[go: up one dir, main page]

CN101461616B - Kitchen cabinet decorative plate and manufacturing method thereof - Google Patents

Kitchen cabinet decorative plate and manufacturing method thereof Download PDF

Info

Publication number
CN101461616B
CN101461616B CN2007101916994A CN200710191699A CN101461616B CN 101461616 B CN101461616 B CN 101461616B CN 2007101916994 A CN2007101916994 A CN 2007101916994A CN 200710191699 A CN200710191699 A CN 200710191699A CN 101461616 B CN101461616 B CN 101461616B
Authority
CN
China
Prior art keywords
glass
surface layer
basic unit
interlayer
decorative
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2007101916994A
Other languages
Chinese (zh)
Other versions
CN101461616A (en
Inventor
张春耉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHENJIANG YOUYUAN DECORATION DESIGN ENGINEERING Co Ltd
Original Assignee
ZHENJIANG YOUYUAN DECORATION DESIGN ENGINEERING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHENJIANG YOUYUAN DECORATION DESIGN ENGINEERING Co Ltd filed Critical ZHENJIANG YOUYUAN DECORATION DESIGN ENGINEERING Co Ltd
Priority to CN2007101916994A priority Critical patent/CN101461616B/en
Publication of CN101461616A publication Critical patent/CN101461616A/en
Application granted granted Critical
Publication of CN101461616B publication Critical patent/CN101461616B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

A cabinet decorative panel and manufacturing method thereof, pertains to the architecture interior decoration plate material and its making method, and is principally used for the production of the cabinet panels. The prior paint-baking decorative plate, whose surface is exposed to the air, not only emits harmful toxic substances to pollute the environment; but also has poor anti-aging properties and its surface often lose its decorative effect in a few years after oxidation, and can not avoid scratches and chemical stains. The invention is characterized in that the cabinet decorative panel is composed by integrating by compounding a glass surface and a decorative sandwich layer on its interior surface with a woody base layer, and then sealing its outer edge by a protective frame; the manufacturing method includes: selecting and cutting of the glass surface and the processing of the inner surface - the coating baking of the decorative sandwich layer - selecting and cutting of the woody base and the processing of the back face - gluing and laminating wit the decorative sandwich layer - gluing and sealing of the protective frame with the outer edge. As shown by the trial, the invention has the following advantages: high environmental safety, good anti-aging properties, and capability of not only withstanding the scratches and collisions of sharp hard object but also preventing the emergence of chemical stains.

Description

A kind of kitchen cabinet decorative plate and manufacture method thereof
Technical field: the present invention relates to building interior decorative boards and manufacture method thereof, particularly a kind of kitchen cabinet decorative plate and manufacture method thereof.
Technical background: in the existing building interior decorative boards, particularly the cabinet decorative sheet mainly uses paint-baking decorative plate.The combination with decorative surfaces of this paint-baking decorative plate exposes in air, constantly gives out poisonous and hazardous material on the one hand, pollute indoor environment, thereby Environmental Safety is low; Loss of properties on aging on the other hand, its combination with decorative surfaces be through the particularly oxidation of kitchen internal contamination gas of air, and be often aging and lose decorative effect in the several years.In addition, the baking vanish combination with decorative surfaces is if running into sharp-pointed hard thing draws and bump, the light then cut that can't remedy of appearance easily, and weighing slightly then causes damage, even peels off and come off; If run into can with the chemical industry pollutant matter of baking vanish generation chemical reaction, variable color gently then occurs, fade, heavy then dissolve fully and expose substrate.This shows that design a kind of Environmental Safety height, ageing-resistant performance is good, and resisting sharp-pointed hard thing, to draw kitchen cabinet decorative plate and the manufacture method thereof of bumping, prevent chemical spot be necessary.
Summary of the invention: the objective of the invention is to overcome the deficiencies in the prior art, design a kind of Environmental Safety height, ageing-resistant performance is good, and can resist sharp-pointed hard thing and draw kitchen cabinet decorative plate and the manufacture method thereof of bumping, prevent chemical spot.
The object of the present invention is achieved like this: a kind of kitchen cabinet decorative plate and manufacture method thereof, it is characterized in that by surface layer of glass, and be positioned at the decoration interlayer of surface layer of glass inner surface, with surface layer of glass and decorate the interlayer whole wooden basic unit that is composited, the frame that protects that is packaged on its whole outer perimeter after compound constitutes; The technology characteristics of its manufacture method comprises: selecting materials of A. surface layer of glass cuts and inner surface treatment, B. decorate the spraying baking of interlayer, C. the select materials sawing and the back side processing of wooden basic unit, D. surface layer of glass and decoration interlayer and the bonding of wooden basic unit press solidly, and E. protects the bonding sealing-in of the whole outer perimeter of frame and compound back.
Described surface layer of glass is selected materials and is cut and inner surface treatment is: select plate glass for use, adopt common process to cut size and reservation cabinet grip hole according to user's needs specification, use its inner surface of glass scavenger specially wiping, the removal of contamination spot is divided the clock time drying through 10-15 under the normal temperature.The spraying baking of described decoration interlayer is: coat with lacquer the modifier that cooperates through the inner surface spraying earlier of cleaning treatment with glass at surface layer of glass, at normal temperatures after 5-15 divides the clock time drying, adopt common process spraying PU glass lacquer (weight proportion is a host: curing agent: diluent=1: 0.5: 0.4-0.6) or the expoxy glass lacquer (weight proportion is a host: curing agent: diluent=4: 1: 2) in the inner surface of surface layer of glass, after keeping 15-30 to divide the clock time drying under 25 ℃ of temperature, move on to again in the drying room at 50-80 ℃ of following low temperature drying or at normal temperatures through air dry in 24-48 hour.The described decoration interlayer that is positioned at the surface layer of glass inner surface can be made of the above-mentioned glass lacquer of selecting for use various colors with the bronze that mixes special impression effect, silver powder, seven color powder, pearl essence, glomerocryst powder, radium-shine powder according to user's request.Such design had both kept colourful decoration functions such as the color, texture, texture of glass lacquer itself, can make the transparent characteristic of glass and ornamental the combining of glass lacquer again, thereby strengthen decorative effect of the present invention.Select materials sawing and the back side of described wooden basic unit are handled and are: the little proportion wooden boards of selecting for use drying to handle, and one of them is as the China fir plate; Adopt common process sawing moulding according to the specification of user's needs, adopt common process to play putty and wipe off at its back side, treated under the normal temperature air dry 12-24 hour, or keep down polishing flat with rubber behind the low temperature drying in 1-3 hour at 30-50 ℃; Adopt common process then, paste with the PVC adhesive glue and go up the PVC cosmetic sheet of selecting for use according to user's needs, the back side of cosmetic sheet and wooden basic unit is combined into one through press quenching.Bonding the pressing solidly of described surface layer of glass and decoration interlayer and wooden basic unit is: select neutral silicone mildew-resistant weather-resistant glue for use, adopt common process evenly to embrocate behind the front of wooden basic unit, surface layer of glass and decoration interlayer are lain against on the front of wooden basic unit, rub gently to press the air between its joint portion all discharged, under the normal temperature through 10-15 hour cure under pressure.Such design had both guaranteed that the poisonous and hazardous material that glass lacquer, adhesive glue are contained was sealed by surface layer of glass, prevented to be dispersed in the air, had improved the impact strength of surface layer of glass again, was enough to resist drawing of sharply hard thing and bumped and general impact.The described bonding sealing-in of protecting the whole outer perimeter of frame and compound back is: at surface layer of glass and decorate interlayer, the wooden basic unit whole outer perimeter in compound back is evenly embrocated neutral silicone mildew-resistant weather-resistant glue, according to specification aluminium alloy or the stainless steel or the plastic shaping thin plate of user's needs, adopt conventional cutting, wrapping process sealing-in to become to protect frame.Such design had both increased the overall aesthetics of kitchen cabinet decorative plate, had prevented further that again the poisonous and hazardous material that glass lacquer, adhesive glue are contained from spilling into the air from whole outer perimeter, also improved waterproof, the fungicidal properties of kitchen cabinet decorative plate.
This kitchen cabinet decorative plate that the invention process obtains has shown following advantage in trying out:
1, Environmental Safety height.Expose in air different with the baking vanish combination with decorative surfaces of prior paint-baking decorative plate, the poisonous and hazardous material that glass coats with lacquer in the present invention, adhesive glue contained is sealed by surface layer of glass, its whole outer perimeter is protected the frame sealing-in again, prevented that preferably poisonous and hazardous material to airborne loss, has increased substantially Environmental Safety.2, ageing-resistant performance is good.Adopt glass lacquer for decorating interlayer among the present invention with rich and varied decoration function; completely cut off with air by skin glass institute's close and protect; air is almost nil to the oxidation of decorating interlayer; the ageing-resistant performance of surface layer of glass is good in addition; therefore compare with prior paint-baking decorative plate; degree of aging reduces significantly, and prolong service life significantly.And, the transparency of glass is combined with the ornamental of baking vanish, utilize varied and colorful glass lacquer seeing through under the effect of light of glass, the light sensation effect that presents by various colors, texture, texture, produce abundant vision change, thereby further strengthened decorative effect.3, can either resist sharp-pointed hard thing and draw and bump, prevent the appearance of chemical spot again.Decorate the inner surface that interlayer is positioned at surface layer of glass among the present invention, again because adopt adhesive to make surface layer of glass, decoration interlayer, wooden basic unit be combined into integral body, thereby improved the impact strength of surface layer of glass, the surface layer of glass of having reinforced can avoid sharp-pointed hard thing to decorating the general impact of bumping and resist hard thing of drawing of interlayer fully.Secondly, well-known, glass can show very high chemical stability to most chemical substances, is enough to stop the appearance of general chemistry spot.
Description of drawings: Fig. 1 is the schematic diagram that meets the subject matter structure.
The specific embodiment: implementation detail of the present invention is described as follows below in conjunction with accompanying drawing:
As shown in Figure 1, a kind of kitchen cabinet decorative plate and manufacture method thereof, it is characterized in that by surface layer of glass (1), and be positioned at the decoration interlayer (2) of surface layer of glass inner surface, with surface layer of glass and decorate the interlayer whole wooden basic unit (3) that is composited, the frame (4) that protects that is packaged on its whole outer perimeter after compound constitutes; The technology characteristics of its manufacture method comprises: selecting materials of A. surface layer of glass cuts and inner surface treatment, B. decorate the spraying baking of interlayer, C. the select materials sawing and the back side processing of wooden basic unit, D. surface layer of glass and decoration interlayer and the bonding of wooden basic unit press solidly, and E. protects the bonding sealing-in of the whole outer perimeter of frame and compound back.
Described surface layer of glass (1) is selected materials and is cut and inner surface treatment is: select plate glass for use, adopt common process to cut size and reservation cabinet grip hole according to user's needs specification, use its inner surface of glass scavenger specially wiping, the removal of contamination spot is divided the clock time drying through 10-15 under the normal temperature.
The spraying of described decoration interlayer (2) baking is: at surface layer of glass on the inner surface of cleaning treatment, the modifier that spraying earlier cooperates with the glass lacquer, at normal temperatures after 5-15 divides the clock time drying, adopt common process spraying PU glass lacquer (weight proportion is a host: curing agent: diluent=1: 0.5: 0.4-0.6) or the expoxy glass lacquer (weight proportion is a host: curing agent: diluent=4: 1: 2), after keeping 15-30 to divide the clock time drying under 25 ℃ of temperature, move on to again in the drying room at 50-80 ℃ of following low temperature drying or at normal temperatures through air dry in 24-48 hour.
Select materials sawing and the back side of described wooden basic unit (3) are handled and are: the little proportion wooden boards of selecting for use drying to handle, and one of them is as the China fir plate; Adopt common process sawing moulding according to user's needs specification, adopt common process to play putty and wipe off at its back side, treated under the normal temperature air dry 12-24 hour, or keep down polishing flat with rubber behind the low temperature drying in 1-3 hour at 30-50 ℃; Adopt common process then, paste with the PVC adhesive glue and go up the PVC cosmetic sheet of selecting for use according to user's needs, the back side of cosmetic sheet and wooden basic unit is combined into one through press quenching.
Described surface layer of glass (1) and decoration interlayer (2) with bonding the pressing solidly of wooden basic unit (3) are: select neutral silicone mildew-resistant weather-resistant glue for use, adopt common process evenly to embrocate behind the front of wooden basic unit, surface layer of glass and decoration interlayer are lain against on the front of wooden basic unit, rub gently to press the air between its joint portion all discharged, under the normal temperature through 10-15 hour mechanical cure under pressure.
The described bonding sealing-in of protecting the whole outer perimeter of frame and compound back is: at surface layer of glass (1) and decorate interlayer (2), wooden basic unit (3) the whole outer perimeter in compound back adopts common process evenly to embrocate neutral silicone mildew-resistant weather-resistant glue, according to specification aluminium alloy or the stainless steel or the plastic shaping thin plate of user's needs, adopt conventional cutting, wrapping process sealing-in to become to protect frame.
In the enforcement, plate glass and scavenger specially, glass lacquer and cooperate modifier, protects frame material and adhesive gum special is all chosen from market at wooden boards and adhesive gum special, PVC cosmetic sheet and adhesive gum special, adopts corresponding common process specifically to implement.
The kitchen cabinet decorative plate that the invention process obtains is mainly used in the panel of making cabinet, also can be used in other occasions of indoor decoration.

Claims (1)

1. kitchen cabinet decorative plate manufacture method, wherein kitchen cabinet decorative plate by surface layer of glass (1), be positioned at the surface layer of glass inner surface decoration interlayer (2), with surface layer of glass and decorate interlayer be composited whole wooden basic unit (3) and be packaged on its whole outer perimeter after compound protect frame (4) formation, it is characterized in that:
Described kitchen cabinet decorative plate manufacture method may further comprise the steps: selecting materials of A. surface layer of glass cuts and inner surface treatment, B. decorate the spraying baking of interlayer, C. the select materials sawing and the back side processing of wooden basic unit, D. surface layer of glass and decoration interlayer and the bonding of wooden basic unit press solidly, and E. protects the bonding sealing-in of the whole outer perimeter of frame and compound back;
Particularly, described surface layer of glass is selected materials and is cut and inner surface treatment is: select plate glass for use, adopt common process to cut size and reservation cabinet grip hole according to user's needs specification, use its inner surface of glass scavenger specially wiping, the removal of contamination spot is divided the clock time drying through 10-15 under the normal temperature;
The spraying of described decoration interlayer baking is: at surface layer of glass on the inner surface of cleaning treatment, the modifier that spraying earlier cooperates with the glass lacquer, at normal temperatures after 5-15 divides the clock time drying, adopt common process spraying PU glass lacquer or expoxy glass lacquer, the weight proportion of described glass lacquer is a host: curing agent: diluent=1: 0.5: 0.4-0.6, the weight proportion of described expoxy glass lacquer is a host: curing agent: diluent=4: 1: 2, earlier after keeping 15-30 to divide the clock time drying under 25 ℃ of temperature, move on to again in the drying room in 50-80 ℃ of following low temperature drying or air dry under 24-48 hour normal temperature; The described decoration interlayer that is positioned at the surface layer of glass inner surface uses various colors and mixes the glass lacquer of the bronze of special impression effect, silver powder, seven color powder, pearl essence, glomerocryst powder, radium-shine powder;
Select materials sawing and the back side of described wooden basic unit are handled and are: the China fir plate of selecting for use drying to handle; Adopt common process sawing moulding according to user's needs specification, adopt common process to play putty and wipe off at its back side, treated under the normal temperature air dry 12-24 hour, or keep down polishing flat with rubber behind the low temperature drying in 1-3 hour at 30-50 ℃; Paste with the PVC adhesive glue then and go up the PVC cosmetic sheet of selecting for use according to user's needs, the back side of cosmetic sheet and wooden basic unit is combined into one through press quenching;
Bonding the pressing solidly of described surface layer of glass and decoration interlayer and wooden basic unit is: select neutral silicone mildew-resistant weather-resistant glue for use, adopt common process evenly to embrocate behind the front of wooden basic unit, surface layer of glass and decoration interlayer are lain against on the front of wooden basic unit, rub gently to press the air between its joint portion all discharged, under the normal temperature through 10-15 hour cure under pressure;
The described bonding sealing-in of protecting the whole outer perimeter of frame and compound back is: at surface layer of glass (1) and decorate interlayer (2), wooden basic unit (3) the whole outer perimeter in compound back, adopt common process evenly to embrocate neutral silicone mildew-resistant weather-resistant glue, according to specification aluminium alloy or the stainless steel or the plastic shaping thin plate of user's needs, adopt conventional cutting, wrapping process sealing-in to become to protect frame.
CN2007101916994A 2007-12-17 2007-12-17 Kitchen cabinet decorative plate and manufacturing method thereof Expired - Fee Related CN101461616B (en)