[go: up one dir, main page]

CN102924988A - Anti-scratching insulating protective liquid for capacitive touch screen - Google Patents

Anti-scratching insulating protective liquid for capacitive touch screen Download PDF

Info

Publication number
CN102924988A
CN102924988A CN2012104740523A CN201210474052A CN102924988A CN 102924988 A CN102924988 A CN 102924988A CN 2012104740523 A CN2012104740523 A CN 2012104740523A CN 201210474052 A CN201210474052 A CN 201210474052A CN 102924988 A CN102924988 A CN 102924988A
Authority
CN
China
Prior art keywords
touch screen
capacitive touch
acrylic resin
protection liquid
dioxide
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012104740523A
Other languages
Chinese (zh)
Inventor
林洁
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Panda Electronics Group Co Ltd
Original Assignee
Nanjing Huaxian High Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nanjing Huaxian High Technology Co Ltd filed Critical Nanjing Huaxian High Technology Co Ltd
Priority to CN2012104740523A priority Critical patent/CN102924988A/en
Publication of CN102924988A publication Critical patent/CN102924988A/en
Pending legal-status Critical Current

Abstract

The invention discloses anti-scratching insulating protective liquid for a capacitive touch screen. The protective liquid is characterized by mainly consisting of the following components in percentage by weight: 10-40% of acrylic resin, 3-10% of silica, 50-85% of reactive diluent, and1-3% of auxiliaries. The sum of contents of each component is 100%. The anti-scratching insulating protective liquid can be made on the surface of the touch screen through a simple dip coating method, and has good transparency and uniform thickness, and forms a film after being dried in an oven with no need of other complicated devices. The solidified film has the advantages of glossy smooth surface, high light transmittance, excellent hardness and adhesion, and good insulating property.

Description

The capacitive touch screen of anti-scratch insulation is with protecting liquid
Technical field
The present invention relates to touch screen technology, especially a kind of long and narrow electrode that plates for the protection of touch-screen four limits and the effect protection liquid that plays insulation, specifically a kind of capacitive touch screen of anti-scratch insulation is with protection liquid.
Background technology
Along with the development of science and technology, touch screen technology has had significant progress, particularly multi-point touch panel, with respect to touch screens, the electric capacity touch screen more easily realizes, As time goes on, capacitance plate might become a trend, more is applied to the touch material of intelligent machine.Also need to solve simultaneously technology and protection problem in the production process in the process of development, the protection of the electrode on touch-screen four limits is exactly an aspect.
The structure of the touch-screen of capacitive technologies mainly is at the thin-film body layer of glass screen plating layer of transparent at present, adds the lastblock protective glass at the thin-film body layer again, and conductive layer and inductive layer can be thoroughly protected in two glass designs.Capacitive touch screen all plates long and narrow electrode on touch-screen four limits, forms a low-voltage AC electric field in electrical conductor.When touch screen, because people's bulk electric field, can form a coupling capacity between finger and conductor layer, the electric current that four limit electrodes send can flow to the contact, be directly proportional with the distance of finger to electrode and electric current is strong and weak, be positioned at ratio and power that controller after the touch screen just can calculate electric current, accurately calculate the position of touch point.
The electrode circuit on touch-screen four limits directly is connected with conductive layer; it is an important step of touch-screen normal operation; for the electrode that prevents touch-screen four limits sustains damage in the process of operation; guarantee simultaneously the insulation of electrode in the use procedure, need to make the layer protecting film guard electrode at the electrode on touch-screen four limits.
Summary of the invention
The present invention be directed in the touch-screen production process and need to make the layer protecting film guard electrode at the electrode on touch-screen four limits; invent a kind of capacitive touch screen of anti-scratch insulation with protection liquid, produce the rete that satisfied protection touch screen protective requires by czochralski process.
One of technical scheme of the present invention is:
A kind of capacitive touch screen of anti-scratch insulation is characterized in that with protection liquid it mainly is comprised of acrylic resin, silicon-dioxide, reactive thinner and auxiliary agent, and the weight proportion of each component is:
Acrylic resin 10-40%;
Silicon-dioxide 3-10%;
Reactive thinner 50-85%;
Auxiliary agent 1-3%;
The each component sum is 100%.
Described acrylic resin is the mixture of thermosetting acrylic resin and Hydroxylated acrylic resin, and both part by weight are 1:1-2.
Described silicon-dioxide is nanometer grade silica.
Described reactive thinner is Virahol, 1-Methoxy-2-propyl acetate, diethylene glycol ethylmethyl ether, tri (propylene glycol) diacrylate, the mixture of one or more in propylene glycol diacrylate or the Viscoat 295.
Described auxiliary agent is flow agent or coupling agent.
Two of technical scheme of the present invention is:
A kind of capacitive touch screen of anti-scratch insulation is characterized in that with acrylic resin silicon-dioxide with the preparation method of protection liquid; reactive thinner is after auxiliary agent mixes in proportion, at grinding in ball grinder 2-5 hour; make the fineness of slurry be no more than 8000 orders, viscosity number is less than 200mPa.s.
The invention has the beneficial effects as follows:
Protection liquid of the present invention can be produced on touch screen surface by simple crystal pulling method, has light transmission good, uniform film thickness; film forming after oven for drying does not need other complex apparatus, and the curing rear surface is smooth smooth; light transmission rate is high, has hardness and sticking power is good, the advantages such as good insulating.
Protection liquid manufacture craft of the present invention is easy, and the rete light transmission rate of making is high, and hardness reaches 4H, and insulation effect is good, the requirement that other physical indexs can satisfy or be above standard and stipulate.
Embodiment
The present invention is further illustrated below in conjunction with embodiment.
Embodiment one.
Take off the row raw material and mix thermosetting acrylic resin 10kg; Hydroxylated acrylic resin 20kg; Silicon-dioxide 5kg; Virahol 45kg; Tri (propylene glycol) diacrylate 20kg and flow agent 2kg placed the ball mill ball milling 3 hours, and making the fineness of the protection liquid behind the ball milling is 8000 orders, and viscosity is that 47.6mPa.s gets final product.The protection liquid of the present embodiment can be produced on touch screen surface by simple crystal pulling method, has light transmission good, uniform film thickness; film forming after oven for drying does not need other complex apparatus, and the curing rear surface is smooth smooth; light transmission rate is high, has hardness and sticking power is good, the advantages such as good insulating.The rete light transmission rate of making is up to 84.7%, and hardness reaches 4H.
Embodiment two.
Take off the row raw material and mix thermosetting acrylic resin B:5kg; Hydroxylated acrylic resin 5kg; Silicon-dioxide: 10kg; Virahol 50kg; Tri (propylene glycol) diacrylate: 35kg; Coupling agent 1kg placed the ball mill ball milling 2 hours, and making the fineness of the protection liquid behind the ball milling is 5000 orders, and viscosity is that 75.3mPa.s gets final product.The rete light transmission rate that the protection liquid of the present embodiment forms is up to 82.3%, and hardness reaches 3.9H.
Embodiment three.
Take off the row raw material and mix thermosetting acrylic resin B:15kg; Hydroxylated acrylic resin 25kg; Silicon-dioxide: 3kg; Virahol 26kg; Tri (propylene glycol) diacrylate: 24kg; Coupling agent 3kg placed the ball mill ball milling 5 hours, and making the fineness of the protection liquid behind the ball milling is 8000 orders, and viscosity is that 25.7mPa.s gets final product.The rete light transmission rate that the protection liquid of the present embodiment forms is up to 85.4%, and hardness reaches 4.2H.
The part that the present invention does not relate to prior art that maybe can adopt same as the prior art is realized.

Claims (6)

1. the capacitive touch screen of an anti-scratch insulation is characterized in that with protection liquid it mainly is comprised of acrylic resin, silicon-dioxide, reactive thinner and auxiliary agent, and the weight proportion of each component is:
Acrylic resin 10-40%;
Silicon-dioxide 3-10%;
Reactive thinner 50-85%;
Auxiliary agent 1-3%;
The each component sum is 100%.
2. the capacitive touch screen of anti-scratch insulation according to claim 1 is characterized in that with protection liquid described acrylic resin is the mixture of thermosetting acrylic resin and Hydroxylated acrylic resin, and both part by weight are 1:1-2.
3. the capacitive touch screen of anti-scratch insulation according to claim 1 is characterized in that with protection liquid described silicon-dioxide is nanometer grade silica.
4. the capacitive touch screen of anti-scratch insulation according to claim 1 is with protecting liquid; it is characterized in that described reactive thinner is Virahol; 1-Methoxy-2-propyl acetate; diethylene glycol ethylmethyl ether; tri (propylene glycol) diacrylate, the mixture of one or more in propylene glycol diacrylate or the Viscoat 295.
5. the capacitive touch screen of anti-scratch insulation according to claim 1 is characterized in that with protection liquid described auxiliary agent is flow agent or coupling agent.
6. the capacitive touch screen of an anti-scratch insulation is characterized in that with acrylic resin silicon-dioxide with the preparation method of protection liquid; reactive thinner is after auxiliary agent mixes in proportion, at grinding in ball grinder 2-5 hour; make the fineness of slurry be no more than 5000 orders, viscosity number is less than 200mPa.s.
CN2012104740523A 2012-11-21 2012-11-21 Anti-scratching insulating protective liquid for capacitive touch screen Pending CN102924988A (en)