CN104194651A - Method for manufacturing leather brightening agent - Google Patents
Method for manufacturing leather brightening agent Download PDFInfo
- Publication number
- CN104194651A CN104194651A CN201410413621.2A CN201410413621A CN104194651A CN 104194651 A CN104194651 A CN 104194651A CN 201410413621 A CN201410413621 A CN 201410413621A CN 104194651 A CN104194651 A CN 104194651A
- Authority
- CN
- China
- Prior art keywords
- parts
- leather
- brightening agent
- water
- silicone
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for manufacturing a leather brightening agent. The method comprises the following steps of mixing a silicone fluid with isopropanol, evenly stirring, then adding acetic acid, continuously stirring until the solution is even, again adding water and silicone emulsion, fully stirring when each of the raw materials is added until the sizing is completed, and thus obtaining the leather brightening agent after the stirring is completed. The leather brightening agent comprises the following raw materials in parts by weight: 90-110 parts of silicone fluid, 90-110 parts of isopropanol, 2.6-3 parts of acetic acid, 630-650 parts of water and140-160 parts of silicone emulsion. After the leather brightening agent prepared by the method disclosed by the invention is applied to the leather, a transparent and water-impermeable durable film is formed on the surface of the leather to protect the leather from damaging; since the durable film is insoluble in water, after the leather brightening agent is applied once, the durable film can be maintained for a long time and thus the trouble of repeated application is reduced.
Description
Technical field
The present invention relates to that leather is antifouling, clean-out system, relate in particular to the making method of leather gloss agent.
Background technology
After the leatherware wearing time is long, easily tarnish, current maintenance leather polishing is all the oil that uses some blasts, not only can damage leather, and needs often to use, cumbersome, is unfavorable for improving people's quality of the life.
Summary of the invention
The invention provides the making method of leather gloss agent, one or more that is used for solving the problems of the technologies described above.
According to an aspect of the present invention, a kind of making method of leather gloss agent is provided, comprise the following steps, by silicone fluid and Virahol mixing and stirring, add again acetic acid to continue to be stirred to evenly, again add water and silicone emulsion, till often adding the same above-mentioned raw materials all will be stirred well to sizing, after having stirred, obtain leather gloss agent;
Above-mentioned each raw material with the proportioning of parts by weight below, 90~110 parts of silicone fluids, 90~110 parts of Virahols, 2.6~3 parts of acetic acid, 630~650 parts, water, 140~160 parts of silicone emulsions.
The making method of leather gloss agent provided by the invention; the leather gloss agent of making can form transparent, fluid-tight durable membranes at leather surface after use, and protection leather is injury-free, due to water insoluble; after covering with paint, lacquer, colour wash, etc. once, can keep for a long time, reduce the trouble of repeatedly covering with paint, lacquer, colour wash, etc.
Embodiment
Embodiment 1:
The invention provides a kind of leather gloss agent making method, comprise the following steps, by silicone fluid and Virahol mixing and stirring, add again acetic acid to continue to be stirred to evenly, again add water and silicone emulsion, till often adding the same above-mentioned raw materials all sizing will be stirred well to, after having stirred, obtain leather gloss agent;
Above-mentioned each raw material with the proportioning of parts by weight below, 90 parts of silicone fluids, 90 parts of Virahols, 2.6 parts of acetic acid, 630 parts, water, 140 parts of silicone emulsions.
The making method of leather gloss agent provided by the invention; the leather gloss agent of making can form transparent, fluid-tight durable membranes at leather surface after use, and protection leather is injury-free, due to water insoluble; after covering with paint, lacquer, colour wash, etc. once, can keep for a long time, reduce the trouble of repeatedly covering with paint, lacquer, colour wash, etc.
Embodiment 2:
The invention provides a kind of leather gloss agent making method, comprise the following steps, by silicone fluid and Virahol mixing and stirring, add again acetic acid to continue to be stirred to evenly, again add water and silicone emulsion, till often adding the same above-mentioned raw materials all sizing will be stirred well to, after having stirred, obtain leather gloss agent;
Above-mentioned each raw material with the proportioning of parts by weight below, 100 parts of silicone fluids, 100 parts of Virahols, 2.8 parts of acetic acid, 640 parts, water, 150 parts of silicone emulsions.
The making method of leather gloss agent provided by the invention; the leather gloss agent of making can form transparent, fluid-tight durable membranes at leather surface after use, and protection leather is injury-free, due to water insoluble; after covering with paint, lacquer, colour wash, etc. once, can keep for a long time, reduce the trouble of repeatedly covering with paint, lacquer, colour wash, etc.
Embodiment 3:
The invention provides a kind of leather gloss agent making method, comprise the following steps, by silicone fluid and Virahol mixing and stirring, add again acetic acid to continue to be stirred to evenly, again add water and silicone emulsion, till often adding the same above-mentioned raw materials all sizing will be stirred well to, after having stirred, obtain leather gloss agent;
Above-mentioned each raw material with the proportioning of parts by weight below, 110 parts of silicone fluids, 90 parts of Virahols, 2.7 parts of acetic acid, 640 parts, water, 145 parts of silicone emulsions.
The making method of leather gloss agent provided by the invention; the leather gloss agent of making can form transparent, fluid-tight durable membranes at leather surface after use, and protection leather is injury-free, due to water insoluble; after covering with paint, lacquer, colour wash, etc. once, can keep for a long time, reduce the trouble of repeatedly covering with paint, lacquer, colour wash, etc.
The above is only optimal way of the present invention; it should be pointed out that to those skilled in the art, without departing from the concept of the premise of the invention; can also make some similar distortion and improvement, within these also should be considered as protection scope of the present invention.
Claims (1)
1. the making method of leather gloss agent, it is characterized in that, comprise the following steps, by silicone fluid and Virahol mixing and stirring, add again acetic acid to continue to be stirred to evenly, again add water and silicone emulsion, till often adding the same above-mentioned raw materials all will be stirred well to sizing, after having stirred, obtain leather gloss agent;
Above-mentioned each raw material with the proportioning of parts by weight below, 90~110 parts of silicone fluids, 90~110 parts of Virahols, 2.6~3 parts of acetic acid, 630~650 parts, water, 140~160 parts of silicone emulsions.