[go: up one dir, main page]

CN103725104B - 一种条形码的制造方法 - Google Patents

一种条形码的制造方法 Download PDF

Info

Publication number
CN103725104B
CN103725104B CN201310713848.4A CN201310713848A CN103725104B CN 103725104 B CN103725104 B CN 103725104B CN 201310713848 A CN201310713848 A CN 201310713848A CN 103725104 B CN103725104 B CN 103725104B
Authority
CN
China
Prior art keywords
silver particles
barcode
mass content
ink composite
bar code
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310713848.4A
Other languages
English (en)
Other versions
CN103725104A (zh
Inventor
黎志春
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shunde District Of Foshan City Chang Hao Dingfeng Adhesive Products Co Ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310713848.4A priority Critical patent/CN103725104B/zh
Publication of CN103725104A publication Critical patent/CN103725104A/zh
Application granted granted Critical
Publication of CN103725104B publication Critical patent/CN103725104B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种条形码的制造方法,包括步骤:步骤一、制备三种油墨组合物,三种油墨组合物中银粒子的质量含量分别为5%、10%和60%;步骤二、在被印刷体上印刷条形码;步骤三、在条形码的至少一对相邻条之间的空隙上印刷银粒子的质量含量为60%的油墨组合物,印刷完成5~10min后,再重叠印刷银粒子的质量含量为10%的油墨组合物,印刷完成5~10min后,再在条形码上印刷银粒子的质量含量为5%的油墨组合物,且覆盖条形码。本发明采用含有银粒子的油墨组合物印刷条形码的空隙位置,当一定时间,条形码空隙处变黑,破坏了条形码的本来的排列规则,导致超市人员无法扫描条码,提醒超市人员食品过期,也可以提醒消费者。本发明为消费者提供方便,保证消费者的身体安全。

Description

一种条形码的制造方法
技术领域
本发明涉及一种条形码的制造方法。
背景技术
食品的保质期的重要性不言而喻。消费者在市场上购买食品时,经常要花很多时间查看食品的保质期;对于超市的工作人员而言,他们需要时刻关注食品的上架时间以及保质期,并对食品进行及时下架,但是却难免发生遗漏的情况。因此,需要一种技术,可以在到达食品的保质期时,在包装袋上给出提示,这将极大的方便消费者;同时也防止超市擅自改变包装袋上的生产日期,保护消费者的权益。
发明内容
针对上述技术问题,本发明设计开发了一种条形码的制造方法。本发明在制造食品的条形码时,采用含有银粒子的油墨组合物印刷条形码的空隙位置,银粒子可以与空气中的硫化气体发生反应生成黑色的硫化银,当一定时间,条形码空隙处变黑,从而破坏了条形码的本来的排列规则,导致超市人员无法扫描条码,达到提醒超市收银人员食品过期的目的;并且,条形码处变黑,也可以起到提醒消费者的目的。本发明可以节省消费者的时间,为消费者提供方便,保证消费者的身体安全,同时也有助于改善超市的工作质量。
本发明提供的技术方案为:
一种条形码的制造方法,包括以下步骤:
步骤一、制备含有银粒子的三种油墨组合物,其中,所述三种油墨组合物中银粒子的质量含量分别为5%、10%和60%;
步骤二、在被印刷体上印刷条形码;
步骤三、在所述条形码的至少一对相邻条之间的空隙上印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物,印刷完成5~10min后,再在印刷有银粒子的质量含量为60%的油墨组合物的位置重叠印刷银粒子的质量含量为10%的油墨组合物,印刷完成5~10min后,再在所述条形码上印刷银粒子的质量含量为5%的油墨组合物,且所述银粒子的质量含量为5%的油墨组合物覆盖所述条形码。
优选的是,所述的条形码的制造方法中,所述步骤一中,按质量百分比计,银粒子的质量含量为60%的油墨组合物还含有15~20%分散剂、15~25%粘合剂以及溶剂水,银粒子的质量含量为10%以及5%的油墨组合物还含有5~10%分散剂、5~15%粘合剂以及溶剂水。
优选的是,所述的条形码的制造方法中,所述步骤一中,银粒子的质量含量为60%的油墨组合物中银粒子的粒径为10~20μm,银粒子的质量含量为5%以及10%的油墨组合物中银粒子的粒径为0.1~0.8μm。
优选的是,所述的条形码的制造方法中,所述步骤二中,所述条形码的条为黑色,所述相邻条之间的空隙为白色。
优选的是,所述的条形码的制造方法中,所述步骤二中,在所述条形码上每两个相邻条之间的空隙上均印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物。
优选的是,所述的条形码的制造方法中,所述分散剂为聚丙烯酸酯。
优选的是,所述的条形码的制造方法中,所述粘合剂为聚氨酯。
本发明所述的条形码的制造方法采用含有银粒子的油墨组合物印刷条形码的空隙位置,银粒子可以与空气中的硫化气体发生反应生成黑色的硫化银,当一定时间,条形码空隙处变黑,从而破坏了条形码的本来的排列规则,导致超市人员无法扫描条码,达到提醒超市收银人员食品过期的目的;并且,条形码处变黑,也可以起到提醒消费者的目的。本发明可以节省消费者的时间,为消费者提供方便,保证消费者的身体安全,同时也有助于改善超市的工作质量。
具体实施方式
下面对本发明做进一步的详细说明,以令本领域技术人员参照说明书文字能够据以实施。
本发明提供一种条形码的制造方法,包括以下步骤:
步骤一、制备含有银粒子的三种油墨组合物,其中,所述三种油墨组合物中银粒子的质量含量分别为5%、10%和60%;
步骤二、在被印刷体上印刷条形码;
步骤三、在所述条形码的至少一对相邻条之间的空隙上印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物,印刷完成5~10min后,再在印刷有银粒子的质量含量为60%的油墨组合物的位置重叠印刷银粒子的质量含量为10%的油墨组合物,印刷完成5~10min后,再在所述条形码上印刷银粒子的质量含量为5%的油墨组合物,且所述银粒子的质量含量为5%的油墨组合物覆盖所述条形码。
所述的条形码的制造方法中,所述步骤一中,按质量百分比计,银粒子的质量含量为60%的油墨组合物还含有15~20%分散剂、15~25%粘合剂以及溶剂水,银粒子的质量含量为10%以及5%的油墨组合物还含有5~10%分散剂、5~15%粘合剂以及溶剂水。
所述的条形码的制造方法中,所述步骤一中,银粒子的质量含量为60%的油墨组合物中银粒子的粒径为10~20μm,银粒子的质量含量为5%以及10%的油墨组合物中银粒子的粒径为0.1~0.8μm。
所述的条形码的制造方法中,所述步骤二中,所述条形码的条为黑色,所述相邻条之间的空隙为白色。
所述的条形码的制造方法中,所述步骤二中,在所述条形码上每两个相邻条之间的空隙上均印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物。
所述的条形码的制造方法中,所述分散剂为聚丙烯酸酯。
所述的条形码的制造方法中,所述粘合剂为聚氨酯。
实施例
步骤一、制备含有银粒子的三种油墨组合物,其中,以质量百分比计,第一种油墨组合物的组分为银粒子60%、15%聚丙烯酸酯、20%聚氨酯以及溶剂水,银粒子的粒径为10~20μm,第二种油墨组合物的组分为银粒子10%、10%聚丙烯酸酯、15%聚氨酯以及溶剂水,银粒子的粒径为0.1~0.8μm,第三种油墨组合物的组分为银粒子10%、5%聚丙烯酸酯、5%聚氨酯以及溶剂水,银粒子的粒径为0.1~0.8μm;
步骤二、在被印刷体上印刷条形码;
步骤三、在条形码上每两个相邻条之间的空隙上都印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物,印刷完成5~10min后,待已经印刷上的油墨组合物干燥,再在印刷有银粒子的质量含量为60%的油墨组合物的位置重叠印刷银粒子的质量含量为10%的油墨组合物,印刷完成5~10min后,待第二次印刷上的油墨组合物再次干燥,再在条形码上印刷银粒子的质量含量为5%的油墨组合物,并且此次印刷要使银粒子的质量含量为5%的油墨组合物覆盖条形码。
使用时,在条形码的外侧设置有一透明壳体,该壳体可以完全罩在条形码的外侧,在壳体内充入含有一定浓度硫化氢气体的氮气。当条形码中的银粒子与壳体内的硫化氢反应,就生成黑色的硫化银。先使用银粒子的含量最高的油墨组合物印刷,形成底层银粒子层;在使用银粒子含量较低的油墨组合物印刷,在底层银粒子层上形成中间层银粒子层;最后使用银粒子含量5%的油墨组合物,形成表层银粒子层。三层银粒子层是逐层印刷形成的,三层银粒子层的粒径从上至下粒径逐渐增大,浓度逐渐增大,由于越位于底层的银粒子的粒径大,其仍然可以突出出来,三层银粒子层实际是形成了一个凸凹不平的表面,位于这个表面的最突出的银粒子最先反应,而位于这个表面的相对不突出的银粒子就会相对较晚的反应。因此,上述三层银粒子层实际是逐渐变色的过程,随着空隙部分的逐渐变色,空隙部分相对于黑条部分的反差就会减小,当减小到一定程度的时候,就无法对条形码进行扫描了。由于银粒子的粒径相对还是较小的,因此,当反应进行到一定程度,空隙部分会呈现出较深的颜色,接近于黑色。
由于银粒子的反应产物呈黑色,因此,优选条形码的条为黑色,相邻条之间的空隙为白色。
由于壳体的空间有限,一般条形码的有效使用时间可为6个月,适用于具有6个月到6个半月的保质期的食品。
尽管本发明的实施方案已公开如上,但其并不仅仅限于说明书和实施方式中所列运用,它完全可以被适用于各种适合本发明的领域,对于熟悉本领域的人员而言,可容易地实现另外的修改,因此在不背离权利要求及等同范围所限定的一般概念下,本发明并不限于特定的细节和这里示出与描述的图例。

Claims (7)

1.一种条形码的制造方法,其特征在于,包括以下步骤:
步骤一、制备含有银粒子的三种油墨组合物,其中,所述三种油墨组合物中银粒子的质量含量分别为5%、10%和60%;
步骤二、在被印刷体上印刷条形码;
步骤三、在所述条形码的至少一对相邻条之间的空隙上印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物,印刷完成5~10min后,再在印刷有银粒子的质量含量为60%的油墨组合物的位置重叠印刷银粒子的质量含量为10%的油墨组合物,印刷完成5~10min后,再在所述条形码上印刷银粒子的质量含量为5%的油墨组合物,且所述银粒子的质量含量为5%的油墨组合物覆盖所述条形码;
使用时,在所述条形码的外侧设置有一透明壳体,该壳体可以完全罩在所述条形码的外侧,在壳体内充入含有一定浓度硫化氢气体的氮气。
2.如权利要求1所述的条形码的制造方法,其特征在于,所述步骤一中,按质量百分比计,银粒子的质量含量为60%的油墨组合物还含有15~20%分散剂、15~25%粘合剂以及溶剂水,银粒子的质量含量为10%以及5%的油墨组合物还含有5~10%分散剂、5~15%粘合剂以及溶剂水。
3.如权利要求1所述的条形码的制造方法,其特征在于,所述步骤一中,银粒子的质量含量为60%的油墨组合物中银粒子的粒径为10~20μm,银粒子的质量含量为5%以及10%的油墨组合物中银粒子的粒径为0.1~0.8μm。
4.如权利要求1所述的条形码的制造方法,其特征在于,所述步骤二中,所述条形码的条为黑色,所述相邻条之间的空隙为白色。
5.如权利要求1所述的条形码的制造方法,其特征在于,所述步骤二中,在所述条形码上每两个相邻条之间的空隙上均印刷所述步骤一得到的银粒子的质量含量为60%的油墨组合物。
6.如权利要求2所述的条形码的制造方法,其特征在于,所述分散剂为聚丙烯酸酯。
7.如权利要求2所述的条形码的制造方法,其特征在于,所述粘合剂为聚氨酯。
CN201310713848.4A 2013-12-20 2013-12-20 一种条形码的制造方法 Active CN103725104B (zh)