[go: up one dir, main page]

CN102553915A - 热轧薄板开轧预调法 - Google Patents

热轧薄板开轧预调法 Download PDF

Info

Publication number
CN102553915A
CN102553915A CN2012100163404A CN201210016340A CN102553915A CN 102553915 A CN102553915 A CN 102553915A CN 2012100163404 A CN2012100163404 A CN 2012100163404A CN 201210016340 A CN201210016340 A CN 201210016340A CN 102553915 A CN102553915 A CN 102553915A
Authority
CN
China
Prior art keywords
rolling
beginning
sensor
pressure
sides
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012100163404A
Other languages
English (en)
Inventor
陈洪亮
苏海
郭智勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tangshan Guofeng Iron and Steel Co Ltd
Original Assignee
Tangshan Guofeng Iron and Steel Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tangshan Guofeng Iron and Steel Co Ltd filed Critical Tangshan Guofeng Iron and Steel Co Ltd
Priority to CN2012100163404A priority Critical patent/CN102553915A/zh
Publication of CN102553915A publication Critical patent/CN102553915A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种热轧薄板生产线开轧的预调方法。技术方案是:压力传感器对上辊压力进行检测,测压头对下辊压力进行检测,调平直=(20%-40%)*传感器两侧轧制力偏差,传感器两侧轧制力偏差大于50T时,选用40%,小于50T时,选用20%。本发明的有益效果是:能够减小了开轧时操作难度,确保开轧时的头部板形,同时大大减少了开轧时因预调错误而导致得头部轧烂,避免产生二级品和废钢。本发明局部科学性,节约成本和时间,提高经济效益。

Description

热轧薄板开轧预调法
技术领域
本发明涉及一种热轧薄板生产线开轧的预调方法,属冶金行业轧钢技术领域。
背景技术
在热轧薄板厂检修更换了支承辊、工作辊后,开轧时,轧机的调平值很难不确定,极易出现浪形,严重时,头部出现轧烂或甩钢现象。同样,每班换工作辊后,也出现此类问题。在支承辊不变的条件下,操作工可根据上一套辊的调平值,根据经验进行调平,但是因各机架阶梯垫使用不一样,所以各机架的调平值变化也较大。所以,每次换辊后,开轧极不稳定,对操作工来说,难度较大,极易出现头部轧烂或甩钢现象。
梅山宝钢1422和攀钢1450厂,其在更换支承辊后,机架内进行压铜棒试验,根据两侧的厚度差对轧机水平值进行预调。此种方法大部分能反应出轧机的走向。但是当机架内辊系存在磨擦力较大或者辊系不实时,由于铜棒的压下量较小,也不能反应出卷板的真实走向。
发明内容
本发明的目的是提供一种热轧薄板开轧预调法,利用传感器两侧轧制力偏差, 计算调平值,解决背景技术存在的上述问题。
本发明的技术方案为:热轧薄板开轧预调法,压力传感器对上辊压力进行检测,测压头对下辊压力进行检测,调平直=(20%-40%)*传感器两侧轧制力偏差,传感器两侧轧制力偏差大于50T时,选用40%,小于50T时,选用20%。
本发明的积极效果是:能够减小了开轧时操作难度,确保开轧时的头部板形,同时大大减少了开轧时因预调错误而导致得头部轧烂,避免产生二级品和废钢。本发明局部科学性,节约成本和时间,提高经济效益。
 
具体实施方式
下面通过实施例对本发明做进一步说明。
压力传感器为上辊压力检测,测压头为下辊压力检测。在标定过程中,压力传感器与测压头均进行压力检测,标定过程中使用测压头时,压力传感器同时进行受力及位置检测。测压头在标定时检测下辊压力检测时,压力传感器从上辊进行压力检测,会出现两侧不同的受力情况。当测压头两侧均为500T力时,而传感器轧制力出现偏差。根据两侧传感器轧制力偏差对辊缝进行预调,传动侧力大时,说明标定时传动辊缝侧压下较多,需将传动侧辊缝抬起;操作侧力大时,需抬起操作侧辊缝。调平直=(20%—40%)*传感器两侧轧制力偏差(DS—OS),传感器两侧轧制力偏差大于50T时,选用40%,小于50T时,选用20%。当偏差力在20T以内时,操作工可不做调整。如果轧制力偏差约为+60T。按照分析估量应在+12―+24,操作工预调先将调平值使用16,随后轧制稳定时使用20。
极特殊情况,会出现压力传感器检测的轧制力偏差与调平值相反或较大时,出现误差此时可反映出由于相关的设备出现问题,造成标定异常。需要着重检查当前的阶梯垫或者下支承辊犯卡,避免事故进一步扩大。
如果两侧传感器力差很小,但DS-OS的辊缝随着轧制力增加而出现偏移,通过现场检查设备,发现当前阶梯垫出现松动,坚固后正常轧制。

Claims (1)

1.一热轧薄板开轧预调法,其特征在于压力传感器对上辊压力进行检测,测压头对下辊压力进行检测,调平直=(20%-40%)*传感器两侧轧制力偏差,传感器两侧轧制力偏差大于50T时,选用40%,小于50T时,选用20%。
CN2012100163404A 2012-01-19 2012-01-19 热轧薄板开轧预调法 Pending CN102553915A (zh)