CN103087648B - The manufacture method of a kind of Nail-free glue sheet - Google Patents
The manufacture method of a kind of Nail-free glue sheet Download PDFInfo
- Publication number
- CN103087648B CN103087648B CN201110344289.5A CN201110344289A CN103087648B CN 103087648 B CN103087648 B CN 103087648B CN 201110344289 A CN201110344289 A CN 201110344289A CN 103087648 B CN103087648 B CN 103087648B
- Authority
- CN
- China
- Prior art keywords
- nail
- free
- sheet
- free glue
- release paper
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
技术领域 technical field
本发明属于胶粘剂的技术领域,特别是一种免钉胶薄片的制造技术。The invention belongs to the technical field of adhesives, in particular to a manufacturing technology of nail-free adhesive sheets.
背景技术 Background technique
现有免钉胶(低溶剂快速固化胶粘剂)为膏状物体,包装在活塞式筒中,通过挤压活塞而从嘴中挤出使用,从三十年前国外发明免钉胶、10年前南海嘉美化工公司在国内开始生产免钉胶直到现在,没有免钉胶薄片的技术。严格意义上说,常用胶粘剂(包括万能胶、免钉胶、不干胶等)技术中就没有薄胶片的技术。比如:万能胶、免钉胶没有制成薄片;双面胶或胶带等是不干胶涂在泡棉或塑料膜等基材上制成,虽是薄片,但不是薄胶片。The existing nail-free glue (low-solvent fast-curing adhesive) is a paste-like object, which is packed in a piston-type barrel and squeezed out of the mouth by squeezing the piston. The nail-free glue was invented abroad 30 years ago, and the South China Sea 10 years ago. Jiamei Chemical Co., Ltd. started to produce nail-free glue in China. Until now, there is no technology for nail-free glue sheets. Strictly speaking, there is no thin film technology in the commonly used adhesive (including universal glue, nail-free glue, self-adhesive, etc.) technology. For example: all-purpose glue and nail-free glue are not made into thin sheets; double-sided adhesive tape or tape is made by applying self-adhesive to foam or plastic film and other substrates. Although it is a thin sheet, it is not a thin film.
那么,不是薄片的免钉胶使用时的缺点是:一、使用干式粘接法(将免钉胶以20至40厘米的间距,涂在待粘合物的一个表面,点涂或涂成长条形均可,将带免钉胶的一面压紧粘接处,两面对合压贴;再将两边粘合面轻轻拉开,让胶水挥发2-5分钟,待胶水表干后将两边紧紧压合、敲紧;大约24小时之后,便可负重),则在面积较大或较重时无法拉开,而且胶水挥发程度比较不容易掌握,影响粘接效果。二、使用湿式粘接法(依照干式粘接法涂上免钉胶;配合钳夹、铁钉或螺丝,立即将粘合两面夹或钉紧;待胶水经过24小时凝固后,再移除钳夹),则需要使用工具且施工速度较慢。三、当小量使用时,容易因为剩胶而造成浪费。四、相对于双面胶或薄胶片使用不方便、施工速度较慢。Then, the disadvantages of using nail-free glue that is not a thin sheet are: 1. Use dry bonding method (apply the nail-free glue on one surface of the object to be bonded at a distance of 20 to 40 cm, and apply it on a long-term basis. Strips are available, press the side with the nail-free glue to the bonding place, and press the two sides together; then gently pull the two sides of the bonding surface apart, let the glue evaporate for 2-5 minutes, and put it on after the glue is dry. The two sides are tightly pressed and tapped tightly; after about 24 hours, the load can be loaded), then it cannot be pulled apart when the area is large or heavy, and the degree of glue volatilization is not easy to grasp, which affects the bonding effect. 2. Use the wet bonding method (apply nail-free glue according to the dry bonding method; cooperate with clamps, iron nails or screws, and immediately clamp or nail the two sides of the bond; wait for the glue to solidify after 24 hours, and then remove it. Clamps), tools are required and the construction speed is slower. 3. When used in small quantities, it is easy to cause waste due to residual glue. 4. Compared with double-sided tape or thin film, it is inconvenient to use and the construction speed is slower.
双面胶有自己的优点,但其缺点是:粘接强度及使用寿命均小于免钉胶及其薄胶片。Double-sided tape has its own advantages, but its disadvantages are: the bonding strength and service life are less than nail-free glue and its thin film.
发明内容 Contents of the invention
本发明的目的在于提供一种使用方便、快速施工、提供较大粘接力、寿命长、没有剩胶的免钉胶薄片的制造方法。The object of the present invention is to provide a method for manufacturing a nail-free glue sheet that is easy to use, fast in construction, provides greater adhesive force, has a long life, and has no glue left.
为实现上述目的,本发明的技术解决方案是:一种免钉胶薄片的制造方法,所述的免钉胶薄片是免钉胶膏状物压制而成,挥发部分溶剂后不粘双面的离型纸(又名硅油纸)、柔软、可以片状使用、具有良好的粘接性能、厚度0.2-3mm的免钉胶薄片。In order to achieve the above object, the technical solution of the present invention is: a method for manufacturing a nail-free glue sheet, the nail-free glue sheet is pressed from a nail-free glue paste, and does not stick to both sides after part of the solvent is volatilized. Release paper (also known as silicone oil paper), soft, can be used in sheet form, has good adhesive performance, and is a nail-free adhesive sheet with a thickness of 0.2-3mm.
一种免钉胶薄片的制造方法如图1所示,由免钉胶膏状物成条状挤出在离型纸的硅油面、另一离型纸的硅油面覆盖条状免钉胶膏状物的另一面、通过滚筒压薄条状免钉胶膏状物、“双层离型纸与免钉胶膏状物薄片的组合物”切块、挥发溶剂、密封包装六个步骤组成。如以下步骤:A manufacturing method of a nail-free adhesive sheet is shown in Figure 1. The nail-free adhesive paste is extruded in strips on the silicone oil surface of the release paper, and the silicone oil surface of the other release paper is covered with a strip-shaped nail-free adhesive paste. The other side of the object is composed of six steps: thinning the strip-shaped nail-free glue paste by a roller, cutting the "composition of double-layer release paper and nail-free glue paste sheet", volatilizing the solvent, and sealing the package. As the following steps:
A、条状免钉胶膏状物挤出在离型纸的硅油面。A. The strip-shaped nail-free glue paste is extruded on the silicone oil surface of the release paper.
B、将另一离型纸的硅油面覆盖条状免钉胶膏状物的另一面。B. Cover the other side of the strip-shaped nail-free glue paste with the silicone oil side of another release paper.
C、将双面覆盖离型纸的条状免钉胶膏状物放入两个滚筒之间,利用滚筒与离型纸非硅油面的摩擦力或施加在离型纸前端的拉力使条状免钉胶膏状物通过滚筒,进而压薄条状免钉胶膏状物,以形成“双层离型纸与免钉胶膏状物薄片的组合物”。C. Put the strip-shaped nail-free glue paste covered with release paper on both sides between the two rollers, use the friction between the roller and the non-silicone oil surface of the release paper or the pulling force applied to the front end of the release paper to make the strip The nail-free adhesive paste passes through the roller, and then the strip-shaped nail-free adhesive paste is thinned to form a "composition of double-layer release paper and nail-free adhesive paste sheet".
D、使用剪切或模切的方法把较大面积的“双层离型纸与免钉胶膏状物薄片的组合物”切成小块。D. Cut the larger "composition of double-layer release paper and nail-free glue paste sheet" into small pieces by cutting or die-cutting.
E、根据需要的薄片硬度,把“双层离型纸与免钉胶膏状物薄片的组合物”稍稍凉置,让免钉胶膏状物挥发出部分溶剂后变成:不粘双面的离型纸、柔软、可以片状使用、具有良好的粘接性能、厚度0.2-3mm的免钉胶薄片。E. According to the required sheet hardness, put the "composition of double-layer release paper and nail-free adhesive paste sheet" in a cool place, let the nail-free adhesive paste evaporate part of the solvent and then become: non-stick double-sided High-quality release paper, soft, can be used in sheet form, has good adhesive performance, and is a nail-free adhesive sheet with a thickness of 0.2-3mm.
F、把小块免钉胶薄片用铝膜袋(或塑料袋)包装,并用封口机封口,使之密封,不能挥发出溶剂,以保持粘接性能。F. Pack the small piece of nail-free adhesive sheet in an aluminum film bag (or plastic bag), and seal it with a sealing machine to make it sealed so that the solvent cannot be volatilized to maintain the adhesive performance.
显然的,以上的步骤可以连续的、自动化的进行。Obviously, the above steps can be performed continuously and automatically.
使用时,只需剪开铝膜袋,取出免钉胶薄片,先撕掉一层离型纸,把免钉胶薄片粘贴在预定位置(如:墙面),然后撕掉另一层离型纸,把待粘接物(如:木板或粘钩等)压紧粘接处,紧紧压合即可。当然,也可以先粘贴在待粘接物上,再粘贴在预定位置。这时的免钉胶薄片就能提供一定的初粘力,支撑粘接物。完全固化后能承受更大重物。When using, just cut open the aluminum film bag, take out the nail-free adhesive sheet, first tear off a layer of release paper, paste the nail-free adhesive sheet on the predetermined position (such as: the wall), and then tear off another layer of release paper Paper, press the object to be bonded (such as: wood board or sticky hook, etc.) to the bonding place, and press it tightly. Of course, it can also be pasted on the object to be bonded first, and then pasted at a predetermined position. At this time, the nail-free adhesive sheet can provide a certain initial adhesion and support the adhesive. After fully cured, it can bear more heavy objects.
本发明的有益效果是:使用方便、快速施工、提供较大粘接力、寿命长、没有剩胶。The beneficial effects of the invention are: convenient use, quick construction, greater adhesive force, long service life and no glue left.
附图说明 Description of drawings
图1是本发明免钉胶膏状物从条状挤出到滚筒压薄的示意图。Fig. 1 is a schematic diagram of the nail-free glue paste of the present invention from strip extrusion to roller thinning.
附图标记说明:Explanation of reference signs:
10、离型纸;20、另一离型纸;30、条状免钉胶膏状物;40、滚筒;50、双层离型纸与免钉胶膏状物薄片的组合物。10. Release paper; 20. Another release paper; 30. Strip-shaped nail-free glue paste; 40. Roller; 50. Composition of double-layer release paper and nail-free glue paste sheet.
实施例1:Example 1:
一种免钉胶薄片的制造方法,所述的免钉胶薄片是免钉胶膏状物压制而成,挥发部分溶剂后不粘双面的离型纸、柔软、可以片状使用、具有良好的粘接性能、厚度0.2-3mm的免钉胶薄片。A method for manufacturing a nail-free glue sheet. The nail-free glue sheet is formed by pressing a nail-free glue paste. After volatile part of the solvent, it does not stick to the double-sided release paper, is soft, can be used in sheet form, and has good Excellent adhesive performance, nail-free adhesive sheet with a thickness of 0.2-3mm.
一种免钉胶薄片的制造方法如图1所示,由条状免钉胶膏状物30挤出在离型纸10的硅油面、另一离型纸20的硅油面覆盖条状免钉胶膏状物30的另一面、通过滚筒40压薄条状免钉胶膏状物30、“双层离型纸与免钉胶膏状物薄片的组合物”50切块、挥发溶剂、密封包装六个步骤组成。如以下步骤:A kind of manufacturing method of nail-free glue sheet is shown in Figure 1, is extruded on the silicone oil surface of release paper 10 by strip-shaped nail-free glue paste 30, and the silicone oil surface of another release paper 20 covers strip-shaped nail-free glue On the other side of the glue paste 30, the strip-shaped nail-free glue paste 30 is thinned by the roller 40, and the "composition of double-layer release paper and nail-free glue paste sheet" 50 is cut into pieces, evaporated solvent, and sealed Packaging consists of six steps. As the following steps:
A、条状免钉胶膏状物30挤出在离型纸10的硅油面。A. The strip-shaped nail-free glue paste 30 is extruded on the silicone oil surface of the release paper 10 .
B、将另一离型纸20的硅油面覆盖条状免钉胶膏状物30的另一面。B. Cover the other side of the strip-shaped nail-free glue paste 30 with the silicone oil side of another release paper 20 .
C、将双面覆盖离型纸10、20的条状免钉胶膏状物30放入两个滚筒40之间,利用滚筒40与离型纸10、20非硅油面的摩擦力或施加在离型纸10、20前端的拉力使条状免钉胶膏状物30通过滚筒40,进而压薄条状免钉胶膏状物30,以形成“双层离型纸与免钉胶膏状物薄片的组合物”50。C. Put the strip-shaped nail-free glue paste 30 covered with release paper 10, 20 on both sides between the two rollers 40, and use the friction between the roller 40 and the non-silicone oil surface of the release paper 10, 20 or apply it on the The pulling force of the front end of the release paper 10, 20 makes the strip-shaped nail-free glue paste 30 pass through the roller 40, and then the strip-shaped nail-free glue paste 30 is thinned to form a "double-layer release paper and nail-free glue paste". Composition of Thin Sheets"50.
D、使用剪切或模切的方法把较大面积的“双层离型纸与免钉胶膏状物薄片的组合物”50切成小块。D. Cut the larger-area "composition of double-layer release paper and nail-free glue paste sheet" 50 into small pieces by cutting or die-cutting.
E、根据需要的薄片硬度,把“双层离型纸与免钉胶膏状物薄片的组合物”50稍稍凉置,让免钉胶膏状物挥发出部分溶剂后变成:不粘双面的离型纸、柔软、可以片状使用、具有良好的粘接性能、厚度0.2-3mm的免钉胶薄片。E. According to the required sheet hardness, put the "composition of double-layer release paper and nail-free adhesive paste sheet" 50 in a cool place, let the nail-free adhesive paste evaporate part of the solvent and then become: non-stick double The release paper on the surface is soft, can be used in sheet form, has good adhesive performance, and is a nail-free adhesive sheet with a thickness of 0.2-3mm.
F、把小块免钉胶薄片用铝膜袋包装,并用封口机封口,使之密封,不能挥发出溶剂,以保持粘接性能。F. Pack the small piece of nail-free adhesive sheet in an aluminum film bag, and seal it with a sealing machine to make it airtight, so that the solvent cannot be volatilized, so as to maintain the adhesive performance.
Claims (1)