CN102555416A - 一种钢质烫金凸模的制作方法 - Google Patents
一种钢质烫金凸模的制作方法 Download PDFInfo
- Publication number
- CN102555416A CN102555416A CN2011104615637A CN201110461563A CN102555416A CN 102555416 A CN102555416 A CN 102555416A CN 2011104615637 A CN2011104615637 A CN 2011104615637A CN 201110461563 A CN201110461563 A CN 201110461563A CN 102555416 A CN102555416 A CN 102555416A
- Authority
- CN
- China
- Prior art keywords
- punch
- path
- knife path
- program
- carving
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种钢质烫金凸模的制作方法,首先准备磁铁平面吸台,选择雕刻钢坯料,将雕刻钢坯料置于该磁铁平面吸台上;然后根据烫印图案编写凸模曲面程序,同时进行雕刻走刀规划,编写走刀程序,对走刀程序的编写包括大刀路径和小刀路径,并计算小刀路径与大刀路径的比例,根据该比例对小刀路径进行缩放,小刀路径编写完成后,计算磨刀的角度和间距,最后由大刀走面、开粗;最后使用CNC雕刻机根据走刀程序对雕刻钢坯料进行雕刻。凸模曲面程序中需要对虚拟曲面和产品曲面的差异进行掌控,可对比树脂凸模台阶的深度差异进行掌控。通过该方法制作的凸模,由于在机器上直接雕刻出来,可以避免变形,能更好的和凹模相匹配,可制作更精细的凹凸烫金。
Description
技术领域
本发明涉及凹凸模烫金印刷技术,尤其涉及一种钢质烫金凸模的制作方法。
背景技术
高质量的烫印版是烫印质量的保证,普通烫印版的制作比较简单,主要采用照相腐蚀制版工艺和电子雕刻制版工艺。常用的版材是铜版或锌版。铜版由于质地细腻、表面光洁、传热性能好、耐磨耐压、不易变形,是目前主流的烫印版。采用优质的铜版可提高烫印图文的光泽和清晰度。而对一些烫印数量较少、质量要求不高的包装印刷品烫印时也可采用锌版。目前国外已经普遍采用雕刻黄铜版,用扫描仪先将要烫印的图案进行扫描,将数据储存进电脑,然后通过电脑及软件的控制进行立体雕刻;形成有丰富层次立体图案的阴模凹版。
立体烫金的底版必须是与烫印版相对应的阳模凸版,即烫印版凹下的部位在底版上应是凸起的,而凸起的高度与烫印版凹下的深度是相对应的。制作底模凸版的方法与凹凸压印的阳模凸版制作方法是一样的,常用的材料有石膏和玻璃纤维。若采用石膏则需在机器上完成制作,因此工艺较复杂,更换底版麻烦,但成本较低,现在国内较为常用。若用玻璃纤维则可以根据烫金版的模型预先制作,并配合加工的铜版制作定位孔,方便更换定位。底模凸版是为配合烫印凹版来形成立体浮雕图案的,其必须与烫印版精确对应。但是立体烫金不同于凹凸压印,凹凸压印多数不需要加热,而立体烫金则必须高温加热。在烫印时,随着温度升高,烫印版会发生膨胀,而底模凸版的温度却基本保持不变,这就会造成烫印版与底模凸版的不配套,造成压碎底模或无法烫印的现象。因此在制作底模凸版时要充分考虑烫印版的膨胀率,以制作出精确的底模凸版。
传统的树脂凸模是先在铜板上做一个模形,在经铜板加温后倒入树脂药水冷却后形成,铜块在加温后会有一定的变形,所在生产出来的凸模也会有一定的误差,这样就会影响凹凸的效果,
发明内容
本发明的目的是提供一种钢质烫金凸模的制作方法,提高印刷生产效率。
本发明为解决其技术问题所采用的技术方案是,
一种钢质烫金凸模的制作方法,包括以下步骤:
1)准备磁铁平面吸台,将雕刻钢坯料置于该磁铁平面吸台上;
2)编写凸模曲面程序和走刀程序;
3)使用CNC雕刻机根据步骤2)中的走刀程序对雕刻钢坯料进行雕刻。
其中,步骤2)中对走刀程序的编写包括大刀路径和小刀路径,并计算小刀路径与大刀路径的比例,根据该比例对小刀路径进行缩放,小刀路径编写完成后,计算磨刀的角度和间距,最后由大刀走面、开粗;
凸模曲面程序中需要对虚拟曲面和产品曲面的差异进行掌控,可对比树脂凸模台阶的深度差异进行掌控。
本发明的优点在于,通过该方法制作的凸模,由于在机器上直接雕刻出来,可以避免变形,能更好的和凹模相匹配,完全适合印刷厂400万次的冲压,在印刷生产过程中要比传统的树脂凸模有效率,更稳定,凹凸效果更理想,克服了普通凸模温度受限、不耐压、易变形的缺陷,同时能应用于各类电雕产品,可制作更精细的凹凸烫金。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体实施例,进一步阐述本发明。
在本实施例中,钢质烫金凸模的制作流程为:首先,准备磁铁平面吸台,选择雕刻钢坯料,将雕刻钢坯料置于该磁铁平面吸台上;然后,根据烫印图案编写凸模曲面程序,同时进行雕刻走刀规划,编写走刀程序,对走刀程序的编写包括大刀路径和小刀路径,并计算小刀路径与大刀路径的比例,根据该比例对小刀路径进行缩放,小刀路径编写完成后,计算磨刀的角度和间距,最后由大刀走面、开粗;最后使用CNC雕刻机根据走刀程序对雕刻钢坯料进行雕刻。凸模曲面程序中需要对虚拟曲面和产品曲面的差异进行掌控,可对比树脂凸模台阶的深度差异进行掌控。
该制作方法采用的流程是选好材质,编程,再生产,材质的光泽度、硬度要合适,编程时改进了走刀的过程,走刀程序的改进使得生产出的凸模更精细,误差约为±0.01mm,编程时在计算机中生成凸模的虚拟曲面,该虚拟曲面再通过CNC雕刻机转换成凸模的产品曲面,如果误差超出范围,可通过对计算机中的虚拟曲面进行调节,普通树脂凸模是通过凹模加热后倒入树脂冷却形成的,容易发生变形,而本发明采用雕刻钢坯料直接雕刻,可有效减少凸模的变形,提高对凸模形状精确度的掌控。
以上显示和描述了本发明的基本原理、主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等同物界定。
Claims (2)
1.一种钢质烫金凸模的制作方法,其特征在于,包括以下步骤:
1)准备磁铁平面吸台,将雕刻钢坯料置于该磁铁平面吸台上;
2)编写凸模曲面程序和走刀程序;
3)使用CNC雕刻机根据步骤2)中的走刀程序对雕刻钢坯料进行雕刻。
2.根据权利要求1所述的一种钢质烫金凸模的制作方法,其特征在于,步骤2)中对走刀程序的编写包括大刀路径和小刀路径,并计算小刀路径与大刀路径的比例,根据该比例对小刀路径进行缩放,小刀路径编写完成后,计算磨刀的角度和间距,最后由大刀走面、开粗。