CN110682389A - 一种木板上色印刷方法 - Google Patents
一种木板上色印刷方法 Download PDFInfo
- Publication number
- CN110682389A CN110682389A CN201810736088.1A CN201810736088A CN110682389A CN 110682389 A CN110682389 A CN 110682389A CN 201810736088 A CN201810736088 A CN 201810736088A CN 110682389 A CN110682389 A CN 110682389A
- Authority
- CN
- China
- Prior art keywords
- wood board
- primer
- coloring
- drying
- polishing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种木板上色印刷方法,其特征在于,包括如下工艺步骤:1)、对木板表面进行300‑500目打磨;2)、打磨完成后去掉木板表面的灰尘;3)、将底漆加热到60‑78℃;4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;5)、对底漆进行烘干,烘干温度为120‑140℃;6)、对烘干底漆后的木板进行上色;7)、上色后对木板表面进行透明材料封面。本发明通过打磨,打磨后上底漆,底漆烘干处理,这样可以保证底漆的稳定性,在底漆具备稳定性的基础上,颜色漆会更稳定,最后通过透明材料进行封装,使颜色漆更长久。
Description
技术领域
本发明涉及印刷技术领域,具体为一种木板上色印刷方法。
背景技术
木板印刷作为很多产业必要的工序之一,其印刷方法非常广泛,比如玩具领域、艺术领域等等。现有的印刷方法上色后,颜色不稳定,长时间使用后容易掉色。
发明内容
(一)解决的技术问题
针对现有技术的不足,本发明提供了一种木板上色印刷方法,根据本发明的上色方法可以让木板上的颜色更稳定,使用寿命更长。
(二)技术方案
为实现上述目的,本发明提供如下技术方案:
一种木板上色印刷方法,其特征在于,包括如下工艺步骤:
1)、对木板表面进行300-500目打磨;
2)、打磨完成后去掉木板表面的灰尘;
3)、将底漆加热到60-78℃;
4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;
5)、对底漆进行烘干,烘干温度为120-140℃;
6)、对烘干底漆后的木板进行上色;
7)、上色后对木板表面进行透明材料封面。
作为上一步优选方案,所述步骤1)中的目数为400目。
作为上一步优选方案,所述步骤3)加热温度为69℃。
作为上一步优选方案,所述步骤5)的烘干温度为130℃。
作为上一步优选方案,所述步骤7)的透明材料为环氧树脂。
作为上一步优选方案,所述步骤7)的透明材料为久烁塑胶。
(三)有益效果
本发明提供了一种木板上色印刷方法,具备以下有益效果:
本发明通过打磨,打磨后上底漆,底漆烘干处理,这样可以保证底漆的稳定性,在底漆具备稳定性的基础上,颜色漆会更稳定,最后通过透明材料进行封装,使颜色漆更长久。
具体实施方式
下面将结合本发明实施例,对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。
实施例1:
一种木板上色印刷方法,其特征在于,包括如下工艺步骤:
1)、对木板表面进行300目打磨;
2)、打磨完成后去掉木板表面的灰尘;
3)、将底漆加热到60℃;
4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;
5)、对底漆进行烘干,烘干温度为120℃;
6)、对烘干底漆后的木板进行上色;
7)、上色后对木板表面进行透明材料封面。
实施例2:
一种木板上色印刷方法,其特征在于,包括如下工艺步骤:
1)、对木板表面进行400目打磨;
2)、打磨完成后去掉木板表面的灰尘;
3)、将底漆加热到69℃;
4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;
5)、对底漆进行烘干,烘干温度为130℃;
6)、对烘干底漆后的木板进行上色;
7)、上色后对木板表面进行透明材料封面。
实施例3:
一种木板上色印刷方法,其特征在于,包括如下工艺步骤:
1)、对木板表面进行500目打磨;
2)、打磨完成后去掉木板表面的灰尘;
3)、将底漆加热到78℃;
4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;
5)、对底漆进行烘干,烘干温度为140℃;
6)、对烘干底漆后的木板进行上色;
7)、上色后对木板表面进行透明材料封面。
需要说明的是,在本文中,诸如第一和第二等之类的关系术语仅仅用来将一个实体或者操作与另一个实体或操作区分开来,而不一定要求或者暗示这些实体或操作之间存在任何这种实际的关系或者顺序。而且,术语“包括”、“包含”或者其任何其他变体意在涵盖非排他性的包含,从而使得包括一系列要素的过程、方法、物品或者设备不仅包括那些要素,而且还包括没有明确列出的其他要素,或者是还包括为这种过程、方法、物品或者设备所固有的要素。在没有更多限制的情况下,由语句“包括一个……”限定的要素,并不排除在包括要素的过程、方法、物品或者设备中还存在另外的相同要素。
尽管已经示出和描述了本发明的实施例,对于本领域的普通技术人员而言,可以理解在不脱离本发明的原理和精神的情况下可以对这些实施例进行多种变化、修改、替换和变型,本发明的范围由所附权利要求及其等同物限定。
Claims (6)
1.一种木板上色印刷方法,其特征在于,包括如下工艺步骤:
1)、对木板表面进行300-500目打磨;
2)、打磨完成后去掉木板表面的灰尘;
3)、将底漆加热到60-78℃;
4)、通过喷涂或者刷漆的方式将底漆涂装在木板表面;
5)、对底漆进行烘干,烘干温度为120-140℃;
6)、对烘干底漆后的木板进行上色;
7)、上色后对木板表面进行透明材料封面。
2.根据权利要求1所述的一种木板上色印刷方法,其特征在于:所述步骤1)中的目数为400目。
3.根据权利要求1所述的一种木板上色印刷方法,其特征在于:所述步骤3)加热温度为69℃。
4.根据权利要求1所述的一种木板上色印刷方法,其特征在于:所述步骤5)的烘干温度为130℃。
5.根据权利要求1所述的一种木板上色印刷方法,其特征在于:所述步骤7)的透明材料为环氧树脂。
6.根据权利要求1或5所述的一种木板上色印刷方法,其特征在于:所述步骤7)的透明材料为久烁塑胶。