CN108453019A - Produce the coating technique of fire-retardant stalk board CPL veneer doors - Google Patents
Produce the coating technique of fire-retardant stalk board CPL veneer doors Download PDFInfo
- Publication number
- CN108453019A CN108453019A CN201810134958.8A CN201810134958A CN108453019A CN 108453019 A CN108453019 A CN 108453019A CN 201810134958 A CN201810134958 A CN 201810134958A CN 108453019 A CN108453019 A CN 108453019A
- Authority
- CN
- China
- Prior art keywords
- fire
- cpl
- stalk board
- coating machine
- rubber roller
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Include being placed on stalk board to be processed in greenhouse after storehouse taking-up to preheat the invention discloses a kind of coating technique producing fire-retardant stalk board CPL veneer doors;PUR hot melt adhesive is put into the glue case of coating machine;The glue box temperature degree of coating machine is set as 198 205 DEG C, sebific duct temperature is 190 197 DEG C, and rubber roller temperature is 185 192 DEG C, and air pressure is 6 megapascal;CPL facing fire-proof plates are placed in the stock roll of coating machine;After rubber roller temperature stabilization, the stalk board is sent in coating machine using material machine is drawn, the PUR hot melt adhesive is filled up by the recess of the stalk board by rubber roller, then coat the CPL facings fire-proof plate;By adopting the above-described technical solution, compared with prior art, PUR hot melt adhesive is added in glue case, glue can be filled to the recess of stalk board during cladding by being preheated to stalk board by the present invention so that cladding CPL facing fire-proof plate rear surfaces are smooth.
Description
Technical field
The invention belongs to building materials technology field more particularly to a kind of coating techniques producing fire-retardant stalk board CPL veneer doors.
Background technology
Batch production decoration panel is suppressed using hot press at this stage, and first facing color paper is laid in above plank,
It is horizontally arranged inside press, is press-formed by heating;The plate surface flatness of stalk board is inadequate, and there is recess on surface, makes
It is serious that surface defect is made with existing heat pressing process.
The content of invention
In view of the deficiencies of the prior art, the invention solves the subproblems in background technology.
To solve the above-mentioned problems, the present invention provides a kind of coating technique producing fire-retardant stalk board CPL veneer doors, packets
Include following steps:Stalk board to be processed is placed on after storehouse taking-up in greenhouse and preheats by step 1);Step 2), will
PUR hot melt adhesive is put into the glue case of coating machine;Step 3) sets the glue box temperature degree of coating machine as 198-205 DEG C, and sebific duct temperature is
190-197 DEG C, rubber roller temperature is 185-192 DEG C, and air pressure is 6 megapascal;CPL facing fire-proof plates are placed on cladding by step 4)
In the stock roll of machine;The stalk board is sent in coating machine after rubber roller temperature stabilization using material machine is drawn by step 5), is led to
It crosses rubber roller and the PUR hot melt adhesive is filled up into the recess of the stalk board, then coat the CPL facings fire-proof plate.
In some embodiments, the step 1) further includes:The temperature of the greenhouse is set as 16-22 DEG C.
In some embodiments, the step 4) further includes:Fire-proof plate is located along the same line with rubber roller center line.
In some embodiments, the step 5) further includes:Glue-spread is 150-200g/ ㎡.
By adopting the above-described technical solution, compared with prior art, the present invention by being preheated to stalk board,
PUR hot melt adhesive is added in glue case, glue can be filled to the recess of stalk board during cladding so that cladding CPL facings fire prevention
Plate rear surface is smooth.
Description of the drawings:
Fig. 1 is the flow diagram for the coating technique that the present invention produces fire-retardant stalk board CPL veneer doors.
Specific implementation mode
The specific implementation mode of the present invention is described in detail below in conjunction with attached drawing.It should be noted that this place is retouched
The specific implementation mode stated is merely to illustrate and explain the present invention, and is not intended to restrict the invention.
As shown in Figure 1, the present invention provides a kind of coating technique producing fire-retardant stalk board CPL veneer doors, including it is as follows
Step:
Step 100, stalk board to be processed is placed on after storehouse taking-up in greenhouse and is preheated;
Step 200, PUR hot melt adhesive is put into the glue case of coating machine;
Step 300, the glue box temperature degree of coating machine is set as 198-205 DEG C, and sebific duct temperature is 190-197 DEG C, rubber roller temperature
It it is 185-192 DEG C, air pressure is 6 megapascal;
Step 400, CPL facing fire-proof plates are placed in the stock roll of coating machine;
Step 500, after rubber roller temperature stabilization, the stalk board is sent in coating machine using material machine is drawn, passes through glue
The PUR hot melt adhesive is filled up the recess of the stalk board by roller, then coats the CPL facings fire-proof plate.
In some optional realization methods of the present embodiment, the temperature of the greenhouse is set as 16-22 DEG C.
In some optional realization methods of the present embodiment, fire-proof plate is located along the same line with rubber roller center line.
In some optional realization methods of the present embodiment, glue-spread is 150-200g/ ㎡.
In some optional realization methods of the present embodiment, the CPL facings fire-proof plate is through impregnated melamine first
Wood grain body paper after aldehyde gum softening and non-woven fabrics laminated continuous sheet made of continuous hot-press.
Embodiment 1:A kind of coating technique producing fire-retardant stalk board CPL veneer doors is present embodiments provided, including as follows
Step:
Step 100, stalk board to be processed is placed on after storehouse taking-up in greenhouse and is preheated;
Step 200, PUR hot melt adhesive is put into the glue case of coating machine;
Step 300, the glue box temperature degree of coating machine is set as 198 DEG C, sebific duct temperature is 190 DEG C, and rubber roller temperature is 185 DEG C,
Air pressure is 6 megapascal;
Step 400, CPL facing fire-proof plates are placed in the stock roll of coating machine;
Step 500, after rubber roller temperature stabilization, the stalk board is sent in coating machine using material machine is drawn, passes through glue
The PUR hot melt adhesive is filled up the recess of the stalk board by roller, then coats the CPL facings fire-proof plate.
In some optional realization methods of the present embodiment, the temperature of the greenhouse is set as 16 DEG C.
In some optional realization methods of the present embodiment, fire-proof plate is located along the same line with rubber roller center line.
In some optional realization methods of the present embodiment, glue-spread is 150g/ ㎡.
In some optional realization methods of the present embodiment, the CPL facings fire-proof plate is through impregnated melamine first
Wood grain body paper after aldehyde gum softening and non-woven fabrics laminated continuous sheet made of continuous hot-press.
Embodiment 2:A kind of coating technique producing fire-retardant stalk board CPL veneer doors is present embodiments provided, including as follows
Step:
Step 100, stalk board to be processed is placed on after storehouse taking-up in greenhouse and is preheated;
Step 200, PUR hot melt adhesive is put into the glue case of coating machine;
Step 300, the glue box temperature degree of coating machine is set as 202 DEG C, sebific duct temperature is 195 DEG C, and rubber roller temperature is 189 DEG C,
Air pressure is 6 megapascal;
Step 400, CPL facing fire-proof plates are placed in the stock roll of coating machine;
Step 500, after rubber roller temperature stabilization, the stalk board is sent in coating machine using material machine is drawn, passes through glue
The PUR hot melt adhesive is filled up the recess of the stalk board by roller, then coats the CPL facings fire-proof plate.
In some optional realization methods of the present embodiment, the temperature of the greenhouse is set as 18 DEG C.
In some optional realization methods of the present embodiment, fire-proof plate is located along the same line with rubber roller center line.
In some optional realization methods of the present embodiment, glue-spread is 180g/ ㎡.
In some optional realization methods of the present embodiment, the CPL facings fire-proof plate is through impregnated melamine first
Wood grain body paper after aldehyde gum softening and non-woven fabrics laminated continuous sheet made of continuous hot-press.
Embodiment 3:A kind of coating technique producing fire-retardant stalk board CPL veneer doors is present embodiments provided, including as follows
Step:
Step 100, stalk board to be processed is placed on after storehouse taking-up in greenhouse and is preheated;
Step 200, PUR hot melt adhesive is put into the glue case of coating machine;
Step 300, the glue box temperature degree of coating machine is set as 205 DEG C, sebific duct temperature is 197 DEG C, and rubber roller temperature is 192 DEG C,
Air pressure is 6 megapascal;
Step 400, CPL facing fire-proof plates are placed in the stock roll of coating machine;
Step 500, after rubber roller temperature stabilization, the stalk board is sent in coating machine using material machine is drawn, passes through glue
The PUR hot melt adhesive is filled up the recess of the stalk board by roller, then coats the CPL facings fire-proof plate.
In some optional realization methods of the present embodiment, the temperature of the greenhouse is set as 22 DEG C.
In some optional realization methods of the present embodiment, fire-proof plate is located along the same line with rubber roller center line.
In some optional realization methods of the present embodiment, glue-spread is 200g/ ㎡.
In some optional realization methods of the present embodiment, the CPL facings fire-proof plate is through impregnated melamine first
Wood grain body paper after aldehyde gum softening and non-woven fabrics laminated continuous sheet made of continuous hot-press.
The preferred embodiment of the present invention is described in detail above in association with attached drawing, still, the present invention is not limited to above-mentioned embodiment party
Detail in formula can carry out a variety of simple changes to technical scheme of the present invention within the scope of the technical concept of the present invention
Type, these simple variants all belong to the scope of protection of the present invention.
It is further to note that specific technical features described in the above specific embodiments, not
It in the case of contradictory, can be combined by any suitable means, in order to avoid unnecessary repetition, how various the present invention is
Possible combination no longer separately illustrates.
In addition, various embodiments of the present invention can be combined randomly, as long as it is without prejudice to originally
The thought of invention, it should also be regarded as the disclosure of the present invention.
Claims (4)
1. a kind of coating technique producing fire-retardant stalk board CPL veneer doors, it is characterised in that include the following steps:
Stalk board to be processed is placed on after storehouse taking-up in greenhouse and preheats by step 1);
PUR hot melt adhesive is put into the glue case of coating machine by step 2);
Step 3) sets the glue box temperature degree of coating machine as 198-205 DEG C, and sebific duct temperature is 190-197 DEG C, and rubber roller temperature is 185-
192 DEG C, air pressure is 6 megapascal;
CPL facing fire-proof plates are placed in the stock roll of coating machine by step 4);
The stalk board is sent in coating machine after rubber roller temperature stabilization using material machine is drawn by step 5), by rubber roller by institute
It states PUR hot melt adhesive and fills up the recess of the stalk board, then coat the CPL facings fire-proof plate.
2. the coating technique of the fire-retardant stalk board CPL veneer doors of production according to claim 1, which is characterized in that the step
It is rapid 1) to further include:The temperature of the greenhouse is set as 16-22 DEG C.
3. the coating technique of the fire-retardant stalk board CPL veneer doors of production according to claim 1, which is characterized in that the step
It is rapid 4) to further include:Fire-proof plate is located along the same line with rubber roller center line.
4. the coating technique of the fire-retardant stalk board CPL veneer doors of production according to claim 1, which is characterized in that the step
It is rapid 5) to further include:Glue-spread is 150-200g/ ㎡.