Ishibe et al., 2008 - Google Patents
Improvement of ZnO element performance by reducing spinel particlesIshibe et al., 2008
- Document ID
- 6770844758222396978
- Author
- Ishibe S
- Kato T
- Takada Y
- Kobayashi M
- Kawamata I
- Publication year
- Publication venue
- IEEE transactions on power delivery
External Links
Snippet
The performance of zinc-oxide (ZnO) elements is strongly dependent on the properties of the boundaries between ZnO grains, which are greatly affected by the formation of spinel particles between ZnO grains during the sintering process. The authors studied the effects of …
- XLOMVQKBTHCTTD-UHFFFAOYSA-N zinc monoxide data:image/svg+xml;base64,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 data:image/svg+xml;base64,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 [Zn]=O 0 title abstract description 99
Classifications
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01C—RESISTORS
- H01C7/00—Non-adjustable resistors formed as one or more layers or coatings; Non-adjustable resistors made from powdered conducting material or powdered semi-conducting material with or without insulating material
- H01C7/10—Non-adjustable resistors formed as one or more layers or coatings; Non-adjustable resistors made from powdered conducting material or powdered semi-conducting material with or without insulating material voltage responsive, i.e. varistors
- H01C7/105—Varistor cores
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01B—CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES
- H01B1/00—Conductors or conductive bodies characterised by the conductive materials; Selection of materials as conductors
- H01B1/06—Conductors or conductive bodies characterised by the conductive materials; Selection of materials as conductors mainly consisting of other non-metallic substances
- H01B1/08—Conductors or conductive bodies characterised by the conductive materials; Selection of materials as conductors mainly consisting of other non-metallic substances oxides
-
- H—ELECTRICITY
- H01—BASIC ELECTRIC ELEMENTS
- H01B—CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES
- H01B3/00—Insulators or insulating bodies characterised by the insulating materials; Selection of materials for their insulating or dielectric properties
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2345168C (en) | Current/voltage non-linear resistor and sintered body therefor | |
Bai et al. | Influence of SiO2 on electrical properties of the highly nonlinear ZnO-Bi2O3-MnO2 varistors | |
Nahm et al. | Microstructure and electrical properties of Y2O3-doped ZnO–Pr6O11-based varistor ceramics | |
Liu et al. | Enhanced voltage gradient and energy absorption capability in ZnO varistor ceramics by using nano-sized ZnO powders | |
Xu et al. | Microstructure and electrical properties of Sc2O3-doped ZnO–Bi2O3-based varistor ceramics | |
Jiang et al. | Progress on rare-earth doped ZnO-based varistor materials | |
Meng et al. | Novel zinc-oxide varistor with superior performance in voltage gradient and aging stability for surge arrester | |
Bai et al. | Influence of Cr2O3 on highly nonlinear properties and low leakage current of ZnO–Bi2O3 varistor ceramics | |
Zhao et al. | High nonlinearity and high voltage gradient ZnO varistor ceramics tailored by combining Ga2O3, Al2O3, and Y2O3 dopants | |
Ji-le et al. | Microstructure and electrical properties of rare earth doped ZnO-based varistor ceramics | |
Chen et al. | Microstructure and electrical properties of Dy2O3-doped ZnO–Bi2O3 based varistor ceramics | |
Chen et al. | Sintering temperature dependence of varistor properties and impedance spectroscopy behavior in ZnO based varistor ceramics | |
Nahm | Microstructure, electrical properties, and aging behavior of ZnO–Pr6O11–CoO–Cr2O3–Y2O3–Er2O3 varistor ceramics | |
He et al. | ZnO varistors with high voltage gradient and low leakage current by doping rare-earth oxide | |
Wang et al. | Electrical characteristics and stability of low voltage ZnO varistors doped with Al | |
Meng et al. | Electrical properties of ZnO varistor ceramics modified by rare earth-yttrium and gallium dopants | |
Peng et al. | Influence of Fe2O3 doping on microstructural and electrical properties of ZnO–Pr6O11 based varistor ceramic materials | |
Shen et al. | Boron and sodium co-doped ZnO varistor with high stability of pulse current surge | |
Liu et al. | High voltage gradient and low leakage current SnO2 varistor ceramics doped with Y2O3 and Nb2O5 | |
KR102120577B1 (en) | Ceramic material, varistor, ceramic material and method of manufacturing varistor | |
SI24523A (en) | The procedure of manufacturing of the varistor ceramics and varistors with a low leakage current | |
JP2017130544A (en) | Voltage Nonlinear Resistor | |
Abdollahi et al. | The degradation behavior of high-voltage SnO2 based varistors sintered at different temperatures | |
Kong et al. | Improvement of current withstand capacity of high gradient ZnO varistors | |
Sedky et al. | Effect of temperature on the electrical properties of Zn 0.95 M 0.05 O (M= Zn, Fe, Ni) |