CN101235447A
CN101235447A CNA2007100343393A CN200710034339A CN101235447A CN 101235447 A CN101235447 A CN 101235447A CN A2007100343393 A CNA2007100343393 A CN A2007100343393A CN 200710034339 A CN200710034339 A CN 200710034339A CN 101235447 A CN101235447 A CN 101235447A
Authority
CN
China
Prior art keywords
alloy
carbon
copper
carbon composite
less
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CNA2007100343393A
Other languages
English (en)
Other versions
CN100537803C (zh
Inventor
张福勤
方勋华
于澍
宋旼
袁铁锤
黄伯云
熊翔
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Central South University
Original Assignee
Central South University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Central South University filed Critical Central South University
Priority to CNB2007100343393A priority Critical patent/CN100537803C/zh
Publication of CN101235447A publication Critical patent/CN101235447A/zh
Application granted granted Critical
Publication of CN100537803C publication Critical patent/CN100537803C/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Manufacture Of Metal Powder And Suspensions Thereof (AREA)
  • Powder Metallurgy (AREA)

Abstract

一种炭/炭复合材料与铜连接用合金,合金元素重量百分比为Cu 50%~90%,Cr 1%~20%,Ti 0%~20%, Ni 0%~30%,Zr 1%~20%,Mn 2%~20%。将上述原料配制,在1500~1700℃、小于10Pa的真空度下感应熔炼、浇铸成锭;采用气体雾化制粉方法,在1500~1700℃、小于10Pa的真空度下,将合金铸锭重熔、制粉;将合金粉末筛选分级。本发明的连接用合金对炭/炭复合材料和铜均具有好的化学和物理相容性。

Description

炭/炭复合材料与铜连接用合金及其制备工艺
技术领域
本发明涉及一种异质材料连接用合金,特别是一种炭/炭复合材料与铜连接用合金。
背景技术
炭/炭复合材料是一种以炭纤维增强炭基体的先进复合材料,具有耐高温、抗辐射、耐腐蚀等优异性能。铜是一种金属材料,具有高导热、导电等性能。如果能够制备出两者的连接件,使之兼具炭/炭复合材料和铜的优异性能,则将拓宽炭/炭复合材料在航空航天、核能、化工等领域的应用范围。
焊接是实现炭/炭复合材料与铜连接的优选方案,但首先必需解决两个关键问题。其一是炭/炭复合材料与铜的润湿性。根据相关理论,要实现可靠连接,金属对炭的润湿角必须小于90度。但铜为140度,不经特殊处理无法实现连接;其次是炭/炭复合材料与铜之间热膨胀的差异。与铜相比,炭/炭复合材料的热膨胀系数小一个数量级,且呈明显的各向异性。在温变过程中,这种差异引致的连接界面热应力集中,将可能引起界面剥离、脱离,最终导致连接失效。
发细内容
本发明的目的是提供一种连接用合金及其制备方法,改进炭/炭复合材料与铜之间润湿性和热膨胀匹配。
本发明采用的技术方案如下:
1、炭/炭复合材料与铜连接用合金,其合金元素重量百分比如下:
Cu 50%~90%,Cr 1%~20%,Ti 0%~20%,Ni 0%~30%Zr 1%~20%,Mn 2%~20%
2、连接用合金的制备方法,包括如下步骤:
1)按合金元素重量百分比:Cu 50%~90%、Cr 1%~20%、Ti 0%~20%、Ni 0%~30%、Zr 1%~20%、Mn 2%~20%配制合金原料;
2)在1500~1700℃、小于10Pa的真空度下感应熔炼、浇铸成锭;
3)采用气体雾化制粉方法,在1500~1700℃、小于10Pa的真空度下,将合金铸锭重熔、制粉;
4)将合金粉末筛选分级。
本发明具有如下优点和积极效果:
加入Cr、Ti、Ni等碳化物生成元素,改善连接合金对炭/炭复合材料的润湿性。加Zr元素,降低连接合金的热膨胀系数。加Cu、Mn元素,降低连接合金的熔化温度,提高连接合金的延展性能,有利于连接界面热应力的松弛。真空感应熔铸+气体雾法制粉方法,确保合金成分的均匀性。本发明的连接用合金对炭/炭复合材料和铜均具有好的化学和物理相容性。
具体实施方式
下面本发明的进行具体的描述:
实施例1
首先,按重量百分比:Cu 51%、Cr 19%、Ti 11%、Zr 1%、Mn 18%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。
实施例2
首先,按重量百分比:Cu 60%、Cr 1%、Ni 26%、Zr 8%、Mn 5%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。
实施例3
首先,按重量百分比:Cu 60%、Cr 1%、Ti 19%、Zr 18%、Mn 2%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。
实施例4
首先,按重量百分比:Cu 71%、Cr 5%、Ti 2%、Zr 12%、Mn 10%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。
实施例5
首先,按重量百分比:Cu 73%、Cr 2%、Ni 14%、Zr 9%、Mn 2%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。
实施例6
首先,按重量百分比:Cu 87%、Cr 10%、Zr 1%、Mn 2%配制成合金原料。其次,将合金原料置于真空感应加热炉内,在1500~1700℃、小于10Pa的真空度下熔炼、浇铸成锭。再次,将铸锭置于气体雾化制粉装置中,在1500~1700℃、小于10Pa的真空度下重熔、制粉。最后,将制得的合金粉末筛选分级。

Claims (3)

1. 炭/炭复合材料与铜连接用合金,其特征在于:合金元素重量百分比为Cu 50%~90%,Cr 1%~20%,Ti 0%~20%,Ni 0%~30%,Zr 1%~20%,Mn 2%~20%。
2. 根据权利要求1所述的炭/炭复合材料与铜连接用合金,其特征在于:合金元素重量百分比:Cu 60%、Cr 1%、Ti 19%、Zr 18%、Mn 2%。
3. 根据权利要求1所述的炭/炭复合材料与铜连接用合金的制备工艺,其特征在于包括以下步骤:
1)配制合金原料;
2)在1500~1700℃、小于10Pa的真空度下感应熔炼、浇铸成锭;
3)采用气体雾化制粉方法,在1500~1700℃、小于10Pa的真空度下,将合金铸锭重熔、制粉;
4)将合金粉末筛选分级。
CNB2007100343393A 2007-01-29 2007-01-29 炭/炭复合材料与铜连接用合金及其制备工艺 Expired - Fee Related CN100537803C (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CNB2007100343393A CN100537803C (zh) 2007-01-29 2007-01-29 炭/炭复合材料与铜连接用合金及其制备工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CNB2007100343393A CN100537803C (zh) 2007-01-29 2007-01-29 炭/炭复合材料与铜连接用合金及其制备工艺

Publications (2)

Publication Number Publication Date
CN101235447A true CN101235447A (zh) 2008-08-06
CN100537803C CN100537803C (zh) 2009-09-09

Family

ID=39919351

Family Applications (1)

Application Number Title Priority Date Filing Date
CNB2007100343393A Expired - Fee Related CN100537803C (zh) 2007-01-29 2007-01-29 炭/炭复合材料与铜连接用合金及其制备工艺

Country Status (1)

Country Link
CN (1) CN100537803C (zh)

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106048294A (zh) * 2016-07-21 2016-10-26 安徽旭晶粉体新材料科技有限公司 一种二次水雾法制备含铬的铜合金粉
CN106736030A (zh) * 2016-12-26 2017-05-31 中南大学 一种焊料及其在焊接C/SiC复合材料和金属中的应用方法
CN109290697A (zh) * 2018-08-15 2019-02-01 中南大学 一种钎焊c/c复合材料的活性钎料及其制备方法和应用
CN113134693A (zh) * 2021-04-30 2021-07-20 吉林大学 一种钎焊钨基粉末合金的Cu基非晶态钎料及其制备方法和应用
CN114592141A (zh) * 2022-03-10 2022-06-07 中机智能装备创新研究院(宁波)有限公司 一种钻头胎体用浸渍合金及其制备方法和应用
CN114952077A (zh) * 2022-04-14 2022-08-30 天诺光电材料股份有限公司 一种复合钎焊膏及其制备方法和应用

Family Cites Families (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3712837A (en) * 1971-11-05 1973-01-23 Olin Corp Process for obtaining copper alloys

Cited By (7)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106048294A (zh) * 2016-07-21 2016-10-26 安徽旭晶粉体新材料科技有限公司 一种二次水雾法制备含铬的铜合金粉
CN106736030A (zh) * 2016-12-26 2017-05-31 中南大学 一种焊料及其在焊接C/SiC复合材料和金属中的应用方法
CN106736030B (zh) * 2016-12-26 2019-05-17 中南大学 一种焊料在焊接C/SiC复合材料和金属中的应用方法
CN109290697A (zh) * 2018-08-15 2019-02-01 中南大学 一种钎焊c/c复合材料的活性钎料及其制备方法和应用
CN113134693A (zh) * 2021-04-30 2021-07-20 吉林大学 一种钎焊钨基粉末合金的Cu基非晶态钎料及其制备方法和应用
CN114592141A (zh) * 2022-03-10 2022-06-07 中机智能装备创新研究院(宁波)有限公司 一种钻头胎体用浸渍合金及其制备方法和应用
CN114952077A (zh) * 2022-04-14 2022-08-30 天诺光电材料股份有限公司 一种复合钎焊膏及其制备方法和应用

Also Published As

Publication number Publication date
CN100537803C (zh) 2009-09-09

Similar Documents

Publication Publication Date Title
CN101235447A (zh) 炭/炭复合材料与铜连接用合金及其制备工艺
CN106222582B (zh) 一种提高轴承钢表面耐腐蚀性的方法
CN100460541C (zh) 复合强化耐热钛合金
CN100516272C (zh) 一种高电阻率高导磁马氏体-铁素体双相不锈钢及其热处理工艺
CN105081597A (zh) 用于钎焊W-Cu复合材料与Fe基合金的钎料及方法和钎焊工艺
CN110355496B (zh) 一种可用于γ-TiAl合金的耐高温焊料及钎焊工艺
CN101367159A (zh) 一种Cu-P基非晶钎料及其制备方法
CN113403555B (zh) 通过热变形工艺改善硅化物增强难熔高熵合金性能的方法
CN101333610A (zh) 超高强、高导电CuNiSi系弹性铜合金及其制备方法
CN108326302A (zh) 一种石墨烯增强铝合金材料及其制备方法
CN108947558A (zh) 一种金属与Ti3SiC2陶瓷的连接方法
CN104232955B (zh) 一种Cu-Cr-FeC复合材料的制备方法
CN101805861B (zh) 一种高压电力线路金具用耐蚀铝合金及制备方法
CN104087876B (zh) 金属玻璃/石墨烯复合材料的制备方法
CN108396335A (zh) 铝电解用金属陶瓷基惰性阳极与导杆连接结构及制备方法
CN105624583B (zh) 一种超高强度钢材及其制备方法
CN105603252B (zh) 一种基于调幅分解的铜镍合金作为强化恒电阻率合金的应用
CN110846596A (zh) 一种Wf/W合金-金刚石复合材料及其制备方法
CN100506461C (zh) 用于颗粒增强铝基复合材料的熔化焊填充焊剂的焊丝
CN101920409B (zh) 一种用于Cf/SiC复合材料钎焊的钯铜金基高温钎料
CN104357712A (zh) 铝合金材料及制备方法
CN102534299B (zh) 无铍多元铜合金
CN103343259A (zh) 高温高耐压铜合金导电材料
CN102002649B (zh) 高强韧镁基块体金属玻璃复合材料及其制备方法
CN106636985A (zh) 一种金属玻璃复合材料及其制备方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
EE01 Entry into force of recordation of patent licensing contract

Assignee: Changsha Heng Heng mechanical and Electrical Equipment Co., Ltd.

Assignor: Central South University

Contract record no.: 2011430000204

Denomination of invention: Alloy for connecting carbon/carbon composite material and copper, and preparation technique thereof

Granted publication date: 20090909

License type: Exclusive License

Open date: 20080806

Record date: 20111008

CF01 Termination of patent right due to non-payment of annual fee

Granted publication date: 20090909

Termination date: 20130129