CN101164746A - Environmental protection regenerative wood residual density board and preparation method thereof - Google Patents
Environmental protection regenerative wood residual density board and preparation method thereof Download PDFInfo
- Publication number
- CN101164746A CN101164746A CNA2006100691768A CN200610069176A CN101164746A CN 101164746 A CN101164746 A CN 101164746A CN A2006100691768 A CNA2006100691768 A CN A2006100691768A CN 200610069176 A CN200610069176 A CN 200610069176A CN 101164746 A CN101164746 A CN 101164746A
- Authority
- CN
- China
- Prior art keywords
- sanding
- density board
- glue
- leftover bits
- parts
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The present invention provides an environment-protecting regenerated wood residue density board and its preparation method. It is made up by using (by weight portion) 20-35 portions of main raw material, 5-15 portions of primary density board sand-grinding powder and 3-10 portions of urea-formaldehyde glue through a certain preparation process. The above-mentioned main raw material is the offcut waste material obtained by producing veneer board, including one of sawdust, wood shavings, tree bark and cotton stalk or mixture of more than two kinds of them.
Description
1, technical field
The present invention relates to a kind of technology of preparing of artificial building board, specifically a kind of environmental protection regenerative wood residual density board and preparation method thereof.
2, background technology
In the building board production process of prior art, can produce a large amount of leftover bits after needing to be sawn into the size of regulation behind the pressboard, thereby produce a large amount of industrial refuses environment is caused severe contamination, handle then can produce large quantity of exhaust gas, can pollute air equally if burn.Good solution is not also arranged at present.
3, summary of the invention
The purpose of this invention is to provide a kind of environmental protection regenerative wood residual density board to leftover bits reuse again and preparation method thereof.
The objective of the invention is to realize in the following manner, environmental protection regenerative wood residual density board is to be made by following materials of weight proportions: main material 20-35 part; Primary density board sanding powder 5-15 part; Urine aldehyde glue 3-10 part, wherein main material is the leftover bits of plywood production; Sawdust; Wood shavings; The composition of one or more in bark, the cotton stalk;
Preparation process is as follows:
The first step: pulverize, the bulk material is ground into the 0.5-1mm granularity with the powder machine;
The 3rd step: oven dry, adding dryers such as good material of powder and saw foam are dried, again sanding powder is dried 5-25 minute baking needed time separately;
The 3rd step: glue mixing, in the oven dry material, add urine aldehyde glue, material glue ratio is 25: 4, it is standby to stir, and adds urine aldehyde glue in sanding powder, Ratio of filler bitumen 10: 1, it is standby to stir;
The 4th step: bed board, four ribs are placed on the steel plate, form a groove, the sanding powder of glue mixing is evenly spread one deck on steel plate, evenly spread the wooden slag of one deck glue mixing again, the superiors repave the sanding powder of one deck glue mixing, with dry plate its slight pressing, put steel plate, repeat above method, repave second, the 3rd, the 4th ... the number of shop meets the pressing machine and meets;
The 5th the step: the steel plate of the centre being completed sizing material pushes the pressing machine, controlled pressure 20-40 atmospheric pressure,, temperature is controlled at 90 ℃-110 ℃, suppresses to get final product ejecting plate in 20-4O minute;
The 6th step: saw the limit behind the ejecting plate, burr around half-finished are amputated, make standard-sized semi-finished product with Sawing machine;
The 7th step: sanding, with sander the sanding processing being carried out on half-finished surface is finished product.
4, embodiment
Embodiment 1
Prescription: 25 parts of main materials; 12 parts of primary density board sanding powders; 8 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; Sawdust; The mixture of wood shavings; The leftover bits of plywood production; Sawdust; The charge ratio of wood shavings is 1: 1: 1.
Preparation process is as follows:
The first step: pulverize, the bulk material is ground into the 0.5-1mm granularity with the powder machine;
The 3rd step: oven dry, adding dryers such as good material of powder and saw foam are dried, again sanding powder is dried 5-25 minute baking needed time separately;
The 3rd step: glue mixing, in the oven dry material, add urine aldehyde glue, material glue ratio is 25: 4, it is standby to stir, and adds urine aldehyde glue in sanding powder, Ratio of filler bitumen 10: 1, it is standby to stir;
The 4th step: bed board, four ribs are placed on the steel plate, form a groove, the sanding powder of glue mixing is evenly spread one deck on steel plate, evenly spread the wooden slag of one deck glue mixing again, the superiors repave the sanding powder of one deck glue mixing, with dry plate its slight pressing, put steel plate, repeat above method, repave second, the 3rd, the 4th ... the number of shop meets the pressing machine and meets;
The 5th the step: the steel plate of the centre being completed sizing material pushes the pressing machine, controlled pressure 20-40 atmospheric pressure,, temperature is controlled at 90 ℃-110 ℃, suppresses to get final product ejecting plate in 20-40 minute;
The 6th step: saw the limit behind the ejecting plate, burr around half-finished are amputated, make standard-sized semi-finished product with Sawing machine;
The 7th step: sanding, with sander the sanding processing being carried out on half-finished surface is finished product.
Embodiment 2
Prescription: 30 parts of main materials; 12 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; Sawdust; The mixture of cotton stalk; The leftover bits of plywood production; The charge ratio of sawdust and cotton stalk is 2: 1: 0.5.
The preparation method is identical with embodiment 1.
Embodiment 3
Prescription: 33 parts of main materials; 15 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; The mixture of bark and cotton stalk; The leftover bits of plywood production; The charge ratio of bark and cotton stalk is 2: 1: 1.
The preparation method is identical with embodiment 1.
Embodiment 4
Prescription: 35 parts of main materials; 15 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; The mixture of bark and wood shavings; The leftover bits of plywood production; The charge ratio of bark and wood shavings is 2: 1: 1.
The preparation method is identical with embodiment 1.
Embodiment 5
Prescription: 35 parts of main materials; 15 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; Sawdust; Wood shavings; The mixture of bark, cotton stalk, the leftover bits of plywood production; Sawdust; Wood shavings; The batch mixing ratio of bark, cotton stalk is 1: 1: 1: 1: 1.
The preparation method is identical with embodiment 1.
Embodiment 6
Prescription: 20 parts of main materials; 5 parts of primary density board sanding powders; 3 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; The mixture of sawdust, the leftover bits of plywood production and sawdust batch mixing ratio are 1: 1:.
The preparation method is identical with embodiment 1.
The characteristics of this product: this product has firm, the surface smoothing of density board, the characteristics such as aesthetic in appearance, Have again the characteristics such as low price, the production process of wooden slag plate, particieboard be simple, and environmental protection, no waste material Discharging has good value for applications.
Claims (5)
1. environmental protection regenerative wood residual density board is characterized in that, it is to be made by following materials of weight proportions: main material 20-35 part; Primary density board sanding powder 5-15 part; Urine aldehyde glue 3-10 part, wherein main material is the leftover bits of plywood production; Sawdust; Wood shavings; The composition of one or more in bark, the cotton stalk;
2. the preparation method of environmental protection regenerative wood residual density board is characterized in that preparation process is as follows:
The first step: pulverize, the bulk material is ground into the 0.5-1mm granularity with the powder machine;
The 3rd step: oven dry, adding dryers such as good material of powder and saw foam are dried, again sanding powder is dried 5-25 minute baking needed time separately;
The 3rd step: glue mixing, in the oven dry material, add urine aldehyde glue, material glue ratio is 25: 4, it is standby to stir, and adds urine aldehyde glue in sanding powder, Ratio of filler bitumen 10: 1, it is standby to stir;
The 4th step: bed board, four ribs are placed on the steel plate, form a groove, the sanding powder of glue mixing is evenly spread one deck on steel plate, evenly spread the wooden slag of one deck glue mixing again, the superiors repave the sanding powder of one deck glue mixing, with dry plate its slight pressing, put steel plate, repeat above method, repave second, the 3rd, the 4th ... the number of shop meets the pressing machine and meets;
The 5th the step: the steel plate of the centre being completed sizing material pushes the pressing machine, controlled pressure 20-40 atmospheric pressure,, temperature is controlled at 90 ℃-110 ℃, suppresses to get final product ejecting plate in 20-40 minute;
The 6th step: saw the limit behind the ejecting plate, burr around half-finished are amputated, make standard-sized semi-finished product with Sawing machine;
The 7th step: sanding, with sander the sanding processing being carried out on half-finished surface is finished product.
3. method according to claim 1 is characterized in that main material 25-30 part; Primary density board sanding powder 8-12 part; Urine aldehyde glue 6-8 part, wherein main material is the leftover bits of plywood production; Sawdust; The mixture of wood shavings; The leftover bits of plywood production; Sawdust; The charge ratio of wood shavings is 1: 1: 1.
4. method according to claim 1 is characterized in that it is to be made by following materials of weight proportions: 30 parts of main materials; 12 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; Sawdust; The mixture of cotton stalk; The leftover bits of plywood production; Sawdust; The charge ratio of cotton stalk is 2: 1: 0.5.
5. method according to claim 2 is characterized in that it is to be made by following materials of weight proportions: 33 parts of main materials; 15 parts of primary density board sanding powders; 10 parts in urine aldehyde glue, wherein main material is the leftover bits of plywood production; The mixture of bark and cotton stalk; The leftover bits of plywood production; The charge ratio of bark and cotton stalk is 2: 1: 1.