CN103031732A - 一种水性聚氨酯皮革黏合剂的制备方法 - Google Patents
一种水性聚氨酯皮革黏合剂的制备方法 Download PDFInfo
- Publication number
- CN103031732A CN103031732A CN2012105218846A CN201210521884A CN103031732A CN 103031732 A CN103031732 A CN 103031732A CN 2012105218846 A CN2012105218846 A CN 2012105218846A CN 201210521884 A CN201210521884 A CN 201210521884A CN 103031732 A CN103031732 A CN 103031732A
- Authority
- CN
- China
- Prior art keywords
- performed polymer
- polyurethane leather
- preparation
- leather glue
- dmpa
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种水性聚氨酯皮革黏合剂的制备方法,是以IPDI、PCL1000、PG、DMPA为原料制备预聚体,加入适量羧基丁苯胶水乳液改性预聚体,加入三乙胺进行中和反应生成盐,加入适量的去离子水制得水性聚氨酯皮革黏合剂。本发明得到的水性聚氨酯皮革黏合剂具有固含量高、粘结力好及环保性强等优点。
Description
技术领域
本发明涉及一种水性聚氨酯皮革黏合剂的制备方法,属化工领域。
技术背景
聚氨酯材料的应用覆盖了生产、生活各个领域,在经济发展中起到了重要的作用。但该材料仍然存在固含量不够高、粘结强度和力学性能不够理想的缺点, 而且市场价格比较高,在实际使用过程中,仍存在少量有机溶剂等不足。故水性聚氨酯材料在研发应用过程中,仍有必要进行深入研究与提高。
因此必须采用改性的水性聚氨酯的方法,使得制得的产品具有较高的固含量、粘结性好、环保性强。本专利采用产量丰富,价格低廉,具有天然生物降解性能的葡萄糖作为交联剂对水性聚氨酯改性,共混羧基丁苯胶水乳液,以此来提高胶黏剂的固含量,提高环保性能及力学性能。
发明内容
本发明的目的是提供一种水性聚氨酯皮革黏合剂的制备方法,得到的水性聚氨酯具有固含量高、粘结力好及环保性强等优点。
为实现以上目的,本发明的一种水性聚氨酯皮革黏合剂的制备方法,其步骤具体为:
(1) 以异佛尔酮二异氰酸酯(IPDI)、聚己内酯二醇(PCL1000)、葡萄糖(PG)、二羟甲基丙酸(DMPA)为原料制备预聚体,反应2h。
(2) 加入羧基丁苯胶水乳液改性预聚体,反应50min。
(3) 降温至40℃,加入三乙胺进行中和反应生成盐,反应3-4min。
(4) 加入水进行乳化60min,得到有水性聚氨酯皮革黏合剂。
步骤(1)中预聚体原料的配比为:IPDI与PCL1000、PG、DMPA的摩尔比为1.2:1-1.3:1,PG占预聚体质量的2%-3%,DMPA占预聚体质量的5%-6%。
步骤(2)中羧基丁苯胶水乳液占预聚体质量的30%-35%。
步骤(3)中三乙胺的物质的量与DMPA的物质的量相同。
步骤(4)中水的用量为预聚体总质量的2倍。
本发明产生的有益效果为,本专利采用产量丰富,价格低廉,具有天然生物降解性能的葡萄糖作为交联剂对水性聚氨酯进行改性。为了进一步提高水性聚氨酯皮革黏合剂的固含量,增大初黏力和缩短固化时间以及降低成本,采用羧基丁苯胶水乳液与预聚体共混改性,制得的皮革黏合剂固含量高、环保性强、力学性能好。
实施例
实施例1:
以异佛尔酮二异氰酸酯(IPDI)、聚己内酯二醇(PCL1000)、葡萄糖(PG)、二羟甲基丙酸(DMPA)为原料制备预聚体,反应2h。IPDI与PCL1000、PG、DMPA的摩尔比为1.2:1,PG占预聚体质量的2%,DMPA占预聚体质量的5%。加入羧基丁苯胶水乳液改性预聚体,羧基丁苯胶水乳液占预聚体质量的35%,反应50min。降温至40℃,加入三乙胺进行中和反应生成盐,三乙胺的物质的量与DMPA的物质的量相同,反应3min。加入水进行乳化60min,水的用量为预聚体总质量的2倍,得到有水性聚氨酯皮革黏合剂。
实施例2:
以异佛尔酮二异氰酸酯(IPDI)、聚己内酯二醇(PCL1000)、葡萄糖(PG)、二羟甲基丙酸(DMPA)为原料制备预聚体,反应2h。IPDI与PCL1000、PG、DMPA的摩尔比为1.3:1,PG占预聚体质量的3%,DMPA占预聚体质量的6%。加入羧基丁苯胶水乳液改性预聚体,羧基丁苯胶水乳液占预聚体质量的30%,反应50min。降温至40℃,加入三乙胺进行中和反应生成盐,三乙胺的物质的量与DMPA的物质的量相同,反应3min。加入水进行乳化60min,水的用量为预聚体总质量的2倍,得到有水性聚氨酯皮革黏合剂。
Claims (5)
1.一种水性聚氨酯皮革黏合剂的制备方法,其特征在于:步骤如下:
(1) 以异佛尔酮二异氰酸酯(IPDI)、聚己内酯二醇(PCL1000)、葡萄糖(PG)、二羟甲基丙酸(DMPA)为原料制备预聚体,反应2h;
(2) 加入羧基丁苯胶水乳液改性预聚体,反应50min;
(3) 降温至40℃,加入三乙胺进行中和反应生成盐,反应3-4min;
(4) 加入水进行乳化60min,得到有水性聚氨酯皮革黏合剂。
2.如权利要求1所述的一种水性聚氨酯皮革黏合剂的制备方法,其特征在于:所述的步骤(1)中预聚体原料的配比为:IPDI与PCL1000、PG、DMPA的摩尔比为1.2:1-1.3:1,PG占预聚体质量的2%-3%,DMPA占预聚体质量的5%-6%。
3.如权利要求1所述的一种水性聚氨酯皮革黏合剂的制备方法,其特征在于:所述的步骤(2)中羧基丁苯胶水乳液占预聚体质量的30%-35%。
4.如权利要求1所述的一种水性聚氨酯皮革黏合剂的制备方法,其特征在于:所述的步骤(3)中三乙胺的物质的量与DMPA的物质的量相同。
5.如权利要求1所述的一种水性聚氨酯皮革黏合剂的制备方法,其特征在于:所述的步骤(4)中水的用量为预聚体总质量的2倍。