CN105484098A CN201410472670.3A CN201410472670A CN105484098A CN 105484098 A CN105484098 A CN 105484098A CN 201410472670 A CN201410472670 A CN 201410472670A CN 105484098 A CN105484098 A CN 105484098A
Authority
CN
China
Prior art keywords
parts
pulp
polychrome
pigment
cork paper
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410472670.3A
Other languages
Chinese (zh)
Inventor
徐祥祥
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU JINHENG NEW STYLE PACKAGE MATERIAL CO Ltd
Original Assignee
JIANGSU JINHENG NEW STYLE PACKAGE MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU JINHENG NEW STYLE PACKAGE MATERIAL CO Ltd filed Critical JIANGSU JINHENG NEW STYLE PACKAGE MATERIAL CO Ltd
Priority to CN201410472670.3A priority Critical patent/CN105484098A/en
Publication of CN105484098A publication Critical patent/CN105484098A/en
Pending legal-status Critical Current

Links

Landscapes

  • Paper (AREA)

Abstract

The present invention discloses a multi-color tipping paper, which is prepared from the following raw materials by weight: 50-80 parts of leaf wood pulp, 10-15 parts of rosin size, 1-3 parts of ethylene glycol, 2-4 parts of acrylic acid, 8-20 parts of a pigment, 1-5 parts of sodium persulfate, 2-4 parts of polyvinyl acetate, 5-10 parts of talc powder, and 90-120 parts of an alcohol solvent. The production method comprises: mixing the pigment, the rosin size, the ethylene glycol, the acrylic acid, the sodium persulfate, the polyvinyl acetate and the talc powder according to a certain weight part ratio, adding the obtained mixture to the alcohol solvent, uniformly stirring, adding a mixing pulp of a needle-leaf wood pulp and a broadleaf wood pulp to the uniformly stirred solution, continuously stirring to achieve a paper pulp concentration of 0.8%, dewatering the paper pulp, drying, and pressing on a paper pressing machine to obtain the multi-color tipping paper. According to the present invention, the pigment is added during the paper pulp production process so as to achieve different colors, and during the use process, the toxicity of the multi-color tipping paper is minimized.

Description

A kind of polychrome cork paper and production method thereof
Technical field
The present invention relates to a kind of packaging material field, especially relate to a kind of wrapping paper field of cigarette holder.
Background technology
Cork paper be body paper is carried out printing processing after the one decoration paper that obtains, its floral designs are with the cross section of tobacco leaf limb for certificate, and color and luster takes pseudo-classic style, tarnish (or few gloss), makes people produce simple and unsophisticated, graceful sense.Having another name called tipping paper, is a kind of cigarette packaging material, specializes in cigarette and is used as filter tip cigarette packaging, belong to special industrial paper using.The coated papers of cork paper mostly in crocus (also having plenty of white), top is printed on gold thread or green line, dull coloring.For reaching the object improving outward appearance, need cigarette holder rich color, but present polychrome cigarette holder achieves the goal mainly through printing coatings (mill base) or ink on the cork paper made, not only increase the consumption contaminated environment of chemicals, this kind of chemicals adhesive force is inadequate simultaneously, is easy to work the mischief to human body.
Summary of the invention
Goal of the invention: the object of the invention is for the deficiencies in the prior art, provides a kind of polychrome cork paper of nontoxic pollution-free;
Another object of the present invention is to provide a kind of method preparing described polychrome yew.
Technical scheme: polychrome cork paper of the present invention, be made up of following raw material:
Leaf wood pulp 50 ~ 80 parts;
Gum rosin 10 ~ 15 parts;
Ethylene glycol 1 ~ 3 part;
2 ~ 4 parts, acrylic acid;
Pigment 8 ~ 20 parts;
Sodium peroxydisulfate 1 ~ 5 part;
Polyvinyl acetate 2 ~ 4 parts;
Talcum powder 5 ~ 10 parts;
Spirit solvent 90 ~ 120 parts;
With parts by weight.
As preferably, described polychrome cork paper, be made up of following raw material:
Leaf wood pulp 65 parts;
Gum rosin 12 parts;
Ethylene glycol 2 parts;
3 parts, acrylic acid;
Pigment 15 parts;
Sodium peroxydisulfate 3 parts;
Polyvinyl acetate 3 parts;
Talcum powder 8 parts;
Spirit solvent 110 parts;
With parts by weight.
As preferably, described pigment is iron oxide red, titanium dioxide, phthalocyanine blue, quinacridone and even one or more yellowish hybrid pigments.
As preferably, described leaf wood pulp is the mixed serum of softwood pulp and hardwood pulp.
The production method of polychrome cork paper of the present invention, comprises the following steps:
(1) prepare burden: select dissimilar pigment to mix by weight with gum rosin, ethylene glycol, acrylic acid, sodium peroxydisulfate, polyvinyl acetate and talcum powder as required and add in spirit solvent, stir;
(2) slurrying: the leaf wood pulp adding weight portion in the solution stirred, continues to stir and adds spirit solvent, until pulp density reaches 0.5 ~ 0.8%;
(3) suppress: by dewatering of pulp, oven dry, nipper is suppressed, and punching obtains described polychrome cork paper.
Beneficial effect: the present invention adds pigment in paper pulp manufacturing process, under prerequisite free from environmental pollution, to reach different color object, strong adhesion simultaneously, in use, at utmost reduces the toxicity of polychrome cork paper; The present invention adopts multiple different organic pigment to mix, and can realize the object of multicolour.
Detailed description of the invention
Below technical solution of the present invention is described in detail, but protection scope of the present invention is not limited to described embodiment.
embodiment 1:a kind of polychrome cork paper, is made up of following raw material: the mixed serum of softwood pulp and hardwood pulp 50 parts; Gum rosin 10 parts; Ethylene glycol 1 part; 2 parts, acrylic acid; Phthalocyanine blue pigment 8 parts; Sodium peroxydisulfate 1 part; Polyvinyl acetate 2 parts; Talcum powder 5 parts; Spirit solvent 90 parts; With parts by weight.
A production method for polychrome cork paper, comprises the following steps:
(1) prepare burden: phthalocyanine blue pigment is mixed by weight with gum rosin, ethylene glycol, acrylic acid, sodium peroxydisulfate, polyvinyl acetate and talcum powder and adds in spirit solvent, stir;
(2) slurrying: add the softwood pulp of weight portion and the mixed serum of hardwood pulp in the solution stirred, continue to stir and add spirit solvent, until pulp density reaches 0.5%;
(3) suppress: by dewatering of pulp, oven dry, nipper is suppressed, and punching obtains described polychrome cork paper.
embodiment 2:a kind of polychrome cork paper, is made up of following raw material: the mixed serum of softwood pulp and hardwood pulp 80 parts; Gum rosin 15 parts; Ethylene glycol 3 parts; 4 parts, acrylic acid; Titanium dioxide 20 parts; Sodium peroxydisulfate 5 parts; Polyvinyl acetate 4 parts; Talcum powder 10 parts; Spirit solvent 120 parts; With parts by weight.
A production method for polychrome cork paper, comprises the following steps:
(1) prepare burden: TiO 2 pigment is mixed by weight with gum rosin, ethylene glycol, acrylic acid, sodium peroxydisulfate, polyvinyl acetate and talcum powder and adds in spirit solvent, stir;
(2) slurrying: the mixed serum adding softwood pulp and hardwood pulp in the solution stirred, continues to stir and adds spirit solvent, until pulp density reaches 0.8%;
(3) suppress: by dewatering of pulp, oven dry, nipper is suppressed, and punching obtains described polychrome cork paper.
embodiment 3:a kind of polychrome cork paper, is made up of following raw material: the mixed serum of softwood pulp and hardwood pulp 65 parts; Gum rosin 12 parts; Ethylene glycol 2 parts; 3 parts, acrylic acid; Quinacridone and even yellowish hybrid pigment 15 parts; Sodium peroxydisulfate 3 parts; Polyvinyl acetate 3 parts; Talcum powder 8 parts; Spirit solvent 110 parts; With parts by weight.
A production method for polychrome cork paper, comprises the following steps:
(1) prepare burden: hybrid pigment yellowish to quinacridone and idol is mixed by weight with gum rosin, ethylene glycol, acrylic acid, sodium peroxydisulfate, polyvinyl acetate and talcum powder and adds in spirit solvent, stir;
(2) slurrying: add the softwood pulp of weight portion and the mixed serum of hardwood pulp in the solution stirred, continue to stir and add spirit solvent, until pulp density reaches 0.65%;
(3) suppress: by dewatering of pulp, oven dry, nipper is suppressed, and punching obtains described polychrome cork paper.
As mentioned above, although represented with reference to specific preferred embodiment and described the present invention, it shall not be construed as the restriction to the present invention self.Under the spirit and scope of the present invention prerequisite not departing from claims definition, various change can be made in the form and details to it.

Claims (5)

1. a polychrome cork paper, is characterized in that being made up of following raw material:
Leaf wood pulp 50 ~ 80 parts;
Gum rosin 10 ~ 15 parts;
Ethylene glycol 1 ~ 3 part;
2 ~ 4 parts, acrylic acid;
Pigment 8 ~ 20 parts;
Sodium peroxydisulfate 1 ~ 5 part;
Polyvinyl acetate 2 ~ 4 parts;
Talcum powder 5 ~ 10 parts;
Spirit solvent 90 ~ 120 parts;
With parts by weight.
2. polychrome cork paper according to claim 1, is characterized in that being made up of following raw material:
Leaf wood pulp 65 parts;
Gum rosin 12 parts;
Ethylene glycol 2 parts;
3 parts, acrylic acid;
Pigment 15 parts;
Sodium peroxydisulfate 3 parts;
Polyvinyl acetate 3 parts;
Talcum powder 8 parts;
Spirit solvent 110 parts;
With parts by weight.
3. polychrome cork paper according to claim 1, is characterized in that: described pigment is iron oxide red, titanium dioxide, phthalocyanine blue, quinacridone and even one or more yellowish hybrid pigments.
4. polychrome cork paper according to claim 1, is characterized in that: described leaf wood pulp is the mixed serum of softwood pulp and hardwood pulp.
5. the production method of polychrome cork paper according to any one of claim 1 ~ 4, is characterized in that, comprise the following steps:
(1) prepare burden: select dissimilar pigment to mix by weight with gum rosin, ethylene glycol, acrylic acid, sodium peroxydisulfate, polyvinyl acetate and talcum powder as required and add in spirit solvent, stir;
(2) slurrying: the leaf wood pulp adding weight portion in the solution stirred, continues to stir and adds spirit solvent, until pulp density reaches 0.5 ~ 0.8%;
(3) suppress: by dewatering of pulp, oven dry, nipper is suppressed, and punching obtains described polychrome cork paper.
CN201410472670.3A 2014-09-17 2014-09-17 Multi-color tipping paper and production method thereof Pending CN105484098A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410472670.3A CN105484098A (en) 2014-09-17 2014-09-17 Multi-color tipping paper and production method thereof

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410472670.3A CN105484098A (en) 2014-09-17 2014-09-17 Multi-color tipping paper and production method thereof

Publications (1)

Publication Number Publication Date
CN105484098A true CN105484098A (en) 2016-04-13

Family

ID=55671344

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410472670.3A Pending CN105484098A (en) 2014-09-17 2014-09-17 Multi-color tipping paper and production method thereof

Country Status (1)

Country Link
CN (1) CN105484098A (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN115142300A (en) * 2021-03-31 2022-10-04 浙江荣丰纸业有限公司 Yellow paper dotted single gold thread tipping paper and preparation method thereof

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN115142300A (en) * 2021-03-31 2022-10-04 浙江荣丰纸业有限公司 Yellow paper dotted single gold thread tipping paper and preparation method thereof

Similar Documents

Publication Publication Date Title
CN102174747B (en) Environment-friendly textile printing pearlescent adhesive cement and preparation method and application thereof
CN101735524A (en) Method for preparing polystyrene (EPS) dyed foam
CN104191853B (en) The production technology of a kind of water-based sub-light waterproof ink jet printing non-woven fabrics
CN107542005A (en) A kind of paint for cork paper bobbin
CN108049207A (en) Composite reactive printing gum
CN103422386B (en) Kraft paper and making method thereof
CN104263159B (en) For environment-friendly type aqueous coating making glitter powder and preparation method thereof
CN102909766A (en) Color bamboo and timber processing method
CN105586804A (en) Modified acrylic resin coating agent for decorating paper and preparation method of modified acrylic resin coating agent
CN107672376B (en) Processing and manufacturing method of cinnabar relief painting
CN105484098A (en) Multi-color tipping paper and production method thereof
CN109594406A (en) A kind of imitation parchment preparation process
CN103241058B (en) Two colour painting manufacture craft
CN103088704B (en) Production method of sandy-dot art paper
CN104108954B (en) Method for enabling porcelain body surface to have painting effect on rice paper
CN107190578A (en) A kind of cork paper and preparation method thereof
CN106149475B (en) Binding and layout paper and its production technology
CN103088698A (en) Papermaking processing process
CN101250839A (en) Method for producing temperature-charging artistic shagreen paper
CN104140719A (en) Preparation method of black or grey toner for archaized floor
CN108467624A (en) Marble paper inorganic pigment and similar reaction glaze marble paper and preparation method thereof
CN101380865A (en) How to make hair sculptures
CN201482203U (en) Color lump canvas board with numeric identifiers
CN206543547U (en) A kind of Paint dilution bucket
CN105837254A (en) Ceramic pigment pretreatment method

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
WD01 Invention patent application deemed withdrawn after publication
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20160413