CN100344715C - Aqueous environmental protection mark paint - Google Patents
Aqueous environmental protection mark paint Download PDFInfo
- Publication number
- CN100344715C CN100344715C CNB031485170A CN03148517A CN100344715C CN 100344715 C CN100344715 C CN 100344715C CN B031485170 A CNB031485170 A CN B031485170A CN 03148517 A CN03148517 A CN 03148517A CN 100344715 C CN100344715 C CN 100344715C
- Authority
- CN
- China
- Prior art keywords
- water
- aqueous
- agent
- present
- portions
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
The present invention relates to aqueous environment protecting marking paint. The present invention is prepared from raw materials of the following weight ratio: 40 to 50 portions of BS1118 acrylic emulsion, 2 to 3 portions of fluorescent powder, 10 portions of water, 40 portions of glass of high refractive indexes, 0.1 to 0.15 portion of aqueous levelling agent, 0.1 to 0.15 portion of aqueous defoaming agent, 0.1 to 0.15 portion of aqueous dispersing agent, 0.15 to 0.2 portion of aqueous anti-settling agent and 0.1 to 0.15 portion of aqueous antiseptic agent. The present invention ha no substances harmful to human bodies or chemical pollution, but has the advantages of high reflecting and shading performance and low cost.
Description
Technical field
The present invention relates to a kind of aqueous, environmental protective label lacquer, described label lacquer is used for the sign board and the billboard of motorway.
Background technology
Reflector marker coating uses on the sign board, billboard of high-grade highway abroad in a large number, also begin on the motorway at home to promote, coating commonly used divides solvent-borne type and hot-melting type two big classes, solvent based coating has a large amount of organic solvent volatilizations in producing and using, contaminate environment influences healthyly, and coating intensity is low, wear no resistance, work-ing life is short.Hot-melting type coating has the cost height, construct loaded down with trivial details, equipment is complicated, inapplicablely use in cold district construction.
Chinese patent 99114412.0 discloses a kind of luminous paint, it is mixed to stir by fluorescent paint or resin paint, multifunctional assistant and rare earth aluminate and forms, and the weight percent of its each composition is: fluorescent paint or resin paint 45-80%, multifunctional assistant 3-8%, rare earth aluminate 15-50%.This patent brushing is on labels such as sign board, billboard, safety notice board, guideboard, they can absorb natural light and when unglazed () luminous demonstration in night by day, simultaneously and remain with the function of fluorescent paint, there is certain contaminative in this patent resene paint to environment.Therefore, need to propose a kind of aqueous, environmental protective label lacquer.
Summary of the invention
The object of the present invention is to provide a kind of aqueous, environmental protective label lacquer, this label lacquer does not contain harmful material, no chemical pollution, and have higher reflective and opacifying property, and cost is lower.
The objective of the invention is to realize by following technical proposals: a kind of aqueous, environmental protective label lacquer, it is characterized in that: formed by following feedstock production, the weight ratio of described raw material is:
BS1118 pure-acrylic emulsion 40-50
Fluorescent material 2-3
Water 10
High refractive index glass micro pearl 40
Water-based flow agent 0.1-0.15
Water-based defoamer 0.1-0.15
Aqueous dispersant 0.1-0.15
Water-based anti-settling agent 0.15-0.2
Water-borne preservative 0.1-0.15.
In the present invention, the BS1118 pure-acrylic emulsion is to metal and glass microballon is had stronger sticking power, and water tolerance is better; Fluorescent material pigment coloring and refracted ray; Glass microballon is used for producing reflection and refracted ray; Flow agent is used for coating nature levelling, improves the brushing performance; Defoamer is used for eliminating the bubble that whipping process produces; Dispersion agent is used for preparation process makes fluorescent material homodisperse in coating; Anti-settling agent is used to prevent that fluorescent material from too much precipitating; Mould inhibitor is used for preventing that the present invention is mouldy, smelly, rotten in the process of depositing.
The present invention compared with prior art has following advantage:
1, do not contain human body and environmentally hazardous substance owing to raw material of the present invention, free from environmental pollution, safe in utilization, belong to environmentally friendly machine.
2, because the present invention adopts the BS1118 pure-acrylic emulsion, the paint adhesion of making is good, strong covering power.
3, to have a production cost low in the present invention, the advantage that the shelf-time is long.
Embodiment
Embodiment one:
A kind of aqueous, environmental protective label lacquer is formed by following feedstock production, and the weight ratio of described raw material is:
BS1118 pure-acrylic emulsion 40
Fluorescent material 2
Water 10
High refractive index glass micro pearl 40
Water-based flow agent 0.15
Water-based defoamer 0.15
Aqueous dispersant 0.15
Water-based anti-settling agent 0.15
Water-borne preservative 0.1.
The present embodiment preparation method is: earlier water, fluorescent material, BS1118 pure-acrylic emulsion and five auxiliary agents are poured in the sand mill according to proportioning and added grinding bead and grind, with discharging after above-mentioned improved grinding 30-60 minute, pour in the homogenizer then, start stirrer and under 300-500 rev/min rotating speed, add glass microballon while stirring, stirred 15-30 minute; After filtering, 100 purpose filtering nets promptly can be made into aqueous, environmental protective label lacquer then.
Product of the present invention is widely used in the motorway guide planks and the billboard of metal, plastics class.
Embodiment two:
A kind of aqueous, environmental protective label lacquer is formed by following feedstock production, and the weight ratio of described raw material is:
BS1118 pure-acrylic emulsion 50
Fluorescent material 3
Water 10
High refractive index glass micro pearl 40
W490 water-based flow agent 0.1
S062 water-based defoamer 0.1
504 aqueous dispersants 0.1
118 water-based anti-settling agents 0.2
981 water-borne preservatives 0.1.
The preparation method of present embodiment and embodiment one are basic identical.In the present embodiment, the product type of water-based flow agent is W490, and the product type of water-based defoamer is S062, and the product type of aqueous dispersant is 504, and the product type of water-based anti-settling agent is 118, and the product type of water-borne preservative is magnificent section 981.
Claims (2)
1, a kind of aqueous, environmental protective label lacquer, it is characterized in that: formed by following feedstock production, the weight ratio of described raw material is:
BS1118 pure-acrylic emulsion 40-50
Fluorescent material 2-3
Water 10
High refractive index glass micro pearl 40
Water-based flow agent 0.1-0.15
Water-based defoamer 0.1-0.15
Aqueous dispersant 0.1-0.15
Water-based anti-settling agent 0.15-0.2
Water-borne preservative 0.1-0.15.
2, aqueous, environmental protective label lacquer according to claim 1, it is characterized in that: formed by following feedstock production, the weight ratio of described raw material is:
BS1118 pure-acrylic emulsion 50
Fluorescent material 3
Water 10
High refractive index glass micro pearl 40
W490 water-based flow agent 0.1
S062 water-based defoamer 0.1
504 aqueous dispersants 0.1
118 water-based anti-settling agents 0.2
981 water-borne preservatives 0.1.