CN107570969A - A kind of method covered with gold leaf on wrist-watch watch rim - Google Patents

A kind of method covered with gold leaf on wrist-watch watch rim Download PDF

Info

Publication number
CN107570969A
CN107570969A CN201710757680.5A CN201710757680A CN107570969A CN 107570969 A CN107570969 A CN 107570969A CN 201710757680 A CN201710757680 A CN 201710757680A CN 107570969 A CN107570969 A CN 107570969A
Authority
CN
China
Prior art keywords
semi
finished product
gold
ring
watch
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710757680.5A
Other languages
Chinese (zh)
Inventor
金平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huizhou Hi Precision Hardware Co Ltd
Original Assignee
Huizhou Hi Precision Hardware Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Huizhou Hi Precision Hardware Co Ltd filed Critical Huizhou Hi Precision Hardware Co Ltd
Priority to CN201710757680.5A priority Critical patent/CN107570969A/en
Publication of CN107570969A publication Critical patent/CN107570969A/en
Pending legal-status Critical Current

Abstract

The present invention relates to metal-pressed machine field and field of machining, specifically disclose a kind of method covered with gold leaf on wrist-watch watch rim, comprise the following steps A, semi-finished product steel ring is made by punch process and machining in steel ring embryo, gold ring embryo is made to the semi-finished product gold ring that form fit at bag is treated with semi-finished product steel ring by punch process and machining;B, treat that soldering paste is coated on Bao Chu surfaces in semi-finished product steel ring, then put semi-finished product gold ring, semi-finished product steel ring and semi-finished product gold ring are carried out into precompressed with Lever machine obtains the product of pre-molding;C, the product of pre-molding is placed in compaction mold, compaction mold was subjected to stove processing;D, the product that will be crossed after stove processing can obtain circle watch rim covered with gold leaf after carrying out smart car, polishing and cleaning, semi-finished product steel ring and semi-finished product gold ring are pressed into an entirety after coating soldering paste in the present invention, increase the fastness of its combination after crossing stove processing again, and the problems such as deformation, depression are occurred without in follow-up smart car and polishing, overall fit is very good, exquisite appearance.

Description

A kind of method covered with gold leaf on wrist-watch watch rim
Technical field
The present invention relates to metal-pressed machine field and field of machining, more particularly to one kind are covered with gold leaf on wrist-watch watch rim Method.
Background technology
With the continuous improvement of people's living standard and appreciation of arts level, wrist-watch has been not only to be used as timing tool , also have the function of ornament concurrently, play a part of certain decoration and show value, in order that wrist-watch disclosure satisfy that consumer There is the wrist-watch of noble metal appearance member in different demand properties, in the market, and bag last layer is thin on traditional stainless steel watch rim Gold plaque, rare and attractive in appearance effect can be reached, and cost is not high, the price that can meet most of consumer receives the heart Reason, existing product covered with gold leaf are usually to be completed with machining and welding procedure, and this product decay resistance is unqualified, The conjugation of gold plaque and watch rim is not high, and also one kind is after applying soldering paste in watch rim outer surface, is welded gold ring and watch rim surely with firelock, The inferior rate of this way is very high, easily occurs serious deformation in the smart car in later stage and polishing, depression, watch rim and gold ring The problems such as conjugation is not high.
The content of the invention
For above-mentioned technical problem, the invention provides one kind to make steel ring high with being firmly combined with property of gold ring, is less prone to change Shape is with being recessed, method covered with gold leaf on the wrist-watch watch rim of exquisite appearance.
In order to solve the above-mentioned technical problem, concrete scheme provided by the invention is as follows:It is a kind of covered with gold leaf on wrist-watch watch rim Method, comprise the following steps:A, semi-finished product steel ring is made by punch process and machining in steel ring embryo, by gold ring embryo through overshoot The semi-finished product gold ring that form fit at bag is treated with semi-finished product steel ring is made in pressure processing and machining;B, wait to wrap in semi-finished product steel ring Place coats soldering paste in surface, then puts semi-finished product gold ring, semi-finished product steel ring and semi-finished product gold ring are carried out into precompressed with Lever machine obtains To the product of pre-molding;C, the product of pre-molding is placed in compaction mold, compaction mold was subjected to stove processing;D、 The product that will be crossed after stove processing can obtain circle watch rim covered with gold leaf after carrying out smart car, polishing and cleaning.
Preferably, the condition for crossing stove processing is 750 ~ 800 DEG C of furnace temperature, and the time is 15 ~ 20 minutes, increases rerolled steel The being firmly combined with property of circle and semi-finished product gold ring.
Preferably, the cleaning is that ultrasonic wave cleans, including step in detail below:It is by additional proportion in ultrasonic container (35~40):(1~5)Water and Wax removal water, after boiling, the product that is put into after smart car, polishing, cleaning takes after 10 ~ 15 minutes Go out and rinsed well with clear water, cleaning performance is more preferable so that the profile of product is more attractive in appearance.
Preferably, it could open, ensure after compaction mold natural cooling after stove processing was also included before the step D The stickiness of semi-finished product steel ring and semi-finished product gold ring, is opened, soldering paste is uncured, is easily destroyed the patch of its product under the high temperature conditions Conjunction property.
Preferably, the compaction mold includes the upper die and lower die that are connected with screw rod, the upper mould be provided with half into The upper bolster that product gold ring profile matches, the lower mould are provided with the die shoe to match with semi-finished product steel ring bottom, pressure die Tool is bonded completely with shape of product, increases the stickiness and fastness of product.
Compared with prior art, the beneficial effects of the present invention are:After semi-finished product steel ring and semi-finished product gold ring coat soldering paste An entirety is compacted into, is placed on the fastness for increasing its combination in compaction mold after crossing stove processing, and in follow-up essence Car is with occurring without deformation, depression in polishing the problems such as, overall fit is very good, exquisite appearance.
Brief description of the drawings
Fig. 1 is the steel ring embryo and rerolled steel loop graph of the present invention;
Fig. 2 is the gold ring embryo and semi-finished product gold ring figure of the present invention;
Fig. 3 is the product figure of pre-molding of the present invention;
Fig. 4 is the semi-finished product embryo figure of the present invention;
Wherein, 1 is steel ring embryo;2 be semi-finished product steel ring;3 be gold ring embryo;4 be semi-finished product gold ring;5 be the product figure of pre-molding.
Embodiment
In order that those skilled in the art is better understood from technical scheme, below in conjunction with the accompanying drawings to the present invention Technical scheme be further elaborated.
Embodiment:A kind of method covered with gold leaf on wrist-watch watch rim, comprises the following steps:A, steel ring embryo is passed through into punch process Semi-finished product steel ring is made with machining, gold ring embryo is made by punch process and machining and treats shape at bag with semi-finished product steel ring The semi-finished product gold ring of matching;B, treat that soldering paste is coated on Bao Chu surfaces in semi-finished product steel ring, then put semi-finished product gold ring, use lever Semi-finished product steel ring and semi-finished product gold ring are carried out precompressed and obtain the product of pre-molding by machine;C, the product of pre-molding is placed on In compaction mold, compaction mold was subjected to stove processing;D, it will cross after the product after stove is handled carries out smart car, polishing and cleaning and be Can obtain circle watch rim covered with gold leaf, could be opened after compaction mold natural cooling after crossing stove processing, ensure semi-finished product steel ring and partly into The stickiness of product gold ring, is opened under the high temperature conditions, and soldering paste is uncured, is easily destroyed the stickiness of its product.
Wherein, the condition for crossing stove processing is 750 ~ 800 DEG C of furnace temperature, and the time is 15 ~ 20 minutes;Cleaning is ultrasonic wave cleaning, Including step in detail below:It will be pressed in ultrasonic container(35~40):(1~2)Ratio add water and Wax removal water, altogether about 70 ~ 80L, after boiling, the product that is put into after smart car, polishing, after cleaning 10 ~ 15 minutes taking-up rinsed well with clear water, this In embodiment, furnace temperature is 780 DEG C, and it is 18 minutes to spend the stove time, is proportionally added into 40:1 water and Wax removal water, 80L is total up to, finally Scavenging period is 10 minutes.
Compaction mold includes the upper die and lower die being connected with screw rod, and upper mould is provided with to match with semi-finished product gold ring profile Upper bolster, lower mould is provided with the die shoe that matches with semi-finished product steel ring bottom, and compaction mold is bonded completely with shape of product, Increase the stickiness and fastness of product.
The method covered with gold leaf of the present invention, it has manufactured steel ring embryo and gold ring embryo according to design requirement first, by punch process Semi-finished product steel ring and semi-finished product gold ring is made with machining, is to process in place at the cooperation of semi-finished product steel ring and semi-finished product gold ring , but its ill-matched place such as end face, individually out smart car is handled reserved 0.10mm after excessively complete stove, semi-finished product steel ring Internal diameter can stay 0.5 ~ 0.6mm.
In specific manufacturing process, comprise the following steps:
1st, as shown in figure 1, steel ring embryo is made into semi-finished product steel ring by punch process and machining.
2nd, as shown in Fig. 2 gold ring embryo to be made by punch process and machining and treat shape at bag with semi-finished product steel ring The semi-finished product gold ring matched somebody with somebody.
3rd, treat that soldering paste is coated on Bao Chu surfaces in semi-finished product steel ring, then put semi-finished product gold ring, with Lever machine will half into Product steel ring and semi-finished product gold ring carry out pre-pressing, obtain the product of pre-molding, as shown in Figure 3.
4th, the product of pre-molding is placed in compaction mold, compaction mold was carried out into stove is handled 15 ~ 20 minutes, mistake The condition of stove processing is 750 ~ 800 DEG C of furnace temperature, obtains semi-finished product embryo figure, as shown in Figure 4.
Opened after crossing stove processing after compaction mold natural cooling, it is i.e. available that smart car, polishing and cleaning are carried out to product Gold filled circle watch rim.
It is the present invention preferably implementation above, it is necessary to illustrate, without departing substantially from of the invention spiritual and its essence In the case of, those skilled in the art should belong to this when various corresponding deformations that can be according to made by the present invention and change The appended scope of the claims of invention.

Claims (5)

  1. A kind of 1. method covered with gold leaf on wrist-watch watch rim, it is characterised in that comprise the following steps:
    A, by steel ring embryo(1)Semi-finished product steel ring is made by punch process and machining(2), by gold ring embryo(3)By punching press plus Work and machining are made and semi-finished product steel ring(2)Treat the semi-finished product gold ring of form fit at bag(4);
    B, in semi-finished product steel ring(2)Surface coat soldering paste, then put semi-finished product gold ring(4), with Lever machine by rerolled steel Circle(2)With semi-finished product gold ring(4)Carry out precompressed and obtain the product of pre-molding(5);
    C, by the product of pre-molding(5)It is placed in compaction mold, compaction mold was subjected to stove processing;
    D, the product that will be crossed after stove processing can obtain circle watch rim covered with gold leaf after carrying out smart car, polishing and cleaning.
  2. 2. method covered with gold leaf on wrist-watch watch rim according to claim 1, it is characterised in that:The condition for crossing stove processing For 750 ~ 800 DEG C of furnace temperature, the time is 15 ~ 20 minutes.
  3. 3. method covered with gold leaf on wrist-watch watch rim according to claim 1, it is characterised in that:The cleaning is that ultrasonic wave is clear Wash, including step in detail below:It is by additional proportion in ultrasonic container(35~40):(1~2)Water and Wax removal water, after boiling, The product being put into after smart car, polishing, cleaning 10 ~ 15 minutes after taking-up rinsed well with clear water.
  4. 4. method covered with gold leaf on wrist-watch watch rim according to claim 1, it is characterised in that:Also wrapped before the step D Included the step of could being opened after compaction mold natural cooling after stove processing.
  5. 5. method covered with gold leaf on wrist-watch watch rim according to claim 1, it is characterised in that:The compaction mold includes using The upper die and lower die that screw rod is connected, the upper mould are provided with and semi-finished product gold ring(4)The upper bolster that profile matches, under described Mould is provided with and semi-finished product steel ring(2)The die shoe that bottom matches.
CN201710757680.5A 2017-08-29 2017-08-29 A kind of method covered with gold leaf on wrist-watch watch rim Pending CN107570969A (en)