CN106078086B - 一种核燃料元件包壳锆合金不锈钢复合管及其制备方法 - Google Patents
一种核燃料元件包壳锆合金不锈钢复合管及其制备方法 Download PDFInfo
- Publication number
- CN106078086B CN106078086B CN201610411172.7A CN201610411172A CN106078086B CN 106078086 B CN106078086 B CN 106078086B CN 201610411172 A CN201610411172 A CN 201610411172A CN 106078086 B CN106078086 B CN 106078086B
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- zirconium alloy
- pipe
- tube
- blank
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (4)