CN105059005A - 一种阻燃浮雕墙纸印刷工艺 - Google Patents
一种阻燃浮雕墙纸印刷工艺 Download PDFInfo
- Publication number
- CN105059005A CN105059005A CN201510543639.9A CN201510543639A CN105059005A CN 105059005 A CN105059005 A CN 105059005A CN 201510543639 A CN201510543639 A CN 201510543639A CN 105059005 A CN105059005 A CN 105059005A
- Authority
- CN
- China
- Prior art keywords
- wallpaper
- semi
- anaglyptic
- flame
- retardant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及印刷领域,尤其是一种阻燃浮雕墙纸印刷工艺,工艺流程如下:通过搅拌器将PVC糊进行搅拌,制成流动性PVC糊;原纸表面涂布均匀平整的PVC糊,加热塑化后成涂层半成品;在涂层半成品的塑胶面进行印刷成为印刷半成品;印刷半成品经过浮雕工序;浮雕工序后的墙纸经过烘干处理;烘干处理后的墙纸表面经过抗煮变耐高温油墨处理后收卷即得阻燃浮雕墙纸。本发明的一种阻燃浮雕墙纸印刷工艺制成的浮雕墙纸具有阻燃效果,安全性更高,耐撕裂强度高,可制成各种图案及凹凸纹,富有很强的质感,易于粘贴,陈旧后也易于更换,且表面不吸水,可用布擦洗,并且具有手感好、压纹深、纹理清晰、立体感强的特点。
Description
技术领域
本发明涉及印刷领域,尤其是一种阻燃浮雕墙纸印刷工艺。
背景技术
目前,墙纸在印刷时,一般都是先将卷筒墙纸展平拉直,然后,将其切割成若干段纸段,再将这些纸段通过手工印刷,但是,这种印刷方式,其操作麻烦,生产效率低,而且,人工印刷效果差;另外采用传统工艺制成的浮雕墙纸手感差、压纹不够清晰、立体感差,生产效率低、材料浪费大、操作麻烦。另外,普通的墙纸不具备阻燃性,存在一定的安全隐患。
发明内容
本发明要解决的技术问题是:为了克服现有技术的缺陷,本发明提供了一种生产效果高、操作简单的阻燃浮雕墙纸的印刷工艺。
本发明解决其技术问题所采用的技术方案是:一种阻燃浮雕墙纸印刷工艺,工艺流程如下:
a.通过搅拌器将PVC糊进行搅拌,制成流动性PVC糊;
b.原纸表面涂布均匀平整的PVC糊,加热塑化后成涂层半成品;
c.在涂层半成品的塑胶面进行印刷成为印刷半成品;
d.印刷半成品经过浮雕工序;
e.浮雕工序后的墙纸经过烘干处理;
f.烘干处理后的墙纸表面经过抗煮变耐高温油墨处理后收卷即得阻燃浮雕墙纸。
进一步地,所述的烘干处理所采用的烘干装置为红外烘箱。
进一步地,所述的烘干处理所采用的温度为200℃-250℃。
本发明的有益效果是,本发明的一种阻燃浮雕墙纸印刷工艺制成的浮雕墙纸具有阻燃效果,安全性更高,耐撕裂强度高,可制成各种图案及凹凸纹,富有很强的质感,易于粘贴,陈旧后也易于更换,且表面不吸水,可用布擦洗,并且具有手感好、压纹深、纹理清晰、立体感强的特点。
具体实施方式
一种阻燃浮雕墙纸印刷工艺,工艺流程如下:
a.通过搅拌器将PVC糊进行搅拌,制成流动性PVC糊;
b.原纸表面涂布均匀平整的PVC糊,加热塑化后成涂层半成品;
c.在涂层半成品的塑胶面进行印刷成为印刷半成品;
d.印刷半成品经过浮雕工序;
e.浮雕工序后的墙纸经过烘干处理;
f.烘干处理后的墙纸表面经过抗煮变耐高温油墨处理后收卷即得阻燃浮雕墙纸。
进一步地,烘干处理所采用的烘干装置为红外烘箱。
进一步地,烘干处理所采用的温度为200℃-250℃。
以上述依据本发明的理想实施例为启示,通过上述的说明内容,相关工作人员完全可以在不偏离本项发明技术思想的范围内,进行多样的变更以及修改。本项发明的技术性范围并不局限于说明书上的内容,必须要根据权利要求范围来确定其技术性范围。
Claims (3)
1.一种阻燃浮雕墙纸印刷工艺,其特征是,工艺流程如下:
a.通过搅拌器将PVC糊进行搅拌,制成流动性PVC糊;
b.原纸表面涂布均匀平整的PVC糊,加热塑化后成涂层半成品;
c.在涂层半成品的塑胶面进行印刷成为印刷半成品;
d.印刷半成品经过浮雕工序;
e.浮雕工序后的墙纸经过烘干处理;
f:烘干处理后的墙纸表面经过抗煮变耐高温油墨处理后收卷即得阻燃浮雕墙纸。
2.根据权利要求1所述的阻燃浮雕墙纸印刷工艺,其特征是:所述的烘干处理所采用的烘干装置为红外烘箱。
3.根据权利要求1所述的阻燃浮雕墙纸印刷工艺,其特征是:所述的烘干处理所采用的温度为200℃-250℃。