CN103820045B - 一种低光畸变pvb胶片配方 - Google Patents
一种低光畸变pvb胶片配方 Download PDFInfo
- Publication number
- CN103820045B CN103820045B CN201410084242.3A CN201410084242A CN103820045B CN 103820045 B CN103820045 B CN 103820045B CN 201410084242 A CN201410084242 A CN 201410084242A CN 103820045 B CN103820045 B CN 103820045B
- Authority
- CN
- China
- Prior art keywords
- pvb film
- parts
- pvb
- optical distortion
- formula
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明涉及一种低光畸变PVB胶片配方,包括以下质量份的组分:PVB树脂:100份;增塑剂:25-40份;抗氧剂:0.5-3份;紫外线吸收剂:0.1-1.5份;改性剂:0.2-3.5份;扩链剂:0.05-2.7份。所得到的配方与普通PVB胶片配方相比,能显著提高PVB胶片的抗拉强度、抗冲击性能等力学指标,以及耐老化性能、抗黄变性能和分子量的稳定性和均匀性,显著降低了PVB胶片性能不均匀引起的光畸变性能。
Description
技术领域
本发明涉及一种低光畸变PVB胶片配方,属于热塑性高分子材料技术领域。
背景技术
随着经济的发展,夹层玻璃的应用领域越来越广,在聚乙烯醇缩丁醛(PVB)树脂中加入增塑剂加工成胶片用于制作夹层玻璃是众所周知的,即在高温高压下,PVB胶片作为粘结此材料,在玻璃表面发生铺展、浸润等过程,最终将两层玻璃复合为一个整体。目前,主要采用在聚乙烯醇缩丁醛中加入增塑剂来制备PVB胶片,比如专利CN1284911、CN1518494分别公开了一种由部分缩醛化的聚乙烯醇制成的含增塑剂的薄膜,CN1484671公开了一种含增塑剂的聚乙烯醇缩丁醛,其制备方法和用途,尤其用于生产夹层玻璃的安全玻璃用膜的用途。
光畸变产生的原因是玻璃表面凹凸不平或局部光学不均匀,使通过的光线产生偏离,从而使物像变形。如光畸变程度较大,则易使驾驶员的眼睛产生疲劳,导致交通事故的发生。与进口产品相比国内PVB胶膜普遍存在抗拉强度低、抗冲击性能差,以及耐老化性能、抗黄变性能差等问题,使得其光畸变性能较差。
发明内容
为了解决现有技术中存在的问题,本发明提供一种低光畸变PVB胶片配方,以克服现有技术中出现的光畸变性能较差的缺点,该PVB胶片配方包括以下质量份的组分:
PVB树脂:100份;
增塑剂:25-40份;
抗氧剂:0.5-3份;
紫外线吸收剂:0.1-1.5份;
改性剂:0.2-3.5份;
扩链剂:0.05-2.7份。
在本发明的优选实施方案中,所述增塑剂优选为3GO增塑剂。
在本发明的优选实施方案中,所述抗氧剂优选为抗氧剂1010。
在本发明的优选实施方案中,所述紫外线吸收剂优选为紫外线吸收剂326。
在本发明的优选实施方案中,所述改性剂优选为ADD3310。
在本发明的优选实施方案中,所述扩链剂优选为扩链剂ADR。
所述ADD3310和扩链剂ADR均可通过市售购买获得,产自巴斯夫中国有限公司。所述ADD3310能将热塑性工程塑料树脂在高温加工过程中因水解而产生降解断链成较短的链重新连接,从而提高分子量。它被用于加工过程中降低因降解而生成低分子聚合物及提升回收再利用物料的性能。
在本发明的优选实施方案中,该低光畸变PVB胶片配方,包括以下质量份的组分:
PVB树脂:100份;
3GO增塑剂:30份;
抗氧剂1010:1份;
紫外线吸收剂326:1份;
ADD3310:1.5份
扩链剂ADR:1.0份。
本发明对胶片的组分和配比进行了长期研究,所得到的配方与普通PVB胶片配方相比,能显著提高PVB胶片的抗拉强度、抗冲击性能等力学指标,以及耐老化性能、抗黄变性能和分子量的稳定性和均匀性,显著降低了PVB胶片性能不均匀引起的光畸变性能。
具体实施方式
下面通过实施例对本发明做进一步的描述。
实施例
生产设备为锐华95双螺杆生产线,低光畸变PVB胶片配方如表1所示。
表1
对上述配方得到的三种配方的胶片进行性能测试,结果列于表2。
表2
进一步的,通过客户使用情况,新配方生产的胶片显优于普通胶片制得的汽车安全玻璃性能,尤其在光畸变性能有明显提高。
以上实施例显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,而不是以任何方式限制本发明的范围,在不脱离本发明范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的范围内。
Claims (5)
1.一种低光畸变PVB胶片,包括以下质量份的组分:
PVB树脂:100份;
增塑剂:25-40份;
抗氧剂:0.5-3份;
紫外线吸收剂:0.1-1.5份;
改性剂:0.2-3.5份;
扩链剂:0.05-2.7份;
所述改性剂为ADD3310;所述扩链剂为扩链剂ADR。
2.根据权利要求1所述的PVB胶片,其特征在于所述增塑剂为3GO增塑剂。
3.根据权利要求1所述的PVB胶片,其特征在于所述抗氧剂为抗氧剂1010。
4.根据权利要求1所述的PVB胶片,其特征在于所述紫外线吸收剂为紫外线吸收剂326。
5.根据权利要求1所述的PVB胶片,其特征在于包括以下质量份的组分:
PVB树脂:100份;
3GO增塑剂:30份;
抗氧剂1010:1份;
紫外线吸收剂326:1份;
ADD3310:1.5份
扩链剂ADR:1.0份。