[go: up one dir, main page]

CN102794002A - 一种碳素羽毛球拍的耐高强度修补方法 - Google Patents

一种碳素羽毛球拍的耐高强度修补方法 Download PDF

Info

Publication number
CN102794002A
CN102794002A CN2012103264464A CN201210326446A CN102794002A CN 102794002 A CN102794002 A CN 102794002A CN 2012103264464 A CN2012103264464 A CN 2012103264464A CN 201210326446 A CN201210326446 A CN 201210326446A CN 102794002 A CN102794002 A CN 102794002A
Authority
CN
China
Prior art keywords
racket
fracture
carbon
carbon fiber
repairing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012103264464A
Other languages
English (en)
Inventor
吴先强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012103264464A priority Critical patent/CN102794002A/zh
Publication of CN102794002A publication Critical patent/CN102794002A/zh
Pending legal-status Critical Current

Abstract

本发明公开一种碳素羽毛球拍的耐高强度修补方法,步骤包括:先将球拍断口两边的两颗胶订拔出来,然后把涂漆清除了,再将断口内的杂物如塑料薄膜、海绵体填充物等清理干净,接着就是把预先制作好的合适球拍断口位置的一定数量的碳纤维条粘附少许AB胶水插入断口里面,然后静置30分钟;切取小段碳纤维布紧紧缠绕在球拍断口的外面,并加热至160℃的温度待其与球拍断口粘合;无需打磨粘合部位,上漆即可。本发明方法的优点:修补好后的球拍的增重很小,一般是在0.5~1.5克,强度极高,超过了原有球拍的所承受的拉力,这是其它使用内置金属、现有的碳素等等补拍技术所不能达到的,且基本保持了原有球拍的平衡点、手感和外观。

Description

一种碳素羽毛球拍的耐高强度修补方法
技术领域
本发明涉及一种体育器材的修补方法,尤其是涉及一种碳素羽毛球拍的耐高强度修补方法。
背景技术
由于碳纤维球拍重量轻、强度高、性能好的众多优点,碳纤维球拍面世40多年来,逐渐占领了网羽球拍的绝大部分市场。但是碳纤维也有一个弱点,那就是脆性高,因此碳纤维球拍容易发生断裂。如今,打羽毛球的人越来越多,当球拍不小心碰撞到其他硬物或者球拍互撞,球拍就会受损甚至断裂而无法再使用,所以现在的断拍也越来越多。能不能将断裂的球拍修理之后再重新使用呢?用什么方法修理?修理后的球拍性能恢复得怎么样?
以前修拍技术是用金属材料来做支撑物,修好后的球拍增重大,效果不理想,断口处容易出现裂纹和变形。即使是现在的某公司的碳素修拍技术也存有缺陷,其使用的是碳素材料做支撑物,效果也不是非常的理想,且操作比较麻烦,修好后,断口也有出现裂纹和变形的情况,导致这些情况的出现的主要原因就是支撑物硬度不够。所以,广大的球迷朋友渴望有一种高强度的修补方法,使得修补后球拍更加坚固,又能和原来球拍一样的使用效果。
发明内容
本发明的目的是克服现有技术存在的缺陷,提供一种新的能承受高强度的球拍修补方法,使得修补后的球拍既能和原来球拍一样的使用效果,且断口的强度是整个拍框最高的,增重也仅有0.5~1.5克。
本发明的技术内容如下:
一种碳素羽毛球拍的耐高强度修补方法,其步骤为:
A、首先将球拍断口两边的两颗胶订拔出来,清除原有的涂漆并将断口内的杂物如塑料薄膜、海绵体填充物等清理干净;
B、将预先制作好的合适断口位置的一定数量的碳纤维条粘附少许AB胶水后插入球拍断口里面,静置大概30分钟;
C、切取小段碳纤维布紧紧缠绕在球拍断口的外面,并加热至160℃的温度待其与球拍断口粘合;
D、无需打磨粘合的部位,上漆即可。
具体实施方式
将一支断了的球拍修补,首先将球拍断口两边的两颗胶订拔出来,清除原有的涂漆并将断口内的杂物如塑料薄膜、海绵体填充物等清理干净;然后将预先制作好的合适断口位置的一定数量的碳纤维条粘附少许AB胶水后插入球拍断口里面,静置30分钟;切取小段碳纤维布紧紧缠绕在球拍断口的外面,并加热至160℃的温度待其与球拍断口粘合;无需打磨粘合部位,上漆即可。
本发明方法的优点:修补好后的球拍的增重很小,一般是在0.5~1.5克,强度极高,超过了原有球拍的所承受的拉力,这是其它使用内置金属、现有的碳素等等补拍技术所不能达到的,且基本保持了原有球拍的平衡点、手感和外观。

Claims (1)

1.一种碳素羽毛球拍的耐高强度修补方法,其特征见于以下所述步骤:
A、首先将球拍断口两边两颗胶订拔出来,清除原有的涂漆并将断口内的杂物如塑料薄膜、海绵体填充物等清理干净;
B、将预先制作好的合适断口位置的一定数量的碳纤维条粘附少许AB胶水后插入球拍断口里面,静置30分钟;
C、切取小段碳纤维布紧紧缠绕在球拍断口的外面,并加热至160℃的温度待其与球拍断口粘合;
D、无需打磨粘合部位,上漆即可;
CN2012103264464A 2012-09-06 2012-09-06 一种碳素羽毛球拍的耐高强度修补方法 Pending CN102794002A (zh)