[go: up one dir, main page]

CN104496367A - 用于制备防水材料的方法 - Google Patents

用于制备防水材料的方法 Download PDF

Info

Publication number
CN104496367A
CN104496367A CN201410730620.0A CN201410730620A CN104496367A CN 104496367 A CN104496367 A CN 104496367A CN 201410730620 A CN201410730620 A CN 201410730620A CN 104496367 A CN104496367 A CN 104496367A
Authority
CN
China
Prior art keywords
parts
weight part
component
preparation
weight
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410730620.0A
Other languages
English (en)
Inventor
张志刚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU GREAT COMPOSITE MATERIAL CO Ltd
Original Assignee
JIANGSU GREAT COMPOSITE MATERIAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU GREAT COMPOSITE MATERIAL CO Ltd filed Critical JIANGSU GREAT COMPOSITE MATERIAL CO Ltd
Priority to CN201410730620.0A priority Critical patent/CN104496367A/zh
Publication of CN104496367A publication Critical patent/CN104496367A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种用于制备防水材料的方法,包括如下步骤:1)将8重量份硫酸锌、3重量份异戊烯醇、13重量份硅丙乳液、0.8重量份四水氟化锌、2重量份水混合均匀,制得A组分;2)将8.1重量份石英砂、1.8重量份纤维素醚、5.6重量份普通硅酸盐水泥、1.5重量份高铝水泥、4.2重量份氨基磺酸混合均匀,制得B组分;3)将5重量份A组分与8重量份B组分混合,加热至64℃,再搅拌均匀,自然冷却,制得防水材料。本发明制备的防水材料具有良好的柔韧性、防水性、防开裂,适合制备厨卫产品。

Description

用于制备防水材料的方法
技术领域
本发明涉及用于制备防水材料的方法。
背景技术
现有的厨卫产品,其柔韧性、防水性、防开裂性能有待改进。
发明内容
本发明的目的在于提供一种用于制备防水材料的方法,其制备的防水材料具有良好的柔韧性、防水性、防开裂,适合制备厨卫产品。
为实现上述目的,本发明的技术方案是设计一种用于制备防水材料的方法,包括如下步骤:
1)将8重量份硫酸锌、3重量份异戊烯醇、13重量份硅丙乳液、0.8重量份四水氟化锌、2重量份水混合均匀,制得A组分;
2)将8.1重量份石英砂、1.8重量份纤维素醚、5.6重量份普通硅酸盐水泥、1.5重量份高铝水泥、4.2重量份氨基磺酸混合均匀,制得B组分;
3)将5重量份A组分与8重量份B组分混合,加热至64℃,再搅拌均匀,自然冷却,制得防水材料。
本发明的优点和有益效果在于:提供一种用于制备防水材料的方法,其制备的防水材料具有良好的柔韧性、防水性、防开裂,适合制备厨卫产品。
具体实施方式
下面结合实施例,对本发明的具体实施方式作进一步描述。以下实施例仅用于更加清楚地说明本发明的技术方案,而不能以此来限制本发明的保护范围。
本发明具体实施的技术方案是:
一种用于制备防水材料的方法,包括如下步骤:
1)将8重量份硫酸锌、3重量份异戊烯醇、13重量份硅丙乳液、0.8重量份四水氟化锌、2重量份水混合均匀,制得A组分;
2)将8.1重量份石英砂、1.8重量份纤维素醚、5.6重量份普通硅酸盐水泥、1.5重量份高铝水泥、4.2重量份氨基磺酸混合均匀,制得B组分;
3)将5重量份A组分与8重量份B组分混合,加热至64℃,再搅拌均匀,自然冷却,制得防水材料。
以上所述仅是本发明的优选实施方式,应当指出,对于本技术领域的普通技术人员来说,在不脱离本发明技术原理的前提下,还可以做出若干改进和润饰,这些改进和润饰也应视为本发明的保护范围。

Claims (1)

1.用于制备防水材料的方法,其特征在于,包括如下步骤:
1)将8重量份硫酸锌、3重量份异戊烯醇、13重量份硅丙乳液、0.8重量份四水氟化锌、2重量份水混合均匀,制得A组分;
2)将8.1重量份石英砂、1.8重量份纤维素醚、5.6重量份普通硅酸盐水泥、1.5重量份高铝水泥、4.2重量份氨基磺酸混合均匀,制得B组分;
3)将5重量份A组分与8重量份B组分混合,加热至64℃,再搅拌均匀,自然冷却,制得防水材料。
CN201410730620.0A 2014-12-05 2014-12-05 用于制备防水材料的方法 Pending CN104496367A (zh)