CN104101916A - Two stage technology for hardening and combining lenses - Google Patents
Two stage technology for hardening and combining lenses Download PDFInfo
- Publication number
- CN104101916A CN104101916A CN201410360092.4A CN201410360092A CN104101916A CN 104101916 A CN104101916 A CN 104101916A CN 201410360092 A CN201410360092 A CN 201410360092A CN 104101916 A CN104101916 A CN 104101916A
- Authority
- CN
- China
- Prior art keywords
- eyeglass
- lenses
- lamp
- time
- hardening
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a two stage technology for hardening and combining lenses. The two stage technology for hardening and combining the lenses includes the following steps: 1) performing lens lamination; 2) performing solidification procedures twice; 3) hardening the lenses; 4) roasting the lenses. According to the two stage technology for hardening and combining the lenses, the lenses obtained by being solidified twice and roasted twice are superior in optical performance, no double image exists in light spots imaged by the lenses, the phenomena of chromatic aberration, spherical aberration, glue failure, core shifting, bubbling and the like are eliminated, image quality is improved, hardening requirements of lens combination are met, and product quality is guaranteed.
Description
Technical field
The present invention relates to eyeglass production technical field, relate in particular to the two-part sclerosis operation that eyeglass engages engineering.
Background technology
In eyeglass production run, the one-part form sclerosis wiping face that eyeglass is original, by directly causing pulling, coming unglued of eyeglass, easily causes core shift, bubble.Eyeglass is temporary transient sclerosis first, rubber, wiping face is formally sclerosis again, the advantage of its two-part hardening process is: the one, and the hot spot ghost image that imaging is occurred, be conducive to color difference eliminating, spherical aberration, improve picture element, the 2nd, optimizing optical design and structural design, the two-part sclerosis operation technique that therefore engages eyeglass seems of crucial importance.
Summary of the invention
For the technological requirement of above-mentioned eyeglass two-part sclerosis operation, the object of this invention is to provide a kind of two sections of sclerosis and engage eyeglass technique, the sclerosis requirement engaging to meet described eyeglass, guarantees product quality.
Technical scheme of the present invention realizes in the following manner: a kind of two sections of sclerosis engage eyeglass technique, comprise the following steps: it is characterized in that:
1), eyeglass laminating: first eyeglass is arranged to basket and cleaned directly upper streamline laminating, then carry out outward appearance gummed, two eyeglasses are solidified and to carry out determining core and guarantee core precision, temporarily harden again, anti-fastening core is not reserved and is caused core shift, then wipe the glue that overflows on surface and surface blot and reach high cleanliness, the more formal sclerosis bright line that prevents from arching upward;
2), regelate program: set illumination by three technical standard sections:
The first standard paragraphs: to sub-this tighter <0.3> of component originally, more than external diameter < Φ 30mm>; Illuminance setting is 1500-2000um/cm
2;
The second standard paragraphs: to more than sub-this tighter <0.5> of component, below external diameter < Φ 30 mm >; Firm time is at 1-3 hour; Structure illuminance setting is 4800-7500um/cm
2;
The 3rd standard paragraphs: high temperature resistant eyeglass is hard, structure illuminance setting is 8.0-1.4um/cm
2, the time is 300 seconds, 500 seconds, 900 seconds;
3), firm time: according to the solid of different model, firm time is: OP-1055H acrylate adhesive solid, arranges duration 1 hour; OP-1020K octyl phenol polyoxyethylene ether solid, arranges duration 1 hour; OP-1080L epoxide-resin glue solid, arranges duration 5 hours;
4), baking: the eyeglass after above-mentioned solidifying is put into oven for baking, described baking box is that a kind of two-part UV lamp solidifies baking box, by upper UV lamp, upper mounting plate, lower UV lamp, lower platform, first paragraph switch, second segment switch, time circuit closer, the strong and weak controller of UV lamp illumination forms, the eyeglass having engaged is positioned on upper mounting plate, service time, relay set the time, open first paragraph switch, according to the difference of the difference of eyeglass specification and first paragraph exposure, use the strong and weak controller of UV lamp, after first paragraph irradiates and finishes, eyeglass is taken out, the glue overflowing after heating is wiped, guarantee after eyeglass precision, again eyeglass is put on lower platform, underhardening again, to meet optics requirement.
The present invention, through its superb optical performance of eyeglass of regelate secondary baking, the hot spot that imaging goes out, without ghost image, has been eliminated aberration, spherical aberration, comes unglued, the phenomenon such as core shift, bubble, has improved picture element, has met the sclerosis requirement that eyeglass engages, and guarantees product quality.
Accompanying drawing explanation
Fig. 1 is Roasting oven structure schematic diagram of the present invention.
Embodiment
Two sections of sclerosis engage an eyeglass technique, comprise the following steps:
1, eyeglass laminating: first eyeglass is arranged to basket and cleaned directly upper streamline laminating, then carry out outward appearance gummed, two eyeglasses are solidified and to carry out determining core and guarantee core precision, temporarily harden again, anti-fastening core is not reserved and is caused core shift, then wipe the glue that overflows on surface and surface blot and reach high cleanliness, more formal sclerosis prevents the bright line that arches upward.
2, regelate program: set illumination by three technical standard sections:
The first standard paragraphs: to sub-this tighter <0.3> of component originally, more than external diameter < Φ 30mm>; Illuminance setting is 1500-2000um/cm
2;
The second standard paragraphs: to more than sub-this tighter <0.5> of component, below external diameter < Φ 30 mm >; Firm time is at 1-3 hour; Structure illuminance setting is 4800-7500um/cm
2;
The 3rd standard paragraphs: high temperature resistant eyeglass is hard, structure illuminance setting is 8.0-1.4um/cm
2, the time is 300 seconds, 500 seconds, 900 seconds;
3, firm time: according to the solid of different model, firm time is: OP-1055H acrylate adhesive solid, arranges duration 1 hour; OP-1020K octyl phenol polyoxyethylene ether solid, arranges duration 1 hour; OP-1080L epoxide-resin glue solid, arranges duration 5 hours;
4, baking: the eyeglass after above-mentioned solidifying is put into oven for baking, described baking box is that a kind of two-part UV lamp solidifies baking box 9, by upper UV lamp 3, upper mounting plate 1, lower UV lamp 4, lower platform 2, first paragraph switch 6, second segment switch 7, time circuit closer 5, the strong and weak controller 8 of UV lamp illumination forms, the eyeglass having engaged is positioned on upper mounting plate 1, service time, relay 5 set the time, open first paragraph switch 6, according to the difference of the difference of eyeglass specification and first paragraph exposure, use the strong and weak controller 8 of UV lamp, after first paragraph irradiates and finishes, eyeglass is taken out, the glue overflowing after heating is wiped, guarantee after eyeglass precision, eyeglass is put on lower platform 2 again, underhardening again, to meet optics requirement.
Claims (1)
1. two sections of sclerosis engage an eyeglass technique, comprise the following steps: it is characterized in that:
1), eyeglass laminating: first eyeglass is arranged to basket and cleaned directly upper streamline laminating, then carry out outward appearance gummed, two eyeglasses are solidified and to carry out determining core and guarantee core precision, temporarily harden again, anti-fastening core is not reserved and is caused core shift, then wipe the glue that overflows on surface and surface blot and reach high cleanliness, the more formal sclerosis bright line that prevents from arching upward;
2), regelate program: set illumination by three technical standard sections:
The first standard paragraphs: to sub-this tighter <0.3> of component originally, more than external diameter < Φ 30mm>; Illuminance setting is 1500-2000um/cm
2;
The second standard paragraphs: to more than sub-this tighter <0.5> of component, below external diameter < Φ 30 mm >; Firm time is at 1-3 hour; Structure illuminance setting is 4800-7500um/cm
2;
The 3rd standard paragraphs: high temperature resistant eyeglass is hard, structure illuminance setting is 8.0-1.4um/cm
2, the time is 300 seconds, 500 seconds, 900 seconds;
3), firm time: according to the solid of different model, firm time is: OP-1055H acrylate adhesive solid, arranges duration 1 hour; OP-1020K octyl phenol polyoxyethylene ether solid, arranges duration 1 hour; OP-1080L epoxide-resin glue solid, arranges duration 5 hours;
4), baking: the eyeglass after above-mentioned solidifying is put into oven for baking, described baking box is that a kind of two-part UV lamp solidifies baking box (9), by upper UV lamp (3), upper mounting plate (1), lower UV lamp (4), lower platform (2), first paragraph switch (6), second segment switch (7), time circuit closer (5), the strong and weak controller of UV lamp illumination (8) forms, the eyeglass having engaged is positioned on upper mounting plate (1), relay service time (5) sets the time, open first paragraph switch (6), according to the difference of the difference of eyeglass specification and first paragraph exposure, use the strong and weak controller (8) of UV lamp, after first paragraph irradiates and finishes, eyeglass is taken out, the glue overflowing after heating is wiped, guarantee after eyeglass precision, again eyeglass is put on lower platform (2), underhardening again, to meet optics requirement.