CN106110880B - A kind of suede body implantation methods with absorption and photocatalyst function - Google Patents

A kind of suede body implantation methods with absorption and photocatalyst function Download PDF

Info

Publication number
CN106110880B
CN106110880B CN201610450173.2A CN201610450173A CN106110880B CN 106110880 B CN106110880 B CN 106110880B CN 201610450173 A CN201610450173 A CN 201610450173A CN 106110880 B CN106110880 B CN 106110880B
Authority
CN
China
Prior art keywords
suede body
suede
body material
implantation methods
carrier surface
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201610450173.2A
Other languages
Chinese (zh)
Other versions
CN106110880A (en
Inventor
李秋梅
杨斐
延思逸
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Li Huibin
Original Assignee
SHAOXING KAISI WODE SOFTWARE TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHAOXING KAISI WODE SOFTWARE TECHNOLOGY Co Ltd filed Critical SHAOXING KAISI WODE SOFTWARE TECHNOLOGY Co Ltd
Priority to CN201610450173.2A priority Critical patent/CN106110880B/en
Publication of CN106110880A publication Critical patent/CN106110880A/en
Application granted granted Critical
Publication of CN106110880B publication Critical patent/CN106110880B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a kind of suede body implantation methods with absorption and photocatalyst function, including suede body material and suede body implantation methods, the suede body material includes villus, nanometer titanium dioxide, zeolite powder and copper powder, suede body material is implanted into carrier surface by the suede body implantation methods, the suede body material is after suede body implantation methods are implanted into carrier surface, the suede body structure of carrier surface has absorption and photocatalyst function, the suede body implantation methods include suede body constituent preprocessing, carrier surface preprocessing, suede body material is added in flocking plant, apply suede body material by medium or electrostatic, cover carrier surface, reheat and rub suede body material.The configuration of the present invention is simple, it is easy to operate, pass through flocking, carrier surface can be made to cover one layer of suede body with absorption and photocatalyst function, it being capable of actively or passively toxic and harmful gas, various bacteria in catalytic degradation air, and the toxin decomposition and harmless treatment that bacterium or fungi release there can be the functions such as deodorization, anti-pollution.

Description

A kind of suede body implantation methods with absorption and photocatalyst function
Technical field
The present invention relates to gas cleaning applications more particularly to a kind of suede body plantation sides with absorption and photocatalyst function Method.
Background technology
Air is the life first element, and the major part of life is spent indoors.It is each that room air is full of human body object Kind metabolin, advantageous microbial reproduction, pollution level are more times of outdoor to humiture appropriate again.Adult's breathing daily is about 20 kg of air per kg of water evaporated, breathing have all retained malicious dirt, cannot be as Metabolism Excretion, and healthhazard is larger: 2000.6.8《In Technology Shi Chang Bao of state》It introduces, the expert of Beijing technical supervision centre of development thinks that indoor pollution is the first killer, 1999.1.15 《Shanghai Volkswagen's health report》Describing the viewpoint of Shanghai institute of Research of Environmental Sciences director Qian Hua, " 80% pathogenic factor derives from The room air not circulated ".Improving the relatively effective method of room air at present has:One, trust to chance and strokes of luck method, to inner wall surface, Coating of the formaldehyde pollutions such as floor, furniture source spraying with absorption, catalysis, is purified with quiescent operation mode and to be touched Air, such method take time and effort, and effect unobvious, cost is high, and cost performance is extremely low.Two, using with " air purifier " , but it is limited by circulation, still there is that the right negative ion concentration of air outlet air cleaner is excessively high, should not directly breathe, and distance Slightly distant place air improves again quite slow, and also strainer is pollutant congestion, and efficiency can be in the shortcoming such as degenerative decaying.People Ventilation is still mostly used to be improved, however takes a breath to make troubles to air-conditioned room again and again and be escaped with energy.With the people The improvement of improvement of living standard and living conditions, house ornamentation are paid attention to by more and more people, thing followed indoor decoration pollution Also it puts in face of people, these harmful substances are mainly formaldehyde, benzene homologues, ammonia and other volatile organic matters (VOCs), And wherein content of formaldehyde highest harm is maximum.With the appearance of nano photo-catalytic, we can utilize the light of nano photo-catalytic Pollutant is carried out photodissociation elimination by Catalysis Principles.Nano-titanium dioxide is widely used in coating with its good chemism In being administered with finishing.Since it is coated on indoor all walls and roof, effect big with the contact area of room air Obviously.But nano photo-catalytic only under conditions of sunlight, ultraviolet light and visible light could decomposing harmful substances, arrive Night does not have just to be stopped when light.And there is the interior wall coating of respiratory function often to possess ratio using diatomite etc. The material of the subtleer pass structure of activated carbon not only has the function of breathing moisture, but also this material strong adsorption force, no Only material itself is environmentally friendly, can absorb nuisance, protects the healthy and safe of domestic environment.But simple diatomite itself It only adsorbs, without degradation function.Suction-operated is a kind of physical function, can not decomposing organic matter.Also, works as and reach After saturation absorption, the gaseous matter adsorbed is certain to be desorbed under conditions of some temperature, humidity variation indoors. This means that pernicious gas is possible to disengage again if be saturated absorption is harmful gas." because of house decoration Or in pernicious gas caused by furniture, the Form aldehyde release time was up to for more than ten years.Therefore, if Formaldehyde Pollution of Indoor Air seriously surpasses Mark, it is difficult persistently to ensure that indoor air quality is up to standard only to lean on the adsorption function of diatomite or other porous materials.If by porous Adsorbent is added in nano photo-catalytic solution, is sprayed on metope, then photocatalyst will can be made to learn from other's strong points to offset one's weaknesses with adsorbent, It plays a role round the clock.By advanced compounded technology, nano-titania particle can be loaded to porous inorganic particulate table Face makes hole surface be covered with " photocatalyst ".Adsorbent itself can be with pernicious gases such as formaldehyde adsorptions, and " photocatalyst " exists Under visible light, these nuisances can be decomposed, to nuisance of degrading.Although have by diatomite and photocatalyst into The report of row compounding, but the sedimentation problem of particle and the agglomeration traits of nano-titanium dioxide can be successfully solved, accomplish true The photocatalyst absorption of positive Nano grade, it is difficult to find useful data and information is referred to.
Invention content
It is an object of the invention to overcome problem above of the existing technology, provide a kind of with absorption and photocatalyst work( The suede body implantation methods of energy will have the length for being referred to as ultrashort fine suede of absorption, photocatalyst function porous less than 0.4mm Velveteen, zeolite, activated carbon, nano-titanium dioxide homogenize mixing and are attached on carrier, and monomer one end is made to be rooted in carrier and this Body is stood on carrier surface, the configuration of the present invention is simple, easy to operate, by flocking, carrier surface can be made to cover one layer Suede body with absorption and photocatalyst function, can actively or passively toxic and harmful gas, various bacteria in catalytic degradation air, And the toxin decomposition and harmless treatment that bacterium or fungi release there can be the functions such as deodorization, anti-pollution.
To realize above-mentioned technical purpose and the technique effect, the invention is realized by the following technical scheme:
A kind of suede body implantation methods with absorption and photocatalyst function, including suede body material and suede body implantation methods, institute It includes villus, nanometer titanium dioxide, zeolite powder and copper powder to state suede body material, and suede body material is implanted into carrier by the suede body implantation methods Surface, for the suede body material after suede body implantation methods are implanted into carrier surface, the suede body structure of carrier surface has absorption and light Catalyst function, the suede body implantation methods include the following steps:
Step 1, to the composition goods and materials of suede body material:Villus, nanometer titanium dioxide, zeolite powder and copper powder carry out preprocessing, institute Preprocessing is stated to include fixed point location charging respectively and/or stir evenly;
Step 2, preprocessing is carried out to carrier surface, the preprocessing includes cleaning treatment and/or the increase of carrier surface The processing of carrier surface adhesive force;
Step 3, the suede body material after preprocessing is added into flocking plant, the flocking plant applies suede body material on demand Material, the suede body material cover carrier surface by medium or electrostatic;
Step 4, the flocking plant stops applying after the suede body material cladding thickness of carrier surface reaches 0.15-5.5mm Add suede body material;
Step 5, according to the heat-resistant quality of suede body material, heated within the temperature range of 20-180 °C suede body material and/or Carrier surface continues 15-120 minutes;
Step 6, with the fluid flushing suede body material surface and/or carrier surface that speed is 0.5-10 meter per seconds;And/or it uses Speed is that the flexible surface of 0.1-1.5 meter per seconds rubs suede body material surface and/or carrier surface 0.5-300 seconds;
Further, fixed point location charging for by instruction, mark or can restriction site, limit shape it is arbitrary Tool fixture feeds.
Further, the cleaning treatment of the carrier surface includes deoiling and/or derusting and/or dedusting;The increase carries The processing of body surface adhesion force includes surface roughening or the processing of the epithelium of non-ferrous metal phosphating process or non-ferrous metal or add list Surface roughness is more than the coating of Ra6.3.
Further, the flocking plant is electrostatic coating machine and/or dust baking vanish assembly line and/or spray, painting, daub Liquid, rubber powder, micelle device and the device that suede body can be sprayed.
Further, the medium or electrostatic covering carrier be glue, rubber powder, micelle and/or curable polyurethane or Epoxide resin material or device.
Further, when flocking, the control system of the suede body material cladding thickness using thickness transducer real time monitoring and/ Or rule of thumb setting application time control and/or in real time suede thickness increase speed monitoring sensor anticipation control and/or suede body material Material applies velocity sensor and the common calculating of timer monitors.
Further, the heat-resistant quality of the suede body material is suede body materials hot deformation characteristic, the temperature model of the heating Enclosing to be less than causes suede body material temperature distortion to lead to 20 °C of irreclaimable temperature of physical chemistry or less.
Further, the fluid is flow, air draught, inert gas flow;The flexible surface includes silica gel, soft Adhesive tape, soft cloth, hairbrush, bubble bags.
The beneficial effects of the invention are as follows:
1. it is simple in structure, it is easy to operate, it is time saving and energy saving;
2. adhesion effect is good, it is not easy to lint;
3. being evenly distributed, appearance is beautiful, and the dirty residual in surface is few
4. can toxic and harmful gas, various bacteria in passive catalytic degradation air, and bacterium or fungi can be released Toxin decompose and harmless treatment;
5. can toxic and harmful gas, various bacteria in active catalytic degradation air, and bacterium or fungi can be released Toxin decompose and harmless treatment, have deodorization, anti-pollution.
Above description is only the general introduction of technical solution of the present invention, in order to better understand the technical means of the present invention, And can be implemented in accordance with the contents of the specification, with presently preferred embodiments of the present invention and attached drawing is coordinated to be described in detail below.This hair Bright specific implementation mode is shown in detail by following embodiment and its attached drawing.
Description of the drawings
Attached drawing described herein is used to provide further understanding of the present invention, and is constituted part of this application, this hair Bright illustrative embodiments and their description are not constituted improper limitations of the present invention for explaining the present invention.In the accompanying drawings:
Fig. 1 is the suede body implantation methods schematic diagram with absorption and photocatalyst function of the present invention;
Figure label explanation:Nothing.
Specific implementation mode
The invention will be further described below in conjunction with the accompanying drawings:
Shown in referring to Fig.1, a kind of suede body implantation methods with absorption and photocatalyst function, including suede body material and suede body Implantation methods, the suede body material include villus, nanometer titanium dioxide, zeolite powder and copper powder, and the suede body implantation methods are by suede body Material is implanted into carrier surface, and the suede body material is after suede body implantation methods are implanted into carrier surface, the suede body structure of carrier surface Include the following steps with absorption and photocatalyst function, the suede body implantation methods:
Step 1, to the composition goods and materials of suede body material:Villus, nanometer titanium dioxide, zeolite powder and copper powder carry out preprocessing, institute Preprocessing is stated to include fixed point location charging respectively and/or stir evenly;
Step 2, preprocessing is carried out to carrier surface, the preprocessing includes cleaning treatment and/or the increase of carrier surface The processing of carrier surface adhesive force;
Step 3, the suede body material after preprocessing is added into flocking plant, the flocking plant applies suede body material on demand Material, the suede body material cover carrier surface by medium or electrostatic;
Step 4, the flocking plant stops applying after the suede body material cladding thickness of carrier surface reaches 0.15-5.5mm Add suede body material;
Step 5, according to the heat-resistant quality of suede body material, heated within the temperature range of 20-180 °C suede body material and/or Carrier surface continues 15-120 minutes;
Step 6, with the fluid flushing suede body material surface and/or carrier surface that speed is 0.5-10 meter per seconds;And/or it uses Speed is that the flexible surface of 0.1-1.5 meter per seconds rubs suede body material surface and/or carrier surface 0.5-300 seconds;
Further, fixed point location charging for by instruction, mark or can restriction site, limit shape it is arbitrary Tool fixture feeds.
Further, the cleaning treatment of the carrier surface includes deoiling and/or derusting and/or dedusting;The increase carries The processing of body surface adhesion force includes surface roughening or the processing of the epithelium of non-ferrous metal phosphating process or non-ferrous metal or add list Surface roughness is more than the coating of Ra6.3.
Further, the flocking plant is electrostatic coating machine and/or dust baking vanish assembly line and/or spray, painting, daub Liquid, rubber powder, micelle device and the device that suede body can be sprayed.
Further, the medium or electrostatic covering carrier be glue, rubber powder, micelle and/or curable polyurethane or Epoxide resin material or device.
Further, when flocking, the control system of the suede body material cladding thickness using thickness transducer real time monitoring and/ Or rule of thumb setting application time control and/or in real time suede thickness increase speed monitoring sensor anticipation control and/or suede body material Material applies velocity sensor and the common calculating of timer monitors.
Further, the heat-resistant quality of the suede body material is suede body materials hot deformation characteristic, the temperature model of the heating Enclosing to be less than causes suede body material temperature distortion to lead to 20 °C of irreclaimable temperature of physical chemistry or less.
Further, the fluid is flow, air draught, inert gas flow;The flexible surface includes silica gel, soft Adhesive tape, soft cloth, hairbrush, bubble bags.
Specific embodiment:
A kind of villus that suede body material recommends, nano grade titanium white powder, zeolite powder, the specification of copper powder and mass fraction For:
Villus:1.5X0.6mm ± 50%, 110 ± 15% g/M of density, material:There is light on nylon, surface;
Nano grade titanium white powder:The size of fine particles is at 0.1 micron hereinafter, per square meter villus consumption nano grade titanium white powder Quality is 0.5-0.95 grams;
Zeolite powder:Quality per square meter villus consumption zeolite powder is 0.7-1.1 grams;
Copper powder:Quality per square meter villus consumption zeolite powder is 0.1-0.45 grams;
Viscose glue:520# glue, solid content >=30% consume 70 grams of glue per square meter villus.
The goods and materials of suede body material are formed after being stirred:Villus, nanometer titanium dioxide, zeolite powder and copper powder, it is full and uniform, add Enter in flocking plant, cleaning treatment is carried out to carrier surface, and increase carrier surface adhesive force, by medium or electrostatic in carrier Surface cladding thickness reaches the suede body material of 0.15-5.5mm, according to the heat-resistant quality of suede body material, in 20-180 °C of temperature Heating suede body material and carrier surface, last about 15-120 minutes in range;
The fluid flushing suede body of low speed in using again;With soft cloth, the soft materials such as silks and satins, rubber block friction suede body material table Face continues 0.5-300 seconds, in this way we can obtain can actively or passively toxic and harmful gas in catalytic degradation air, Various bacteria, and the toxin decomposition and harmless treatment that bacterium or fungi release can be had the article of the functions such as deodorization, anti-pollution .
The above description is merely a specific embodiment, but scope of protection of the present invention is not limited thereto, any Those familiar with the art in the technical scope disclosed by the present invention, can easily think of the change or the replacement, and should all contain Lid is within protection scope of the present invention.Therefore, the protection scope of the present invention shall be subject to the protection scope of the claims.

Claims (8)

1. a kind of suede body implantation methods with absorption and photocatalyst function, including suede body material and suede body implantation methods, described Suede body material includes villus, nanometer titanium dioxide, zeolite powder and copper powder, and suede body material is implanted into carrier table by the suede body implantation methods Face, it is characterised in that:After suede body implantation methods are implanted into carrier surface, the suede body structure of carrier surface has the suede body material Absorption and photocatalyst function, the suede body implantation methods include the following steps:
Step 1, to the composition goods and materials of suede body material:Villus, nanometer titanium dioxide, zeolite powder and copper powder carry out preprocessing, described pre- Processing includes fixed point location charging respectively and/or stirs evenly;
Step 2, preprocessing is carried out to carrier surface, the preprocessing includes the cleaning treatment and/or increase carrier of carrier surface The processing of surface adhesion force;
Step 3, the suede body material after preprocessing is added into flocking plant, the flocking plant applies suede body material, institute on demand It states suede body material and carrier surface is covered by medium or electrostatic;
Step 4, the flocking plant stops applying suede after the suede body material cladding thickness of carrier surface reaches 0.15-5.5mm Body material;
Step 5, according to the heat-resistant quality of suede body material, suede body material and/or carrier are heated within the temperature range of 20-180 °C Surface continues 15-120 minutes;
Step 6, with the fluid flushing suede body material surface and/or carrier surface that speed is 0.5-10 meter per seconds;And/or use speed It rubs suede body material surface and/or carrier surface 0.5-300 seconds for the flexible surface of 0.1-1.5 meter per seconds.
2. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Institute It states in step 1 there are when fixed point location charging, the fixed point location charging is passes through instruction, mark or being capable of restriction site, limit The arbitrary tool fixture of shape processed feeds.
3. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Institute When stating in step 2 cleaning treatment there are carrier surface, the cleaning treatment of the carrier surface include deoil and/or derust with/ Or dedusting;When there is the processing for increasing carrier surface adhesive force in the step 2, the processing for increasing carrier surface adhesive force Including surface roughening or the processing of the epithelium of non-ferrous metal phosphating process or non-ferrous metal or additional surface roughness more than Ra6.3's Coating.
4. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Step Flocking plant described in rapid 3 is electrostatic coating machine and/or dusts and baking vanish assembly line and can spray the device of suede body.
5. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Step There are when medium in rapid 3, the medium is glue, rubber powder or micelle.
6. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Step In rapid 4 when flocking, the control system of the suede body material cladding thickness is monitored in real time using thickness transducer and/or is rule of thumb set Determine application time control and/or in real time suede thickness increase speed monitoring sensor anticipation control and/or suede body material apply speed pass The common calculating of sensor and timer monitors.
7. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Step The heat-resistant quality of suede body material described in rapid 5 is suede body materials hot deformation characteristic, and the temperature range of the heating, which should be less than, to be caused Suede body material temperature distortion leads to 20 °C of irreclaimable temperature of physical chemistry or less.
8. a kind of suede body implantation methods with absorption and photocatalyst function according to claim 1, it is characterised in that:Institute It states there are when fluid in step 6, the fluid is flow, air draught or inert gas flow;There are flexible in the step 6 When surface, the flexible surface includes silica gel, flexible glue bar, soft cloth, hairbrush or bubble bags.
CN201610450173.2A 2016-06-19 2016-06-19 A kind of suede body implantation methods with absorption and photocatalyst function Active CN106110880B (en)