CN100349065C - Method for improving projection screen performance - Google Patents
Method for improving projection screen performance Download PDFInfo
- Publication number
- CN100349065C CN100349065C CNB2004100183827A CN200410018382A CN100349065C CN 100349065 C CN100349065 C CN 100349065C CN B2004100183827 A CNB2004100183827 A CN B2004100183827A CN 200410018382 A CN200410018382 A CN 200410018382A CN 100349065 C CN100349065 C CN 100349065C
- Authority
- CN
- China
- Prior art keywords
- projection screen
- millimeter
- hyaline membrane
- hair
- weight
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present invention relates to a method for enhancing projection screen performance, which belongs to the technical field of projection screen manufacture. The reflection surface of the existing projection screen is covered with a transparent film of which the surface is provided with lots of regular micro-bulges and lots of regular longitudinal fuscous fine cracks. The present invention has the advantages of simple method, low equipment requirement, cheap raw material, easy operation and good processing effect. The transparent film processed by the method can be covered on the reflection surface of any existing hard and soft projection screens, the viewing angle of the projection screen can be enlarged, and the contrast of a projection image area of the projection screen can be enhanced.
Description
Technical field
The present invention relates to a kind of method that improves the projection screen performance, belong to the technical field that projection screen is made.
Background technology
In shadow casting technique, projection screen is very big to the show quality influence of picture, and the problem that existing projection screen exists usually shows aspects such as watching angle, brightness and contrast.Some screen, as the metal screen, the brightness height, but watch the angle less, also can produce " solar effect " sometimes; Surround lighting in addition when strong, descends the contrast of projection screen as sunlight, light, causes the picture atomizing, just as coveing with the white mist of one deck on the picture, influences appreciation effect.
Summary of the invention
The technical problem to be solved in the present invention is to release a kind of method that improves the projection screen performance, definitely says, releases a kind of method that projection screen is watched angle and contrast of improving.This method is applicable to any existing hard and soft projection screen.
Technical scheme of the present invention is, posting the hyaline membrane that a large amount of well-regulated microspikes is arranged on the surface and a large amount of well-regulated vertical dark hair checks are arranged on the reflecting surface of existing projection screen: on the surface of macromolecule hyaline membrane, form a large amount of well-regulated microspikes earlier, again this hyaline membrane is posted on the reflecting surface of existing projection screen, then on this hyaline membrane surface, depict a large amount of vertically hair checks, in hair check, infiltrate dark dye at last.Microspike on the hyaline membrane is dispersed the reflected light of projection screen, and playing increases the effect that projection screen is watched the angle; Dark dye absorbing environmental light in the hair check on the hyaline membrane plays the effect that improves the projection screen contrast.
Now describe technical scheme of the present invention in detail.A kind of method that improves the projection screen performance is characterized in that, is that the macromolecule hyaline membrane of 0.1-0.2 millimeter is a raw material with thickness, and specific operation process is as follows:
The first step forms a large amount of well-regulated microspikes
By the mould thermoplastic, on the surface of macromolecule hyaline membrane, form a large amount of well-regulated microspikes, the height of microspike is the 0.02-0.10 millimeter, makes the hyaline membrane that the surface contains a large amount of well-regulated microspikes;
Second step coating cementing agent
At the back side of described hyaline membrane coating cementing agent, the thickness of adhesive layer is the 0.01-0.05 millimeter;
The 3rd step posted hyaline membrane
Described hyaline membrane posted at needs improve on the reflecting surface of projection screen of performance;
The 4th step delineation hair check
With row's cutter that thin blade is formed, on described hyaline membrane surface, depict a large amount of vertically hair checks, the hair check spacing is the 0.5-1.5 millimeter, hair check degree of depth 0.06-0.18 millimeter;
The 5th step was infiltrated dark dye
In described hair check, infiltrate dark dye.
Technical scheme of the present invention is further characterized in that the macromolecule hyaline membrane is the tygon transparent membrane.
Technical scheme of the present invention is further characterized in that, in the first step, the microspike of formation is lengthwise bar ripple, grow crosswise bar ripple or bar ripple in length and breadth, waviness width 0.3-1.5 millimeter, ripple stripe pitch 0.5-1.5 millimeter.
Technical scheme of the present invention is further characterized in that cementing agent is the acrylate adhesive sticker.
Technical scheme of the present invention is further characterized in that the order of specific operation process can be: the first step; The 4th step; Second step; The 3rd step and the 5th step.
Technical scheme of the present invention is further characterized in that the order of specific operation process can be: the first step; The 4th step; The 5th step; Second step and the 3rd step.
Technical scheme of the present invention is further characterized in that the order of specific operation process can be: the first step; Second step and the 3rd step.
Technical scheme of the present invention is further characterized in that in the first step, the height of microspike is 0 millimeter, promptly skips the first step, and the order of all the other operating process is: second step; The 3rd step; The 4th step and the 5th step.
Advantage of the present invention:
1. method of the present invention is simple, and equipment requirements is low, and raw material is inexpensive, and is easy to implement.
2. the processing effect of method of the present invention is good.The hyaline membrane of method processing of the present invention is posted on the reflecting surface of any existing hard and soft projection screen, just can increase watching the angle and improving the contrast that this projection screen is shown picture of this projection screen.
3. method flexible operation of the present invention can change the order of operating process according to the performance deficiency of projection screen reality, and orientation is improved the performance of projection screen.
Description of drawings
Fig. 1 is the sectional view of the projection screen processed of the present invention, and 1 is the reflecting surface of projection screen among the figure, the 2nd, and hair check, the 3rd, hyaline membrane, the 4th, dark dye, the 5th, adhesive layer.
Embodiment
The projection screen that needs the raising performance is the soft curtain of metal.The tygon transparent membrane that with thickness is the 0.10-0.20 millimeter is a raw material, molded by mold hot, form the lengthwise bar ripple of projection, grow crosswise bar ripple or bar ripple in length and breadth at film surface, waviness width is the 0.5-1.5 millimeter, the ripple stripe pitch is the 0.5-1.5 millimeter, makes hyaline membrane;
At described hyaline membrane back side coating acrylate adhesive sticker, thickness is the 0.01-0.05 millimeter;
Described hyaline membrane is posted on the reflecting surface of the soft curtain of metal;
Depict a large amount of vertically hair checks with row's cutter on described hyaline membrane surface, the hair check spacing is the 0.8-1.5 millimeter, and the hair check degree of depth is the 0.08-0.18 millimeter, or the hair check degree of depth to choose not destroy reflecting surface be principle;
In hair check, infiltrate dark dye.The prescription of the dark dye of 100 parts of weight of preparation:
Carbon black 4-8 part weight
Methacrylate and acrylic acid 3-8 part weight
Methacrylate and acrylic acid weight ratio are 3: 7
0 part of weight of isoamylol
The general assembly (TW) that water adds to four components is 100 parts of weight.
Needing the projection screen of raising performance is high brightness metallic hard curtain.The tygon transparent membrane that with thickness is the 0.10-0.20 millimeter is a raw material, molded by mold hot, form the lengthwise bar ripple of projection, grow crosswise bar ripple or bar ripple in length and breadth, waviness width 0.5-1.5 millimeter at film surface, the ripple stripe pitch is the 0.5-1.5 millimeter, makes hyaline membrane;
At described hyaline membrane back side coated acrylate adhesive sticker, thickness is at the 0.01-0.05 millimeter;
Described hyaline membrane is posted on the reflecting surface of metallic hard curtain, to reach " solar effect " of eliminating brightness irregularities.
Need to improve the projection screen of performance for moulding curtain in vain.The tygon hyaline membrane that with thickness is the 0.10-0.20 millimeter is a raw material, hyaline membrane is posted moulding in vain on act reflecting surface;
On described hyaline membrane surface, depict a large amount of vertically hair checks with row's cutter, hair check spacing 0.8-1.5 millimeter, hair check degree of depth 0.08-0.18 millimeter, or crack depth to choose not destroy reflecting surface be principle;
Infiltrate dark dye in hair check, the preparation of dark dye is identical with embodiment 1, does not just repeat here.
Claims (7)
1. a method that improves the projection screen performance is characterized in that, is that the macromolecule hyaline membrane of 0.1-0.2 millimeter is a raw material with thickness, and specific operation process is as follows:
The first step forms microspike
By the mould thermoplastic, form a large amount of microspikes on the surface of macromolecule hyaline membrane, the height of microspike is the 0.02-0.10 millimeter, makes the hyaline membrane (3) that the surface contains a large amount of microspikes;
Second step coating cementing agent
At the back side of described hyaline membrane (3) coating cementing agent, the thickness of adhesive layer (5) is the 0.01-0.05 millimeter;
The 3rd step posted hyaline membrane (3)
Described hyaline membrane (3) posted at needs improve on the reflecting surface (1) of projection screen of performance;
The 4th step delineation hair check (2)
With row's cutter that thin blade is formed, on described hyaline membrane (3) surface, depict a large amount of vertically hair checks (2), hair check (2) spacing is the 0.8-1.5 millimeter, hair check (2) degree of depth is the 0.08-0.18 millimeter;
The 5th step was infiltrated dark dye (4)
In described hair check, infiltrate dark dye (4).
2. the method for raising projection screen performance according to claim 1 is characterized in that, the macromolecule hyaline membrane is the tygon transparent membrane.
3. the method for raising projection screen performance according to claim 1 is characterized in that, in the first step, the microspike of formation is a lengthwise bar ripple, grow crosswise bar ripple or bar ripple in length and breadth, waviness width 0.5-1.5 millimeter, ripple stripe pitch 0.5-1.5 millimeter.
4. the method for raising projection screen performance according to claim 1 is characterized in that, cementing agent acrylate adhesive sticker.
5. the method for raising projection screen performance according to claim 1 is characterized in that, the prescription of the dark dye (4) of 100 parts of weight of preparation:
Carbon black 4-8 part weight
Methacrylate and acrylic acid 3-8 part weight
Methacrylate and acrylic acid weight ratio are 3: 7
10 parts of weight of isoamylol
The general assembly (TW) that water adds to four components is 100 parts of weight.
6. according to the method for claim 1,2,3,4 or 5 described raising projection screen performances, it is characterized in that the order of specific operation process is: the first step; The 4th step; Second step; The 3rd step and the 5th step.
7. according to the method for claim 1,2,3,4 or 5 described raising projection screen performances, it is characterized in that the order of specific operation process is: the first step; The 4th step and the 5th step; Second step and the 3rd step.