[go: up one dir, main page]

CN106947304A - A kind of art painting and preparation method thereof - Google Patents

A kind of art painting and preparation method thereof Download PDF

Info

Publication number
CN106947304A
CN106947304A CN201710108441.7A CN201710108441A CN106947304A CN 106947304 A CN106947304 A CN 106947304A CN 201710108441 A CN201710108441 A CN 201710108441A CN 106947304 A CN106947304 A CN 106947304A
Authority
CN
China
Prior art keywords
parts
stirring
distilled water
dried
gum
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710108441.7A
Other languages
Chinese (zh)
Inventor
李慧红
刘华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Xinxiang University
Original Assignee
Xinxiang University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Xinxiang University filed Critical Xinxiang University
Priority to CN201710108441.7A priority Critical patent/CN106947304A/en
Publication of CN106947304A publication Critical patent/CN106947304A/en
Pending legal-status Critical Current

Abstract

本发明公开了一种美术颜料及其制备方法,涉及美术用品领域,用以解决现有技术中存在颜料色彩偏淡,不易携带的问题。该颜料包括:由以下质量分数的:0.2~0.6份甲基纤维素,1~2份胶原料,6~12份滑石粉,1~4份高岭土,1~2份氧化锌,1~2份淀粉,0.2~0.5份保湿剂,0.2~0.5份防腐剂,1~2份蒸馏水,0.2~0.6份香料,0.2~0.5份催干剂和1~2份天然色素。The invention discloses an art paint and a preparation method thereof, relates to the field of art supplies, and is used to solve the problems in the prior art that the color of the paint is light and it is not easy to carry. The pigment comprises: 0.2-0.6 parts of methyl cellulose, 1-2 parts of gum material, 6-12 parts of talcum powder, 1-4 parts of kaolin, 1-2 parts of zinc oxide, 1-2 parts of Starch, 0.2-0.5 parts of humectants, 0.2-0.5 parts of preservatives, 1-2 parts of distilled water, 0.2-0.6 parts of spices, 0.2-0.5 parts of drier and 1-2 parts of natural pigments.

Description

一种美术颜料及其制备方法A kind of art paint and preparation method thereof

技术领域technical field

本发明涉及美术用品领域,更具体的涉及一种美术颜料及其制备方法。The invention relates to the field of art supplies, in particular to an art paint and a preparation method thereof.

背景技术Background technique

绘画是一门艺术素养很高的学问,从古至今,绘画艺术可以勾勒出一条历史发展的轨迹。绘画要用到画笔、颜料,颜料质量的好坏直接影响到画卷品质的高低。Painting is a subject with high artistic literacy. From ancient times to the present, the art of painting can outline a track of historical development. Painting requires brushes and pigments, and the quality of the pigments directly affects the quality of the scroll.

现有技术中,颜料的质量参差不齐,存在着诸多原因。例如,颜料的透明度不高,着色较浅,容易退色,不易保存,耐水性差等问题严重影响颜料的品质。因此,需要技术的进步,配方的改进,使颜料的质量更高,更适合绘画使用。In the prior art, the quality of pigments is uneven, and there are many reasons. For example, the transparency of the pigment is not high, the coloring is shallow, it is easy to fade, it is not easy to store, and the water resistance is poor, which seriously affects the quality of the pigment. Therefore, technical progress and formula improvement are needed to make the pigments of higher quality and more suitable for painting.

发明内容Contents of the invention

本发明实施例提供一种美术颜料及其制备方法,用以解决现有技术中存在颜料色彩偏淡,不易携带的问题。The embodiments of the present invention provide an art paint and a preparation method thereof, which are used to solve the problems in the prior art that the color of the paint is light and the paint is not easy to carry.

本发明实施例提供一种美术颜料,包括:由以下质量分数的:0.2~0.6份甲基纤维素,1~2份胶原料,6~12份滑石粉,1~4份高岭土,1~2份氧化锌,1~2份淀粉,0.2~0.5份保湿剂,0.2~0.5份防腐剂,1~2份蒸馏水,0.2~0.6份香料,0.2~0.5份催干剂和1~2份天然色素。An embodiment of the present invention provides an art paint, comprising: 0.2 to 0.6 parts of methyl cellulose, 1 to 2 parts of glue material, 6 to 12 parts of talc, 1 to 4 parts of kaolin, 1 to 2 1-2 parts of zinc oxide, 1-2 parts of starch, 0.2-0.5 parts of humectant, 0.2-0.5 parts of preservative, 1-2 parts of distilled water, 0.2-0.6 parts of spices, 0.2-0.5 parts of drier and 1-2 parts of natural pigment .

优选地,所述保湿剂为甘油。Preferably, the humectant is glycerin.

优选地,所述胶原料包括桃胶和阿拉伯树胶。Preferably, the gum raw material includes peach gum and gum arabic.

本发明实施例还提供一种美术颜料的制备方法,具体包括如下步骤:The embodiment of the present invention also provides a kind of preparation method of art paint, specifically comprises the following steps:

按照质量份数称取胶原料,保湿剂和蒸馏水,将所述胶原料,所述保湿剂和所述蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the number of parts by mass, uniformly stirring and heating the rubber raw material, the moisturizing agent and the distilled water, adding a preservative after heating, and obtaining an adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将所述混合物倒入所述胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for a second stirring to obtain a wet material;

将所述湿润物料放置在烘箱内烘干得到烘干物料;placing the wet material in an oven to dry to obtain a dried material;

将所述烘干物料放入筛子进行筛选,将筛选后的所述物料放入第二搅拌器内,并在所述第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

优选地,所述第一次搅拌时间介于20~30分钟;所述第二次搅拌时间介于20~40分钟。Preferably, the first stirring time is between 20-30 minutes; the second stirring time is between 20-40 minutes.

优选地,所述将所述湿润物料在烘箱内烘干,得到烘干物料,包括:Preferably, the said wet material is dried in an oven to obtain a dried material, comprising:

将所述湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

优选地,所述筛子为60~80目。Preferably, the sieve is 60-80 mesh.

本发明实施例中,提供了一种美术颜料,包括:按照质量份数称取胶原料,保湿剂和蒸馏水,将所述胶原料,所述保湿剂和所述蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;将所述混合物倒入所述胶黏剂内进行第二次搅拌,得到湿润物料;将所述湿润物料放置在烘箱内烘干得到烘干物料;将所述烘干物料放入筛子进行筛选,将筛选后的所述物料放入第二搅拌器内,并在所述第二搅拌器内添加香料,搅拌均匀后得到美术颜料。本发明实施例所提供的颜料采用的原料种类比较少,且来源比较广泛,制作方法比较简单,通过上述方法得到颜料,色彩鲜艳,由于是粉状,方便携带,且可以根据实际需要确定颜料的使用量,从而避免了浪费颜料的问题。In the embodiment of the present invention, a kind of art paint is provided, comprising: weighing the gum material, humectant and distilled water according to the mass parts, stirring the gum material, the moisturizer and the distilled water evenly and heating, after heating Put into antiseptic, obtain adhesive after continuous heating; Put natural pigment, talcum powder, kaolin, zinc oxide and starch into first stirrer and carry out first stirring, obtain the mixture of uniform color; put into the adhesive for the second stirring to obtain a wet material; place the wet material in an oven to dry to obtain a dried material; put the dried material into a sieve for screening, and filter all The materials are put into the second agitator, and spices are added in the second agitator, and the art paint is obtained after stirring evenly. The pigments provided by the embodiments of the present invention use relatively few types of raw materials, and the sources are relatively wide, and the production method is relatively simple. The pigments obtained by the above method are bright in color, and are convenient to carry because they are in powder form, and the color of the pigments can be determined according to actual needs. usage amount, thereby avoiding the problem of wasting paint.

具体实施方式detailed description

下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅仅是本发明一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其他实施例,都属于本发明保护的范围。The technical solutions in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only some of the embodiments of the present invention, but not all of them. Based on the embodiments of the present invention, all other embodiments obtained by persons of ordinary skill in the art without making creative efforts belong to the protection scope of the present invention.

本发明实施例提供一种美术颜料,包括由以下质量分数的:0.2~0.6份甲基纤维素,1~2份胶原料,6~12份滑石粉,1~4份高岭土,1~2份氧化锌,1~2份淀粉,0.2~0.5份保湿剂,0.2~0.5份防腐剂,1~2份蒸馏水,0.2~0.6份香料,0.2~0.5份催干剂和1~2份天然色素。An embodiment of the present invention provides an art pigment, comprising the following mass fractions: 0.2-0.6 parts of methyl cellulose, 1-2 parts of glue material, 6-12 parts of talcum powder, 1-4 parts of kaolin, 1-2 parts Zinc oxide, 1-2 parts of starch, 0.2-0.5 parts of humectant, 0.2-0.5 parts of preservative, 1-2 parts of distilled water, 0.2-0.6 parts of spices, 0.2-0.5 parts of drier and 1-2 parts of natural pigment.

需要说明的是,在实际应用中,保湿剂为甘油;胶原料包括桃胶和阿拉伯树胶。It should be noted that, in practical applications, the moisturizing agent is glycerin; the gum raw materials include peach gum and gum arabic.

基于上述美术颜料的配方,可以通过下列制备方法,制作美术颜料,具体的制作步骤包括:Based on the formula of the above-mentioned art paint, the art paint can be made through the following preparation methods, and the specific production steps include:

按照质量份数称取胶原料,保湿剂和蒸馏水,将胶原料,保湿剂和蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the parts by mass, uniformly stirring the rubber raw material, humectant and distilled water and heating, adding preservative after heating, and obtaining the adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将混合物倒入胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for the second stirring to obtain a wet material;

将湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

将烘干物料放入筛子进行筛选,将筛选后的物料放入第二搅拌器内,并在第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

需要说明的是,第一次搅拌时间介于20~30分钟;第二次搅拌时间介于20~40分钟;筛子为60~80目。It should be noted that the first stirring time is 20-30 minutes; the second stirring time is 20-40 minutes; the sieve is 60-80 mesh.

本发明实施例提供一种美术颜料及其制备方法,其中,美术颜料的配方可以包括多种,但是美术颜料的制备方法只包括一种,基于上述区别,以下分别以实施例一至实施例四为例,来具体介绍不同的美术颜料配方对应的美术颜料制备方法。The embodiment of the present invention provides a kind of art paint and its preparation method, wherein, the formula of art paint can include many kinds, but the preparation method of art paint only includes one kind, based on the above-mentioned difference, the following are examples 1 to 4 respectively For example, to specifically introduce the art paint preparation methods corresponding to different art paint formulas.

实施例一Embodiment one

本发明实施例提供一种美术颜料,包括由以下质量分数的:0.2份甲基纤维素,1份胶原料,6份滑石粉,1份高岭土,1份氧化锌,1份淀粉,0.2份保湿剂,0.2份防腐剂,1份蒸馏水,0.2份香料,0.2份催干剂和1份天然色素。An embodiment of the present invention provides a kind of art paint, comprising the following mass fractions: 0.2 parts of methylcellulose, 1 part of gum material, 6 parts of talcum powder, 1 part of kaolin, 1 part of zinc oxide, 1 part of starch, 0.2 part of moisturizing agent, 0.2 part of preservative, 1 part of distilled water, 0.2 part of fragrance, 0.2 part of drying agent and 1 part of natural color.

需要说明的是,在实际应用中,保湿剂为甘油;胶原料包括桃胶和阿拉伯树胶。It should be noted that, in practical applications, the moisturizing agent is glycerin; the gum raw materials include peach gum and gum arabic.

基于上述美术颜料的配方,可以通过下列制备方法,制作美术颜料,具体的制作步骤包括:Based on the formula of the above-mentioned art paint, the art paint can be made through the following preparation methods, and the specific production steps include:

按照质量份数称取胶原料,保湿剂和蒸馏水,将胶原料,保湿剂和蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the parts by mass, uniformly stirring the rubber raw material, humectant and distilled water and heating, adding preservative after heating, and obtaining the adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将混合物倒入胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for the second stirring to obtain a wet material;

将湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

将烘干物料放入筛子进行筛选,将筛选后的物料放入第二搅拌器内,并在第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

需要说明的是,第一次搅拌时间为20分钟;第二次搅拌时间为20分钟;筛子为60~80目。It should be noted that the first stirring time is 20 minutes; the second stirring time is 20 minutes; the sieve is 60-80 mesh.

实施例二Embodiment two

本发明实施例提供一种美术颜料,包括由以下质量分数的:0.6份甲基纤维素,2份胶原料,12份滑石粉,4份高岭土,2份氧化锌,2份淀粉,0.5份保湿剂,0.5份防腐剂,2份蒸馏水,0.6份香料,0.5份催干剂和2份天然色素。An embodiment of the present invention provides a kind of art paint, comprising the following mass fractions: 0.6 parts of methyl cellulose, 2 parts of gum material, 12 parts of talcum powder, 4 parts of kaolin, 2 parts of zinc oxide, 2 parts of starch, 0.5 part of moisturizing agent, 0.5 parts preservative, 2 parts distilled water, 0.6 parts fragrance, 0.5 parts drier and 2 parts natural coloring.

需要说明的是,在实际应用中,保湿剂为甘油;胶原料包括桃胶和阿拉伯树胶。It should be noted that, in practical applications, the moisturizing agent is glycerin; the gum raw materials include peach gum and gum arabic.

基于上述美术颜料的配方,可以通过下列制备方法,制作美术颜料,具体的制作步骤包括:Based on the formula of the above-mentioned art paint, the art paint can be made through the following preparation methods, and the specific production steps include:

按照质量份数称取胶原料,保湿剂和蒸馏水,将胶原料,保湿剂和蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the parts by mass, uniformly stirring the rubber raw material, humectant and distilled water and heating, adding preservative after heating, and obtaining the adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将混合物倒入胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for the second stirring to obtain a wet material;

将湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

将烘干物料放入筛子进行筛选,将筛选后的物料放入第二搅拌器内,并在第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

需要说明的是,第一次搅拌时间为30分钟;第二次搅拌时间为40分钟;筛子为60~80目。It should be noted that the first stirring time is 30 minutes; the second stirring time is 40 minutes; the sieve is 60-80 mesh.

实施例三Embodiment three

本发明实施例提供一种美术颜料,包括由以下质量分数的:0.4份甲基纤维素,1.5份胶原料,0.9份滑石粉,2.5份高岭土,1.5份氧化锌,1.5份淀粉,0.2份保湿剂,0.4份防腐剂,2份蒸馏水,0.6份香料,0.2份催干剂和1份天然色素。An embodiment of the present invention provides a kind of art pigment, comprising the following mass fractions: 0.4 parts of methyl cellulose, 1.5 parts of gum material, 0.9 parts of talcum powder, 2.5 parts of kaolin, 1.5 parts of zinc oxide, 1.5 parts of starch, 0.2 parts of moisturizing agent, 0.4 part of preservative, 2 parts of distilled water, 0.6 part of fragrance, 0.2 part of drying agent and 1 part of natural color.

需要说明的是,在实际应用中,保湿剂为甘油;胶原料包括桃胶和阿拉伯树胶。It should be noted that, in practical applications, the moisturizing agent is glycerin; the gum raw materials include peach gum and gum arabic.

基于上述美术颜料的配方,可以通过下列制备方法,制作美术颜料,具体的制作步骤包括:Based on the formula of the above-mentioned art paint, the art paint can be made through the following preparation methods, and the specific production steps include:

按照质量份数称取胶原料,保湿剂和蒸馏水,将胶原料,保湿剂和蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the parts by mass, uniformly stirring the rubber raw material, humectant and distilled water and heating, adding preservative after heating, and obtaining the adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将混合物倒入胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for the second stirring to obtain a wet material;

将湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

将烘干物料放入筛子进行筛选,将筛选后的物料放入第二搅拌器内,并在第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

需要说明的是,第一次搅拌时间介于15~20分钟;第二次搅拌时间介于25~30分钟;筛子为60~80目。It should be noted that the stirring time for the first time is 15-20 minutes; the stirring time for the second time is 25-30 minutes; the sieve is 60-80 mesh.

实施例四Embodiment Four

本发明实施例提供一种美术颜料,包括由以下质量分数的:0.5份甲基纤维素,0.5份胶原料,8份滑石粉,3份高岭土,1份氧化锌,2份淀粉,0.3份保湿剂,0.4份防腐剂,2份蒸馏水,0.5份香料,0.2份催干剂和2份天然色素。An embodiment of the present invention provides a kind of art pigment, comprising the following mass fractions: 0.5 parts of methyl cellulose, 0.5 parts of gum material, 8 parts of talcum powder, 3 parts of kaolin, 1 part of zinc oxide, 2 parts of starch, 0.3 part of moisturizing agent, 0.4 parts preservative, 2 parts distilled water, 0.5 parts fragrance, 0.2 parts drier and 2 parts natural coloring.

需要说明的是,在实际应用中,保湿剂为甘油;胶原料包括桃胶和阿拉伯树胶。It should be noted that, in practical applications, the moisturizing agent is glycerin; the gum raw materials include peach gum and gum arabic.

基于上述美术颜料的配方,可以通过下列制备方法,制作美术颜料,具体的制作步骤包括:Based on the formula of the above-mentioned art paint, the art paint can be made through the following preparation methods, and the specific production steps include:

按照质量份数称取胶原料,保湿剂和蒸馏水,将胶原料,保湿剂和蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the parts by mass, uniformly stirring the rubber raw material, humectant and distilled water and heating, adding preservative after heating, and obtaining the adhesive after continuous heating;

将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color;

将混合物倒入胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for the second stirring to obtain a wet material;

将湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material.

将烘干物料放入筛子进行筛选,将筛选后的物料放入第二搅拌器内,并在第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint.

需要说明的是,第一次搅拌时间介于20~25分钟;第二次搅拌时间介于30~40分钟;筛子为60~80目。It should be noted that the first stirring time is 20-25 minutes; the second stirring time is 30-40 minutes; the sieve is 60-80 mesh.

综上所述,本发明实施例中,提供了一种美术颜料,包括:按照质量份数称取胶原料,保湿剂和蒸馏水,均匀搅拌,加热后放入防腐剂,持续加热后得到胶黏剂;将天然色素,滑石粉,高岭土,氧化锌和淀粉放入搅拌器内进行第一次搅拌,得到颜色均匀的混合物;将所述混合物倒入所述胶黏剂内进行第二次搅拌,得到湿润物料;将所述湿润物料在烘箱内烘干,得到烘干物料;对所述烘干物料放入筛子进行筛选,将筛选后的所述物料放入容器内,并在容器内添加香料,得到美术颜料。本发明实施例所提供的颜料采用的原料种类比较少,且来源比较广泛,制作方法比较简单,通过上述方法得到颜料,色彩鲜艳,由于是粉状,方便携带,且可以根据实际需要确定颜料的使用量,从而避免了浪费颜料的问题。To sum up, in the embodiment of the present invention, a kind of art paint is provided, which includes: weighing the glue material, humectant and distilled water according to the parts by mass, stirring evenly, adding preservative after heating, and obtaining the glue after continuous heating agent; put the natural pigment, talcum powder, kaolin, zinc oxide and starch into the mixer for the first stirring to obtain a uniformly colored mixture; pour the mixture into the adhesive for the second stirring, Obtain wet material; dry the wet material in an oven to obtain dried material; put the dried material into a sieve for screening, put the screened material into a container, and add spices into the container , to obtain art paints. The pigments provided by the embodiments of the present invention use relatively few types of raw materials, and the sources are relatively wide, and the production method is relatively simple. The pigments obtained by the above method are bright in color, and are convenient to carry because they are in powder form, and the color of the pigments can be determined according to actual needs. usage amount, thereby avoiding the problem of wasting paint.

尽管已描述了本发明的优选实施例,但本领域内的技术人员一旦得知了基本创造性概念,则可对这些实施例作出另外的变更和修改。所以,所附权利要求意欲解释为包括优选实施例以及落入本发明范围的所有变更和修改。While preferred embodiments of the invention have been described, additional changes and modifications to these embodiments can be made by those skilled in the art once the basic inventive concept is appreciated. Therefore, it is intended that the appended claims be construed to cover the preferred embodiment as well as all changes and modifications which fall within the scope of the invention.

显然,本领域的技术人员可以对本发明进行各种改动和变型而不脱离本发明的精神和范围。这样,倘若本发明的这些修改和变型属于本发明权利要求及其等同。Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. In this way, provided that these modifications and variations of the present invention belong to the claims of the present invention and their equivalents.

Claims (7)

1.一种美术颜料,其特征在于,包括:由以下质量分数的:0.2~0.6份甲基纤维素,1~2份胶原料,6~12份滑石粉,1~4份高岭土,1~2份氧化锌,1~2份淀粉,0.2~0.5份保湿剂,0.2~0.5份防腐剂,1~2份蒸馏水,0.2~0.6份香料,0.2~0.5份催干剂和1~2份天然色素。1. A kind of art pigment, it is characterized in that, comprises: by following mass fraction: 0.2~0.6 parts of methyl cellulose, 1~2 parts of gum material, 6~12 parts of talcum powder, 1~4 parts of kaolin, 1~ 2 parts of zinc oxide, 1 to 2 parts of starch, 0.2 to 0.5 parts of humectant, 0.2 to 0.5 parts of preservative, 1 to 2 parts of distilled water, 0.2 to 0.6 parts of fragrance, 0.2 to 0.5 parts of drier and 1 to 2 parts of natural pigment. 2.如权利要求1所述的颜料,其特征在于,所述保湿剂为甘油。2. The pigment according to claim 1, wherein the humectant is glycerin. 3.如权利要求1所述的颜料,其特征在于,所述胶原料包括桃胶和阿拉伯树胶。3. The pigment according to claim 1, wherein the gum material comprises peach gum and gum arabic. 4.一种美术颜料的制备方法,其特征在于:具体包括如下步骤:4. a kind of preparation method of art paint, is characterized in that: specifically comprise the steps: 按照质量份数称取胶原料,保湿剂和蒸馏水,将所述胶原料,所述保湿剂和所述蒸馏水均匀搅拌并加热,加热后放入防腐剂,持续加热后得到胶黏剂;Weighing the rubber raw material, humectant and distilled water according to the number of parts by mass, uniformly stirring and heating the rubber raw material, the moisturizing agent and the distilled water, adding a preservative after heating, and obtaining an adhesive after continuous heating; 将天然色素,滑石粉,高岭土,氧化锌和淀粉放入第一搅拌器内进行第一次搅拌,得到颜色均匀的混合物;Put natural pigment, talcum powder, kaolin, zinc oxide and starch into the first mixer for the first stirring to obtain a mixture with uniform color; 将所述混合物倒入所述胶黏剂内进行第二次搅拌,得到湿润物料;Pour the mixture into the adhesive for a second stirring to obtain a wet material; 将所述湿润物料放置在烘箱内烘干得到烘干物料;placing the wet material in an oven to dry to obtain a dried material; 将所述烘干物料放入筛子进行筛选,将筛选后的所述物料放入第二搅拌器内,并在所述第二搅拌器内添加香料,搅拌均匀后得到美术颜料。Put the dried material into a sieve for screening, put the screened material into a second agitator, add spices into the second agitator, and stir evenly to obtain an art paint. 5.如权利要求4所述的方法,其特征在于,所述第一次搅拌时间介于20~30分钟;所述第二次搅拌时间介于20~40分钟。5. The method according to claim 4, characterized in that, the first stirring time is between 20-30 minutes; the second stirring time is between 20-40 minutes. 6.如权利要求4所述的方法,其特征在于,所述将所述湿润物料在烘箱内烘干,得到烘干物料,包括:6. The method according to claim 4, wherein the drying of the wet material in an oven to obtain a dried material comprises: 将所述湿润物料放在温度为90°的烘箱内烘干5个小时,得到烘干物料。The wet material was dried in an oven at a temperature of 90° for 5 hours to obtain a dried material. 7.如权利要求4所述的方法,其特征在于,所述筛子为60~80目。7. The method according to claim 4, characterized in that, the sieve is 60-80 mesh.
CN201710108441.7A 2017-02-27 2017-02-27 A kind of art painting and preparation method thereof Pending CN106947304A (en)