CN104411136B - The manufacturing method of mobile terminal shell, mobile terminal and mobile terminal shell - Google Patents
The manufacturing method of mobile terminal shell, mobile terminal and mobile terminal shell Download PDFInfo
- Publication number
- CN104411136B CN104411136B CN201410586830.7A CN201410586830A CN104411136B CN 104411136 B CN104411136 B CN 104411136B CN 201410586830 A CN201410586830 A CN 201410586830A CN 104411136 B CN104411136 B CN 104411136B
- Authority
- CN
- China
- Prior art keywords
- mobile terminal
- metal body
- layer
- shell
- chamfering
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
本发明适用于移动终端技术领域,公开了一种移动终端壳体、移动终端和移动终端壳体的制造方法。移动终端壳体包括金属本体,金属本体的表面具有电泳层,金属本体的至少一处边缘设置有倒角,倒角处设置有阳极氧化层。移动终端具有上述的移动终端壳体。制造方法包括以下步骤:制备金属本体,使金属本体表面附着有电泳层,对电泳后的金属本体进行倒角,再使金属本体的倒角面形成有阳极氧化层。本发明所提供的移动终端壳体、移动终端和移动终端壳体的制造方法,其壳体由电泳层和阳极氧化层包覆,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,电泳层与阳极氧化层的质感不同,产品壳体的外观表现力强。
The invention is applicable to the technical field of mobile terminals, and discloses a mobile terminal casing, a mobile terminal and a manufacturing method for the mobile terminal casing. The mobile terminal casing includes a metal body, the surface of the metal body has an electrophoretic layer, at least one edge of the metal body is provided with a chamfer, and an anodic oxidation layer is provided at the chamfer. The mobile terminal has the above-mentioned mobile terminal case. The manufacturing method includes the following steps: preparing a metal body, attaching an electrophoretic layer to the surface of the metal body, chamfering the electrophoresed metal body, and forming an anodic oxidation layer on the chamfered surface of the metal body. The mobile terminal casing provided by the present invention, the mobile terminal and the manufacturing method of the mobile terminal casing, the casing is covered by the electrophoretic layer and the anodic oxidation layer, which can effectively protect the casing from corrosion, and the casing is in use. It is not easy to scratch, the reliability of the shell is high, the texture of the electrophoretic layer and the anodized layer are different, and the appearance of the product shell is strong.
Description
技术领域technical field
本发明属于移动终端技术领域,尤其涉及一种移动终端壳体、移动终端和移动终端壳体的制造方法。The invention belongs to the technical field of mobile terminals, and in particular relates to a mobile terminal casing, a mobile terminal and a method for manufacturing the mobile terminal casing.
背景技术Background technique
目前的移动终端,其壳体一般采用塑胶或铝合金材质。现有技术中铝合金壳体,其表面处理技术一般采用喷砂或拉丝,产品表面效果单一,使用过程中容易划伤,可靠性较差。Currently, the casing of the mobile terminal is generally made of plastic or aluminum alloy. In the prior art, the surface treatment technology of the aluminum alloy shell generally adopts sandblasting or wire drawing, and the surface effect of the product is single, and it is easy to be scratched during use, and the reliability is poor.
发明内容Contents of the invention
本发明的目的在于克服上述现有技术的不足,提供了一种移动终端壳体、移动终端和移动终端壳体的制造方法,其壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层与阳极氧化层的质感不同,产品壳体的外观表现力强。The purpose of the present invention is to overcome the shortcomings of the above-mentioned prior art, and provide a mobile terminal casing, a mobile terminal and a manufacturing method for the mobile terminal casing. The casing is not easily scratched during use, and the casing has high reliability. Moreover, the texture of the electrophoretic layer is different from that of the anodized layer, and the appearance of the product shell is highly expressive.
本发明的技术方案是:一种移动终端壳体,包括金属本体,所述金属本体的表面具有电泳层,所述金属本体的至少一处边缘设置有倒角,所述倒角处设置有阳极氧化层。The technical solution of the present invention is: a mobile terminal housing, including a metal body, the surface of the metal body has an electrophoretic layer, at least one edge of the metal body is provided with a chamfer, and the chamfer is provided with an anode oxide layer.
可选地,所述金属本体采用铝合金材料制成。Optionally, the metal body is made of aluminum alloy.
可选地,所述金属本体的正面或/和背面的边缘均设置有所述倒角。Optionally, the front and/or back edges of the metal body are provided with the chamfers.
可选地,所述电泳层与所述阳极氧化层的颜色不同。Optionally, the color of the electrophoretic layer is different from that of the anodized layer.
本发明还提供了一种移动终端,所述移动终端具有上述的移动终端壳体。The present invention also provides a mobile terminal, which has the above-mentioned mobile terminal housing.
可选地,所述移动终端为手机或平板电脑。Optionally, the mobile terminal is a mobile phone or a tablet computer.
本发明还提供了一种移动终端壳体的制造方法,包括以下步骤:制备金属本体,将所述金属本体进行电泳处理使金属本体表面附着有电泳层,对电泳后的金属本体进行倒角,将倒角后的金属本体进行阳极氧化处理以使所述金属本体的倒角面形成有阳极氧化层。The present invention also provides a method for manufacturing a mobile terminal housing, comprising the following steps: preparing a metal body, performing electrophoretic treatment on the metal body so that an electrophoretic layer is attached to the surface of the metal body, chamfering the electrophoresed metal body, The chamfered metal body is anodized so that the chamfered surface of the metal body is formed with an anodic oxidation layer.
可选地,所述金属本体采用铝合金材料制成。Optionally, the metal body is made of aluminum alloy.
可选地,所述金属本体采用铝合金材料通过机加工加工而成。Optionally, the metal body is made of aluminum alloy material through machining.
可选地,所述倒角通过机加工而成。Optionally, the chamfer is formed by machining.
本发明所提供的移动终端壳体、移动终端和移动终端壳体的制造方法,其通过先对金属壳体进行电泳处理使金属本体表面形成有电泳层,再对电泳后的金属本体进行倒角,将倒角后的金属本体进行阳极氧化处理以使所述金属本体的倒角面形成有阳极氧化层,金属本体的表面具有电泳层,倒角处具有阳极氧化层,壳体由电泳层和阳极氧化层包覆,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层与阳极氧化层的质感不同,产品壳体的外观表现力强,产品外观效果更有个性,更有科技感。The mobile terminal shell provided by the present invention, the mobile terminal and the manufacturing method of the mobile terminal shell, firstly perform electrophoretic treatment on the metal shell to form an electrophoretic layer on the surface of the metal body, and then chamfer the electrophoresis metal body The chamfered metal body is anodized so that the chamfered surface of the metal body is formed with an anodized layer, the surface of the metal body has an electrophoretic layer, and the chamfered area has an anodized layer, and the shell is composed of an electrophoretic layer and an anodized layer. Anodized layer coating can effectively protect the shell from corrosion, the shell is not easy to scratch during use, and the shell has high reliability. Moreover, the texture of the electrophoretic layer and the anodized layer are different, and the appearance of the product shell Powerful, the appearance of the product is more personalized and has a sense of technology.
附图说明Description of drawings
为了更清楚地说明本发明实施例中的技术方案,下面将对实施例中所需要使用的附图作简单地介绍,显而易见地,下面描述中的附图仅仅是本发明的一些实施例,对于本领域普通技术人员来讲,在不付出创造性劳动的前提下,还可以根据这些附图获得其他的附图。In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following will briefly introduce the accompanying drawings that need to be used in the embodiments. Obviously, the accompanying drawings in the following description are only some embodiments of the present invention. For Those of ordinary skill in the art can also obtain other drawings based on these drawings without making creative efforts.
图1是本发明实施例提供的移动终端壳体的局部剖面示意图。FIG. 1 is a schematic partial cross-sectional view of a mobile terminal housing provided by an embodiment of the present invention.
具体实施方式Detailed ways
为了使本发明的目的、技术方案及优点更加清楚明白,以下结合附图及实施例,对本发明进行进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定本发明。In order to make the object, technical solution and advantages of the present invention clearer, the present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the present invention, not to limit the present invention.
需要说明的是,当元件被称为“固定于”或“设置于”另一个元件,它可以直接在另一个元件上或者可能同时存在居中元件。当一个元件被称为是“连接于”另一个元件,它可以是直接连接到另一个元件或者可能同时存在居中元件。It should be noted that when an element is referred to as being “fixed on” or “disposed on” another element, it may be directly on the other element or there may be an intervening element at the same time. When an element is referred to as being "connected to" another element, it can be directly connected to the other element or intervening elements may also be present.
还需要说明的是,本实施例中的左、右、上、下等方位用语,仅是互为相对概念或是以产品的正常使用状态为参考的,而不应该认为是具有限制性的。It should also be noted that the orientation terms such as left, right, up, and down in this embodiment are only relative concepts or refer to the normal use state of the product, and should not be regarded as limiting.
如图1所示,本发明实施例提供的一种移动终端壳体,包括金属本体100,所述金属本体100的表面具有电泳层210,所述金属本体100的至少一处边缘设置有倒角101,所述倒角101处设置有阳极氧化层220,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层210与阳极氧化层220的质感不同,产品壳体的外观表现力强。As shown in FIG. 1 , a mobile terminal case provided by an embodiment of the present invention includes a metal body 100 , the surface of the metal body 100 has an electrophoretic layer 210 , and at least one edge of the metal body 100 is provided with a chamfer. 101, the chamfer 101 is provided with an anodized layer 220, which can effectively protect the shell from corrosion, the shell is not easy to scratch during use, and the shell has high reliability. Moreover, the electrophoretic layer 210 and the anodized layer The texture of the 220 is different, and the appearance of the product shell is highly expressive.
具体地,所述金属本体100可以采用铝合金材料制成,其质轻。倒角101的角度可为45度。Specifically, the metal body 100 can be made of aluminum alloy material, which is light in weight. The angle of the chamfer 101 may be 45 degrees.
具体地,所述金属本体100的正面或/和背面的边缘均设置有所述倒角101。倒角101设置的区段可根据实际情况设定。可以在金属本体100的正面或/和背面的整个边缘设置有连续的倒角,也可以在金属本体100的正面或/和背面的边缘局部设置倒角或间隔设置倒角等。可以通过CNC(Computer numerical control)机加工(数控加工)在金属本体100形成倒角101,其成型精度高,成型质量好。Specifically, the edges of the front or/and back of the metal body 100 are provided with the chamfers 101 . The section where the chamfer 101 is set can be set according to actual conditions. Continuous chamfers may be provided on the entire edge of the front or/and back of the metal body 100 , or chamfers may be provided locally or at intervals on the front or/and back edges of the metal body 100 . The chamfer 101 can be formed on the metal body 100 by CNC (Computer numerical control) machining (numerical control machining), which has high forming precision and good forming quality.
具体地,所述电泳层210与所述阳极氧化层220的颜色可以不同,其质感也不同,壳体在使用过程中不易划伤,产品外观表现力强。Specifically, the colors of the electrophoretic layer 210 and the anodized layer 220 may be different, and their textures may also be different, so that the shell is not easily scratched during use, and the appearance of the product is highly expressive.
本发明实施例还提供了一种移动终端,所述移动终端具有上述的移动终端壳体。所述移动终端可为手机或平板电脑等。An embodiment of the present invention also provides a mobile terminal, the mobile terminal has the above-mentioned mobile terminal housing. The mobile terminal can be a mobile phone or a tablet computer or the like.
本发明实施例所提供的移动终端壳体和具有该移动终端壳体的移动终端,其壳体表面具有电泳层210且边缘处的倒角101上具有阳极氧化层220,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层210与阳极氧化层220的质感不同,产品壳体的外观表现力强。The mobile terminal casing provided by the embodiment of the present invention and the mobile terminal having the mobile terminal casing have an electrophoretic layer 210 on the surface of the casing and an anodized layer 220 on the chamfer 101 at the edge, which can effectively protect the casing No corrosion, the shell is not easily scratched during use, and the shell has high reliability. Moreover, the texture of the electrophoretic layer 210 and the anodized layer 220 are different, and the appearance of the product shell is strong.
本发明实施例还提供了一种移动终端壳体的制造方法,可用于制造上述移动终端壳体,包括以下步骤:制备金属本体100,将所述金属本体100进行电泳处理使金属本体100表面附着有电泳层210,对电泳后的金属本体100进行倒角处理而形成倒角101,倒角处理时,将金属本体100的边缘与边缘处的电泳层210去除,此时倒角101的表面为裸露的金属面,将倒角101后的金属本体100进行阳极氧化处理,以使所述金属本体100的倒角面(裸露的金属面)形成有阳极氧化层220,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层210与阳极氧化层220的质感不同,产品壳体的外观表现力强。The embodiment of the present invention also provides a method for manufacturing a mobile terminal casing, which can be used to manufacture the above-mentioned mobile terminal casing. There is an electrophoretic layer 210, and the metal body 100 after electrophoresis is chamfered to form a chamfer 101. During the chamfering process, the edge of the metal body 100 and the electrophoretic layer 210 at the edge are removed. At this time, the surface of the chamfer 101 is For the exposed metal surface, the metal body 100 after chamfering 101 is anodized, so that the chamfered surface (bare metal surface) of the metal body 100 is formed with an anodized layer 220, which can effectively protect the shell from Due to corrosion, the casing is not easily scratched during use, and the reliability of the casing is high. Moreover, the texture of the electrophoretic layer 210 and the anodized layer 220 are different, and the appearance of the product casing is strong.
对金属本体100进行电泳处理时可采用水溶性涂料,并以水为溶解介质,可节省大量有机溶剂,大大降低了大气污染和环境危害,安全卫生,同时避免了火灾的隐患而且,涂装效率高,涂料损失小,涂料的利用率可达95%以上;电泳形成的电泳层,其涂膜厚度均匀,附着力强,涂装质量好,工件各个部位如内层、凹陷、焊缝等处都能获得均匀、平滑的漆膜,对复杂形状工件的涂装也可轻松实现;而且电泳处理还具有生产效率高的优点,可实现自动化连续生产,大大提高了生产效率。Water-soluble paint can be used for the electrophoresis treatment of the metal body 100, and water is used as the dissolution medium, which can save a large amount of organic solvents, greatly reduce air pollution and environmental hazards, and is safe and hygienic, while avoiding the hidden danger of fire. Moreover, the coating efficiency High, small loss of paint, the utilization rate of paint can reach more than 95%; the electrophoretic layer formed by electrophoresis has uniform coating thickness, strong adhesion, and good coating quality. A uniform and smooth paint film can be obtained, and the coating of workpieces with complex shapes can be easily realized; and the electrophoretic treatment also has the advantage of high production efficiency, which can realize automatic continuous production and greatly improve production efficiency.
具体应用中,所述金属本体100可以采用铝合金材料制成,其重量轻且强度高。In a specific application, the metal body 100 can be made of aluminum alloy material, which is light in weight and high in strength.
具体应用中,所述金属本体100采用铝合金材料通过机加工加工而成,可以采用CNC(Computer numerical control)机加工成型金属本体100,其生产精度高、效率高。In a specific application, the metal body 100 is machined from an aluminum alloy material, and the metal body 100 can be formed by CNC (Computer numerical control), which has high production precision and high efficiency.
具体应用中,金属本体100通过电泳处理后,所述倒角101通过CNC机加工而成。其生产精度高、效率高。In a specific application, after the metal body 100 is processed by electrophoresis, the chamfer 101 is processed by CNC machining. It has high production precision and high efficiency.
通过CNC机加工成型倒角101后,将金属本体100置于电解液中作为阳极,在特定条件和外加电流作用下,进行电解。阳极的金属本体100中裸露的倒角面将氧化,倒角面的表面上形成氧化铝薄层,其厚度可以为5~30微米,硬质的阳极氧化层220可达25~150微米。阳极氧化后的金属本体100,其硬度和耐磨性将有效提高,耐磨性可达250~500千克/平方毫米,且具有良好的耐热性,阳极氧化层220熔点高达2320K,还具有优良的绝缘性,耐击穿电压高达2000V,同时增强了抗腐蚀性能,阳极氧化层在ω=0.03NaCl盐雾中经几千小时而不腐蚀,可靠性高。After the chamfer 101 is formed by CNC machining, the metal body 100 is placed in an electrolyte solution as an anode, and electrolysis is performed under specific conditions and an applied current. The exposed chamfered surface of the metal body 100 of the anode will be oxidized, and a thin aluminum oxide layer is formed on the surface of the chamfered surface, the thickness of which can be 5-30 microns, and the hard anodized layer 220 can reach 25-150 microns. The hardness and wear resistance of the anodized metal body 100 will be effectively improved, the wear resistance can reach 250-500 kg/mm2, and it has good heat resistance. The melting point of the anodized layer 220 is as high as 2320K, and it also has excellent Excellent insulation, the breakdown voltage is as high as 2000V, and the corrosion resistance is enhanced at the same time. The anodized layer does not corrode after thousands of hours in ω=0.03NaCl salt spray, and the reliability is high.
本发明实施例所提供的移动终端壳体的制造方法,其通过先对金属壳体进行电泳处理使金属本体100表面形成有电泳层210,再对电泳后的金属本体100进行倒角101,将倒角后的金属本体100进行阳极氧化处理以使所述金属本体100的倒角面形成有阳极氧化层220,金属本体100的表面具有电泳层210,倒角101处具有阳极氧化层220,可以有效地保护壳体不受侵蚀,壳体在使用过程中不易划伤,壳体可靠性高,而且,电泳层210与阳极氧化层220的质感不同,产品壳体的外观表现力强,产品外观效果更有个性,更有科技感。The manufacturing method of the mobile terminal shell provided by the embodiment of the present invention firstly performs electrophoretic treatment on the metal shell to form the electrophoretic layer 210 on the surface of the metal body 100, and then chamfers 101 the metal body 100 after electrophoresis. The chamfered metal body 100 is anodized to form an anodized layer 220 on the chamfered surface of the metal body 100, the surface of the metal body 100 has an electrophoretic layer 210, and the chamfered corner 101 has an anodized layer 220, which can Effectively protect the shell from corrosion, the shell is not easy to scratch during use, and the shell has high reliability. Moreover, the texture of the electrophoretic layer 210 and the anodized layer 220 are different, and the appearance of the product shell is strong. The effect is more personalized and more technological.
以上所述仅为本发明的较佳实施例而已,并不用以限制本发明,凡在本发明的精神和原则之内所作的任何修改、等同替换或改进等,均应包含在本发明的保护范围之内。The above description is only a preferred embodiment of the present invention, and is not intended to limit the present invention. Any modification, equivalent replacement or improvement made within the spirit and principles of the present invention shall be included in the protection of the present invention. within range.
Claims (5)