[go: up one dir, main page]

CN106267914A - A kind of efficient compound defoamer and preparation method thereof - Google Patents

A kind of efficient compound defoamer and preparation method thereof Download PDF

Info

Publication number
CN106267914A
CN106267914A CN201610789651.2A CN201610789651A CN106267914A CN 106267914 A CN106267914 A CN 106267914A CN 201610789651 A CN201610789651 A CN 201610789651A CN 106267914 A CN106267914 A CN 106267914A
Authority
CN
China
Prior art keywords
polydimethylsiloxane
warmed
fatty acid
acid ester
modified polydimethylsiloxane
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610789651.2A
Other languages
Chinese (zh)
Inventor
田坤
耿学辉
杨开柱
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
HUBEI XINSIHAI CHEMICAL CO Ltd
Original Assignee
HUBEI XINSIHAI CHEMICAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by HUBEI XINSIHAI CHEMICAL CO Ltd filed Critical HUBEI XINSIHAI CHEMICAL CO Ltd
Priority to CN201610789651.2A priority Critical patent/CN106267914A/en
Publication of CN106267914A publication Critical patent/CN106267914A/en
Pending legal-status Critical Current

Abstract

The present invention proposes a kind of efficient compound defoamer and preparation method thereof, the present invention uses modified polyorganosiloxane as main froth breaking composition, by introducing hydrophilic group on polysiloxanes, improve the compatibility with foaming system, and improve the dispersibility of product, avoid the various drawbacks using pure organic silicon defoamer to bring, and froth breaking and the suds ability of product can be significantly improved.

Description

A kind of efficient compound defoamer and preparation method thereof
Technical field
The present invention relates to defoamer synthesis technical field, particularly relate to a kind of efficient compound defoamer and preparation side thereof Method.
Background technology
In the industrial production, substantial amounts of foam can be produced, bring various trouble to production and processing, such as: produce Ability significantly limits, causes raw material and the waste of product, the reaction time of prolongation production, affects product quality, pollution environment etc. Deng.Have to eliminate foam the most in the industrial production, most common method is to add defoamer, and the kind of defoamer is a lot, Effect most preferably organic silicon defoamer, but the hydrophobic performance of organosilicon is very strong, causes pure organic silicon defoamer using In easily produce the phenomenons such as silicon speckle, shrinkage cavity, reunion, cannot use in industries such as water color ink, textile printing and dyeing, papermaking.
Summary of the invention
In view of this, the present invention propose that a kind of dispersion effect is good, froth breaking and the strong efficient compound froth breaking of suds ability Agent and preparation method thereof.
The technical scheme is that and be achieved in that: on the one hand, the invention provides a kind of efficient compound defoamer, It includes the component of following mass fraction,
Polydimethylsiloxane 3-7 part;
Long chain alkyl modified polydimethylsiloxane 12-18 part;
Polyether-modified polydimethylsiloxane 8-12 part;
Water 50-70 part;
Sorbitol anhydride monostearate 1-5 part;
Single, diglycerine fatty acid ester 1-5 part;
Sorbitan fatty acid ester polyoxyethylene ether 0.5-1.5 part;
Hydrophobic silica 0.5-1.5 part;
Sodium carboxymethyl cellulose 0.5-1.5 part.
On the basis of above technical scheme, it is preferred that described efficient compound defoamer includes following mass fraction Component,
Polydimethylsiloxane 5 parts;
Long chain alkyl modified polydimethylsiloxane 15 parts;
Polyether-modified polydimethylsiloxane 10 parts;
60 parts of water;
Sorbitol anhydride monostearate 3 parts;
Single, diglycerine fatty acid ester 3 parts;
Sorbitan fatty acid ester polyoxyethylene ether 1 part;
Hydrophobic silica 1 part;
Sodium carboxymethyl cellulose 1 part.
Second aspect present invention provides the preparation method of efficient compound defoamer described in first aspect, and it includes following Step,
S1, mixes sodium carboxymethyl cellulose with water, is warmed up to 70-90 DEG C, makes sodium carboxymethyl cellulose be completely dissolved, To aqueous thickener solution;
S2, by polydimethylsiloxane, long chain alkyl modified polydimethylsiloxane, polyether-modified polydimethylsiloxanes Alkane, sorbitol anhydride monostearate, sorbitan fatty acid ester polyoxyethylene ether, list, diglycerine fatty acid ester and hydrophobic two Silicon oxide, puts in reactor together, is warmed up to 60-70 DEG C, stirring insulation 0.5-1.5 hour, is slowly dropped into step S1 and obtains Aqueous thickener solution, stirring insulation 0.5-1.5 hour, cooling, filter i.e. obtain efficient compound defoamer finished product.
On the basis of above technical scheme, it is preferred that the preparation bag of described long chain alkyl modified polydimethylsiloxane Include following steps, by containing hydrogen silicone oil that hydrogen content is 0.2-0.8 and 16 alkene, put in reactor together, be warmed up to 85-95 DEG C, evacuation is dehydrated 0.4-0.6 hour, is then warmed up between 120-140 DEG C reaction 2-4 hour, i.e. prepares chain alkyl and change Property polydimethylsiloxane.
On the basis of above technical scheme, it is preferred that the preparation of described polyether-modified polydimethylsiloxane include with Lower step, by containing hydrogen silicone oil that hydrogen content is 0.2-0.8 and 1-propenol-3 polyoxyalkyl ether, puts in reactor together, is warmed up to 85-95 DEG C, evacuation is dehydrated 0.4-0.6 hour, is then warmed up between 120-140 DEG C reaction 2-4 hour, i.e. prepares polyethers and change Property polydimethylsiloxane.
Efficient compound defoamer of the present invention and preparation method thereof has the advantages that this relative to prior art Invention uses modified polyorganosiloxane as main froth breaking composition, by introducing hydrophilic group on polysiloxanes, improves and foams The compatibility of system, and improve the dispersibility of product, it is to avoid the various drawbacks that the pure organic silicon defoamer of use brings, and And froth breaking and the suds ability of product can be significantly improved.
Detailed description of the invention
Below in conjunction with embodiment of the present invention, technical solution of the present invention is clearly and completely described, it is clear that institute The embodiment described is only a part of embodiment of the present invention rather than whole embodiments.Based in the present invention Embodiment, the every other embodiment party that those of ordinary skill in the art are obtained under not making creative work premise Formula, broadly falls into the scope of protection of the invention.
Embodiment 1
The efficient compound defoamer of the present embodiment, its composition of raw materials is as follows:
Polydimethylsiloxane 3kg;
Long chain alkyl modified polydimethylsiloxane 12kg;
Polyether-modified polydimethylsiloxane 8kg;
Water 50kg;
Sorbitol anhydride monostearate 1kg;
Single, diglycerine fatty acid ester 1kg;
Sorbitan fatty acid ester polyoxyethylene ether 0.5kg;
Hydrophobic silica 0.5kg;
Sodium carboxymethyl cellulose 0.5kg.
Preparation process is as follows:
First, long chain alkyl modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.2 and 16 alkene, Putting in reactor together, be warmed up to 85 DEG C, evacuation is dehydrated 0.4 hour, is then warmed up to 120 DEG C and reacts 2 hours, the most prepared Long chain alkyl modified polydimethylsiloxane.
Secondly, polyether-modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.2 and 1-propenol-3 polyoxy alkane Base ether, puts in reactor together, is warmed up to 85 DEG C, and evacuation is dehydrated 0.4 hour, is then warmed up to 120 DEG C and reacts 2 hours, I.e. prepare polyether-modified polydimethylsiloxane.
Then, sodium carboxymethyl cellulose is mixed with water, be warmed up to 70 DEG C, make sodium carboxymethyl cellulose be completely dissolved, To aqueous thickener solution;
Finally, by polydimethylsiloxane, long chain alkyl modified polydimethylsiloxane, polyether-modified polydimethylsiloxanes Alkane, sorbitol anhydride monostearate, sorbitan fatty acid ester polyoxyethylene ether, list, diglycerine fatty acid ester and hydrophobic two Silicon oxide, puts in reactor together, is warmed up to 60 DEG C, adjusts speed of agitator to 600 revs/min, is incubated 0.5 hour, slowly drips Enter aqueous thickener solution, adjust the rotating speed to 1000 revs/min of stirring, be incubated 0.5 hour, cooling, filter and i.e. obtain high efficiency composition Type defoamer finished product.
Embodiment 2
The efficient compound defoamer of the present embodiment, its composition of raw materials is as follows:
Polydimethylsiloxane 5kg;
Long chain alkyl modified polydimethylsiloxane 15kg;
Polyether-modified polydimethylsiloxane 10kg;
Water 60kg;
Sorbitol anhydride monostearate 3kg;
Single, diglycerine fatty acid ester 3kg;
Sorbitan fatty acid ester polyoxyethylene ether 1kg;
Hydrophobic silica 1kg;
Sodium carboxymethyl cellulose 1kg.
Preparation process is as follows:
First, long chain alkyl modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.5 and 16 alkene, Putting in reactor together, be warmed up to 90 DEG C, evacuation is dehydrated 0.5 hour, is then warmed up to 130 DEG C and reacts 3 hours, the most prepared Long chain alkyl modified polydimethylsiloxane.
Secondly, polyether-modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.5 and 1-propenol-3 polyoxy alkane Base ether, puts in reactor together, is warmed up to 90 DEG C, and evacuation is dehydrated 0.5 hour, is then warmed up to 130 DEG C and reacts 3 hours, I.e. prepare polyether-modified polydimethylsiloxane.
Then, sodium carboxymethyl cellulose is mixed with water, be warmed up to 80 DEG C, make sodium carboxymethyl cellulose be completely dissolved, To aqueous thickener solution;
Finally, by polydimethylsiloxane, long chain alkyl modified polydimethylsiloxane, polyether-modified polydimethylsiloxanes Alkane, sorbitol anhydride monostearate, sorbitan fatty acid ester polyoxyethylene ether, list, diglycerine fatty acid ester and hydrophobic two Silicon oxide, puts in reactor together, is warmed up to 65 DEG C, adjusts speed of agitator to 600 revs/min, is incubated 1 hour, is slowly dropped into Aqueous thickener solution, adjusts the rotating speed to 1100 revs/min of stirring, is incubated 1 hour, cooling, and filtration i.e. obtains efficient compound and disappears Infusion finished product.
Embodiment 3
The efficient compound defoamer of the present embodiment, its composition of raw materials is as follows:
Polydimethylsiloxane 7kg;
Long chain alkyl modified polydimethylsiloxane 18kg;
Polyether-modified polydimethylsiloxane 12kg;
Water 70kg;
Sorbitol anhydride monostearate 5kg;
Single, diglycerine fatty acid ester 5kg;
Sorbitan fatty acid ester polyoxyethylene ether 1.5kg;
Hydrophobic silica 1.5kg;
Sodium carboxymethyl cellulose 1.5kg.
Preparation process is as follows:
First, long chain alkyl modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.8 and 16 alkene, Putting in reactor together, be warmed up to 95 DEG C, evacuation is dehydrated 0.6 hour, is then warmed up to 140 DEG C and reacts 4 hours, the most prepared Long chain alkyl modified polydimethylsiloxane.
Secondly, polyether-modified polydimethylsiloxane is prepared.By containing hydrogen silicone oil that hydrogen content is 0.8 and 1-propenol-3 polyoxy alkane Base ether, puts in reactor together, is warmed up to 95 DEG C, and evacuation is dehydrated 0.6 hour, is then warmed up between 140 DEG C reaction 4 little Time, i.e. prepare polyether-modified polydimethylsiloxane.
Then, sodium carboxymethyl cellulose is mixed with water, be warmed up to 90 DEG C, make sodium carboxymethyl cellulose be completely dissolved, To aqueous thickener solution;
Finally, by polydimethylsiloxane, long chain alkyl modified polydimethylsiloxane, polyether-modified polydimethylsiloxanes Alkane, sorbitol anhydride monostearate, sorbitan fatty acid ester polyoxyethylene ether, list, diglycerine fatty acid ester and hydrophobic two Silicon oxide, puts in reactor together, is warmed up to 70 DEG C, adjusts speed of agitator to 600 revs/min, is incubated 1.5 hours, slowly drips Enter aqueous thickener solution, adjust the rotating speed to 1100 revs/min of stirring, be incubated 1.5 hours, cooling, filter and i.e. obtain high efficiency composition Type defoamer finished product.
The foregoing is only the better embodiment of the present invention, not in order to limit the present invention, all the present invention's Within spirit and principle, any modification, equivalent substitution and improvement etc. made, should be included within the scope of the present invention.

Claims (5)

1. an efficient compound defoamer, it is characterised in that: it includes the component of following mass fraction,
Polydimethylsiloxane 3-7 part;
Long chain alkyl modified polydimethylsiloxane 12-18 part;
Polyether-modified polydimethylsiloxane 8-12 part;
Water 50-70 part;
Sorbitol anhydride monostearate 1-5 part;
Single, diglycerine fatty acid ester 1-5 part;
Sorbitan fatty acid ester polyoxyethylene ether 0.5-1.5 part;
Hydrophobic silica 0.5-1.5 part;
Sodium carboxymethyl cellulose 0.5-1.5 part.
2. efficient compound defoamer as claimed in claim 1, it is characterised in that: it includes the component of following mass fraction,
Polydimethylsiloxane 5 parts;
Long chain alkyl modified polydimethylsiloxane 15 parts;
Polyether-modified polydimethylsiloxane 10 parts;
60 parts of water;
Sorbitol anhydride monostearate 3 parts;
Single, diglycerine fatty acid ester 3 parts;
Sorbitan fatty acid ester polyoxyethylene ether 1 part;
Hydrophobic silica 1 part;
Sodium carboxymethyl cellulose 1 part.
3. the preparation method of efficient compound defoamer as claimed in claim 1, it is characterised in that: it comprises the following steps,
S1, mixes sodium carboxymethyl cellulose with water, is warmed up to 70-90 DEG C, makes sodium carboxymethyl cellulose be completely dissolved, is increased Thick dose of aqueous solution;
S2, by polydimethylsiloxane, long chain alkyl modified polydimethylsiloxane, polyether-modified polydimethylsiloxane, mountain Pears alcohol acid anhydride monostearate, sorbitan fatty acid ester polyoxyethylene ether, list, diglycerine fatty acid ester and hydrophobic titanium dioxide Silicon, puts in reactor together, is warmed up to 60-70 DEG C, stirring insulation 0.5-1.5 hour, is slowly dropped into the increasing that step S1 obtains Thick dose of aqueous solution, stirring insulation 0.5-1.5 hour, cooling, filter and i.e. obtain efficient compound defoamer finished product.
4. the preparation method of efficient compound defoamer as claimed in claim 3, it is characterised in that: described long chain alkyl modified The preparation of polydimethylsiloxane comprises the following steps, and by containing hydrogen silicone oil that hydrogen content is 0.2-0.8 and 16 alkene, puts into together In reactor, being warmed up to 85-95 DEG C, evacuation is dehydrated 0.4-0.6 hour, is then warmed up between 120-140 DEG C react 2-4 little Time, i.e. prepare long chain alkyl modified polydimethylsiloxane.
5. the preparation method of efficient compound defoamer as claimed in claim 3, it is characterised in that: described polyether-modified poly-two The preparation of methylsiloxane comprises the following steps, by containing hydrogen silicone oil that hydrogen content is 0.2-0.8 and 1-propenol-3 polyoxyalkyl ether, and one Rising in input reactor, be warmed up to 85-95 DEG C, evacuation is dehydrated 0.4-0.6 hour, is then warmed up between 120-140 DEG C anti- Answer 2-4 hour, i.e. prepare polyether-modified polydimethylsiloxane.
CN201610789651.2A 2016-08-31 2016-08-31 A kind of efficient compound defoamer and preparation method thereof Pending CN106267914A (en)