CN104404733A - Worsted knitted cashmere sweater fulling softening treatment process - Google Patents
Worsted knitted cashmere sweater fulling softening treatment process Download PDFInfo
- Publication number
- CN104404733A CN104404733A CN201410639017.1A CN201410639017A CN104404733A CN 104404733 A CN104404733 A CN 104404733A CN 201410639017 A CN201410639017 A CN 201410639017A CN 104404733 A CN104404733 A CN 104404733A
- Authority
- CN
- China
- Prior art keywords
- cashmere sweater
- drying
- fabric
- minutes
- treatment
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a worsted knitted cashmere sweater fulling softening treatment process, the concrete steps include: 1) fulling treatment, to be more specific, dissolving Monogen with hot water, adding the Monogen into a cashmere sweater, turning once every 10 minutes, then putting into a washing machine to rotate for 10 minutes, finally using clear water to rinse until the cashmere sweater is clean, and dehydrating; 2) softening treatment, to be more specific, adding a softening agent, a smoothing agent and a bulking agent into the cashmere sweater, turning once every few minutes, and then dehydrating for drying; 3) airing treatment: airing or hanging for drying until the cashmere sweater is 70-80% dry, and ironing; 4) drying treatment, to be more specific, performing drum-type drying on the fabric; and 5) ironing treatment, to be more specific, ironing the dried fabric. In the way, the worsted knitted cashmere sweater fulling softening treatment process can make the fabric texture close, length shortened, weight per square meter and thickness increased, and strength, elasticity and heat retention property improved, and can make appearance beautiful, hand feeling rich and soft, and color soft.
Description
Technical field
The present invention relates to garment industry, particularly relate to a kind of spinning knitted cashmere sweater fulling milling soft treatment technique.
Background technology
Cashmere sweater have passed through a variety of operation from suede to ready-made clothes, there is no the ready-made clothes of fulling milling to have remained various chemical greasy dirt, Chinese wax and even also have ether etc., fulling milling is exactly the process of washing in fact, can well clean cashmere sweater, the object of woollen sweater fulling milling is mainly in order to improve inherent quality and the appearance effect of woollen sweater product.
Summary of the invention
The technical problem that the present invention mainly solves is to provide a kind of spinning knitted cashmere sweater fulling milling soft treatment technique, this spinning knitted cashmere sweater fulling milling soft treatment technique can make fabric texture tight, contraction in length, weight per square meter and thickness increase, powerful raising, elasticity and warmth retention property strengthen, and also make its attractive appearance, the abundant softness of feel, color and luster is soft.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is: a kind of spinning knitted cashmere sweater fulling milling soft treatment technique, and concrete steps comprise:
1), fulling milling process: hair can be melted with 50 DEG C of-55 DEG C of hot water only, the clean addition of hair energy is the 3%-8% of cashmere sweater dry weight, bath raio 1:30, temperature 40 DEG C-50 DEG C, soak 50-55 minute, dark clothes soak time is longer, stirs once every 10 minutes, then drops into washing machine and rotates 10 minutes, if when needing matte large, can many turns a little while, finally use clear water rinsed clean, and dewater;
2), soft treatment: the addition of softener, smooth agent, leavening agent is respectively the 2%-4% of clothes dry weight, and bath raio is 1:30, water temperature 40 DEG C-50 DEG C, pH value is 6-7, and soak time is 30-60 minute, stirs once every a few minutes, then dewatered drying, attention can not use clear water rinsing;
3), dry process: dry or hang to be dried to and do very likely, carry out whole scalding, now whole scalding does not note size;
4), drying and processing: fabric is carried out drum-type drying;
5), whole boiling hot process: by whole boiling hot for the fabric after drying, the fabric after arrangement wants clean mark, and size is accurate.
In a preferred embodiment of the present invention, during described whole boiling hot process, steam temperature remains on 150 degree of-160 degree, distance fabric face 1.0-1.5CM.
In a preferred embodiment of the present invention, described drying and processing maintains the temperature at about 80 degree and continues to dry about 5 minutes.
In a preferred embodiment of the present invention, described whole boiling hot pattern comprises: shank flower and scar trace.
The invention has the beneficial effects as follows: a kind of spinning knitted cashmere sweater fulling milling soft treatment technique of the present invention can make fabric texture tight, contraction in length, and weight per square meter and thickness increase, powerful raising, elasticity and warmth retention property strengthen, and also make its attractive appearance, the abundant softness of feel, color and luster is soft.
Detailed description of the invention
Below preferred embodiment of the present invention is described in detail, can be easier to make advantages and features of the invention be readily appreciated by one skilled in the art, thus more explicit defining is made to protection scope of the present invention.
The embodiment of the present invention comprises: a kind of spinning knitted cashmere sweater fulling milling soft treatment technique, and concrete steps comprise:
1), fulling milling process: hair can be melted with 50 DEG C of-55 DEG C of hot water only, the clean addition of hair energy is the 3%-8% of cashmere sweater dry weight, bath raio 1:30, temperature 40 DEG C-50 DEG C, soak 50-55 minute, dark clothes soak time is longer, stirs once every 10 minutes, then drops into washing machine and rotates 10 minutes, if when needing matte large, can many turns a little while, finally use clear water rinsed clean, and dewater;
2), soft treatment: the addition of softener, smooth agent, leavening agent is respectively the 2%-4% of clothes dry weight, and bath raio is 1:30, water temperature 40 DEG C-50 DEG C, pH value is 6-7, and soak time is 30-60 minute, stirs once every a few minutes, then dewatered drying, attention can not use clear water rinsing;
3), dry process: dry or hang to be dried to and do very likely, carry out whole scalding, now whole scalding does not notice that described in size, whole boiling hot pattern comprises: shank flower and scar trace;
4), drying and processing: fabric is carried out drum-type drying, and described drying and processing maintains the temperature at about 80 degree and continues to dry about 5 minutes;
5), whole boiling hot process: by whole boiling hot for the fabric after drying, the fabric after arrangement wants clean mark, and size is accurate, and during described whole boiling hot process, steam temperature remains on 150 degree of-160 degree, distance fabric face 1.0-1.5CM.
Compared with prior art, a kind of spinning knitted cashmere sweater fulling milling soft treatment technique of the present invention can make fabric texture tight, contraction in length, weight per square meter and thickness increase, powerful raising, and elasticity and warmth retention property strengthen, also make its attractive appearance, the abundant softness of feel, color and luster is soft.
The foregoing is only embodiments of the invention; not thereby the scope of the claims of the present invention is limited; every utilize description of the present invention to do equivalent structure or equivalent flow process conversion; or be directly or indirectly used in other relevant technical fields, be all in like manner included in scope of patent protection of the present invention.
Claims (4)
1. a spinning knitted cashmere sweater fulling milling soft treatment technique, it is characterized in that, concrete steps comprise:
1), fulling milling process: hair can be melted with 50 DEG C of-55 DEG C of hot water only, the clean addition of hair energy is the 3%-8% of cashmere sweater dry weight, bath raio 1:30, temperature 40 DEG C-50 DEG C, soak 50-55 minute, dark clothes soak time is longer, stirs once every 10 minutes, then drops into washing machine and rotates 10 minutes, if when needing matte large, can many turns a little while, finally use clear water rinsed clean, and dewater;
2), soft treatment: the addition of softener, smooth agent, leavening agent is respectively the 2%-4% of clothes dry weight, and bath raio is 1:30, water temperature 40 DEG C-50 DEG C, pH value is 6-7, and soak time is 30-60 minute, stirs once every a few minutes, then dewatered drying, attention can not use clear water rinsing;
3), dry process: dry or hang to be dried to and do very likely, carry out whole scalding, now whole scalding does not note size;
4), drying and processing: fabric is carried out drum-type drying;
5), whole boiling hot process: by whole boiling hot for the fabric after drying, the fabric after arrangement wants clean mark, and size is accurate.
2. one according to claim 1 spinning knitted cashmere sweater fulling milling soft treatment technique, is characterized in that: during described whole boiling hot process, steam temperature remains on 150 degree of-160 degree, distance fabric face 1.0-1.5CM.
3. one according to claim 1 spinning knitted cashmere sweater fulling milling soft treatment technique, is characterized in that: described drying and processing maintains the temperature at about 80 degree and continues to dry about 5 minutes.
4. one according to claim 1 spinning knitted cashmere sweater fulling milling soft treatment technique, is characterized in that: described whole boiling hot pattern comprises: shank flower and scar trace.