped into by Mierocrystalline cellulose, phosphoric acid and/or one-tenth such as its acid anhydride and water, this aqueous solution is found in is not only auxiliary washing assistant in the cleaning composition, but also is greyish white dose of resistance or anti-deposition agent and dispersion agent.Auxiliary washing assistant refers specifically to the polymkeric substance that is added in the washing composition, and they contain zeolite mostly as washing assistant.The auxiliary effect of washing assistant altogether is to be suppressed in the detergent to deposit, for example CaCO
3Generation and growth.By the ashing fabric to measure the formation of deposits degree.
The washing composition of usefulness of being generally used in West Europe weaving generally contains the zeolite of 20-35% weight.When use is of the present invention, these washing composition will contain the phosphorylated cotton of maximum 10% weight, be preferably 1-5% weight, more preferably 2-4% weight.
The phosphorylated cotton that obtains by aforesaid method be found to be specially adapted to not moisture, i.e. the detergent composition of Ganing (with the form of powder or sheet).Find to contain therein in the known cleaning composition of zeolite, this phosphorylated cotton is effective especially as auxiliary washing assistant, and is bigger than the well-known auxiliary washing assistant effect that contains poly carboxylic acid and sodium salt.
But also find that in this cleaning composition, phosphorylated cotton also is effectively anti-greyish white dose or anti redeposition agent.
When using phosphorylated cotton of the present invention, except the above-mentioned relevant effect of scourability, this phosphorylated cotton also has the favorable properties of the biological degradability of said composition.
Find that also the content of Mierocrystalline cellulose bonded phosphorus and the cellulosic polymerization degree (DP) have some influence to the character of phosphorylated cotton.Be to be equivalent to phosphorylated cotton of the present invention as best found that under the situation of washing composition, the content of its Mierocrystalline cellulose bonded phosphorus is the P of 3-10% weight, be preferably the P of 4-8% weight, cellulosic degree of polymerization is for being lower than 1000, and preferred cellulosic degree of polymerization is 100-750.
The used phosphorylated cotton of the present invention is specially adapted to the washing composition of textile product and washes the dish washing composition.
Be used for preferably powdered acid Mierocrystalline cellulose of washing powder.Perhaps, can use granular or staple fibre (fibril and/or fibrid) form.Making the method for various forms phosphorylated cotton discussed at WO 97 30090.
Measuring method
The mensuration of the polymerization degree
1 (k=0.01) measures the cellulosic polymerization degree (DP) by means of crow uncle class moral type.For this reason, the Mierocrystalline cellulose sample that will measure after neutralization was 50 ℃ of vacuum-dryings 16 hours, and the water yield in copper II ethylenediamine/water mixture considers that the water in the Mierocrystalline cellulose is proofreaied and correct.Use this method, make the solution of the cellulose of 0.3% weight with copper II ethylenediamine/water mixture (1/1).To measured in solution relative viscosity (visc.rat. or the η that obtains
Rel), and thus according to following formula determination limit viscosity (η):
[η]=visc.rat.-1/C+(K×C×(visc.rat.-1)×100
In the formula, the cellulose concentration of C=solution (Grams Per Minute liter)
K=constant=0.25
Formula thus, measure polymerization degree DP as follows:
DP=[η]/0.42 (for [η]<450 milliliter/gram) or
DP
0.76=[η]/2.29 (for [η]>450 milliliter/gram)
After following processing, as measure (phosphoric acid) the cellulosic DP in the solution above-mentionedly.
-the solution Wei Lin that packs into of 20 grams is admixed machine (1 liter), adds 400 milliliters of acetone, then with integral body in the highest mixing down 10 minutes that are provided with.The mixture that obtains is transferred to sieve go up and fully wash with acetone, last, use 2%-NaHCO
3/ the aqueous solution pH that neutralizes in acetone is about 7, washes with acetone thereupon.
Begin from preparation copper II quadrol/water cellulose cellulose solution, as measure the DP of the product that obtains above-mentionedly.
The mensuration of phosphorus content
Mierocrystalline cellulose bonded phosphorus can be used in the mensuration of WO 96/06208 narration method.
But, also have simple method to measure the phosphorus content of cellulose prods.For this reason, at 50 ℃ in vacuum after dry about 15 hours, with the cellulose prods film-making.Use x-ray fluorescence emission spectrometer (for example with the Philips PW 1400 of chromium pipe, line: K α, 50 kilovolts, 50 milliamperes, GE crystal, angle: 141.025, timing: 50 seconds) to measure the x-ray fluorescence intensity of phosphorus in the sheet then.Sheet with known phosphorus content is proofreaied and correct spectrometer, the intensity that records is changed into the phosphorus content of sample with the known simple method of those skilled in the art.
Washing test
Use so-called standardized washing test to measure the effect that additive adds washing composition.These methods are as follows.
-laboratory the washing machine that will be called Linitest is heated to 60 ℃ of temperature.
-with 1.56 gram CaCl
22H
2O and 1.50 gram Na
2SO
4Be dissolved in 2 liters of softening waters the preparation standard hard water solution.
-will contain 1.25 gram Na
2CO
3, 1.15 the gram NaHCO
3, 1.80 gram water glass 27/8,1.00 gram LABS acid, 1.00 gram Elfapur LT 65 SLN and 12.00 gram zeolites are dissolved in preparation concentrated base washings in 1 liter of softening water.
The acidity adjustment of this washing soln is arrived pH=10,50 milliliters neutralizing treatment solution are heated to 40 ℃, and the quantity of material that will test is dissolved in wherein.
-following standard the towel of use in each test is provided with:
Table I coding gross weight (gram) size (square centimeter) the number notes greyish white fabric EMPA 211 8 10 in EMPA 101 17 * 72 * white PE/ cotton in 10 9 white cotton EMPA 213 1 10 * 10 1-150 milliliters standard hard water solution is poured in the cup, add 10 steel balls in cup, each steel ball weighs 1 gram.Add 10 standard towels and 50 milliliters therein in regular turn and contain the alkaline detergent solution that to test composition,, and be placed in the Linitest washing machine the cup sealing.-the Linitest washing machine is kept operation 30 minutes.-after test, with each cup turned letter, rinsing standard towel in the beaker that contains 1 premium on currency.-twist a towel and on bath towel, spread out with hand.-after each wash(ing)cycle, EMPA 101 standard towels are removed.-in a word, washing step is carried out 10 times, uses new EMPA 101 standard towels in every washing step.Wash every day three times.At night, with standard towel drying.-behind 10 washing steps, the dry and ironing with towel.-use Minolta CR110 reflexometer to measure the reflectance of Yxy and C pattern.-in 900 ℃ porcelain crucible, restrain (m with 2
0) 1 hour amount with the mensuration residual ash of EMPA 211 towel pyrolysis.After the off-test, measure the weight (m of residue ash content
i).Pass through m
i/ m
0* 100% calculates ash oontent (%).-measure with the difference of the reflectance of that handled and untreated towel and to turn greyish white degree.Embodiment 1
In above-mentioned washing test, by with known washing composition in the comparison of additive, measure turing greyish white degree and the influence of ash oontent, measure and add the effect of phosphorylated cotton to alkaline detergent solution.
Record following result:
The composition that Table II adds adds quantitative change greyish white degree Δ R (%) ash oontent (%)--24 2.4Sokalan CP 5
1)300 mg/litre, 24 0.9 CMC
2)75 mg/litre, 6 2.1 phosphorylated cottons
3)300 mg/litre 14 0.6
1)Multipolymer with sodium hydroxide part neutral vinylformic acid and maleic anhydride.This multipolymer uses in washing composition in a large number.
2)A large amount of carboxymethyl celluloses that use in washing composition, it is white to be used to prevent to become ashing.
3)Dissolving cellulos obtains the phosphorylated cotton phosphoric acid ester in the solvent of phosphoric acid, 94-100% weight is Mierocrystalline cellulose, phosphoric acid and/or compositions such as its acid anhydride and water in the solution that obtains in this process, content=5.3% of DP=484 and Mierocrystalline cellulose bonded phosphorus.
These results show that it all is effective that phosphorylated cotton turns greyish white to the reduction ash oontent with minimizing.
Embodiment 2
The following examples show that water soluble dyes of the present invention also can be successfully used to preparation and wash the dish washing composition.
Example as typical A utomatic Dish Wash Detergent (ADD) uses following prescription:
The present invention of Table III composition, weight % prior art weight % yellow soda ash 24 24 sodium disilicates, anhydrous 26 26 Trisodium Citrates, dihydrate 32 32 Sodium peroxoborate, monohydrate 6 6TAED 22 tensio-active agents, Plurafac LF 22 amylase, Duramyl 60T 0.5 0.5 proteolytic enzyme, Savinase 6,0T 0.5 0.5 phosphorylated cottons (DP=130 and Mierocrystalline cellulose 7--bonded P=5.1%) Sokolan CP 5
, powdered--carry out under the 7 washing tests condition below: amount of reagent: 20 gram water hardness (
*DH) (Ca/Mg=3/1): 15 dishwasher types: the program univ.55 ℃ of used composition according to the method solid loading of DIN 44990 (in July, 1989) of Miele G 765 SCi has following variation: the drying of the concentration 10 grams per liter cups of tea carries out there was not rinse-added prescription in 1 hour at 90 ℃.Method according to DIN 44990 is also estimated the dish of washing.The result represents with the scale of 1-5, the best result of 5 representatives.Result in the following table is three mean values of estimating:
Table IV
The result who washes dish in the last table clearly illustrates that, phosphorylated cotton of the present invention at least with SokalanCP5
Performance suitable, the latter be difficult for biodegradable.
Polymkeric substance | Phosphorylated cotton | Sokalan?CP5 |
Soil types | Estimate | Estimate |
The meat spinach tea milk of oil ester yolk thick soup chopping is estimated at last | ?5.0 ?4.9 ?2.3 ?4.9 ?3.5 ?4.5 ?2.9 ?4.0 | ??5.0 ??4.9 ??2.5 ??4.9 ??3.9 ??4.8 ??2.4 ??4.0 |
Claims (8)
1. the purposes of water-soluble phosphorus acid cellulose in detergent composition, it is characterized in that, by cellulose dissolution is obtained phosphorylated cotton in the solvent of phosphoric acid, the 94-100% weight of the solution that obtains is made up of Mierocrystalline cellulose, phosphoric acid and/or its acid anhydride and water.
2. the purposes of claim 1 is characterized in that, the DP of phosphorylated cotton<1000, and Mierocrystalline cellulose is a 3-10% weight in conjunction with the content of phosphorus.
3. the purposes of claim 1 is characterized in that, the DP of phosphorylated cotton is 100-750, and the content of Mierocrystalline cellulose bonded phosphorus is 4-8% weight.
4. contain the cellulosic cleaning composition of zeolite and water-soluble phosphoric acid.
5. the cleaning composition of claim 4 is characterized in that, by cellulose dissolution is obtained phosphorylated cotton in the phosphoric acid solvent, the 94-100% weight of the solution that obtains is grouped into by Mierocrystalline cellulose, phosphoric acid and/or one-tenth such as its acid anhydride and water.
6. claim 4 or 5 cleaning composition is characterized in that the DP of phosphorylated cotton is lower than 1000, and the content of Mierocrystalline cellulose bonded phosphorus is 3-10% weight.
7. claim 4 or 5 cleaning composition is characterized in that the DP of phosphorylated cotton is 100-750, and the content of Mierocrystalline cellulose bonded phosphorus is 4-8% weight.
8. the washing composition or the dish washing agent that cleaning composition arbitrary among the claim 4-7 are used for used for textiles.