CN105319278A - 一种超声对比试块嵌入件放置方法 - Google Patents
一种超声对比试块嵌入件放置方法 Download PDFInfo
- Publication number
- CN105319278A CN105319278A CN201410323227.XA CN201410323227A CN105319278A CN 105319278 A CN105319278 A CN 105319278A CN 201410323227 A CN201410323227 A CN 201410323227A CN 105319278 A CN105319278 A CN 105319278A
- Authority
- CN
- China
- Prior art keywords
- artificial defect
- discs
- test block
- disc
- contrast test
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明属于无损检测技术领域,提供一种超声对比试块嵌入件放置方法,能解决实际铺层时薄膜极易发生错位的问题。本发明的技术方案包括:将两个人工缺陷圆片并排粘贴在胶带上;沿两个人工缺陷圆片的公切线方向将胶带对折,使两个人工缺陷圆片重叠在一起;从胶带上剪下人工缺陷圆片;将剪下的人工缺陷圆片放入铺层中。具体的,所述人工缺陷圆片为聚四氟乙烯薄膜圆片。
Description
技术领域
本发明属于无损检测技术领域,涉及一种超声对比试块嵌入件放置方法。
背景技术
在进行复合材料超声波检测时,需用相应的试块作为对比,调整灵敏度后进行零件的检测。在制作对比试块时,需要嵌入人工缺陷,目前仅是把两片薄膜重叠后放置铺层上,当在上面铺设其它材料时,这两片薄膜极易发生错位,使得人工缺陷的面积大于10mm2,无法满足检测要求,同时费时费料。
发明内容
本发明要解决的技术问题:提供一种超声对比试块嵌入件放置方法,能解决实际铺层时薄膜极易发生错位的问题。
本发明的技术方案:一种超声对比试块嵌入件放置方法,包括:
将两个人工缺陷圆片并排粘贴在胶带上;
沿两个人工缺陷圆片的公切线方向将胶带对折,使两个人工缺陷圆片重叠在一起;
从胶带上剪下人工缺陷圆片;
将剪下的人工缺陷圆片放入铺层中。
具体的,所述人工缺陷圆片为聚四氟乙烯薄膜圆片。
本发明的有益效果:本发明复合材料超声波检测对比试块嵌入物的放置方法,通过使用胶带粘贴人工缺陷后嵌入试块,不仅避免了发生错位,还增强了衰减,使用方便,能有效得提高产品质量和工作效率。
具体实施方式
本发明一种超声对比试块嵌入件放置方法,包括以下步骤:
1.1)按照分层对比试片制作示意图制作试块,在不同的铺层不同的位置放置嵌入物——聚四氟乙烯薄膜。
先准备两个φ3.6毫米的聚四氟乙烯薄膜圆片,此圆片为标准用材。
1.2)准备一专用的蓝色胶带,有一定的粘力。
1.3)将两个φ3.6毫米的聚四氟乙烯薄膜圆片依次挨着粘贴在蓝胶带上,有一个接触点,接触面要100%粘贴上,不要有褶皱和气泡。
1.4)在接触点处对折,使得两个圆片重叠在一起,然后把其它部位粘贴在一起,沿着薄膜边缘连蓝胶带一起剪下,由于蓝胶带中间有接连,所以对折后的两层聚四氟乙烯薄膜就会连在一起,不会发生错位,
1.5)将圆片放入铺层中,进行试片的制作。
Claims (2)
1.一种超声对比试块嵌入件放置方法,其特征在于,包括:
将两个人工缺陷圆片并排粘贴在胶带上;
沿两个人工缺陷圆片的公切线方向将胶带对折,使两个人工缺陷圆片重叠在一起;
从胶带上剪下人工缺陷圆片;
将剪下的人工缺陷圆片放入铺层中。
2.如权利要求1所述的一种超声对比试块嵌入件放置方法,其特征在于,所述人工缺陷圆片为聚四氟乙烯薄膜圆片。