SU103536A1 - The method of obtaining synthetic fiber - Google Patents
The method of obtaining synthetic fiberInfo
- Publication number
- SU103536A1 SU103536A1 SU452578A SU452578A SU103536A1 SU 103536 A1 SU103536 A1 SU 103536A1 SU 452578 A SU452578 A SU 452578A SU 452578 A SU452578 A SU 452578A SU 103536 A1 SU103536 A1 SU 103536A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- synthetic fiber
- obtaining synthetic
- fiber
- obtaining
- stretching
- Prior art date
Description
Известны способы получени синтетических и искусственных волокон с ирименением в осадительных ваинах жирных кислот.Methods are known for the production of synthetic and artificial fibers with fatty acid irization in precipitating wines.
Описываемый сиособ получени вилокна «Нитрон ио сравнению с известными позвол ет иовысить физико-механические свойства синтетического волокна, что достигаетс применением в качестве осадительной ванны стеариновой кислоты.The described method of obtaining forks "Nitron and comparing with the known ones allows to improve the physicomechanical properties of synthetic fiber, which is achieved by using stearic acid as a precipitation bath.
Пример. 15-15,5%-ный ир дильный раствор полиакрилонитрила в дпметилформамиде . ириготовлениый из ирбдукта с удельной в зкостью 1,500-1,600 ио вискозиметру Оствальда и имеющий по шарику в зкость 300-400 сек.., продавливают черел (1и1льеру с отверсти ми диамстрсм 0,08-0.12 ММ в стеариновую |К().атул дионнуш ванну с т-емпературоЛ 70-.Example. 15-15.5% hydrochloride solution of polyacrylonitrile in dpmethylformamide. Irrigated irbduct with a specific viscosity of 1,500-1,600 and an Ostwald viscometer and having a ball viscosity of 300-400 seconds. with t-temperature 70-.
Подачу растворов устанавливают из расчета иолучени элементарного волокна с номером 4000-5000 после его выт жки.The supply of the solutions is established on the basis of the calculation of the yield of the elementary fiber with the number 4000-5000 after its stretching.
11р д«н)№ Bc/ivT при скорости 4-5 м/Мин, причем длина иути в ванне составл ет 80-40 см.11 p d "n) No. Bc / ivT at a speed of 4-5 m / min, and the length of the bath in it is 80-40 cm.
После выхода из коагулшишнной ванны нить подвергают выт жке при 160- 170° в ваннах, содерл;ащих соответствующие жидкости, например, глицерин. Ве .тичина выт жки 2000-3000%.After leaving the coagulation bath, the thread is subjected to stretching at 160-170 ° in baths containing suitable liquids, for example, glycerin. The amount of stretching is 2000-3000%.
После выт жки волокно поступает на бобины.After drawing, the fiber enters the reels.
Спр денное волокно подвергают промывке , сушке и последующпм операци м окоичательно отделки.The spun fiber is subjected to washing, drying and subsequent operations around sharpening.
Пред м с т и 3 U 6 р о т е н и Before m with t and 3 U 6 p about e and U
Сносоо иол чени синтетического волокна с применением осадительных ванн, содержащих жирные кислоты, о т л п ч аю щ и и с тем, что, с целью повышени физико-механических свойств волокна на осиове полиакрилоиитрила в диметилформампде , в качестве осадительной ванны примен ют стеариновую кислоту.Removing synthetic fibers with the use of precipitation baths containing fatty acids, so on, and in order to improve the physicomechanical properties of the fiber on the axis of polyacryloyitrile in dimethylformamph, stearic acid is used as a precipitation bath .